The article presents the results of research aimed at studying the structural and phase stability of a high-temperature intermetallic alloy based on nickel VIN4M. It is shown that the greatest effect of dissolution of the eutectic γ'-phase, affecting the stress state of the alloy of a certain chemical composition, is observed in the temperature range 1310–1330 °C. The critical points of material are determined after vacuum induction melting and vacuum induction casting by the method of directional solidification with a crystallographic orientation of <001> and the characteristics of alloy samples for short and long-term strength after hardening heat treatment.
2. Kablov E.N. There is no future without new materials. Metallurg, 2013, no. 12, pp. 4–8.
3. Kablov E.N. For the 80th anniversary of VIAM. Zavodskaya laboratoriya. Diagnostika materialov, 2012, vol. 78, no. 5, pp. 79–82.
4. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Features of single-crystal high-temperature nickel alloys doped with rhenium. Metally, 2006, no. 5, pp. 47–58.
5. Kablov E.N., Petrushin N.V., Svetlov I.L. Computer design of heat-resistant nickel alloy of the IV generation for monocrystalline blades of gas turbines. Liteynye zharoprochnye splavy. Effekt S.T. Kishkina. Moscow: Nauka, 2006, pp. 98–115.
6. Kablov E.N., Buntushkin V.P., Morozova G.I., Bazyleva O.A. Basic principles of alloying the Ni3Al intermetallic compound in the creation of high-temperature alloys. Materialovedenie, 1998, no. 7, pp. 13-15.
7. Bazyleva O.A., Ospennikova O.G., Arginbaeva E.G., Letnikova E.Yu., Shestakov A.V. Development trends of nickel-based intermetallic alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 104–115. DOI: 10.18577/2071-9140-2017-0-S-104-115.
8. Kolobov Yu.R., Kablov E.N., Kozlov E.V., Koneva N.A. et al. Structure and properties of intermetallic materials with nanophase hardening. Moscow: Ed. House MISIS, 2008, 328 p.
9. Bondarenko Yu.A., Kablov E.N. Directional crystallization of high-temperature alloys with elevated temperature gradient. Metal Science and Heat Treatment, 2002, vol. 44, no. 7-8, pp. 288-291.
10. Kablov E.N., Lomberg B.S., Buntushkin V.P., Golubovsky E.R., Muboyadzhyan S.A. An alloy based on the Ni3Al intermetallic compound is a promising material for turbine blades. Metallovedeniye i termicheskaya obrabotka metallov, 2002, no. 7, pp. 16–19.
11. Bondarenko Yu.A., Deev V.V., Kablov E.N. Directed crystallization of GTE blades during casting with an increased temperature gradient. Aviacionnye materialy i tehnologii, 2003, no. 1, pp. 53–63.
12. Bondarenko Yu.A., Bazyleva O.A., Rayevskikh A.N., Narskiy A.RResearch on the creation of a new high-temperature heat-resistant matrix based on intermetallic compounds NiAl–Ni3Al. Trudy VIAM, 2018, no. 11 (71), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 06, 2019). DOI: 10.18577/2307-6046-2018-0-11-3-11.
13. Cast blades of gas turbine engines: alloys, technologies, coatings / ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, 632 p.
14. Bondarenko Yu.A., Kablov E.N. Directional crystallization of heat-resistant alloys with an increased temperature gradient. Metallovedeniye i termicheskaya obrabotka metallov, 2002, no. 7, pp. 20–23.
15. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Features of structure and heat resisting properties of monocrystals of <001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization. Aviacionnye materialy i tehnologii, 2011, no. 4, pp. 25–31.
16. Kablov E.N., Petrushin N.V., Morozova G.I., Svetlov I.L. Physicochemical factors of heat resistance of nickel alloys containing rhenium. Liteynye zharoprochnye splavy. Effekt S.T. Kishkina. Moscow: Nauka, 2006, pp. 116–130.
17. Kablov E.N., Bondarenko Yu.A., Surova V.A. Features of high-gradient directional solidification and equipment for casting single-crystal specimens and turbine blades from heat-resistant alloys containing rhenium. Liteynye zharoprochnye splavy. Effekt S.T. Kishkina. Moscow: Nauka, 2006, pp. 194–205.
18. Arginbaeva E.G., Nazarkin R.M., Shestakov A.V., Karachevtsev F.N. Research of heat treatment influence on structural-phase parameters of intermetallic nickel based alloys. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 8–13. DOI: 10.18577/2071-9140-2017-0-3-8-13.
19. Bazyleva O.A., Unchikova M.V., Turenko E.Yu., Bagetov V.V., Shestakov A.VStudy of heat treatment effect on structure, dendritic liquation parameters and time to failure of Ni3Al-based alloy containing Re). Trudy VIAM, 2016, no. 10, paper no. 4. Available at: http://www.viam.ru (accessed: June 01, 2020) DOI: 10.18577/2307-6046-2016-0-10-4-4.
According to the results of scientific and technical literature analysis one can conclude that a large number of factors influence the processes which take place during cooling, as well as the structure and properties after isothermal exposures. Among those factors there are structural and phase transformations features and the completeness of recrystallization processes. The effect of various cooling rates on the structure and properties of isothermally exposed metastable β-titanium VT47 alloy has been studied. It has been revealed that cooling in the selected rate ranges does not exert a significant effect on the Rockwell hardness and microstructure of the VT47 alloy. It has been shown that grains with an increased number of the secondary α-phase precipitates are characteristic for the initial stages of isothermal exposures.
2. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Kondrateva A.R. The influence of heat treatment conditions on structure and properties of pilot forgings from VT41 alloy with fine grained structure. Aviacionnye materialy i tehnologii, 2017, no. 3, pp. 3–7. DOI: 10.18577/2071-9140-2017-0-3-3-7.
3. Kolli R.P., Devaraj A. A review of metastable beta titanium alloys. Metals, 2018, vol. 8, pp. 1–41.
4. Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. The efficiency of rare earth metals for filler materials alloying. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
6. Kablov E.N. Marketing of materials science, aircraft construction and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5-6, pp. 40–44.
7. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
8. High-strength titanium-based alloy and a product made of high-strength titanium-based alloy: pat. 2569285 Rus. Federation, no. 2014153690/02; filed 29.12.14; publ. 20.11.15.
9. Kablov E.N., Nochovnaya N.A., Gribkov Yu.A., Shiryaev A.A. Development of high-strength titanium pseudo-β-alloy and technologies for obtaining semi-finished products from it. Voprosy materialovedeniya, 2016, no. 3 (87), pp. 23–31.
10. Azimzadeh S., Rack H.J. Phase transformations in Ti–6.8Mo–4.5Fe–1.5Al. Metallurgical and materials transactions A, 1998, vol. 29A. P. 2455–2467.
11. Ilyin A.A. Mechanism and kinetics of phase and structural transformations in titanium alloys. Moscow: Nauka, 1994, 304 p.
12. Chaudhuri K., Perepezko J.H. Microstructural Study of the Titanium Alloy Ti–15Mo–2.7Nb–3Al–0.2Si (TIMETAL 21S). Metallurgical and materials transactions A, 1994, vol. 25A, pp. 1109–1118.
13. Ivasishin O.M., Markovsky P.E., Semiatin S.L., Ward C.H. Aging response of coarse- and fine-grained β titanium alloys. Materials Science and Engineering A, 2005, vol. 405, pp. 296–305.
14. Furuhara T. Role of defects on microstructure development of beta titanium alloys. Metal and materials, 2000, vol. 6, no. 3, pp. 221–224.
15. Boyer R.R., Rack H.J., Venkatesh V. The influence of thermomechanical processing on the smooth fatigue properties of Ti–15V–3Cr–3Al–3Sn. Materials Science and Engineering A243, 1998, pp. 97–102.
16. Morita T., Yoshimoto T., Maeda T., Matsumoto S. Influence of Hot-Rolling and Aging on Mechanical Properties and Fatigue Strength of Ti–20V–4Al–1Sn Alloy. Ti-2007 Science and Technology. The Japan Institute of Metals, 2007, vol. 1, pp. 555–558.
17. Schmidt P., El-Chaikh A., Christ H.-J. Effect of Duplex Aging on the Initiation and Propagation of Fatigue Cracks in the Solute-rich Metastable β Titanium Alloy Ti 38-644. Metallurgical and Materials Transactions A, 2011, vol. 42A, pp. 2652–2667.
18. Shiryaev A.A., Nochovnaya N.A. Investigation of structure formation during aging of high-strength pseudo-β titanium alloy VT47. Metallurgist, 2020, vol. 63 (9), pp. 967–977. DOI: 10.1007/s11015-020-00914-z.
19. Illarionova S.M., Elkina O.A., Illarionov A.G. Phase transformations in a metastable β-solid solution during heat treatment of a pseudo-β titanium alloy with rare earth metals. Titan, 2016, no. 3, pp. 14–18.
20. Dehghan-Manshadi A., Dippenaar R.J. Development of α-phase morphologies during low temperature isothermal heat treatment of a Ti–5Al–5Mo–5V–3Cr alloy. Materials Science and Engineering A, 2011, vol. 528, pp. 1833–1839.
Рrovides a review of publications in the field of the research of aluminum-lithium alloys deformation processes, which are used in the construction of aircraft and space technology products. The review summarizes the research that are devoted to the influence of parameters of pressure treatment on structure formation processes in aluminum-lithium alloys and the mathematical modeling as applied to hot deformation processes. The article discusses the approaches that are used by researchers in the development of optimal deformation modes of aluminum-lithium alloys.
2. Grigorenko I.B., Zhegina I.P., Fomina M.A., Kablov E.N., Morozova L.V. Investigation of the influence of a corrosive environment on the process of damage accumulation and the nature of destruction of structural aluminum alloys 1441 and B-1469 during tensile tests and low-cycle fatigue. Nauka i tekhnologii, 2017, no. 1, pp. 41–48.
3. Annin B.D., Fomin V.M., Karpov E.V., Malikov A.G., Orishich A.M. Complex research of laser welding of high-strength alloy V-1469. Aviacionnye materialy i tehnologii, 2016, no. 3 (42), pp. 9–16. DOI: 10.18577/2071-9140-2016-0-3-9-16.
4. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2107-9140-2017-0-S-195-211.
5. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
6. Knyazev M.I., Betzofen S.Ya., Antipov V.V. Alloys of the Al – Cu – Li and Al – Mg – Li systems: phase composition, texture and anisotropy of mechanical properties (review). Deformatsiya i razrusheniye materialov, 2015, no. 11, pp. 10-26.
7. Klochkov G.G., Grushko O.E., Klochkova Ju.Ju., Romanenko V.A. Industrial development of strength alloy V-1469 of Al–Cu–Li–Mg. Trudy VIAM, 2014, no. 7, paper no. 01. Available at: http://viam-works.ru (accessed: February 17, 2020). DOI: 10.18577/2307-6046-2014-0-7-1-1.
8. Oglodkov M.S., Klochkova Yu.Yu., Kolobnev N.I., Khokhlatova L.B. High-strength alloys of the Al – Cu – Li system with increased fracture toughness for aircraft structures. Tsvetnye metally, 2013, no. 9, pp. 66–70.
