Influence of directed crystallization parameters on structure and properties of alnico 5-7 alloy permanent magnets

Cherednichenko I.V., Bavina M.A., Bondarenko Yu.A., Shurygin V.D., Ovchinnikov A.D., Galimullin S.A.
Cherednichenko I.V., Bavina M.A., Bondarenko Yu.A., Shurygin V.D., Ovchinnikov A.D., Galimullin S.A. Influence of directed crystallization parameters on structure and properties of alnico 5-7 alloy permanent magnets // Proceedings of VIAM. 2023. No. 11. DOI: 10.18577/2307-6046-2023-0-11-77-89. URL: https://www.viam-works.ru/en/journal/2023/11/8
Keywords
column grain structure magnets, monocrystalline magnets, directional solidification, magnetic properties, high temperature gradient casting
Abstract

In this paper has been investigated influence of direct crystallizations parameters on permanent magnets alloy UNDKBA (Alnico 5-7) for non-defective percent. For this paper were produced permanent magnets by using different types of seeds and technological parameter. It established that the main parameters for manufacturing castings permanent magnets are temperature, broaching speed, composition and type of the seed. Revealed that slow broaching speed, monocrystalline seed with the crystallographic orientation allows to obtain permanent magnets with non-defective percent higher than 80.

Reference list
  1. Cherednichenko I.V., Bondarenko Yu.A., Kolodiazniy M.Yu., Kuzmina N.A., Shubakov V.S., Zhukov D.G. The structure and properties of permanent magnetic alloys UNDK25BA, manufacturing by directional solidification methods with liquid metal cooler. Trudy VIAM, 2017, no. 11 (59), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 03, 2023). DOI: 10.18577/2307-6046-2017-0-11-4-4.
  2. Altman A.B., Vernikovsky E.E., Gerberg A.N. Permanent magnets: a reference book. Moscow: Energiya, 1980, 478 p.
  3. Kekalo I.B. Physical materials science of precision alloys. Moscow: Metallurgiya, 1989, 497 p.
  4. Chumakov V.A., Stepanov V.M., Verin A.S. Technology of casting blades of gas turbine engines using the method of directional crystallization. Liteynoe proizvodstvo, 1978, no. 1, pp. 23–24.
  5. Gerasimov V.V., Visik E.M., Kolyadov E.V. On unused reserves of directional crystallization in improving the performance characteristics of gas turbine engines and gas turbine units. Liteynoe proizvodstvo, 2013, no. 9, pp. 30–32.
  6. Kolyadov E.V., Gerasimov V.V. The influence of the reduced size of the casting on the axial temperature gradient and the macrostructure of casting for directional solidification at the facility UVNK-15. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 3–9. DOI: 10.18577/2071-9140-2014-0-3-3-9.
  7. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Role of the directed crystallization in the resource-saving production technology of details of GTE. Trudy VIAM, 2013, no. 3, paper no. 01. Available at: http://www.viam-works.ru (accessed: August 02, 2023).
  8. Kolyadov E.V., Visik E.M., Gerasimov V.V., Arginbaeva E.G. The influence of directional solidification parameters on the structure and properties of the intermetallic alloys. Trudy VIAM, 2019, no. 3 (75), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 01, 2023). DOI: 10.18577/2307-6046-2019-0-3-14-26.
  9. Kuzmina N.A., Ostroukhova G.A. Blockiness and substructure in single-crystal castings of nickel heat-resistant alloys. Trudy VIAM, 2022, no. 6 (112), paper no. 02. Available at: http://www.viam-works.ru (accessed: August 03, 2023). DOI: 10.18577/2307-6046-2022-0-7-13-26.
  10. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: August 07, 2023). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  11. Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines’ blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), paper no. 02. Available at: http://www.journal.viam.ru (accessed: August 12, 2023). DOI: 10.18577/2071-9140-2021-0-3-11-18.
  12. Kolyadov E.V., Mezhin Yu.A. Automation of the technological process of single-crystal castings of superalloys on UVNK type installations. Trudy VIAM, 2016, no. 4, paper no. 4. Available at: http://www.viam-works.ru (accessed: August 14, 2023). DOI: 10.18577/2307-6046-2016-0-4-4-4.
