Structural features destruction of monocrystalline materials
Grigorenko V.B., Lukinа E.A., Terekhin A.M. Structural features destruction of monocrystalline materials // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-3-16. URL: https://www.viam-works.ru/en/journal/2023/11/1
Keywords
monocrystalline nickel alloy, microstructure, fractographic analysis, scanning electron microscopy, grain recrystallization
Abstract
The features of the production of single-crystal blades from nickel heat-resistant alloys are considered. Metallographic and fractographic studies of the destroyed blades were performed to identify the causes of destruction. The features of fatigue and static destruction of single-crystal turbine blades have been studied by optical and scanning electron microscopy using X-ray spectral microanalysis. Recommendations are given to prevent the formation of recrystallized polyhedral grains.
Reference list
- Vostrikov A.V., Lomberg B.S., Sumynikov M.N., Ovsepyan S.V. Modern heat-resistant deformable nickel alloys of VIAM for GTD details. Modern heat-resistant nickel deformable alloys and technologies for their production: Materials All-Rus. Scientific and Technical Conf. (Moscow, September 24, 2021) Moscow: NIC «Kurchatov Institute» – VIAM, 2021, pp. 5–14.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G. The metallurgical fundamentals for high quality maintenance of single crystal heat-resistant nickel alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 55–71. DOI: 10.18577/2071-9140-2017-0-S-55-71.
- Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 15, 2023). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Kablov E.N. The role of fundamental research in the creation of materials of the new generation. Reports of XXI Mendeleevsky Congress for General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
- Toloraya V.N., Kablov E.N., Demonis I.M. The technology for obtaining monocrystalline castings of turbine blades of the GTD of a given crystallographic orientation from renius-containing heat-resistant alloys. Aviacionnye materialy i tehnologii, 2004, no. 1, pp. 107–118.
- Sims Ch.T., Norman S.S., Wilman S.Kh. Superplanes II: in 2 vols. Moscow: Metallurgiya, 1995, vol. 1: Heat-resistant materials for aerospace and industrial power plants, 384 p.
- Sidorov V.V., Kablov D.E., Chabina E.B., Ospennikova O.G., Simonov V.N., Puchkov Yu.A. The influence of impurities and microlegy on the structure and operational properties of monocristals of heat-resistant nickel alloys. Moscow: VIAM, 2020, 335 p.
- Lomberg B.S., Shestakova A.A., Bakradze M.M., Karachevtsev F.N. The investigation of the stability of γʹ-phase with size below 100 nm in Ni-base superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 3–10. DOI: 10.18577/2071-9140-2018-0-4-3-10.
- Letnikov M.N., Lomberg B.S., Ospennikova O.G., Bakradze M.M. The influence of quench rate on microstructure and mechanical properties of nickel-based wrought superalloy VZh175-ID. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 21–30. DOI: 10.18577/2071-9140-2019-0-2-21-30.
- Gerasimov S.A., Kuksenova L.I., Lapteva V.G., Ospennikova O.G., Alekseeva M.S., Gromov V.I. Surface engineering and operational properties of the nitrogenized structural steels. Moscow: VIAM, 2019, 599 p.
- Kablov E.N., Ospennikova O.G., Kudinov I.I., Golovkov A.N., Generalov A.S., Knyazev A.V. Assessment of the probability of identifying operational defects in the details of aviation equipment from heat-resistant alloys using flaw detective fluids of domestic and foreign production. Defektoskopiya, 2021, no. 1, pp. 64–71.
- Bytsenko O.A., Grigorenko V.B., Lukina E.A., Morozova L.V. Development of methods for metal-physical research: methodological issues and practical significance. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 498–515. DOI: 10.18577/2071-9140-2017-0-S-498-515.
- Belyaev M.S., Morozova L.V., Gorbovets M.A. Destruction of the samples of monocrystals of experimental heat-resistant nickel alloy, tested for multicycle fatigue. Materialovedenie, 2020, no. 8, pp. 7–13.
- Grigorenko V.B., Morozova L.V. Application of the scanning electron microscopy for studying of initial destruction stages. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.
- Naprienko S.A., Orlov M.R. Damage of single-crystal turbine blades of GTP. Trudy VIAM, 2016, no. 2 (38), paper no. 03. Available at: http://www.viam-works.ru (accessed: May 15, 2023). DOI: 10.18577/2307-6046-2016-0-2-3-3.