9. Oglodkov M.S., Filatov A.A., Popova Yu.A., Khokhlatova L.B., Kolobnev N.I. Prospects for the use of low-density high-strength alloy V-1461 plates in aircraft structures. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 2, pp. 16–22.
10. Kolobnev N.I. History of development, phase composition and properties of alloys of the Al – Cu – Li system. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 46–52.
11. Oglodkov M.S., Erisov Ya.A., Grechnikov F.V. Influence of modes of making sheets from alloy V-1461 on crystallography of structure and anisotropy of properties. Izvestiya vuzov. Tsvetnaya metallurgiya, 2015, no. 6, pp. 36–42.
12. Liu M., Hu Y., Chen Y. et al. Analysis of empirical relation between microstructure, texture evolution and fatigue properties of an Al–Cu–Li alloy during different pre deformation processes. Materials Science and Engineering: A, 2018, vol. 72, pp. 309–319.
13. Zhou J., Dang L., Xiao W. et al. Influence of process parameters on deep drawing of 2060 Al–Li alloy under hot stamping process. Journal of Lightweight Materials and Manufacture, 2019, vol. 3, no. 1, pp. 36–42.
14. Guo X., Zhang S., Ma Y. et al. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al–Li alloys: a review. Journal of Advanced Research, 2018, vol. 10, pp. 49–67.
15. Khokhlatova L.B., Oglodkov M.S., Kolobnev N.I., Setiukov O.A. Influence of crystallographic orientations on the properties of plates made of Al–Li alloys B-1461 and 1424. Tekhnologiya legkikh splavov, 2010, no. 1, pp. 100–106.
16. Knyazev M.I., Oglodkov M.S., Betzofen S.Ya., Antipov V.V. Study of the effect of heat treatment on the phase composition, texture and mechanical properties of the alloy В-1461 systems Al – Cu – Li. Metally, 2015, no. 6, pp. 77–84.
17. Crooks R.E., Pagan D.C., Tayon W.A., Nygren K.E. In-situ study of planar slip in a commercial aluminum-lithium alloy using high energy x-ray diffraction microscopy. Acta Materialia, 2019, vol. 173, pp. 231–241.
18. Ponchivalov Yu.I., Panin S.V., Kolobnev N.I., Panin V.E., Kablov E.N. Influence of nanostructuring of the surface layer of aluminum-lithium alloy 1424 on deformation mechanisms, technological characteristics and fatigue life, increasing plasticity and technological characteristics. Fizicheskaya mezomekhanika, 2012, no. 6, pp. 107-111.
19. Li J.F., Chen Y.L., Zhang X.-H. et al. Flow curve correction and processing map of 2050 Al–Li alloy. Transactions of Nonferrous Metals Society of China, 2018, vol. 28, pp. 404–414.
20. Nie Y., Jian H., Ou L., Zheng Z. Hot deformation behavior of 2060 alloy. Journal of Alloys and Compounds, 2015, vol. 648, pp. 681–689.
21. Krishtal M.M. Instability and mesoscopic heterogeneity of plastic deformation (analytical review). Part 1. Fizicheskaya mezomekhanika, 2004, no. 7, pp. 5–29.
22. Kolupaeva S.N., Popov L.E., Starenchenko V.A. Instabilities of plastic deformation of crystals and the formation of dislocation defect structures. Matematicheskoye modelirovaniye sistem i protsessov, 1995, no. 3, pp. 77–87.
23. Milevskaya T.V., Ruschits S.V., Tkachenko E.A., Antonov S.M. Deformation behavior of high-strength aluminum alloys in conditions of hot deformation. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 3–9. DOI: 10.18577/2071-9140-2015-0-2-3-9.
24. Rajput S.K., Nath S.K., Kumar N., Kumar S. Modelling of flow stress and prediction of workability by processing map for hot compression of 43CrNi steel. ISIJ International, 2017, vol. 573, pp. 497–505.
25. Saha P. Aluminum extrusion technology. ASM International, 2000, pp. 25.
26. Soboyejo W.O. Mechanical properties of engineered materials. Marcel Dekker, 2003, pp. 222–228.
27. Hernandez C.A., Medina S.F. General expression of the Zener-Hollomon parameter as a function of the chemical composition of low alloy and microalloyed steels. Acta Materialia, 1996, vol. 44, pp. 137–148.
28. Smirnov M.A., Akhmedyanov A.M., Ruschits S.V. Physical and mathematical modeling of hot deformation of steel 20X13. Vestnik YUUrGU, 2013, no. 13, pp. 116-124.
29. Jonas J.J., Laasraoui A. Prediction of steel flow stresses at high temperatures and strain rates. Metallurgical transactions A, 1991, vol. 22, pp. 1545–1558.
30. Singh S.B., Pal S.K. Computational Methods and Production Engineering, chapter Finite element modeling of hot rolling: Steady- and unsteady-state analyses. Mechanical Engineering Series, 2017, pp. 83–124.
31. Nourani M., Sajadifar S.V., Ketabchi M. Modeling of mechanical characteristics in hot deformation of 4130 steel. Transactions of the Metallurgical Society of AIME, 2011, vol. 82, pp. 934–939.
32. Li C., Wan M., Meng B., Du Z. Constitutive behavior and microstructural evolution in hot deformed 2297 Al–Li alloy. Chinese Journal of Aeronautics, 2019, vol. 11, pp. 77–87.
33. Luo A., Miao J., Sutton S. Microstructure and hot deformation behavior of a new aluminum–lithium–copper based aa2070 alloy. Materials Science Engineering, 2020, vol. A777, pp. 2–14.
34. Murty N.S.V.S., Jha A.K., Pant B. et al. Microstructure and micro-texture evolution during large strain deformation of an aluminium–copper–lithium alloy aa2195. Materials and Design, 2015, vol. 65, pp. 862–868.
35. Du R., Zhao M., Wang Z. et al. Characteristic constitution model and microstructure of an Al–3.5C–1.5Li alloy subjected to thermal deformation. Materials Characterization, 2018, vol. 145, pp. 53–64.
36. Chhangani S., Prakash A., Prasad M.J.N.V. et al. Effect of temperature and strain rate on hot deformation behavior and microstructure of Al–Cu–Li alloy. Journal of Alloys and Compounds, 2017, vol. 723, pp. 548–558.
37. Li G.-A., Wang X.-M., Sun J. et al. Effects of coarse Al2CuLi phase on the hot deformation behavior of Al–Li alloy. Journal of Alloys and Compounds, 2020, vol. 815, pp. 77–87.
38. Uvira J.J., Jonas J.L. Hot compression of ARMCO iron and silicon steel. Transactions of the Metallurgical Society of AIME, 1969, vol. 242, pp. 1619–1626.
39. Antonov S.M., Akhmedyanov A.M., Ruschits S.V. Investigation of the deformation behavior of 20Kh13 steel under hot upsetting conditions. Vestnik YUUrGU, 2012, no. 19, pp. 89–93.
40. Doraivelu S.M., Malas J.C., Morgan J.T. et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242. Metallurgical transactions A, 1984, vol. 15A, pp. 1883–1892.
41. Seshacharyulu T., Prasad Y.V.R.K. Processing maps for hot working of titanium alloys. Materials Science and Engineering, 1998, vol. A243, pp. 82–88.
42. Vargasov N.R., Rybin V.V. Optimization of temperature and rate regimes of plastic deformation by the criterion of dissipation of mechanical energy. Metal Science and Heat Treatment, 1999, vol. 41, pp. 9–10.
43. Feng Z., Lu Z., Zhu C. et al. Hot deformation characterization of as-homogenized Al–Cu–Li X2A66 alloy through processing maps and microstructural evolution. Journal of Materials Science Technology, 2019, vol. 35, pp. 2409–2421.
44. Nemets A.M., Khlusova E.I., Barakhtin B.K., Vargasov N.R. The choice of modes of thermo-mechanical treatment of steels and alloys based on system analysis of the structure and simulation. Materials Physics and Mechanics, 2011, no. 12, pp. 30–42.
45. Li J., Xiang S., Chen Y. et al. Dynamic restoration mechanism and physically based constitutive model of 2050 Al–Li alloy during hot compression. Journal of Alloys and Compounds, 2015, vol. 650, pp. 75–85.
46. Song M., Liang X., Guo F. et al. Hot deformation behavior and microstructural evolution of Ag-containing 2519 aluminum alloy. Materials and Design, 2010, vol. 31, pp. 2171–2176.
47. Liu G., Sun L., Chen L. et al. Microstructure evolution and mechanical properties of 2196 Al–Li alloy in hot extrusion process. Journal of Materials Processing Technology, 2020, vol. 275, pp. 2–14.
48. Kokovikhin E.A., Salikhyanov D.R., Dvoynikov D.A. et al. Determining the plastic strain resistance of metallic materials on an automated plastometric complex. Diagnostics, Resource and Mechanics of materials and structures, 2015, vol. 2, pp. 24–43.
49. Galkin A.M., Polukhin P.I., Gun G.Ya. Resistance to plastic deformation of metals and alloys: reference book. Moscow: Metallurgiya, 1983, pp. 82–88.
50. Stefani N., Blackwell P., Bylya O., Gomez-Gallegos A. Al–Li alloys – the industrial analysis hot of material during forging behavior during industrial hot forging. Procedia Engineering, 2017, vol. 207, pp. 7–12.
51. Liu J., Li C., Li Z. et al. Hot stamping of an Al–Li alloy: a feasibility study. Manufacturing Review, 2016, vol. 9, pp. 2–5.
Being based on a number of sources works on data and synthesis of survey information of the devoted history of development, the comparison of properties of domestic and foreign organosilicon sealant materials and application sealants made on the basis of low-molecular organosilicon and fluorosiloxane rubbers. Features of application of low-molecular weight siloxane rubbers are considered when manufacturing pressurizing materials. The comparative analysis sealants type of VICSINT, compounds and type of VGF.
2. Buznik V.M., Kablov E.N. Arctic materials science. Tomsk: Tomsk. State Un-t, 2018, is. 3, 44 p.
3. Kablov E.N. Formation of domestic space materials science. Vestnik RFFI, 2017, no. 3, pp. 97–105.
4. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, no. 10, pp. 61–71.
5. Andrianov K.A. Organosilicon polymer compounds. Moscow: GEI, 1946, 136 p.
6. Bejder E.Ya., Petrova G.N. The thermoplastic binder for polymeric composite materials. Trudy VIAM, 2015, no. 11, paper no. 05. Available at: http://viam-works.ru. (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2015-0-11-5-5.
7. Bryk Ya.A., Eliseev O.A., Smirnov D.N. Corrosion protection of magnesium alloys polysulphide sealants. Trudy VIAM, 2017, no. 10 (58), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2017-0-10-10-10.
8. Nanushyan S., Semenkova N., Trokhachenkova O., Polivanov A.N. Dispersiveness study of nanosize fillers in organosilicon environment. Conf. 5th European Silicon Days. Venna, 2009, pp. 168.
9. Bryk Ya.A., Smirnov D.N. Research of frost resistance of aeronautical sealants. Trudy VIAM, 2018, no. 1 (61), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2018-0-1-9-9.
