Phase composition and structure of hydrogenated titanium alloy VT6 after vacuum annealing
UDC
669.295.615.46
DOI
10.18577/2307-6046-2016-0-2-5-5
Article PDF (Russian)
(1001.16 KB)
How to cite
Panin P.V., Dzunovich D.А., Alexeev E.B. Phase composition and structure of hydrogenated titanium alloy VT6 after vacuum annealing // Proceedings of VIAM. 2016. No. 2. DOI: 10.18577/2307-6046-2016-0-2-5-5. URL: https://www.viam-works.ru/en/journal/2016/2/5
Keywords
titanium alloy VT6, hydrogen doping, thermo-hydrogen treatment, vacuum annealing, phase composition, structure.
Abstract
Phase composition and structure analyses have been carried out on hydrogenated samples of VT6 (Ti–6,25Al–4,1V, wt.%) titanium alloy after low-temperature vacuum annealing. It has been shown that nanoscale α-phase particles can precipitate in (α+β)-structure upon low-temperature vacuum annealing if preceding hydrogenation process was ended in β-area and as a result a single β-phase structure was kinetically achieved at room temperature.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn. 2010. №4. S. 2–7.
- Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Nochovnaya N.A. Perspektivy i problemy primeneniya titanovyh splavov [Perspectives and problems of application of titanium alloys] / V sb. Aviacionnye materialy i tehnologii. Vyp. «Perspektivy razvitiya i primeneniya titanovyh splavov dlya samoletov, raket, dvigatelej i sudov»: sb. dokladov yubilejnogo soveshhaniya, posvyashhennogo 55-letiyu titanovoj laboratorii VIAM. M.: VIAM. 2007. S. 4–8.
- Horev A.I. Fundamentalnye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravleniya ih razvitiya [Fundamental and applied works on structural titanium alloys and perspective directions of their development] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 04. Available at: http://www.viam-works.ru (accessed: July 14, 2015).
- Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Ekonomnolegirovannye titanovye splavy dlya sloistyh metallopolimernyh kompozicionnyh materialov [Low-cost alloyed titanium alloys for metal-polymer laminates] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. Available at: http://www.viam-works.ru (accessed: July 14, 2015). DOI: 10.18577/2307-6046-2014-0-11-2-2.
- Ilin A.A., Kolachev B.A., Nosov V.K., Mamonov A.M. Vodorodnaya tehnologiya titanovyh splavov [Hydrogen technology of titanium alloys]. M.: Izdatelskij dom MISiS, 2002. 392 s.
- Panin P.V., Dzunovich D.A., Alekseev E.B. Sposoby opisaniya fazovogo sostava titanovyh splavov, dopolnitelno legirovannyh vodorodom (obzor) [Ways of phase areas representation in titanium alloys additionally doped with hydrogen (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 03. Available at: http://www.viam-works.ru (accessed: July 14, 2015). DOI: 10.18577/2307-6046-2015-0-3-3-3.
- Panin P.V., Shiryaev A.A., Dzunovich D.A. Postroenie temperaturno-koncentracionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitelno legirovannogo vodorodom [Creation of the temperature and concentration chart of phase composition of the VT6 titanium alloy which has been in addition alloyed by hydrogen] // Tehnologiya mashinostroeniya. 2014. №3. S. 5–9.
- Ilin A.A., Skvorcova S.V., Mamonov A.M., Kollerov M.Yu. Fazovye i strukturnye prevrashheniya v titanovyh splavah raznyh klassov pod dejstviem vodoroda [Phase and structural transformations in titanium alloys of different classes under the influence of hydrogen] // Titan. 2007. №1. S. 32–37.
- Skvortsova S.V., Panin P.V., Nochovnaya N.A., Grushin I.A., Mitropolskaya N.G. Vliyanie vodoroda na fazovye i strukturnye prevrashheniya v titanovom splave VT6 [Influence of hydrogen on phase and structural transformations in BT6 titanium alloy] //Tehnologiya legkih splavov. 2011. №4. S. 35–40.
- Skvortsova S.V., Panin P.V., Dzunovich D.A., Zasypkin V.V., German M.A. Sozdanie kompozitnoj struktury v titanovom splave Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Creation of composite structure in Ti-6Al titanium alloy by means of thermohydrogen treating] / V sb. tezisov dokladov VII Mezhdunarodnogo ajerokosm. kongressa (IAC’12). M.: MGU im. M.V. Lomonosova, 2012. S. 197–198.
- Panin P.V., Dzunovich D.A., Zasypkin V.V. Sozdanie dvuhfaznoj kompozitnoj struktury v alfa-splave Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Creation of diphasic composite structure in Ti–6Al alpha alloy by means of thermohydrogen treating] // Nauchnye trudy (Vestnik MATI). 2012. №19 (91). S. 33–37.
- Panin P.V., Lukina E.A., Dzunovich D.A., German M.A. Preobrazovanie struktury titanovogo splava Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Transformation of structure of Ti-6Al titanium alloy by means of thermohydrogen treating] / V sb. materialov Vserossijskoj nauch.-tehnich. konf. «Novye materialy i tehnologii – 2012». M.: MATI. 2012. S. 83–84.
- Panin P.V., Grushin I.A., Mitropolkaya N.G. Issledovanie zakonomernostej izmeneniya strukturno-fazovogo sostoyaniya titanovogo splava VT6 pri dopolnitelnom legirovanii vodorodom [Research of patterns of change of structural and phase condition of BT6 titanium alloy at additional alloying hydrogen] // Nauchnye trudy (Vestnik MATI). 2013. №20 (92). S. 31–34.
- Ilin A.A., Skvortsova S.V., Panin P.V., Shalin A.V. Vliyanie termovodorodnoj obrabotki i plasticheskoj deformacii na strukturoobrazovanie v titanovyh splavah raznyh klassov [Influence of thermohydrogen treating and plastic strain on structurization in titanium alloys of different classes] //Aviacionnaya promyshlennost. 2009. №4. S. 31–36.
- Ovchinnikov A.V., Nosov V.K., Afonin V.E., Panin P.V. Osnovnye zakonomernosti deformacii splavov titan-vodorod [Main patterns of deformation of alloys titanium-hydrogen] // Tehnologiya legkih splavov. 2007. №3. S. 96–99.
- Panin P.V., Dzunovich D.A., Lukina E.A. Upravlenie strukturoj i svojstvami titanovyh splavov pri obratimom legirovanii vodorodom i plasticheskoj deformacii [Management of structure and properties of titanium alloys at reversible alloying hydrogen and plastic strain] / V sb. materialov XIX nauch.-tehnich. konf. molodyh uchenyh i specialistov RKK «Energiya». Ser. XII. 2012. Vyp. 1–2. S. 103–107.
- Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] // Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33.
- Panin P.V. Zakonomernosti formirovaniya fazovogo sostava i struktury v titanovyh splavah pri termovodorodnoj obrabotke i plasticheskoj deformacii [Patterns of forming of phase structure and structure in titanium alloys at thermohydrogen treating and plastic strain]: avtoref. dis. … kand. tekhn. nauk. M., 2009. 24 s.