• 1
    Grigorenko V.B., Lukinа E.A., Terekhin A.M.

    The features of the production of single-crystal blades from nickel heat-resistant alloys are considered. Metallographic and fractographic studies of the destroyed blades were performed to identify the causes of destruction. The features of fatigue and static destruction of single-crystal turbine blades have been studied by optical and scanning electron microscopy using X-ray spectral microanalysis. Recommendations are given to prevent the formation of recrystallized polyhedral grains.

  • 2
    Deynega G.I., Kuzmina I.G., Bityutskaya O.N., Narskiy A.R.
    Part 1

    In the first part of the study conducted at the National Research Center «Kurchatov Institute» – VIAM, the technology of manufacturing foam ceramic filters designed to purify the melt from non-metallic inclusions is considered. Technological parameters for the manufacture of foam ceramic filters using domestic refractory materials have been developed, several experimental samples of filters based on aluminum oxide (III) and zirconium oxide (IV) have been manufactured, their physical and mechanical properties have been determined. The full compliance of the properties of the manufactured filters with the requirements of the technical specification has been established.

  • 3
    Kulagina G.S., Zhelezina G.F., Levakova N.M., Safonov P.E.

    The article discusses synthetic heatresistant polymer fibers that for the manufacture of antifriction composite materials. The properties of fibre of various chemical nature (para- and metaаramid, polyimide, fluorinecontaining, etc.) are given. Doublesided fabrics based on heat-resistant polymer fibers containing two types of fibers with antifriction and reinforcing properties for use as part of selflubricating antifriction materials are considered.

  • 4
    Kulagina G.S., Zhelezina G.F., Kan A.Ch., Kurshev E.V.

    The article studied the exploitation properties of antifriction organoplastics based on a new reinforcing fabric consisting of two types of fibers: polytetrafluoroethylene and polyoxadiazole fiber Arcelon. The nature of destruction during delamination of organoplastic from a metal substrate and the influence of various factors (temperature, humidity, salt fog, tropical chamber conditions, etc.) on adhesive strength were studied. It has been shown that, under the influence of operational factors, organoplastic has high adhesive strength values – above the allowable minimum level.

  • 5
    Kolokoltseva T.V., Popov J.O., Usacheva M.N., Gromova A.A.

    This article presents the main results on the development of prepregs and polymer composite materials (fiberglass and carbon fiber) based on the melting epoxy resin union and reinforcing fillers-glass-circuits of the T-64(VMP)-78, glass-winding RVMPN10-1200-14 and carbon fiber UMT49S-12K-EP. The process of developing prepregs, technologies for their manufacture on the impregnation, the choice of the main parameters of impregnation is described. The results of a study of the properties of the prepregs obtained under selected technological regimes and made from them PCM are also given.

  • 6
    Kolokoltseva T.V., Popov J.O., Lantsov I.A., Gusev Y.A.

    This article presents the main results on the development of prepreg and carbon fiber based on the VSR-3M resin and carbon fabric grade VTkU-2.200. The process of studying prepreg, the technology of its production in an impregnation installation, and the selection of the main parameters of impregnation are described. Correct selection of impregnation parameters guarantees the production of materials with the required properties. The results of a study of the properties of prepreg obtained using the selected technological mode and carbon fiber reinforced plastic made from it are also presented. 

  • 7
    Shoshev F.L., Bogachev I.A., Sukhov D.I.

    The structure of aluminum matrix composite powder reinforced by silicon carbide particles and then spheroidized is investigated. The structure of selective laser melting material made of this powder is investigated as well. The main principles of forming of such structure are determined. In addiction an effect of gasostatic and heat treatment on selective laser melting material structure is considered.

  • 8
    Cherednichenko I.V., Bavina M.A., Bondarenko Yu.A., Shurygin V.D., Ovchinnikov A.D., Galimullin S.A.

    In this paper has been investigated influence of direct crystallizations parameters on permanent magnets alloy UNDKBA (Alnico 5-7) for non-defective percent. For this paper were produced permanent magnets by using different types of seeds and technological parameter. It established that the main parameters for manufacturing castings permanent magnets are temperature, broaching speed, composition and type of the seed. Revealed that slow broaching speed, monocrystalline seed with the crystallographic orientation allows to obtain permanent magnets with non-defective percent higher than 80.

  • 9
    Kozlov I.A., Volkov I.A., Fomina M.A., Zakharov К.Е.

    The work is devoted to the adaptation of the traditional technology of chemical oxidation of parts and workpieces made of aluminum alloys obtained by traditional methods for surface treatment of parts manufactured by selective laser fusion and metal powder composition of the VAC1 alloy. The work investigated the compatibility and influence of the main chemical components of electrolytes on the stability of solutions and the quality of the formed coating. The performance of electrolytes for oxidation and various options for chemical preparation of the surface of samples from the alloy VAC1 are considered.

  • 10
    Kuznetsov B.Yu., Vlasov I.I., Grinevich D.V., Sorokin O.Ju.

    The purpose of this work is to determine the effect of the transitional diffusion zone at the interfacial boundary of the layers of the ceramic composite material of the Mo–Si–B system on the nature of destruction and physical and mechanical properties. Qualitative models have been created that make it possible to predict the most critical fracture zones of a composite material, and the effect of microstructure on the fracture mechanisms has been studied. Field tests of a ceramic-metal composite material with a multilayer structure were carried out, as a result of which a high convergence with the calculated models was established.

  • 11
    Ryzhkov P.V., Gorbovets M.A., Khodinev I.A.

    Tests for low-cycle fatigue of a heat-resistant nickel alloy were carried out at operating temperature, deformation of tensile cycle and a frequency of 1 Hz. On the example of the obtained data of elastic-plastic deformation, the material constants of the Manson–Coffin and Ramberg–Osgood equations are determined. The main relationships that use the energy of destruction, necessary for predicting fatigue life, are considered. It is shown that the application of the energy criterion in terms of the accumulated strain energy density parameter more accurately describes the fatigue behavior in the low-cycle fatigue regime. The data obtained will make it possible in the second part of the article to use the energy criterion to predict the durability of the alloy under study under conditions of stress concentration.

  • 12
    Grinevich A.V.

    The article, along with the achievements of N.M. Sklyarov, which have received universal recognition, examines the provisions developed by him, which determine the activities of the institute at the present time. The defining role of N.M. Sklyarov in the formation of the ideology of aviation armor, the creation of high-strength steel and in the development of a quality system of aviation materials is presented. The algorithm for the development of aviation materials formed by N.M.  Sklyarov is the basis for meeting the requirements of the Airworthiness Standards of aircraft in terms of ensuring their safety and durability.