10. Krasnov L.L., Kirina ZV, Venediktova M.A., Bryk Ya.A. Approbation of tape sealant for sealing removable constructive elements operable at temperatures from -60 to +180 °С. Trudy VIAM, 2019, no. 3 (75), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 28, 2020). DOI: 10.18577/2307-6046-2019-0-3-53-60.
11. Nanushyan S.R. Organosilicon materials of accelerated vulcanization: the history of the creation and development of the direction. Khimicheskaya promyshlennost segodnya, 2015, no. 11, pp. 21.
12. Semenkova N., Nanushyan S., Polivanov A., Storozhenko P. Divinilpolydiorganosiloxane based composites with nanodispersed fillers. Conf. 5th European Silicon Days. Venna, 2009, pp. 191.
13. Semenkova N., Nanushyan S., Storozhenko P. et al. Protective insulating Coatings Based on Siloxanes and Submicro- and Nano-Size Fillers. 17th International Symposium on Silicon Chemistry. Berlin, 2014, pp. 236.
14. Savenkova A.V., Tikhonova I.V., Trebukova E.D. Heat and frost-resistant sealants. Aviation materials at the turn of the XX–XXI centuries. Moscow: VIAM, 1994, pp. 432–439.
15. Petrova A.P., Donskoy A.A., Chalykh A.E., Shcherbina A.A. Adhesive materials. Sealants: reference book. Saint Petersburg: Professional, 2008, 589 p.
16. Nikitina A.N., Nightingale V.V. Fuel-resistant sealants. Aviation materials at the turn of the XX–XXI centuries. Moscow: VIAM, 1994, pp. 374–378.
17. Severny V.V., Minasyan R.M., Makarenko I.A., Biryuzova N.M. Mechanism of «cold» curing of low-molecular polyorgansiloxan rubbers. High molecular weight compounds. Ser.: A. 1976, vol. 18, pp. 1276–1281.
18. Low-viscosity siloxane composition: pat. 2356117 Rus. Federation; fied 20.06.07; publ. 20.05.09.
9. Minakov V.T., Savenkova A.V., Donskoy A.A. Organosilicon sealants. Rossiyskiye polimernye novosti, 2003, vol. 8, no. 4, pp. 37–41.
20. Kornev A.E., Bukanov A.M., Sheverdyaev O.N. Elastomeric materials technology. Moscow: Publ. House Mosk. State Open University, 2000, pp. 64–72.
21. Khairullin I.K., Pomanskaya M.P., Serebrennikova N.D. and others. New domestic one-pack sealants for installation of main blocks with double-glazed windows. Klei. Germetiki. Tekhnologii, 2006, no. 6, pp. 34–38.
22. Zaglyadova S.V., Lyusova L.R., Glagolev V.A. et al. Rubber-bitumen sealing mastics. Klei. Germetiki. Tekhnologii, 2005, no. 10, pp. 24–26.
23. Kablov E.N. Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode. Aviacionnye materialy i tehnologii, 2013, no. S1, pp. 3–9.
24. Kablov E.N. Materials and chemical technologies for aviation technology. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
25. Khakimullin Yu.N., Gubaidullin L.Yu. Modern approaches to the production of curing sealants. Second Kirpichnikov Readings: plenary reports. Kazan, 2001, pp. 63–68.
26. Gerasimov D.M., Ilyukhina M.A., Glazov P.A. Features of the use of low-molecular organosilicon rubbers in sealing compositions. All-Russian Scientific and Technical Conf. «Fundamental applied research in the field of sealing, sealing and fire and heat protection materials». Moscow, 2019, pp. 45.
27. Aronovich D.A., Murokh A.F., Sineokov A.L. Heat-resistant anaerobic sealants and adhesives. Plasticheskiye massy, 2006, no. 6, pp. 37–41.
28. Mezhikovsky S.M., Irzhak V.I. Chemical physics of oligomer curing. Moscow: Nauka, 2008, 269 p.
The use of composite materials is carried out more on the widest scale. More and more relatively small, but structurally complex and critical parts of machines and mechanisms began to be made of polymers, and at the same time, polymers began to be used more and more often in the manufacture of large-sized body parts that carry significant loads. Polymer composite materials have firmly won a place among structural materials. Composite materials can no doubt be attributed to the most promising products of both modern and future industrial production.
2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
3. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
4. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt & Tekhnologii, 2016, no. 4, pp. 41–46.
3. Kablov E.N. VIAM Materials and Technologies for Aviadvigatel. Permskiye aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
24. 6. Kablov E.N. On the present and future of VIAM and Russian materials science: interviews. Rossiyskaya akademiya nauk: 2015. 19 January. Available at: https://www.ras.ru/news/shownews.aspx?id=824e2453-383e-4d9e-b78d-87v9f7bf16ee (accessed: June 27, 2020).
7. Kablov E.N. Composites: Today and Tomorrow. Metally Evrazii, 2015, no. 1, pp. 36–39.
8. Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: June 27, 2020). DOI: 10.18577/2307-6046-2020-0-1-68-77.
9. Carbon fiber drive shaft: pat. US4089190A; filed 14.04.76; publ. 16.05.78.
10. Biaxial mesh structure made of composite material: pat. RU183461 Rus. Federation; filed 25.06.18; publ. 24.09.18.
11. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Features of prepregs intended for automated laying by ATL and AFP technologies. Trudy VIAM, 2015, no. 3, paper no. 06. Available at: http://www.viam-works.ru (accessed: September 19, 2019). DOI: 10.18577/2307-6046-2015-0-3-6-6.
12. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Melt binding for perspective methods of production of PCM of new generation. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 260–265.
13. Timoshkov P.N., Platonov A.A., Hrulkov A.V. Film resin infusion as an advanced method for out-of-autoclave processing of polymer composites. Trudy VIAM, 2015, no. 5, paper no. 09. Available at: http://www.viam-works.ru (accessed: November 11, 2019). DOI: 10.18577/2307-6046-2015-0-5-9-9.
14. Donetskij K.I., Kogan D.I., Hrulkov A.V. The use of thecnology of braiding in production of structural elements of polymer composites materials. Trudy VIAM, 2013, no. 10, paper no. 04. Available at: http://www.viam-works.ru (accessed: September 19, 2019).
15. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
16. Perov B.V., Gunyaev G.M., Rumyantsev A.F., Stroganov G.B. Application of high-modulus polymer composite materials in aircraft products. Available at: https://viam.ru/public/files/1982/1982-198546.pdf (accessed: July 27, 2020).
17. Drive shaft made of composite materials: pat. 2601971 Rus. Federation; filed 08.09.15; publ. 10.11.16.
18. Wagner B. Cutting Weight: Why You Should Use A Carbon Fiber Driveshaft. Available at: www.streetmusclemag.com/news/cutting-weight-why-you-should-use-a-carbon-fiber-driveshaft (accessed: April 05, 2020).
19. Carbon fiber driveshaft Driveshaft Shop. Available at: https://www.drive2.ru/l/3888355/ (accessed: June 22, 2020).
20. Carbon Shaft, All C63. Available at: http://weistec.com.ua/product/carbon-fiber-drive-shaft-c63-all (accessed: June 22, 2020).
21. Shaft made of plastic. Carbon fiber. Hollow. Azimuth. Available at: https://www.directindustry.com.ru/prod/centa/product-9279-717567.html (accessed: April 05, 2020).
22. Carbon, carbon and carbon fiber. Available at: https://carbocarbo.ru/shop/carbon_fabric (accessed: July 27, 2020).
23. Manufacturing and repair of carbon fiber cooling tower shafts and drive shafts of sea and river vessels Centa. Available at: http://safit.info/carbon-fiber-shaft.html (accessed: April 05, 2020).
Provides an overview of the highly porous ceramic materials currently used for filtration of metal melts and hot gases, filter manufacturers and methods for their production. Gas permeability and high specific surface area in combination with refractory properties allow using of highly porous oxides in processes carried out at high temperatures in chemical media when other materials are not applicable. Ways of improving the operational properties of porous ceramic filters, such as operating temperature, strength, oxidative resistance, bimodal porosity, as well as possibilities of improving the technological process of their production: reduced cost, increased environmental safety of production, reduced time of the technological cycle wereconsidered.
2. Antsiferov V.N., Beklemyshev A.M., Gilev V.G. et al. Problems of powder materials science. Part II. Highly porous permeable materials. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2002, 262 p.
3. Ivanchenkova L.G. Classification of filters for metal refining. Ogneupory, 1991, no. 2, pp. 28–29.
4. Catalog of products of LLC «SpheroLit». Available at: https://sferolit.ru (accessed: July 20, 2020).
5. Method of manufacturing a ceramic foam filter from titanium carbide: pat. 2280536 Rus. Federation; filed 27.12.04; publ. 27.07.06.
6. Ceramic mass and method of making porous products from it: pat. 2047582 Rus. Federation; filed 17.07.92; publ. 10.11.95.
7. FineWay Ceramics (Canada). Available at: http://finewayceramics.com (accessed: July 20, 2020).
8. Ceramic mass for the manufacture of filter products: certificate of authorship 1323551 USSR; filed 19.11.85; publ. 15.07.87.
9. A method of manufacturing a ceramic composite material: pat. 2355665 Rus. Federation; filed 25.07.07; publ. 20.05.08.
10. Mukanova A.Zh., Kanygina ON. The problem of creating a pore space in siliceous ceramics for environmentally friendly filters. Vektor nauki TGU, 2013, no. 3, pp. 77–79.
11. A method of manufacturing highly porous cellular ceramic products: pat. 2377224 Rus. Federation; filed 14.04.08; publ. 27.12.09.
12. Method of manufacturing highly porous cellular ceramic materials: pat. 2580959 Rus. Federation; filed 08.04.15; publ. 10.04.16.
13. Method for producing porous ceramics with bimodal distribution of porosity: pat. 2691207 Rus. Federation; filed 26.12.17; publ. 11.06.19.
14. Talsicukur Z., Balaban C., Kuskonmaz N. Production of ceramic foam filters for molten metal filtration using expanded polystyrene. Journal of the European Ceramic Society, 2007, vol. 27, p. 637–640.
15. Method of manufacturing lightweight ceramic products: certificate of authorship 1323554 USSR; filed 119.11.85; publ. 15.07.87.
16. Gonzenback U.T., Studart A.R., Steinlin D., Tervoot E., Gauckler J.L. Processing of particle-stabilized wet foams into porous ceramics. Journal of the American Ceramic Society. 2007, vol. 90, no. 11, pp. 3407–3414.
17. Salomao R., Villas Boas M.O.C., Pandolfelli V.C. Porous alumina-spinel ceramics for high temperature applications. Ceramics International, 2011, vol. 37, pp. 1393–1399.
18. A method of obtaining a porous structure of a ceramic material: pat. 2483043 Rus. Federation; filed 12.05.11; publ. 20.11.12.
19. Zo E Mo U. Porous and highly porous ceramics from aluminum oxide and silicon carbide: thesis, Dr. Sc. (Tech.). Moscow: D. Mendeleev University of Chemical Technology of Russia, 2019, 35 p.
