Polymer fibers in the composition of fabrics for self-lubricating antifriction materials

Kulagina G.S., Zhelezina G.F., Levakova N.M., Safonov P.E.
Kulagina G.S., Zhelezina G.F., Levakova N.M., Safonov P.E. Polymer fibers in the composition of fabrics for self-lubricating antifriction materials // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-26-36. URL: https://www.viam-works.ru/en/journal/2023/11/3
Keywords
aramid fibers, fluorinated polymer fibers, fabrics from polymer fibers, antifriction materials
Abstract

The article discusses synthetic heatresistant polymer fibers that for the manufacture of antifriction composite materials. The properties of fibre of various chemical nature (para- and metaаramid, polyimide, fluorinecontaining, etc.) are given. Doublesided fabrics based on heat-resistant polymer fibers containing two types of fibers with antifriction and reinforcing properties for use as part of selflubricating antifriction materials are considered.

Reference list
  1. Perepelkin K.E. Reinforcing fibers and fibrous polymer composites. St. Petersburg: Scientific principles and technologies, 2009, 380 p.
  2. Mikhailin Yu.A. Fibrous polymer composite materials in technology. St. Petersburg: Scientific principles and technologies, 2013, 720 p.
  3. Lubin J. Handbook of composite materials: in 2 books. Ed. B.E. Geller. Moscow: Mechanical Engineering, 1988, book 1, 448 p.
  4. Perepelkin K.E. High-strength, high-modulus yarns based on linear polymers: principles of production, structure, properties, application. Khimicheskiye volokna, 2010, no. 2, pp. 3–10.
  5. Mikhailin Yu.A. Structural polymer composite materials. 2nd ed. St. Petersburg: Scientific principles and technologies, 2013, 822 p.
  6. Kobylkin I.F., Selivanov V.V. Materials and structures of light armor protection: textbook. Moscow: MSTU im. N.E. Bauman, 2014, 191 p.
  7. Gladkov A.N. Development of a process for producing high-strength and high-modulus Armalon threads: thesis, Cand. Sc. (Tech.). Moscow: MSTU im. A.N. Kosygin, 2007, 109 p.
  8. Hearle J.W.S., Lomas B., Cooke W.D. Atlas of fibre fracture and damage to textiles. 2nd ed. Woodhead Publishing Ltd., 1998, 477 p.
  9. Kablov E.N., Kulagina G.S., Zhelezina G.F., Lonskii S.L., Kurshev E.V. Microstructure research of the unidirectional organoplastic based on Rusar-NT aramid fibers and epoxy-polysulfone binder. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 19–26. DOI: 10.18577/2071-9140-2020-0-4-19-26.
  10. Mikhailin Yu.A. Heat, thermal and fire resistance of polymer materials. St. Petersburg: Scientific principles and technologies, 2011, 416 p.
  11. Lee G., Stoffey D., Neville K. New linear polymers. Moscow: Khimiya, 1972, 280 p.
  12. Mikhailin Yu.A. Heat-resistant polymers and polymer materials. St. Petersburg: Profession, 2012, 624 p.
  13. Musina T.K., Volokhina A.V., Shchetinin A.M. et al. Polyimide and aramid fibers and threads with special properties and products based on them. V mire oborudovaniya, 2010, no. 2 (91), pp. 4–8.
  14. Dresvyanina E.N., Makarova R.A., Trusov Yu.D. High-heat-resistant polyoxadisole fibers, threads and textiles based on them. Tekhnicheskiy tekstil, 2007, no. 16, pp. 15–20.
  15. Perepelkin K.E., Malanyina O.B., Pakshver E.A., Makarova R.A. Comparative assessment of the thermal characteristics of aromatic threads (polyoxazole, polyimide and polyaramid). Khimicheskiye volokna, 2004, no. 5, рр. 45–48.
  16. Korneeva N.V. Development of fibrous polymer composite materials reinforced with UHMWPE fibers, fabrics and non-woven materials treated with nonequilibrium low-temperature plasma: thesis, Dr. Sc. (Tech.). Kazan, 2011, 296 p.
  17. Kuzharov A.S., Ryadchenko V.G., Grechko V.O. et al. Study of tribological properties of various textile structures based on fibrous polytetrafluoroethylene. Trenie i iznos, 1986, vol. 7, no. 5, pp. 945–950.
  18. Kuzharov A.S., Ryadchenko V.G. Composite antifriction coatings based on polytetrafluoroethylene fibers. Wearlessness: interuniversity collection scientific works. Rostov-on-Don: RISHM, 1992, vol. 2, pp. 140–147.
  19. Kan A.Ch., Kulagina G.S., Ayupov T.R., Zhelezina G.F. The influence of environmental factors on the characteristics of antifriction organoplasty Orgalon AF-1M. Trudy VIAM, 2018, no. 3 (109), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 01, 2023). DOI: 10.18577/2307-6046-2022-0-3-91-101.
  20. Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, рр. 7–27.
  21. Kablov E.N. Main directions of development of materials for aerospace technology of the XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
  22. Kulagina G.S., Zhelezina G.F., Levakova N.M. Antifriction organoplastics for high-loaded friction knots. Trudy VIAM, 2019, no. 2 (74), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 01, 2023). DOI: 10.18577/2307-6046-2019-0-2-89-96
  23. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: September 01, 2023). DOI: 10.18577/2071-9140-2022-0-1-41-50.