Archive - Электронный научный журнал "ТРУДЫ ВИАМ"

Articles

 


№1 | №2 | №3 | №4 | №5 | №6 | №7 | №8 | №9 | №10 | №11 | №12





1.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-3-12
УДК 620.172
Petrushin N.V., Golinets S.A, Rimsha E.G., Ryzhkov P.V.
MECHANICAL PROPERTIES OF CORROSION-RESISTANT NICKEL-BASED SUPERALLOY VZhL23

The results of experimental studies of short-term strength, long-term strength, multi-cycle fatigue and low-cycle fatigue of the castable corrosion-resistant nickel-based superalloy VZhL23 for turbine blades of GTI and GTE are presented.

Comparative analysis of the obtained values of long-term strength, multi-cycle fatigue and low-cycle fatigue of VZhL23 with the most heat-resistant foreign alloy IN-792 is carried out. It has been established that according to the set of mechanical properties VZhL23 is not inferior to IN-792.

Read in Russian

2.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-13-24
УДК 669.018.44
Echin A.B., Deynega G.I., Narskiy A.R.
NEW DEVELOPMENTS OF NRC «KURCHATOV INSTITUTE» – VIAM IN THE FIELD OF MATERIALS FOR CASTING PROCESSES OF SUPERALLOYS

The main results of the research work carried out at the NRC "Kurchatov Institute" – VIAM in the period from 2015 to the present in the field of creating new materials for casting processes of nickel superalloys are considered. Serial production and supply of a number of materials to machine-building enterprises has been established. A promising task is the organization of low-tonnage production of blades for power turbine installations in order to solve the problem of import substitution and expansion of domestic production.

Read in Russian

3.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-25-34
УДК 669.15
Krokhinа V.A., Arislanov A.A., Putyrskiy S.V., Naprienko S.A.
INVESTIGATION OF THE INFLUENCE OF HEAT TREATMENT MODES IN THE β-REGION ON THE STRUCTURE AND MECHANICAL PROPERTIES OF SEMI-FINISHED PRODUCTS FROM THE VT22M ALLOY

. Presents the results of a study of the structure and mechanical properties of semi-finished products from the VT22M alloy after various modes of heat treatment with heating in the β-region. The regimes differed in the rate of cooling from the β-region and the presence of intermediate exposures. The study of mechanical properties in tension, impact strength and fracture toughness was carried out, the analysis of macrostructure and microstructure was carried out. After testing for fracture toughness, fractographic studies were performed to assess the nature of the fracture of the samples. The effect of heat treatment modes in the β-region on the structure and mechanical properties of semi-finished products from the VT22M alloy is shown.

Read in Russian

4.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-35-51
УДК 669.295
Shiryaev A.A., Nochovnaya N.A.
MODERN TRENDS IN THE FIELD OF HEAT TREATMENT AND THERMOMECHANICAL PROCESSING OF METASTABLE β-TITANIUM ALLOYS

Presents the classification and features of various subgroups of metastable β-titanium alloys, considers typical approaches for their heat treatment and thermomechanical processing. The results of recent studies that form trends for further development in the field of heat treatment and thermomechanical processing technologies for metastable β-titanium alloys are presented. It is noted that the main trend of most publications is the use of modern high-tech research methods: SEM, HRTEM, EBSD. Among the most important trends in the study area, one can single out works related to obtaining and controlling the characteristics of a bimodal and multimodal structure in order to increase the level and ensure a balance of the complex of mechanical and operational properties.

Read in Russian

5.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-52-63
УДК 621.7
Yashin M.S., Kapitanenko D.V.
INVESTIGATION OF THE STRUCTURE AND PROPERTIES OF THE VT3-1 ALLOY IN RELATION TO THE TECHNOLOGY FOR OBTAINING STAMPINGS OF DISKS AND TURBINE BLADES

Рroperties and structure of forgings made of titanium alloy VT3-1, obtained by isothermal deformation under the conditions of the National Research Center «Kurchatov Institute» – VIAM presented in present paper. The draft was carried out according to the scheme of blades with a degree of deformation of 60 % and according to the scheme of disks with a degree of deformation of 80 %. The forgings were subjected to low-temperature, isothermal and double annealing. It has been investigated that the VT3-1 alloy has a high technological plasticity in the temperature range below the polymorphic transformation limit. Stampings show the required level of properties when deformed in the (α β)-area.