20. Guo X., Nakanishi K., Kanamori K. et al. Preparation of macroporous cordierite monoliths via the sol–gel process accompanied by phase separation. Journal of the European Ceramic Society, 2014, vol. 34, pp. 817–823.
21. Ceramic Foam Filter: pat. 3947363 US; filed 28.03.75; publ. 30.03.76.
22. Method of Preparation of Ceramic Foam: pat. 4075303 US; filed 22.02.77; publ. 21.02.78.
23. Molten Metal Filter: pat. 4265659 US; filed 09.10.79; publ.05.05.81.
24. Molten Metal Filter: pat. 4342664 US; filed 23.05.80; publ. 03.08.82.
25. Process of Preparing a Ceramic Foam: pat. 4610832 US; filed 26.09.84; publ. 09.09.86.
26. Porous Ceramic Filter Body and Manufacturing Method Thereof: pat. 4678758 US; filed 27.01.84; publ. 07.07.87.
27. Ceramic Foam: pat. 4803025 US; filed 23.04.84; publ. 07.02.89.
28. Method and Apparatus for Removing Liquid Salts From Liquid Metal: pat. 6036743 USA; filed 27.10.97; publ. 14.03.00.
29. Dual Stage Ceramic Foam Filtration System and Method: pat. EP863217; filed 03.03.97; publ. 09.09.98.
30. Ceramic Foam Filter Having a Protective Sleeve: pat. 5456833 US; filed 02.05.94; publ. 10.10.95.
31. Die folgenden Angaben sind den vom Anmelder eingereichten Unterlagen entnommen: pat. 20318773U1 DE; filed 01.12.03; publ. 12.05.05.
32. Ceramic Material Permitting the Passage of Fluids and Based on Silicon Powder Reaction-banded in the Presence of Carbon: pat. 5093289 US; filed 14.02.89; publ. 03.03.92.
33. Ceramic Foam Filters: pat. 5190897 US; filed 20.09.91; publ. 02.03.93.
34. Low Expansion Corrosion Resistant Ceramic Foam Filters for Molten Aluminum Filtration: pat. 8518528 US; filed 02.04.07; publ. 27.08.13.
35. Process for the Production of Porous Ceramic Molded Articles: pat. 4472331 US; filed 22.02.83; publ. 18.09.84.
36. Manufacturing Method of a Ceramics Body Having Through Holes: pat. 4664858 US; filed 13.08.85; publ. 12.05.87.
37. High-Temperature Ceramic Filter: pat. 5676833 US; filed 08.02.96; publ. 14.10.97.
38. Silicon carbide foam ceramic filter: pat. 100536985 China; filed 24.08.07; publ. 09.09.09.
39. Preparation method of magnesian foamed ceramic filter for casting: pat. 101138691 China; filed 10.07.07; publ. 12.03.08.
40. Method for preparing ceramic filter with composite pore diameter: pat. 101165003 China; filed 06.09.07; publ. 23.04.08.
41. Shengguan Group «SQ Group» company (China) (official representative in Russia LLC «Scientific and technical center of industrial technologies»). Available at: www.sq-spb.ru (accessed: July 21, 2020).
42. The company OOO Kit-Stroy SPb. Available at: http://t-tiss.com (accessed: July 20, 2020).
43. Tarasovsky V.P., Krasny B.L., Koshkin V.I. et al. Quantitative analysis of the structure of permeable ceramics made of narrowly fractionated electrocorundum powder and hollow corundum microspheres. Novye ogneupory, 2016, no. 6, pp. 49–52.
44. Buchilin N.V., Prager E.P. Reologicheskie harakteristiki shlikernyh suspenzij na osnove oksida alyuminiya. Trudy VIAM, 2015, no. 5, paper no. 06. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2015-0-5-6-6.
45. Buchilin N.V., Prager E.P. On rheological characteristics of alumina-based slip suspensions. Trudy VIAM, 2015, no. 8, paper no. 06. Available at: http://viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2015-0-8-6-6.
46. Buchilin N.V., Lyulyukina G.Yu. Characteristics of sintering of highly porous alumina-based ceramic materials. Aviacionnye materialy i tehnologii, 2016, No. 4 (45), pp. 40–46. DOI: 10.18577/2071-9140-2016-0-4-40-46.
47. Buchilin N.V., Prager E.P., Ivahnenko Yu.A. The influence of plasticizating additives on rheology of slip for porous ceramic materials based on aluminum oxide. Trudy VIAM, 2016, no. 8, paper no. 6. Available at: http://www.viam-works.ru (accessed: June 25, 2020). DOI: 10.18577/2307-6046-2016-0-8-6-6.
48. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and pro-perties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (57), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
49. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
The difference in weathering of carbon-reinforced plastics on the exposed (front) and shaded (back) side of the samples was studied during the natural exposure in a moderately warm climate for 75 months. Surface profile parameters of the exposed samples were studied on both sides of the samples. Peak and valley height distribution peaks are 30–85% higher on the exposed side compared to the shaded side. The application of static load to the exposed or shaded side of the samples during the exposure resulted in different flexural strength.
2. Startsev V.O. Climatic resistance of polymer composite materials and protective coatings in moderately warm climates: thesis, Dr. Sc. (Tech.). Moscow: VIAM, 2018. 308 p.
3. Slavin A.V., Startsev O.V. Properties of aircraft glass- and carbonfibers reinforced plastics at the early stage of natural weathering. Trudy VIAM, 2018, no. 09 (69), paper no. 8. Available at: http://www.viam-works.ru (accessed: February 28, 2020). DOI: 10.18577/2307-6046-2018-0-9-71-82.
4. Bulmanis V.N., Startsev O.V. Prediction of changes in the strength of polymer fiber composites as a result of climatic effects. Yakutsk: Yakutsk branch of the Siberian Branch of the USSR Academy of Sciences; Institute of Physical and Technical Problems of the North, 1988, 32 p.
5. Vapirov Y.M., Krivonos V.V., Startsev O.V. Interpretation of the anomalous change in the properties of carbon-fiber-reinforced plastic KMU-1u during aging in different climatic regions. Mechanics of Composite Materials, 1994, vol. 30, no. 2, pp. 190–194.
6. Panin S.V., Startsev O.V., Krotov A.S. Initial stage environmental degradation of the polymer matrix composites evaluated by Water diffusion coefficient. Trudy VIAM, 2014, no. 7, paper no. 09. Available at: http://viam-works.ru (accessed: February 28, 2020). DOI: 10.18577/2307-6046-2014-0-7-9-9.
7. Startsev O.V., Sortyakov E.D., Isupov V.V. et al. Acoustic spectroscopy of polymer composite materials exposed in open space. Experimental methods in the physics of structurally inhomogeneous media: proc. All-Russian Scientific and Technical Conf. Barnaul: ASU Publishing House, 1997, pp. 32–39.
8. Filistovich D.V., Startsev O.V., Kuznetsov A.A., Krotov A.S., Anikhovskaya L.I., Dementeva L.A. Effect of moisture on the anisotropy of the dynamic shear modulus of glass-reinforced plastics. Doklady Physics, 2003, vol. 48, no. 6, pp. 306–308.
9. Matveenko V.P., Smetannikov O.Yu., Trufanov N.A., Shardakov I.N. Thermomechanics of polymer materials under conditions of relaxation transition. Fizicheskaya mezomekhanika, 1999, vol. 2, no. 4, pp. 23–29.
10. Valiotti N.B., Zaikov G.E. Investigation of relaxation transitions in polycaproamide by linear dilatometry. Plasticheskiye massy, 1989, no. 10, pp. 90–92.
11. Startsev V.O., Lebedev M.P., Frolov A.S. Measurement of surface relief indicators in the study of aging and corrosion of materials. 1. Russian and foreign standards. Vse materialy. Entsiklopedicheskiy spravochnik, 2018, no. 6, pp. 32–38.
12. Weber M. Confocal microscopy of micro- and nanostructured surfaces of materials. Nanoindustriya, 2011, no. 4 (28), pp. 42–47.
13. Startsev V.O., Nizina T.A., Startsev O.V. A color criterion of the climatic aging of an epoxy polymer. International Polymer Science and Technology, 2016, vol. 43, no. 8, pp. 45–48.
14. Nizina T.A., Selyaev V.P., Nizin D.R., Chernov A.N. Modeling the influence of actinometric parameters on the change in the decorative characteristics of epoxy composites exposed in natural conditions. Regionalnaya arkhitektura i stroitelstvo, 2015, no. 2 (23), pp. 27–36.
15. Startsev O.V., Krotov A.S., Startseva L.T. Interlayer shear strength of polymer composite materials during long term climatic aging. Polymer Degradation and Stability, 1999, vol. 63, pp. 183-186.
16. Startsev V.O. Across-the-thickness gradient of the interlaminar shear strength of a CFRP after its long-term exposure to a marine climate. Mechanics of Composite Materials, 2016, vol. 52, no. 2, pp. 171-176.
17. Startseva L.T. Climatic aging of organic fiber reinforced plastics. Mechanics of Composite Materials, 1994, vol. 29, no. 6, pp. 620-626.
18. Startsev O.V., Isupov V.V., Nikishin E.F. The Gradient of Mechanical Characteristics Across the Thickness of Composite Laminates After Exposure to a Low Earth Orbit Environment. Polymer Composites, 1998, vol. 19.No. 1, pp. 65–70.
19. Roylance D., Roylance M. Weathering of fiber-reinforced epoxy composites. Polymer Engineering and Science, 1978, vol. 18.No. 4, pp. 249–254.
20. Belec L., Nguyen T.H., Nguyen D.L., Chailan J.F. Comparative effects of humid tropical weathering and artificial aging on a model composite properties from nano- to macro-scale. Composites, part A, 2015, vol. 68, no. 1, pp. 235–241.
21. de Bruijn J.C.M., Meijer H.D.F. The design and application of a microfoil tensile test apparatus for monitoring the degree of ultraviolet degradation of polymers. Review of Scientific Instruments. 1991, no. 62, pp. 1620-1623.
22. de Bruijn J.C.M. Degradation profiles of thick high-density polyethylene samples after outdoor and artificial weathering. Polymer durability: degradation, stabilization, and lifetime prediction. Washington: American Chemical Society, 1996, pp. 599-620.
23. Gu X., Dickens B., Stanley D. et al. Linking accelerating laboratory test with outdoor performance results for a model epoxy coating system. Iowa State University. 2008, pp. 1–47.
24. Panin S.V., Startsev V.O., Course M.G., Varchenko E.A. Development of methods of climatic testing of materials for mechanical engineering and construction at the GTSKI VIAM im. G.V. Akimova. Vse materialy. Entsiklopedicheskiy spravochnik, 2016, no. 10, pp. 50–61.
25. Kablov E.N. Structural composite materials. Moscow: VIAM, 2012, 58 p.
26. Muhametov R.R., Petrova A.P., Ponomarenko S.A., Ahmadieva K.R., Pavlyuk B.F. Influence of woven fibrous fillers of various types on properties of cured binder VS-2526K). Trudy VIAM, 2018, no. 3 (63), paper no. 04. Available at: http//www.viam-works.ru (accessed: February 28, 2020). DOI: 10.18577/2307-6046-2018-0-3-28-36.