  13. Kolyadov E.V., Gerasimov V.V., Visik E.M., Mezhin Yu.A. Casting by the method of directional crystallization with a controlled temperature gradient at the crystallization front. Liteynoe proizvodstvo, 2016, no. 8, pp. 24–26.
  14. McCallum R.W., Lewis L.H., Skomski R. et al. Practical Aspects of Modern. Annual Review of Materials Research, 2014, no. 44, pp. 451–477. DOI: 10.1146/aanurev-matsci-070813-113457.
  15. Zhou L., Cuo W., Jonathan D.P. et al. On spinodal decomposition in alnico – A transmission electron microscopy and atom probe tomography study. Acta Materialia, 2018, no. 153, pp. 15–22. DOI: 10.1016/j.actamat.2018.04.042.
  16. Fan M., Liu Y., Ra R. et al. On the evolution of Cu–Ni-rich bridges of Alnico alloys with tempering // Journal of Magnetism and Magnetic Materials, 2016, vol. 420, pp. 296–302. DOI: 10.1016/j.jmmm.2016.07.040.
  17. Zhou L., Hamilton W.E.M., Liqin K. et al. Microstructure and coercivity in alnico 9. Journal of Magnetism and Magnetic Materials, 2018, vol. 471, pp. 142–147. DOI: 10.1016/j.jmmm.2018.09.085.
  18. Zhou L., Tang W., Ke L. et al. Microstructural and magnetic property evolution with different heat-treatment conditions in an alnico alloy. Acta Materialia, 2017, vol. 133, pp. 73–80. DOI: 10.1016/j.actamat.2017.05.012.
  19. Rehman S.U., Jiang Q., Lei W. et al. Microstructures and magnetic properties of cast alnico 8 permanent magnets under various heat treatment conditions. Physica B: Condensed Matter, 2018, vol. 552, pp. 136–141. DOI: 10.1016/j.physb.2018.10.007.
  20. Rehman S.U., Wei C., Huang Q. et al. Tailoring the microstructure, magnetic properties and interaction mechanisms of Alnico-Ta alloys by magnetic field treatment. Journal of Alloys and Compounds, 2021, vol. 857, p. 157. DOI: 10.1016/j.jallcom.2020.157586.
  21. Rehman S.U., Zubair A., Haq A. et al. Effects of Zr alloying on the microstructure and magnetic properties of Alnico permanent magnets. Journal of Magnetism and Magnetic Materials, 2017, vol. 442, pp. 136–140. DOI: 10.1016/j.jmmm.2017.06.114.
  22. Rehman S.U., Jiang Q., Ge Q. et al. Microstructure and magnetic properties of alnico permanent magnetic alloys with Zr–B additives. Journal of Magnetism and Magnetic Materials, 2017, vol. 451, pp. 136–140. DOI: 10.1016/j.jmmm.2017.11.043.
  23. Zubair A., Liu Z., Haq A. et al. Synthesis, magnetic and microstructural properties of Alnico magnets with additives. Journal of Magnetism and Magnetic Materials, 2017, vol. 428, pp. 125. DOI: 10.1016/j.jmmm.2016.12.023.
  24. Zhao J.T., Sun Y.L., Lydiaway L. et al. Correlations of phase structure and thermal stability for Alnico 8 alloys. Journal of Magnetism and Magnetic Materials, 2017, vol. 442, pp. 208–211. DOI: 10.1016/j.jmmm.2017.06.118.
  25. Zhang S.-D., Wang S., Chen S.-Y. et al. Structure and magnetic properties of alnico 8 ribbons. Physica B: Condensed Matter, 2020, vol. 597, p. 412423. DOI: 10.1016/j.physb.2020.412423.
  26. Zhang C., Li Y., Han X.-H. et al. Structure and magnetic properties of Alnico ribbons. Journal of magnetism and magnetic materials, 2017, vol. 451, pp. 200–207. DOI: 10/1016/j.jmmm.2017.11.045.
  27. Hosseini S.M., Novak P., Vesely M. et al. Positive temperature dependence of compressive properties in an AlNiCo poly-quasicrystal fabricated by mechanical alloying and spark plasma sintering. Scripta Materialia, 2020, vol. 187, pp. 169–174. DOI: 10.1016/j.scriptamat.2020.06.023.
  28. Rehman S.U., Huang Q., Sagar R. et al. Interaction mechanism, magnetic properties and microstructure of Ce–Fe–B-Alnico spark plasma sintered magnets. Journal of Magnetism and Magnetic Materials, 2021, vol. 537, pp. 168237. DOI: 10.1016/j.jmmm.2021.168237.
