Exploitation properties of antifriction selflubricating organoplastic based on fabric made of polytetrafluoroethylene and arcelon fibers

Kulagina G.S., Zhelezina G.F., Kan A.Ch., Kurshev E.V.
Kulagina G.S., Zhelezina G.F., Kan A.Ch., Kurshev E.V. Exploitation properties of antifriction selflubricating organoplastic based on fabric made of polytetrafluoroethylene and arcelon fibers // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-37-46. URL: https://www.viam-works.ru/en/journal/2023/11/4
Keywords
antifriction organoplastic, antifriction selflubricating material, polymer fibers, polytetrafluoroethylene, fibers Arcelon, exploitation properties
Abstract

The article studied the exploitation properties of antifriction organoplastics based on a new reinforcing fabric consisting of two types of fibers: polytetrafluoroethylene and polyoxadiazole fiber Arcelon. The nature of destruction during delamination of organoplastic from a metal substrate and the influence of various factors (temperature, humidity, salt fog, tropical chamber conditions, etc.) on adhesive strength were studied. It has been shown that, under the influence of operational factors, organoplastic has high adhesive strength values – above the allowable minimum level.

Reference list
  1. Kablov E.N. The main directions of the development of materials for the Authoric technique of the XXI century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
  2. Kulagina G.S., Zhelezina G.F., Levakova N.M. Antifriction organoplastics for high-loaded friction knots. Trudy VIAM, 2019, no. 2 (74), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 22, 2023). DOI: 10.18577/2307-6046-2019-0-2-89-96.
  3. Kablov E.N., Startsev V.O. Climate aging of polymer composite aviation materials. I. Assessment of the influence of significant factors of exposure. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16.
  4. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  5. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
  6. Kulagina G.S., Kan A.Ch., Zhelezina G.F., Levakova N.M. Antifriction materials based on polymer fibers. Trudy VIAM, 2022, no. 11 (117), paper no. 05. Available at: http://www.viam-works.ru (accessed: September 22, 2023). DOI: 10.18577/2307-6046-2022-0-11-48-59.
  7. Pashin Yu.A., Malkevich S.G., Dunaevskaya I.S. Fluoroplasts. Leningrad: Khimiya, 1978, p. 232.
  8. Sagalaev G.V. The tribotechnical properties of antifriction self-losing plastics. Moscow: Publ. house of standards, 1982, 64 p.
  9. Kuzharov A.S., Rygchenko V.G., Grechko V.O. et al. Study of the tribotechnical properties of various textile structures based on fibrous political radiator-ethyl. Trenie i iznos, 1986, vol. 7, no. 5, pp. 945–950.
  10. Kuzharov A.S., Rygchenko V.G. Compositional antifriction coatings based on the fibers of political radiatorethnicity. Consistency: interuniversity collection scientific works. Rostov-on-Don: RISHM, 1992, is. 2, pp. 140–147.
  11. Voinstein V.E., Troyanovskaya G.I. Dry lubricants and selflubricating materials. Moscow: Mechanical Engineering, 1968, p. 179.
  12. Permant antifriction organoplasty and product made from it: pat. 2404202 Rus. Federation; No. 2009111566/05; appl. 31.03.09; publ. 20.11.10.
  13. Perepelkin K.E. Reinforcing fibers and fibrous polymer composites. St. Petersburg: Scientific foundations and technologies, 2009, 380 p.
  14. Dresvyanina E.N., Makarova R.A., Trusov Yu.D. Highterm-resistant polyoxadiazol fibers, threads and textiles based on them. Tekhnicheskiy tekstil, 2007, no. 16, pp. 15–20.
  15. Poghosyan A.K. Friction and wear of filler materials filled. Moscow: Science, 1977, 138 p.
  16. Myshkin N.K., Petrookovets M.I. Tribology. Principles and applications. Gomel: IMMS NANB, 2002, 310 p.
  17. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: September 22, 2023). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  18. Deev I.S., Kobets L.P. Study of microstructure and micropolis of deformations in polymer composites by the method of raster electron microscopy. Zavodskaya laboratoriya. Diagnostika materialov, 1999, vol. 65, no. 4, pp. 27–34.
  19. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading. Trudy VIAM, 2014, no. 7, paper no. 06. Available at: http://www.viam-works.ru (accessed: September 22, 2023). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  20. Grigorenko V.B., Morozova L.V. Application of the scanning electron microscopy for studying of initial destruction stages. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.