27. Gulyaev I.N., Zelenina I.V., Raskutin A.E. Carbon plastics based on imported carbon fabrics and Russian mortar binders. Voprosy materialovedeniya, 2014, no. 1 (77), pp. 116–125.
28. Raskutin A.E. Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
29. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R. Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis Part 2. Substantiation of the choice of modes and conducting heat aging of polymeric composite materials based on epoxy matrix. Trudy VIAM, 2016, no. 1 (37), paper no. 10. Available at: http://www.viam-works.ru (accessed: February 28, 2020). DOI: 10.18577/2307-6046-2016-0-1-80-89.
30. Platonov A.A., Dushin M.I. Carbon composites VKU-25 based on unidirectional prepregs. Trudy VIAM, 2015, no. 11, paper no. 06. Available at: http://www.viam-works.ru (accessed: February 28, 2020). DOI: 10.18577/2307-6046-2015-0-11-6-6.
31. Iskhodzhanova I.V., Bondarenko Yu.A., Lapteva M.A. Evaluation of the structure of monocrystalline Ni superalloys derived in different conditions of directional solidification using methods of quantitative analysis of video images. Trudy VIAM, 2015, no. 12, paper no. 06. Available at: http://www.viam-works.ru (accessed: February 28, 2020). DOI: 10.18577/2307-6046-2015-0-12-6-6.
32. Tarnapolsky Yu.M., Kintsis T.Ya. Methods for static testing of reinforced plastics. 3rd ed. Moscow: Khimiya, 1981, 272 p.
33. Amelina E.V., Golushko S.K., Erasov V.S., Idimeshev S.V., Nemirovsky Yu.V., Semisalov B.V., Yurchenko A.V., Yakovlev N.O. On nonlinear deformation of carbon plastics: experiment, model, calculation. Vychislitelnye tekhnologii, 2015, vol. 20, no. 5, pp. 27–52.
34. Gunyaeva A.G., Veshkin E.A., Antyufeeva N.V., Panafidnikova A.N., Efimik V.A. Research of influence of the condensation moisture on carbon fiber plastic prepreg on the basis of solution epoxy binder and PСM on its basis. Trudy VIAM, 2019, no. 9 (81), paper no. 09. Available at: http://www.viam-works.ru (accessed: February 28, 2020). DOI: 10.18577 / 2307-6046-2019-0-9-80-88.
35. de Verdiere M.C, Skordos A.A., Walton A. Characterization of Reinforced Carbon Composites with Full Field Measurements: Long Gauge Length Compressive Apparatus. Open Journal of Composite Materials, 2013, vol. 03, no. 1, pp. 7–15.
36. Sevostianov I., Sookay N.K., von Klemperer C.J., Verijenko V.E. Environmental degradation using functionally graded material approach. Composite Structure, 2003, vol. 62, no. 3-4, pp. 417–421.
37. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. 1. Assessment of the influence of significant influencing factors. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16.
The cold spray allows to develop coatings on different materials, and to give them wide set of functional properties. Besides this method of drawing coverings allows to recover the geometrical sizes of the details damaged in use and to carry out recovery of protective corrosion preventive coatings without labor-consuming dismantle of design. Simplicity and technological effectiveness of process, mobility of installations for drawing coatings by cold spray, allows to apply this method as in industrial conditions using the robotized systems, and in «field» conditions.
2. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
3. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
4. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
5. Vinogradov S.S., Nikiforov A.A., Demin S.A., Chesnokov D.V. Protection against corrosion of carbon steel. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 242–263. DOI: 10.18577/2071-9140-2017-0-S-242-263.
6. Abiev R.Sh., Bibik E.E., Vlasov E.A. et al. New reference book of chemist and technologist. Electrode processes. Chemical kinetics and diffusion. Colloidal chemistry. Saint Petersburg: Professional, 2004, 838 p.
7. Koktsinskaya E.M., Roshal A.G. et al. Aging Tests of the High Current Aluminum–Copper Contact Connections in the ITER DC Busbar System. IEEE Transactions on Plasma Science, 2014, vol. 42, is. 3, pp. 443–448.
8. Kosarev V.F., Alkhimov A.P. Technology, equipment, tools. Obrabotka metallov, 2003, no. 3, pp. 28-30
9. Alkhimov A.P., Gulidov A.I., Kosarev V.F., Nesterovich N.I. Features of deformation of microparticles upon impact on a solid obstacle. Prikladnaya mekhanika i tekhnicheskaya fizika, 2000, vol. 41, no. 1, pp. 204–209.
10. Alkhimov A.P., Klinkov S.V., Kosarev V.F., Fomin V.M. Cold gas-dynamic spraying. Theory and practice. Moscow: Fizmatlit, 2010, 536 p.
11. Katanoda H., Fukuhara M., Iino N. Numerical study of combination parameters for particle impact velocity and temperature in cold spray. Journal of Thermal Spray Technology, 2007, vol. 16. No. 5–6, pp. 627–633. DOI: 10.1007/s11666-007-9087-7.
12. Alkhimov A.P., Kosarev V.F., Papyrin A.N. Method of «cold» gas-dynamic spraying. Doklady Akademii nauk SSSR, 1990, vol. 315, no. 5, pp. 1062–1065.
13. Device for spraying coating: pat. 1674585 Rus. Federation; filed 19.10.89; publ. 15.05.93.
14. Gas dynamic spraying method for applying a coating: pat. US5302414A; filed 19.05.90; publ. 12.04.94.
15. Champagne V., Helfritch D. A demonstration of the antimicrobial effectiveness of various copper surfaces. Journal of Biological Engineering, 2013, vol. 7, pp. 1–8. Available at: www.jbioleng.org/content/7/1/8 (accessed: March 15, 2020).
16. Rokni M.R., Nutt S.R., Widener C.A. et al. Review of relationship between particle deformation, coating microstructure, and properties in high-pressure cold spray. Journal of Thermal Spray Technology, 2017, vol. 26, pp. 1–6.
17. Irissou E., Legoux J.-G., Ryabinin A. et al. Review of cold spray process and technology: part I – intellectual property. Journal of Thermal Spray Technology, 2008, vol. 17, no. 4, pp. 495–516.
18. Moridi A., Hassani-Gangaraj S., Guagliano M., Dao M. Cold spray coating: review of material systems and future perspectives. Surface Engineering, 2014, vol. 36, no. 6, pp. 369–395.
19. Gärtner F., Stoltenhoff T., Schmidt T., Kreye H. The cold spray process and its potential for industrial applications. Journal of Thermal Spray Technology, 2006, vol. 15, no. 2, pp. 223–232.
20. Champagne V., Helfritch D. Mainstreaming cold spray – push for Applications. Surface Engineering, 2014, vol. 30, no. 6, pp. 396–403.
21. Van Steenkiste T., Smith J. Evaluation of coatings produced via kinetic and cold spray processes. Journal of Thermal Spray Technology, 2004, vol. 13, no. 2, pp. 274–282.
22. Marx S., Paul A., Köhler A., Hüttl G. Cold spraying: innovative layers for new applications. Journal of Thermal Spray Technology, 2006, vol. 15, no. 2, pp. 177–183.
23. Champagne V., Helfritch D. The unique abilities of cold spray deposition. International Materials Reviews, 2016, vol. 61 (7), pp. 437–455. DOI: 10.1080/09506608.2016.1194948.
24. Champagne V., Helfritch D., Leyman P., Grendahl S., Klotz B. Interface material mixing formed by the deposition of copper on aluminum by means of the cold spray process. Journal of Thermal Spray Technology, 2005, vol. 14, no. 3, pp. 330–334.
25. Champagne V., Helfritch D., Dinavahi S., Leyman P. Theoretical and experimental particle velocity in cold spray. Journal of Thermal Spray Technology, 2011, vol. 20, no. 3, pp. 425–431.
26. Ning X.-J., Jang J.-H., Kim H.-J. The effects of powder properties on in-flight particle velocity and deposition process during low pressure cold spray process. Applications, Surface Engineering, 2007, vol. 253, no. 18, pp. 7449–7455.
27. Jodoin B., Raletz F., Vardelle M. Cold spray modeling and validation using an optical diagnostic method. Surface and Coatings Technology, 2006, vol. 200, is. 14–15, pp. 4424–4432.
28. Schmidt T., Assadi H., Gartner F. et al. From particle acceleration to impact and bonding in cold spraying. Journal of Thermal Spray Technology, 2009, vol. 18, no. 5–6, pp. 794–808.
29. Lupoi R. Current design and performance of cold spray nozzles: experimental and numerical observations on deposition efficiency and particle velocity. Surface Engineering, 2014, vol. 30, no. 5, pp. 316–322.
30. Assadi H., Schmidt T., Richter H. et al. On parameter selection in cold spraying. Journal of Thermal Spray Technology, 2011, vol. 20, no. 6, pp. 1161–1176.
31. Li W.-Y., Liao H., Douchy G., Coddet C. Optimal design of a cold spray nozzle by numerical analysis of particle velocity and experimental validation with 316L stainless steel powder. Materials and Design, 2007, vol. 28, no. 7, pp. 2129–2137.
32. Li W.-Y., Liao H., Wang H.-T. et al. Optimal design of a convergent-barrel cold spray nozzle by numerical method. Applied Surface Science, 2006, vol. 253, pp. 708–713.
33. Huang G., Gu D., Li X. et al. Numerical simulation on syphonage effect of laval nozzle for low pressure cold spray system. Journal of Materials Processing Technology, 2014, vol. 214. P. 2497–2504.
34. Dykhuizen R.C., Smith M.F. Gas dynamic principles of cold spray. Journal of Thermal Spray Technology, 1998, vol. 7, no. 2, pp. 205–212.
35. Li W.Y., Zhang D.D., Huang C.J. et al. Modelling of impact behaviour of cold spray particles: review. Surface Engineering, 2014, vol. 30, no. 5, pp. 299–308.
36. Li W.Y., Zhang C., Li C.J., Liao H.L. Modelling aspects of high velocity impact of particles in cold spraying by explicit finite element analysis. Journal of Thermal Spray Technology, 2009, vol. 18, no. 5–6, pp. 921–933.
37. Rahmati S., Ghaei A. The use of particle/substrate material models in simulation of cold-gas dynamic-spray process. Journal of Thermal Spray Technology, 2014, vol. 23, no. 3, pp. 530–540.
38. King P., Bae G., Zahiri S. et al. An experimental and finite element study of cold spray copper impact onto two aluminum substrates. Journal of Thermal Spray Technology, 2010, vol. 19, no. 3, pp. 620–634.
39. Assadi H., Gartner F., Stoltenhoff T., Kreye H. Bonding mechanism in cold gas spraying. Acta Materialia, 2003, vol. 51, no. 15, pp. 4379–4394.
40. Ghelichi R., Bagherifard S., Guagliano M., Verani M. Numerical simulation of cold spray coating. Surface and Coatings Technology, 2011, vol. 205, pp. 5294–5301.