  29. Wang H.-W., Wang S., Cao Y.-F. et al. Structure and magnetic properties of alnico alloy doped SmCo5–xCux ribbons. Journal of Magnetism and Magnetic Materials, 2021, vol. 528, pp. 167821. DOI: 10.1016/j.jmmm.2021.167821.
  30. Rehman S.U., Jiang Q., He L. et al. Microstructure and magnetic properties of NdFeB alloys by co-doping alnico elements. Physics Letters A, 2019, vol. 383, p. 125878. DOI: 10.1016/j.physleta.2019.125878.
  31. Han X.-H., Sun J.-B., Wang H.-W. et al. Excellent magnetic properties determined by spinodal decomposition structure of Alnico alloy doped SmCo5-based ribbons. Journal of Alloys and Compounds, 2019, vol. 806, pp. 1188–1199. DOI: 10.1016/j.jallcom.2019.07.336.
  32. Rehman S.U., Jiang Q., He L. et al. Synthesis, microstructures, magnetic properties and thermal stabilities of isotropic alnico ribbons. Journal of Magnetism and Magnetic Materials, 2018, vol. 466, pp. 277–282. DOI: 10.1016/j.jmmm.2018.07.020.
  33. Rehman S.U., Ouyang H., Jiang Q. et al. Magnetic properties, phase transition temperatures and microstructure of CeFeB-alnico ribbons. Journal of Magnetism and Magnetic Materials, 2019, vol. 486, p. 165252. DOI: 10.1016/j.jmmm.2019.165252.
  34. Shakirov I.V., Zhukov A.S., Perevislov S.N., Olisov A.V. Influence of selective laser alloying modes on the structure of the UNDC alloy. Fizika metallov i metallovedenie, 2022, vol. 123, no. 3, pp. 248–259.
  35. Zhukov A.S., Shakirov I.V., Olisov A.V. Structural and mechanical state of the YUNDK35 alloy obtained by selective laser melting. Metallurg, 2021, no. 10, pp. 72–77.
  36. Novikov S.V., Ramazanov K.N. Additive technologies: state and prospects: textbook. Ufa: UGATU, 2022. Available at: https://ugatu.su/media/uploads/MainSite/Ob%20universitete/Izdateli/El_izd/2022‐41.pdf (accessed: August 05, 2023).
  37. Lyapkov A.A. Polymer additive technologies: textbook. Tomsk: Tomsk Polytech. Univ. Publ. House, 2016, 114 p.
  38. Huber C., Abert C., Bruckner F. 3D Print of Polymer Bonded Rare-Earth Magnets, and 3D Magnetic Field Scanning With an End-User 3D Printer. Applied Physics Letters, 2016, vol. 109, no. 109 (16), pp. 1–5. https://doi.org/10.1063/1.4964856.
  39. Khazdozian H.A., Manzano J.S., Gandha K. et al. Recycled Sm–Co bonded magnet filaments for 3D-printing of magnets. AIP Advances, 2018, vol. 8, p. 056722. DOI: 10.1063/1.5007669.
  40. White E., Kassen A., Simsek E. Net shape processing of Alnico magnets by additive manufacturing // IEEE Transaction on magnetics, 2017, vol. 53, рр. 1–7. DOI: 10.1109/TMAG.2017.2711965.
  41. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Development of the process of directional crystallization of gas turbine engine blades from heat-resistant and intermetallic alloys with a single-crystal structure. Vestnik moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mashinostroyenie, 2011, no. S2, pp. 20–25.
  42. Pikunov M.V., Belyaev I.V., Sidorov E.V. Crystallization of alloys and directional solidification of castings. Vladimir: VSU, 2002, 213 p.
  43. Kablov E.N. Cast blades of gas turbine engines: alloys, technologies, coatings. Moscow: Nauka, 2006, 632 p.
  44. Methods of smelting with directional crystallization of an alloy of the Fe–Al–Ni–Co system: pat. 2662004 Rus. Federation; appl. 14.11.17; publ. 23.08.18.
  45. Method for producing oriented single-crystalline seeds from alloys with peretectic transformation: pat. 2084561 Rus. Federation; appl. 05.03.94; publ. 20.07.97.