T. G. Sevalneva, K.D. Oblivantsev, D. Yu. Nefedkin Assessing tendency to strain hardening of wires of various diameters made from austenitic-martensitic steel VNS9-Sh // Proceedings of VIAM. 2026. No. 9 (163). С. 3-13. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-3-13.

Assessing tendency to strain hardening of wires of various diameters made from austenitic-martensitic steel VNS9-Sh

T. G. Sevalneva, K.D. Oblivantsev, D. Yu. Nefedkin
Abstract

The effect of deformation rate (0,1–15 mm/min) on the mechanical properties and strain hardening of wires with diameters of 0,36–2,4 mm made from austenitic-martensitic TRIP steel VNS9-Sh after cold drawing with a degree of deformation of 31,5–86 % was investigated. It was established that the volume fraction of martensite increases linearly from 15 to 57 %. The ultimate tensile strength of wires with diameter of 0,36 and 2,4 mm reaches 2520 and 1758 MPa, respectively. According to the determined parameters of the Johnson–Cook model, VNS9-Sh steel wire is practically not susceptible to strain hardening.

Keywords
TRIP effect, austenitic-martensitic steels, VNS9-Sh steel, cold drawing, deformation, mechanical properties, microstructure, phase composition, martensite, austenite
Reference list
  1. Alekseeva M.S., Slobodskoy P.A., Lukina E.A., Yakusheva N.A. Patterns of structure formation for open-hearth steel of the Fe-Cr-Ni-Mo-Ti system during heat treatment. Trudy VIAM, 2024, no. 2 (132), pp. 3-12. Available at: http://www.viam-works.ru (accessed: April 01, 2026). DOI: 10.18577/2307-6046-2024-0-2-3-12.
  2. Sevalnev G.S., Dulnev K.V., Ryzhkov P.V., Leonov A.V., Voznesenskaya N.M. Optimization of heat treatment for high-strength corrosion-resistant nitrogen-containing steel to produce seamless thin-walled tubes. Trudy VIAM, 2025, no. 8 (150), pp. 41-52. Available at: http://www.viam-works.ru (accessed: April 01, 2026). DOI: 10.18577/2307-6046-2025-0-8-41-52.
  3. Dulnev K.V., Sevalnev G.S., Pahomkina T.N., Buzenkov A.V. Study of changes in microstructure, grain size and nitrogen concentration depending on heat treatment temperature of high-strength structural high-nitrogen steel. Aviation materials and technologies, 2025, no. 3 (80), pp. 3-14. Available at: http://www.journal.viam.ru (accessed: April 01, 2026). DOI: 10.18577/2713-0193-2025-0-3-3-14.
  4. Eliseev E.A., Karpukhin S.D., Druzhinina M.E. The effect of nickel on the structure of the nitrided layer of low-carbon martensitic steels. Aviation materials and technologies, 2025, no. 1 (78), pp. 18-27. Available at: http://www.journal.viam.ru (accessed: April 01, 2026). DOI: 10.18577/2713-0193-2025-0-1-18-27.
  5. Jacques P.J., Furmenton Q., Lani F. et al. Multiscale mechanics of TRIP assisted multiphase steels. Philosophical Magazine A, 2001, vol. 81 (6), pp. 1789-1812. DOI: 10.1080/01418610108216636.
  6. Olson G.B., Cohen M. Kinetics of strain-induced martensitic nucleation. Metallurgical Transaction A, 1975, vol. 6 (4), pp. 791-795. DOI: 10.1007/BF02672301.
  7. Zackay V.F., Parker E., Feldman H. Transformation-induced plasticity in steels. Transaction ASM, 1967, vol. 60, pp. 252-259.
  8. Jimenez-Melero E., van Dijk N.H., Zhao L. et al. Effect of the stability of retained austenite on the mechanical behavior of TRIP steels. Acta Materialia, 2007, vol. 55 (20), pp. 6713-6723. DOI: 10.1016/j.actamat.2007.08.038.
  9. Prosvirnin D.V., Sevalnev G.S., Kaplan M.A. et al. Effect of the Degree of Compression on the Phase Composition and Mechanical Properties of VNS9-Sh TRIP Steel Wire under Static and Cyclic Loading. Deformatsiya i razrushenie materialov, 2023, no. 6, pp. 16-22. DOI: 10.31044/1814-4632-2023-6-16-22.
  10. Sevalnev G.S., Sevalneva T.G., Romanenko D.N. et al. Study of the Mechanism of Austenite Formation in the Surface Layer during Cold Drawing of VNS9-Sh Austenitic-Martensitic Steel Wire. Uprochnyayushchie tekhnologii i pokrytiva, 2022, vol. 18, no. 7 (211), pp. 306-310.
  11. Sevalneva T.G., Terentyev V.F., Sevalnev G.S., Vlasov I.I. Features of the formation of the structure of wire from austenitic-martensitic TRIP steel VNS9-Sh during drawing. Deformatsiya i razrushenie materialov, 2021, no. 2, pp. 26-31.
  12. Lee S.J., De Cooman B.C. Effect of Al on the mechanical stability of austenite in Fe-Mn-Al-Si TRIP steels. Metallurgical and Materials Transaction A, 2013, vol. 44 (1), pp. 5119-5131. DOI: 10.1007/s11661-013-1823-3.
  13. Meyer L.W., Kruger L., Eckner R. et al. High rate deformation behavior of austenitic TRIP steels. International Journal of Impact Engineering, 2011, vol. 38 (3), pp. 282-290. DOI: 10.1016/j.ijimpeng.2010.10.002.
  14. Zerilli F.J., Armstrong R.W. Dislocation-mechanics-based constitutive relations for metals. Journal of Applied Physics, 1987, vol. 61 (5), pp. 1816–1825. DOI: 10.1063/1.338024.
  15. Chen S., Huang C.Y., Wang Y.T. et al. Rate dependent plastic behavior of TRIP-assisted steels. Materials Science and Engineering A, 2016, vol. 676, pp. 458–468. DOI: 10.1016/j.msea.2016.08.013.
  16. Wang C., Li J., Zhang Y. et al. Strain-rate effect on deformation behavior of Fe–Cr–Ni–N austenitic steels. Metallurgical and Materials Transaction A, 2019, vol. 50, pp. 1278–1288. DOI: 10.1007/s11661-018-5051-1.
  17. Johnson G.R., Cook W.N. A constitutive model and data for metals subjected to large strains. High rates and high temperatures. Proceedings of the 7th International symposium on ballistics. Hague, 1983, pp. 541–547.
  18. Johnson G.R., Cook W.H. Fracture characteristics of three metals subjected to various strains, strain rates, temperatures, and pressures. Engineering Fracture Mechanism, 1985, vol. 21, no. 1, pp. 31–48.