41. Moridi A., Hassani-Gangaraj S.M., Guagliano M. A hybrid approach to determine critical and erosion velocities in the cold spray process. Applied Surface Science, 2013, vol. 273, pp. 617–624.
42. Vucko M.J., King P.C., Poole A.J. et al. Cold spray metal embedment: an innovative antifouling technology. The Journal of Bioadhesion and Biofilm Research, 2012, vol. 28, no. 3, pp. 239–248.
43. King P., Vucko M., Poole A. et al. Cold spray antifouling of marine seismic streamers, CSIRO Wealth From Oceans Flagship. Available at: https://publications.csiro.au/rpr/download?pid=csiro:EP124574&dsid=DS1 (accessed: 07.03.2020).
44. Tapphorn R., Henness J., Gabel H. Direct write of antenna aperstructures and electronic interconnects using kinetic metallization. Proceedings of the International Thermal Spray Conference. Las Vegas, 2009, pp. 589–595.
45. Helfritch D., Champagne V. Electromagnetic interference shielding by cold spray deposition. Journal of Advanced Materials, 2008, vol. 40, no. 1, pp. 20–26.
46. Rastjagaev E., Wilde J., Wielage B. et al. Development and testing of cold gas sprayed circuit boards for power electronics applications. Proceedings of 7th International Conference on Integrated Power Electronics Systems. Nuremberg, 2012, pp. 154–159.
47. Ajdelsztajn L., Jodoin B., Richer P. et al. Cold gas dynamic spraying of iron-base amorphous alloy. Journal of Thermal Spray Technology, 2006, vol. 15, no. 4, pp. 495–500.
48. Henao J., Concustell A., Cano I. et al. Influence of cold gas spray process conditions on the microstructure of Fe-based amorphous coatings. Journal of Alloys and Compounds, 2015, vol. 622, pp. 995–999.
49. Lee K.A., Jung D.J., Park D.Y. et al. Study on the fabrication and physical properties of cold sprayed, Cu-based amorphous coating. Journal of Physics: Conference Series, 2009, vol. 144, pp. 12–15.
50. Koh P.K., Cheang P., Loke K. et al. Deposition of amorphous aluminium powder using cold spray. Thermal Spray 2012: Proceedings from the International Thermal Spray Conference and Exposition, Houston, 2012, pp. 22–24.
51. Li C.-J., Yang G.-J., Gao P.-H. et al. Characterization of nanostructured WC-codeposited by cold spraying. Journal of Thermal Spray Technology, 2007, vol. 16, no. 5–6, pp. 1011–1020.
52. De Force B., Eden T., Potter J. Cold spray Al-5% Mg coatings for the corrosion protection of magnesium alloys. Journal of Thermal Spray Technolog, 2011, vol. 20, no. 6, pp. 1352–1358.
53. Method of obtaining a coating on a steel plate: pat. 2621088 Rus. Federation; filed 30.03.16; publ. 31.05.17.
54. Method of coating a steel base: pat. 2542196 Rus. Federation; filed 19.12.13; publ. 20.02.15.
55. Wear-corrosion-resistant aluminum-based alloy for nanostructured coatings: pat. 2413024 Rus. Federation; filed 16.11.09; publ. 27.02.11.
56. Alloy, in particular for a bearing coating: pat. US8147981; filed 19.11.10; publ. 03.04.12.
57. A method of spraying particles for obtaining a multilayer material by the method of cold gas-dynamic spraying: pat. DE102006047101; filed 31.05.10; publ. 01.12.11.
58. Wang H.-R., Hou B.-R., Wang J. et al. Effect of process conditions on microstructure and corrosion resistance of cold-sprayed Ti coatings. Journal of Thermal Spray Technology, 2008, vol. 17, no. 5– 6, pp. 736–741.
59. Barbosa M., Cinca N., Dosta S., Guillemany J.M. Cold spray deposition of titanium onto aluminium alloys. Science and Technology of Materials, 2010, vol. 22, no. 1–2, pp. 48–56.
60. Zhang Y.Y., Wu X.K., Cui H., Zhang J.S. Cold-spray processing of a high density nanocrystalline aluminum alloy 2009 coating using a mixture of as-atomized and as-cryomilled powders. Journal of Thermal Spray Technology, 2011, vol. 20, pp. 1125–1132.
61. Novoselova T., Fox P., Morgan R., O’Neill W. Experimental study of titanium/aluminium deposits produced by cold gas dynamic spray. Surface and Coatings Technology, 2006, vol. 200, pp. 2775–2783.
62. Kong L.Y., Shen L., Lu B. et al. Preparation of TiAl3-Al composite coating by cold spray and its high temperature oxidation behavior. Journal of Thermal Spray Technology, 2010, vol. 19. P. 1206–1210.
63. Lee H., Shin H., Ko K. Effects of gas pressure of cold spray on the formation of Al-based intermetallic compound. Journal of Thermal Spray Technology, 2010, vol. 19, pp. 102–109.
64. Liang Y., Shi B., Yang X. et al. Microstructure and nano-mechanical property of cold spray Co-base refractory alloy coating. Acta Metallurgica Sinica (English Letters), 2011, vol. 24, pp. 190–194.
65. Al-Mangour B., Mongrain R., Irissou E., Yue S. Improving the strength and corrosion resistance of 316L stainless steel for biomedical applications using cold spray. Surface and Coatings Technology, 2013, vol. 216, pp. 297–307.
66. Kang H.-K., Kang S.B. Tungsten/copper composite deposits produced by a cold spray. Scripta Materialia, 2003, vol. 49, pp. 1169–1174.
67. King P.C., Zahiri S.H., Jahedi M.Z. Rare earth/metal composite formation by cold spray. Journal of Thermal Spray Technology, 2008, vol. 17, pp. 221–227.
68. Bu H., Yandouzi M., Lu C. et al. Cold spray blended Al+Mg17Al12 coating for corrosion protection of AZ91D magnesium alloy. Surface and Coatings Technology, 2012, vol. 207, pp. 155–162.
69. Feng C., Guipont V., Jeandin M. et al. 4C/Ni Composite coatings prepared by cold spray of blended or CVD-coated powders. Journal of Thermal Spray Technology, 2012, vol. 21, pp. 561–570.
70. Sun L., Berndt C.C., Gross K.A., Kucuk A. Material fundamentals and clinical performance of plasma-sprayed hydroxyapatite coatings: a review. Journal of Biomedical Materials Research, 2001, vol. 58, pp. 570–592.
71. Choudhuri A., Mohanty P. S., Karthikeyan J. Bio-ceramic composite coatings by cold spray technology. International Thermal Spray Conference, 2009, pp. 391–396.
72. Cho S., Takagi K., Kwon H. et al. Multi-walled carbon nanotube-reinforced copper nanocomposite coating fabricated by low-pressure cold spray process. Surface and Coatings Technology, 2012, vol. 206, pp. 3488–3494.
73. Seo D., Sayar M., Ogawa K. SiO2 and MoSi2 formation on Inconel 625 surface via SiC coating deposited by cold spray. Surface and Coatings Technology, 2012, vol. 206, pp. 2851–2858.
74. Lee H.Y., Yu Y.H., Lee Y.C. et al. Thin film coatings of WO3 by cold gas dynamic spray: a technical note. Journal of Thermal Spray Technology, 2005, vol. 14, pp. 183–186.
75. Yang G.-J., Li C.-J., Han F. et al. Low temperature deposition and characterization of TiO2 photocatalytic film through cold spray. Applied Surface Science, 2008, vol. 254, pp. 3979–3982.
76. Lupoi R., O’Neill W. Deposition of metallic coatings on polymer surfaces using cold spray. Surface and Coatings Technology, 2010, vol. 205, pp. 2167–2173.
77. Zhou X.L., Chen A.F., Liu J.C. et al. Preparation of metallic coatings on polymer matrix composites by cold spray. Surface and Coatings Technology, 2011, vol. 206, pp. 132–136.
78. Affi J., Okazaki H., Yamada M., Fukumoto M. Fabrication of aluminum coating onto CFRP substrate by cold spray. Materials Transactions, 2011, vol. 52, pp. 1759–1763.
79. Lee J.H., Jang H.L., Lee K.M. et al. In vitro and in vivo evaluation of the bioactivity of hydroxyapatite-coated polyetheretherketone biocomposites created by cold spray technology. Acta Biomaterialia, 2013, vol. 9, pp. 6177–6187.
80. Kumar K., Van Swygenhoven H., Suresh S. Mechanical behavior of nanocrystalline metals and alloys. Acta Materialia, 2003, vol. 51, pp. 5743–5774.
81. Dao M., Lu L., Asaro R. et al. Toward a quantitative understanding of mechanical behavior of nanocrystalline metals. Acta Materialia, 2007, vol. 55, pp. 4041–4065.
82. Metal spraying technology. Available at: https://dimet.info/catalog/avtomatizirovannye-kompleksy-/kompleks-dimet-c5/ (accessed: March 20, 2020).
83. Obninsk Powder Coating Center. Available at: http://dymet.net/ (accessed: March 22, 2020).
84. Liu L.M., Wang Z., Song G. Study on corrosion resistance properties of hydrothermal sealed arc sprayed aluminium coating. Surface Engineering, 2010, vol. 26, pp. 399–406.
85. Equipment and technology. Available at: http://www.dimet-r.narod.ru/application.html (accessed: March 27, 2020).
The article is devoted to issues in the field of creation of radar absorbing materials (RAM) in order to solve the problem of electromagnetic compatibility (EMC) in modern aircrafts. The characteristics of a number of RAM developed at FSUE «VIAM» are provided that are designed to ensure coordination and operability of aircraft antenna systems and to provide EMC for on-board radio-electronic equipment in the microwave range. The materials presented in the work differ in their overall dimensions, operating frequency range, method of attachment (application/installation) and have different purposes for use on aircrafts.
2. Klyagin V.A., Petrova I.A., Shkurin M.V. Analysis of the placement of airborne radio-electronic equipment units on airplanes of various types. Trudy MAI, 2017, no. 95. Available at: http://www.trudymai.ru/published.php?ID=84442 (accessed: November 01, 2019).
3. Koptev A.N. Aviation and radio-electronic equipment of civil aviation aircraft. Samara: SSAU Publishing House, 2011, 196 p.
4. Bespalova E.E., Belyaev A.A., Shirokov V.V. Radar-absorbing materials for protection against high power microwave radiation. Trudy VIAM, 2015, no. 3, paper no. 07. Available at: http://www.viam-works.ru (accessed: November 1, 2019). DOI: 10.18577/2307-6046-2015-0-3-7-7.
5. Romanov A.M., Belyaev A.A., Shirokov V.V. Peculiar features of optimization of resonant radar-absorbing materials of nonmagnetic type. Trudy VIAM, 2014, no. 11, paper no. 05. Available at: http://www.viam-works.ru (accessed: November 1, 2019). DOI: 10.18577/2307-6046-2014-0-11-5-5.
6. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy, ser.: Chemistry and Chemical Technology, 2016, vol. 59, no. 10, pp. 61–71.
7. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
8. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing - the basis of innovation. Krylya rodiny, 2016, no. 5, pp. 8-18.
