Energy criteria for fatigue fracture of a heat-resistant nickel alloy

Ryzhkov P.V., Gorbovets M.A., Khodinev I.A.
Ryzhkov P.V., Gorbovets M.A., Khodinev I.A. Energy criteria for fatigue fracture of a heat-resistant nickel alloy // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-111-122. URL: https://www.viam-works.ru/en/journal/2023/11/11
Keywords
mechanical properties, fatigue characteristics, high-temperature wrought nickel alloys, strain energy density, Manson–Coffin and Ramberg–Osgood equations
Abstract

Tests for low-cycle fatigue of a heat-resistant nickel alloy were carried out at operating temperature, deformation of tensile cycle and a frequency of 1 Hz. On the example of the obtained data of elastic-plastic deformation, the material constants of the Manson–Coffin and Ramberg–Osgood equations are determined. The main relationships that use the energy of destruction, necessary for predicting fatigue life, are considered. It is shown that the application of the energy criterion in terms of the accumulated strain energy density parameter more accurately describes the fatigue behavior in the low-cycle fatigue regime. The data obtained will make it possible in the second part of the article to use the energy criterion to predict the durability of the alloy under study under conditions of stress concentration.

Reference list
  1. Kablov E.N. Heat-resistant structural materials. Liteynoe proizvodstvo, 2005, no. 7, pp. 2–7.
  2. Socie D., Marquis G. Multiaxial Fatigue. SAE International, 1999, 502 p.
  3. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
  4. Erasov V.S., Oreshko E.I. Tests for fatigue of metal materials (review). Part 2. Analysis of the Basquin–Manson–Coffin equation. Methods of testing and processing of results. Aviation materials and technology, 2021, no. 1 (62), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 10, 2023). DOI: 10.18577/2071-9140-2021-0-1-80-94.
  5. Liao D., Zhu S.-P. Energy field intensity approach for notch fatigue analysis. International Journal of Fatigue, 2019, vol. 127, pp. 190–202. DOI: 10.1016/j.ijfatigue.2019.06.010.
  6. Rigon D., Berto F., Meneghetti G. Estimating the multiaxial fatigue behaviour of C45 steel specimens by using the energy dissipation. International Journal of Fatigue, 2021, vol. 151, p. 106381. DOI: 10.1016/j.ijfatigue.2021.106381.
  7. Benedetti M., Berto F., Le Bone L., Santus C. A novel Strain-Energy-Density based fatigue criterion accounting for mean stress and plasticity effects on the medium-to-high-cycle uniaxial fatigue strength of plain and notched components. International Journal of Fatigue, 2020, vol. 133, p. 105397. DOI: 10.1016/j.ijfatigue.2019.105397.
  8. Volkov I.A., Korotkikh Yu.G. Equations of state of viscoelastoplastic media with damage. Moscow: Fizmatlit, 2008, 424 p.
  9. Halford G.R. The energy required for fatigue (Plastic strain hystersis energy required for fatigue in ferrous and nonferrous metals). Journal of materials, 1966, vol. 1, рр. 3–18.
  10. Hellouin de Menibus A., Auzoux Q., Besson J., Crépin J. Temperature increase of Zircaloy-4 cladding tubes due to plastic heat dissipation during tensile tests at 0.1–10s−1 strain rates. Journal of Nuclear Materials, 2014, vol. 454, is. 1–3, pp. 247–254. DOI: 10.1016/ j.jnucmat.2014.08.011.
  11. Ellyin F. Fatigue Damage, Crack Growth and Life Prediction. London: Chapman & Hall, 1997. 486 р.
  12. Park J., Nelson D. Evaluation of an energy-based approach and a critical plane approach for predicting constant amplitude multiaxial fatigue life. International Journal of Fatigue, 2000, vol. 22, is. 1, pp. 23–39. DOI: 10.1016/S0142-1123(99)00111-5.
  13. Lian Y., Wang X., Wang J. et al. Application of strain energy based approach for evaluation of fatigue crack growth retardation effect under random overload. Engineering Fracture Mechanics, 2022, vol. 269, p. 108522. DOI: 10.1016/j.engfracmech.2022.108522.
  14. Hao M.-F., Zhu S.-P., Xia F.-L. Multiaxial fatigue life evaluation using strain energy-based critical plane approach. Procedia Structural Integrity, 2019, vol. 22, pp. 78–83. DOI: 10.1016/j.prostr.2020.01.011.
  15. Mahtabi M.J., Shamsaei N. A modified energy-based approach for fatigue life prediction of superelastic NiTi in presence of tensile mean strain and stress. International Journal of Mechanical Sciences, 2016, vol. 117, pp. 321–333. DOI: 10.1016/j.ijmecsci.2016.08.012.
  16. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  17. Moyer J.M., Jackman L.A., Adasczik C.B. et al. Advances in triple melting superalloys 718, 706, and 720. Superalloys 718, 625, 706 and Various Derivatives. TMS, 1994, рр. 39–48.
  18. Kablov E.N., Letnikov M.N., Ospennikova O.G., Bakradze M.M., Shestakova A.A. Particulars of the precipitation strengthening γʹ-phase during aging of heat-resistant wrought nickel superalloy VZh175-ID. Trudy VIAM, 2019, no. 9 (81), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 15, 2023). DOI: 10.18577/2307-6046-2019-0-9-3-14.
  19. Lomberg B.S., Shestakova A.A., Letnikov M.N., Bakradze M.M. The influence of temperature and stresses on nature of nanosize γʹ-phase in Ni-base superalloy VZh175-ID. Trudy VIAM, 2019, no. 12 (84), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 13, 2023). DOI: 10.18577/2307-6046-2019-0-12-3-10.
  20. Gorbovets M.A., Khodinev I.A., Ryzhkov P.V. Equipment for testing carrying out the strain-controlled low-cycle fatigue. Trudy VIAM, 2018, no. 9 (69), paper no. 06. Available at: http://www.viam-works.ru (accessed: August 03, 2023). DOI: 10.18577/2307-6046-2018-0-9-51-60.
  21. Shun‐Peng Z., Lei Q., Huang H. et al. Mean stress effect correction in strain energy-based fatigue life prediction of metals. International Journal of Damage Mechanics, 2017, vol. 26, pp. 1219–1241.
  22. Łagoda T. Energy models for fatigue life estimation under uniaxial random loading. Part I: The model elaboration. International Journal of Fatigue, 2001, vol. 23, is. 6, pp. 467–480.