Read in Russian

6.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-64-73
УДК 678.8
Mukhametov R.R., Mosiyuk V.N., Shosheva A.L., Bukharov S.V.
EPOXYBISMALEIMIDE RESINS:FEATURES AND ADVANTAGES

The review of the released epoxybismaleimide materials of various scopes is provided in the real work on the basis of the analysis of domestic and foreign patent and scientific and technical literature: binding, adhesives. The physical and thermomechanical properties of polymer matrices of epoxybismaleimide resins and adhesives are presented. Modification of the epoxy polymer matrix with bismaleimides increases the heat resistance, strength, and crack resistance of polymer composite materials (PCMs) based on them.

Read in Russian

7.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-74-84
УДК 678.8
Kuznetcova P.A., Tkachuk A.I., Karavaev R.Y., Donetskiy K.I.
THE USE OF SEMI-PREGS FOR THE MANUFACTURE OF PANELS OF HOUSING STRUCTURES FROM POLYMER COMPOSITE MATERIALS BY VACUUM BAG ONLY

This paper provides an overview of the scientific and technical literature on the use of molten epoxy binders for the manufacture of semi-pregs processed by vacuum bag only for the manufacture of large-sized products from polymer composite materials for structural purposes. The comparison of porosity values of materials obtained by vacuum bag only of semi-pregs and prepregs is given. The main necessary technological requirements for epoxy binders for the production of semi-pregs are listed, as well as technologies used in industry for the manufacture of semi-pregs.

Read in Russian

8.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-85-99
УДК 678.8
Putilina P.M., Kutsevich K.E., Isaev A.Yu.
CARBON FIBER-REINFORCED AND GLASS FIBER-REINFORCED POLYMER COMPOSITES FOR THE MANUFACTURE OF COMPONENTS FOR UNMANNED AERIAL VEHICLES AND THEIR DEVELOPING PROSPECTS

Foreign and Russian publications on the use of carbon fiber-reinforced plastics (CFRPs) and glass fiber-reinforced plastics (GFRPs) in the structural elements of unmanned aerial vehicles (UAVs) were reviewed. The advantages of their application and the influence of strength-to-weight ratio of the materials on the efficiency of the UAV were described. The types of components made of polymer composite materials, their creation methods and the influence of manufacturing technology on the properties of plastics were explored. Adhesive prepregs with carbon and glass reinforcements developed by the NRC «Kurchatov Institute» – VIAM are proposed for possible use in the design of UAVs.

Read in Russian

9.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-100-112
УДК 629.7.023
Kozlov I.A., Fomina M.A., Dyomin S.A., Vasiliev A.S.
TENDENCIES IN THE DEVELOPMENT OF POWDER MATERIALS FOR THE APPLICATION OF PROTECTIVE AND FUNCTIONAL COATINGS BY THE CGN METHOD

The method of cold gas-dynamic spraying (CGS) of coatings has certain advantages, such as simplicity of the technological process, environmental friendliness, as well as the possibility of obtaining coatings with a wide range of functional properties (corrosion resistance, fire resistance, electrical insulating properties, etc.) through the use of various powder materials and ways to make them. The article presents the results of research in the field of application of powder materials for coating, describes composite powder materials with a complex structure obtained as a result of mechanical alloying, including those containing ceramic particles and particles of intermetallides.

Read in Russian

10.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-113-128
УДК 620.1
Veligodsky I.M., Koval T.V., Gulyaev I.N.
INFLUENCE OF CLIMATIC CONDITIONS ON CFRP VKU-39 AFTER THREE YEAR OUTDOOR EXPOSITION IN EIGHT CLIMATIC ZONES

The climatic resistance of CFRP to influence of eight types of climate of different climatic zones during the three year exposition were investigated. Exposed polymer composite was studied by optical microscopy, dynamical mechanical analysis, moisture saturation, flexural strengthandcompressive strength of polymer composite were determined. Deterioration of upper layer of polymer matrices after exposition was shown. Relationship between climatic factors influence on polymer composites, changing of polymer matrices condition and decreasing of material strength was found.