9. Bogush V.A., Borbotko T.V., Gusinsky A.V. et al. Electromagnetic radiation. Methods and means of protection. Minsk: Bestprint, 2003.401 p.
10. Mikhailin Yu.A. Special polymer materials. Saint Petersburg: Nauchnye osnovy i tekhnologii, 2008, 660 p.
11. Alekseev A.G., Shtager E.A., Kozyrev S.V. Physical foundations of stealth technology. Saint Petersburg: VVM, 2007, 284 p.
12. Kovneristy Yu.K., Lazarev I.Yu., Ravaeva A.A. Materials that absorb microwave radiation. Moscow: Nauka, 1982, 162 p.
13. Kazantseva N.E., Ryvkina N.G., Chmutin I.A. Promising materials for absorbers of microwave electromagnetic waves. Radiotekhnika i elektronika, 2003, vol. 48, no. 2, pp. 196–209.
14. Simamura S., Shindo A., Kotsuka K. et al. Carbon fibers. Moscow: Mir, 1987, 304 p.
15. Fitzer E. Carbon fibers and carbon composites. Moscow: Mir, 1988, 336 p.
16. Devin K.L., Bortsov A.N., Devin E.A. Gradient absorber of electromagnetic waves. Perspektivnyye materialy, 2018, no. 9, pp. 79–84.
17. Bespalova E.E., Belyaev A.A., Romanov A.M., Shirokov V.V. Investigation of the dielectric characteristics of designed for anechoic chambers laminated radar absorbing material layers based with carbonized fiber filled foam asbestos. Trudy VIAM, 201, no. 8, paper no. 12. Available at: http://www.viam-works.ru (accessed: November 1, 2019). DOI: 10.18577/2307-6046-2014-0-8-12-12.
18. Agafonova A.S., Belyaev A.A., Kondrashov E.K., Romanov A.M. Features of the formation of monolithic structural radio absorbing materials based on composites filled with resistive fibers. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 56–59.
19. Berkhovskikh L.M. Waves in layered media. Moscow: Nauka, 1973, 343 p.
The content of 19 elements (B, Al, Si, P, Ti, Cr, Fe, Co, Ni, Zr, Nb, Mo, Hf, Ta, W, Se, As, Pb, Bi) in the samples of nickel alloys was determined by high resolution glow discharge mass spectrometry. The selection of analysis conditions is given. Spectral interference is eliminated by the use of high resolution. The correctness of the results obtained is confirmed by analysis of a certified standard samples of nickel alloy. The range of determined concentrations: 0,000002–53,4% (of the mass), the relative standard deviation does not exceed 0,05.
2. Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
3. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72−103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
4. Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
5. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRM and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
6. State Standard 6689.5–92. Nickel, nickel and copper-nickel alloys. Methods for the determination of iron. Moscow: Gosstandart of Russia. 1992, pp. 1–5.
7. State Standard 6689.12–92. Nickel, nickel and copper-nickel alloys. Methods for the determination of magnesium. Moscow: Gosstandart of Russia, 1992, pp. 1–5.
8. State Standard 6689.6–92. Nickel, nickel and copper-nickel alloys. Methods for the determination of manganese. Moscow: Gosstandart of Russia, 1992, pp. 9–11.
9. Dvoretskov R.M., Karachevtsev F.N., Zagvozdkina T.N., Mechanic E.A. Determination of alloying elements of nickel alloys for aviation use by the AES-ICP method in combination with microwave sample preparation. Zavodskaya laboratoriya. Diagnostika materialov, 2013, vol. 79, no. 9, pp. 6–9.
10. ASTM E2594-09. Standard Test Method for Analysis of Nickel Alloys by Inductively Coupled Plasma Atomic Emission Spectrometry. 2014, pp. 1–9.
11. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS. Mikrochimica Acta, 2001, vol. 137, pp. 149–155.
12. Letov A.F., Karachevtsev F.N., Zagvozdkina T.N. Development the set of methods measurements of the chemical composition of nickel-based alloys. Trudy VIAM, 2018, no. 8 (68), paper no. 09. Available at: http://www.viam-works.ru (accessed: March 23, 2020). DOI: 10.18577/2307-6046-2018-0-8-89-97.
13. Pupyshev A.A., Epova E.N. Spectral interference of polyatomic ions in the method of mass spectrometry with inductively coupled plasma. Analitika i kontrol, 2001, vol. 5, no. 4, pp. 335–369.
14. ASTM F2405-04. Standard Test Method for Trace Metallic Impurities in High Purity Copper by High-Mass-Resolution Glow Discharge Mass Spectrometer, 2011. pp. 1–5.
15. Yakimovich P.V., Alekseev A.V. Determination of sulfur in casting heat-resistant nickel alloys by GD-MS. Trudy VIAM, 2020, no. 1, paper no. 11. Available at: http://www.viam-works.ru (accessed: March 23, 2020). DOI: 10.18557/2307-6046-2020-0-1-101-108.
Рresents a review of various numerical methods use for modeling of the ice deformation and brittle fracture. The application of the finite element method, smoothed particle hydrodynamics, and the discrete element method is considered. The paper deals with modeling of sea and freshwater ice, impact, explosive loading, three-point and four-point bending, compression, contact interaction «ship–ice» and «support–ice», falling from a height, and the use of reinforcement etc.
2. Oreshko E.I., Erasov V.S., Lutsenko A.N. Mathematical modeling of deformation constructional carbon fiber at a bend. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 50–59. DOI: 10.18577/2071-9140-2016-2-50-59.
3. Oreshko E.I., Erasov V.S., Podzhivotov N.Yu., Lutsenko A.N. Strength calculation of hybrid wing panel on the basis of sheets and profiles from high-strength aluminum lithium alloy and laminated aluminum fiberglass. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 53–61. DOI: 10.18577/2071-9140-2016-0-1-53-61.
4. Yakovlev N.O., Grinevich D.V., Mazalov P.B. Mathematical modeling of the stress-strain state during compression of a mesh structure synthesized by the method of selective laser fusion. Vestnik MGTU im. N.E. Baumana, ser.: Natural sciences, 2018, no. 6 (81), pp. 113–127. DOI: 10.18698/1812-3368-2018-6-113-127.
5. Dynkin A.A., Vernikovsky V.A., Dobretsov N.L., Buznik V.M., Kablov E.N. et al. Scientific and technical problems of the development of the Arctic. Moscow: Nauka, 2015, 490 p.
6. Buznik V.M., Kablov E.N. State and prospects of Arctic materials science. Vestnik RAN, 2017, vol. 87, no. 9, pp. 827–839.
7. Kablov E.N. New generation materials – the basis for innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
8. Lavrov V.V. Deformation and strength of ice. Leningrad: Gidrometeoizdat, 1969, 206 p.
9. Sea ice: a reference guide. Saint Petersburg: Gidrometeoizdat, 1997, 402 p.
10. Kablov E.N. Materials are the basis of any business. Delovaya slava Rossii, 2013, no. 2 (40), pp. 4–9.
11. Pounder E. Ice Physics. Moscow: Mir, 1967, 189 p.
12. Grinevich D.V., Nuzhny G.A., Buznik V.M., Yakovlev N.O., Goncharova G.Yu., Razomasov N.D. Fracture of reinforced ice composite materials under flexural mechanical loading. Materialovedenie, 2020, no. 1, pp. 18–24.
13. Cherepanov G.P. Brittle fracture mechanics. Moscow: Nauka, 1974, 640 p.
14. Erasov V.S., Oreshko E.I., Lucenko A.N. Area of a free surface as criterion of brittle fracture. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 69–79. DOI: 10.18577/2071-9140-2017-0-2-69-79.
15. Lobanov V.A. Simulation of ice in problems with a finite element formulation. Differential equations and control processes, 2008, no. 4. Available at: https://diffjournal.spbu.ru/RU/numbers/2008.4/article.1.2.html (accessed: April 20, 2020).
16. Balandin V.V., Krylov S.V., Poverennov E.Yu., Sadovsky V.V. Numerical modeling of the shock interaction of an elastic cylinder with ice. Problems of Strength and Plasticity, 2017, vol. 79, no. 1, pp. 93–103. DOI: 10.32326/1814-9146-2017-79-1-93-103.
17. Balandin V.V., Bragov A.M., Glazova E.G., Konstantinov A.Yu., Kochetkov A.V., Krylov S.V. Numerical-experimental study of ice shock loading processes. Polar mechanics: materials of the Third Intern. conf. Vladivostok, 2016, pp. 293–305.
18. Glazyrin VP, Orlova Yu.N., Orlov M.Yu., Poverennov E.Yu. Calculation of the process of introducing a large-sized striker into polycrystalline ice. Izvestiya vysshikh uchebnykh zavedenij, ser.: Physics, 2012, vol. 55, no. 9/3, pp. 42–45.
19. Orlova Yu.N., Orlov M.Yu. Study of the process of explosive loading of ice. Vestnik Tomskogo gosudarstvennogo universiteta, ser.: Mathematics and Mechanics, 2015, no. 6 (38), pp. 81–89.
20. Glazyrin V.P., Orlov M.Yu., Orlova Yu.N. Investigation of ice behavior during impact and explosion. Materials, technologies and equipment for the development of the Arctic and Siberia: collection of articles abstracts III Int. conf. Tomsk: Publishing house of Tomsk State University, 2019, p. 13.
21. Kozin V.M., Vasiliev A.S., Zemlyak V.L., Ipatov K.I. Investigation of the limiting state of the ice cover in conditions of pure bending with reinforcement with reinforcing elements. Vestnik Tomskogo gosudarstvennogo universiteta, ser .: Mathematics and Mechanics, 2019, no. 61, pp. 61–69.
22. Ipatov K.I., Vasiliev A.S., Zemlyak V.L., Leskov E.V. Load-bearing capacity of ice cover during surface reinforcement. Vestnik ISH DVFU, 2019, no. 3 (40), pp. 3–12.
23. Leskov E.V., Ipatov K.I., Vasiliev A.S., Zemlyak V.L. Investigation of the use of basalt and carbon composites for surface reinforcement of ice crossings. Vestnik PGU im. Sholom-Aleykhema, 2018, no. 1 (30), pp. 59–63.
24. Taranukha N.A., Vasiliev A.S. Analysis of the criteria for the limiting state of structures made of composite materials. Uchenye zapiski Komsomolskogo-na-Amure gosudarstvennogo tekhnicheskogo universiteta, 2015, vol. 1, no. 3 (23), pp. 81–87.
25. Ehlers S., Kujala P. Optimization-based material parameter identification for the numerical simulation of sea ice in four-point bending. Journal of Engineering for the Maritime Environment, 2013, no. 228, pp. 70–80. DOI: 10.1177/1475090213486892.
26. Herrnring H., Kellner L., Kubiczek J., Ehlers S. Simulation of Ice-Structure Interaction with CZM-Elements. 2018. Available at: https://www.researchgate.net/publication/328611406_Simulation_of_Ice-Structure_Interaction_with_CZM-Elements (accessed: April 20, 2020).
27. Herrnring H., Kellner L., Kubiczek J., Ehlers S. A cohesive model for ice and its verification with tensile splitting tests, 2019. Available at: https://www.dynalook.com/conferences/12th-european-ls-dyna-conference-2019/adhesive-rivets/03_herrnring_tuhh.pdf (accessed: April 20, 2020).
28. Nisja H.A. Numerical Modeling of Brittle Failure in Ice Structures: Master thesis. Norwegian University of Science and Technology, 2014. Available at: https://ntnuopen.ntnu.no/ntnu-xmlui/handle/11250/237581 (accessed: April 20, 2020).
29. Hallquist J.O. LS-DYNA Theory Manual. Livermore Software Technology Corporation, 2006, 680 p.
30. Gagnon R.E. A numerical model of ice crushing using a foam analogue. Cold Regions Science and Technology, 2011, no. 65 (3), pp. 335–350. DOI: 10.1016/j.coldregions.2010.11.004.
31. Gagnon R.E., Derradji-Aouat A. First results of numerical simulations of bergy bit collisions with the CCGS Terry Fox Icebreaker. IAHR. 2006, no. 49 (3), pp. 206–214. DOI: 10.1016/j.coldregions.2007.03.016.
32. Gagnon R.E., Wang J. Numerical simulations of a tanker collision with a bergy bit incorporating hydrodynamics, a validated ice model and damage to the vessel. Cold Regions Science and Technology, 2012, no. 81, pp. 26–35.
33. Holmquist T.J., Johnson G.R., Cook W.H. A computational constitutive model for concrete subjected to large strains, high strain rates, and high pressures. The 14th International Symposium on Ballistic, 1993, pp. 591–600.
34. Von Bock P.R., Ehlers S. Model scale ice – part B: Numerical model. Cold Regions Science and Technology, 2013, no. 94, pp. 74–81.
35. Tomac T., Klanac A., Katalinić M. et al. Numerical simulations of ship resistance in model ice. Developments in Maritime Transportation and Exploitation of Sea Resources, 2013, pp. 847–851. DOI: 10.1201/b15813-106.
36. Oreshko E.I., Erasov V.S., Lutsenko A.N. Calculation features of cores and plates stability. Aviacionnye materialy i tehnologii, 2016, no. 4 (45), pp. 74–79. DOI: 10.18577/2071-9140-2016-0-4-74-79.
37. Monaghan J.J. Smoothed particle hydrodynamics. Annual Review of Astronomy and Astrophysics, 1992, vol. 30, is. 1, pp. 543–574.
38. Benz W., Asphaug E. Simulations of brittle solids using smooth particle hydrodynamics. Computer Physics Communications, 1995, vol. 87, is. 1-2, pp. 253–265.
39. Deb D., Pramanik R. Failure process of brittle rock using smoothed particle hydrodynamics. Journal of Engineering Mechanics, 2013, vol. 139, is. 11, pp. 1551–1565.
40. Gray J.P., Monaghan J.J., Swift R.P. SPH elastic dynamics. Computer Methods in Applied Mechanics and Engineering, 2001, vol. 190 (49–50), pp. 6641–6662. DOI: 10.1016/s0045-7825(01)00254-7.
41. Zhang N., Zheng X., Ma Q. Updated Smoothed Particle Hydrodynamics for Simulating Bending and Compression Failure Progress of Ice. Water, 2017, no. 9 (11), pp. 3–24. DOI: 10.3390/w9110882.
42. Zhang N., Zheng X., Ma Q., Hu Z. A numerical study on ice failure process and ice-ship interactions by Smoothed Particle Hydrodynamics. International Journal of Naval Architecture and Ocean Engineering, 2019, vol. 11, is. 2, pp. 796–808.
43. Tsvetkov D.O. Small motions of an ideal stratified fluid partially covered with elastic ice. Vestnik Udmurtskogo Universitets, ser.: Mathematics. Mechanics. Computer science, 2018, vol. 28, is. 3, pp. 328–347. DOI: 10.20537/vm180305.
44. Pan W., Tartakovsky A., Monaghan J. A smoothed-particle hydrodynamics model for ice-sheet and ice-shelf dynamics. Journal of Glaciology, 2012, no. 58 (208), pp. 216–222. DOI: 10.3189/2012JoG11J084.
45. Staroszczyk R. SPH Modeling of Sea-ice Pack Dynamics. Archives of Hydro-Engineering and Environmental Mechanics, 2017, no. 64 (2), pp. 115–137. DOI: 10.1515/heem-2017-0008.
46. Shen H.T., Su J.Sh., Lin L.W. SPH Simulation of River Ice Dynamics. Journal of Computational Physics, 2000, vol. 165, is. 2, pp. 752–770.
47. Alder B.J., Wainwright T.E. Phase Transition for a Hard Sphere System. The Journal of Chemical Physics, 1957, no. 27 (5), pp. 1208–1209. DOI: 10.1063/1.1743957.
48. Cundall P.A. The measurement and analysis of accelerations in rock slopes: PhD thesis. Imperial College London, 1971, 237 p.
49. Williams J.R., Hocking G., Mustoe G.G.W. The Theoretical Basis of the Discrete Element Method. Proceedings from Conference Numerical Methods of Engineering, Theory and Applications, 1985, pp. 897–906.
50. Cundall P.A. A discrete numerical model for granular assemblies. Géotechnique, 1979, no. 29 (1), pp. 47–65. DOI: 10.1680/geot.1979.29.1.47.
51. Potyondy D.O., Cundall P.A. A bonded-particle model for rock. Journal of Rock Mechanics and Minimg Sciences, 2004, no. 41, pp. 1329–1364.
52. Ji S., Di S., Long X. DEM Simulation of Uniaxial Compressive and Flexural Strength of Sea Ice: Parametric Study. Journal of Engineering Mechanics, 2017, no. 143 (1), pp. 4–11. DOI: 10.1061/(asce) em.1943-7889.0000996.
53. Ji S. Discrete element modeling of ice loads on ship and offshore structures. Proceedings of the 7th International Conference on Discrete Element Methods, 2017, no. 188, pp. 45–54. DOI: 10.1007/978-981-10-1926-5_6.
54. Hisette Q., Alekseev A., Seidel J. Discrete Element Simulation of Ship Breaking Through Ice Ridges. Proceedings from the 27th International Ocean and Polar Engineering Conference. International Society of Offshore and Polar Engineers, 2017, pp. 1–15.
55. Neto A.V. Improvement of Rubble Ice Generation in Numerical Simulation of Ice Ridge and Structure Interaction: Master thesis, Liège: Université de Liège, 2017, 77 p. Available at: https://matheo.uliege.be/handle/2268.2/4432 (accessed: April 04, 2020).
56. Polojärvi A. Sea ice ridge keel punch through experiments: model experiments and numerical modeling with discrete and combined finite-discrete element methods: thesis, PhD. Aalto University. Finland, 2013, 60 p. Available at: https: //aaltodoc.aalto.fi/bitstream/handle/123456789/8957/isbn9789526050829.pdf?sequence=1&isAllowed= y (accessed: April 04, 2020).
57. Tuhkuri J., Polojärvi A. A review of discrete element simulation of ice-structure interaction. Philosophical transactions, ser. A: Mathematical, physical, and engineering sciences, 2018, no. 376 (2129), article no. 20170335. DOI: 10.1098/rsta.2017.0335 Available at: https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6107613/ (accessed: April 04, 2020).
Operational characteristics of currently created materials and products of aviation equipment. Such conditions, especially in the winter period, largely correspond to the quality of clothes and shoes. The paper presents the results of experimental studies of the thermal conductivity of different types of insoles for shoes. Physical and mathematical models of heat transfer are proposed when a person moves from a warm room to the street. The thermal insulation ability of three types of insoles for shoes was studied and time is shown.
2. Zhitnyuk S.V. Oxygen-free ceramic materials for the space technics (review) Trudy VIAM, 2018, no. 8 (68), paper no. 8. Available at: http://www.viam-works.ru (accessed: June 17, 2020). DOI: 10.18577/2307-6046-2018-0-8-81-88.
3. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577 / 2071-9140-2020-0-1-3-11.
4. Gunyaev G.M., Chursova L.V., Komarova O.A., Raskutin A.E., Gunyaeva A.G. Structural polymer carbon-nanocomposites – a new direction of materials science. Vse materialy. Entsiklopedicheskiy spravochnik, 2011, no. 12, pp. 2–9.
5. Armor for «Buran». Materials and technologies of VIAM for the ISS «Energia–Buran». Ed. E.N. Kablov. Moscow: Nauka i zhizn, 2013,128 p.
6. Eliseev O.A., Naumov I.S., Smirnov D.N., Bryk Ya.A. Rubbers, sealants, fireproof and heat-shielding materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 437–451. DOI: 10.18577/2071-9140-2017-0-S-437-451.
7. Nefedov N.I., Semenova L.V., Kuznecova V.A., Vereninova N.P. Paint coatings for protection of metallic and polymer composite materials against aging, corrosion and biodeterioration. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 393–404. DOI: 10.18577/2071-9140-2017-0-S-393-404.
8. Kolyadov E.V., Mezhin Yu.A. Automation of the technological process of single-crystal castings of superalloys on UVNK type installations. Trudy VIAM, 2016, no. 4, paper no. 4. Available at: http://www.viam-works.ru (accessed: June 20, 2020). DOI: 10.18577/2307-6046-2016-0-4-32-40.
9. Medical and sanitary unit of the Ministry of Internal Affairs of Russia in the Saratov region: officer. website of the Federal State Healthcare Institution. Available at: https://xn--l1aks.64.xn--b1aew.xn--p1ai/document/6654393 (accessed: June 17, 2020).
10. Insoles. Their types and functions. Available at: https://gutboot.ru/poleznye-stati/307-stelki-ikh-vidy-i-funktsii.html (accessed: June 17, 2020).
11. ASTM E 1461-01. Standard Test Method for Thermal Diffusivity by the Flash Method. 2001, pp. 1– 13.
12. State Standard R 57943–2017. Plastics. Determination of thermal conductivity and thermal diffusivity. Part 4. Laser flash method. Moscow: Standartinform, 2017, 11 p.
13. Blumm J., Opfermann J. Improvement of the mathematical modeling of flash measurements. High Temperatures – High pressures. 2002, vol. 34, pp. 515–521. DOI: 10.1068/htjr061.
14. State Standard 7076–99. Building materials and products. Method for determination of thermal conductivity and thermal resistance under stationary thermal conditions. Moscow: Gosstroy of Russia, GUP TsPP, 2000, 22 p.
15. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
16. Isachenko V.P., Osipova V.A., Sukomel A.S. Heat transfer: a textbook for universities. 4th ed. Moscow: Energoizdat, 1981, 416 p.
17. Technical tables. Human physics. Heat dissipation of a person depending on the type of load. Dry and latent heat. Available at: http://tehtab.ru/Guide/Engineers/HumanBeing/MetabolicHeatGain / (accessed: June 17, 2020).
18. Introduction to COMSOL Multiphysics. 2018, 216 p. Available at: https://cdn.comsol.com/doc/5.4/IntroductionToCOMSOLMultiphysics.ru_RU.pdf (accessed: June 17, 2020).