Read in Russian

11.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-129-137
УДК 620.1
Min P.G., Yakimovitch P.V., Alekseev A.V.
DEVELOPMENT OF A SET OF REFERENCE SAMPLES OF CASTING HEAT-RESISTANT ALLOY VZHL718

Рresents the results of the development of a set of standard samples of cast superalloy VZhL718. The process of choosing the optimal composition of the alloy is described, as well as the use of various technologies for obtaining a material suitable for calibrating various spectral equipment: mass spectrometers with a glow discharge, optical emission and х-ray fluorescence spectrometers, etc. The determination of 22 elements (Fe, Al, Cr, Co , Mo, Ti, Nb, Ta, P, Mn, Cu, Zn, As, Se, Cd, Sb, Te, Pb, Bi, V, Ag, Sn) in the obtained standard samples.

Read in Russian

12.
dx.doi.org/ 10.18577/2307-6046-2023-0-8-138-148
УДК 678.8
Ermishev V.Yu., Laptev A.B., Startsev V.O.
PECULIARITIES OF ASSESSING THE RESISTANCE OF POLYMERIC MATERIALS TO BIODEGRADATION IN LABORATORY CONDITIONS Part 2. Samples and methods for their analysis

Рresents a brief comparative analysis of domestic and foreign standards for testing non-metallic materials when interacting with microorganisms. Laboratory methods for analyzing the degree of biodegradation of materials used, among other things, in the test standards for synthetic polymers, are given. The significance of the physical dimensions of polymer samples for the search and testing of microorganism strains for the ability to use the chemical component of the material as a nutrient substrate is shown.

Read in Russian

13.
CONTENТS

Heat-resistant alloys and steels

 

Petrushin N.V., Golinets S.A., Rimsha E.G., Ryzhkov P.V.Mechanical properties of corrosion-resistant nickel-based superalloy VZhL23

 

Echin A.B., Deynega G.I., Narsky A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys

 

 

Light-metal alloys

 

Krokhinа V.A., Arislanov A.A., Putyrskiy S.V., Naprienko S.A. Investigation of the influence of heat treatment modes in the β-region on the structure and mechanical properties of semi-finished products from the VT22M alloy

 

Shiryaev A.A., Nochovnaya N.A. Modern trends in the field of heat treatment and thermomechanical processing of metastable β-titanium alloys

 

Yashin M.S., Kapitanenko D.V. Investigation of the structure and properties of the VT3-1 alloy in relation to the technology for obtaining stampings of disks and turbine blades

 

Polymer materials

 

Mukhametov R.R., Mosiyuk V.N., Shosheva A.L., Bukharov S.V. Epoxybismaleimide resins: features and advantages

 

Composite materials

 

Kuznetsova P.A., Tkachuk A.I., Karavaev R.Yu., Donetskiy K.I. The use of semi-pregs for the manufacture of panels of housing structures from polymer composite materials by vacuum bag only

 

Putilina P.M., Kutsevich K.E., Isaev A.Yu. Carbon fiber-reinforced and glass fiber-reinforced polymer composites for the manufacture of components for unmanned aerial vehicles and their developing prospects

 

Protective and functional

coatings

 

Kozlov I.A., Fomina M.A., Demin S.A., Vasiliev A.S. Tendencies in the development of powder materials for the application of protective and functional coatings by the CGN method

 

Material tests

 

Veligodskiy I.M., Koval T.V., Gulyaev I.N. Influence of climatic conditions on CFRP VKU-39 after three year outdoor exposition in eight climatic zones

 

 

Min P.G., Yakimovich P.V., Alekseev A.V. Development of a set of reference samples of casting heat-resistant alloy VZhL718

 

 

Ermishev V.Yu., Laptev A.B., Startsev V.O. Peculiarities of assessing the resistance of polymeric materials to biodegradation in laboratory conditions. Part 2. Samples and methods for their analysis

 