Phase composition and structure of hydrogenated titanium alloy VT6 after vacuum annealing

Panin P.V., Dzunovich D.А., Alexeev E.B.
Panin P.V., Dzunovich D.А., Alexeev E.B. Phase composition and structure of hydrogenated titanium alloy VT6 after vacuum annealing // Proceedings of VIAM. 2016. No. 2. DOI: 10.18577/2307-6046-2016-0-2-5-5. URL: https://www.viam-works.ru/en/journal/2016/2/5
Keywords
titanium alloy VT6, hydrogen doping, thermo-hydrogen treatment, vacuum annealing, phase composition, structure.
Abstract

Phase composition and structure analyses have been carried out on hydrogenated samples of VT6 (Ti–6,25Al–4,1V, wt.%) titanium alloy after low-temperature vacuum annealing. It has been shown that nanoscale α-phase particles can precipitate in (α+β)-structure upon low-temperature vacuum annealing if preceding hydrogenation process was ended in β-area and as a result a single β-phase structure was kinetically achieved at room temperature.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn. 2010. №4. S. 2–7.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Nochovnaya N.A. Perspektivy i problemy primeneniya titanovyh splavov [Perspectives and problems of application of titanium alloys] / V sb. Aviacionnye materialy i tehnologii. Vyp. «Perspektivy razvitiya i primeneniya titanovyh splavov dlya samoletov, raket, dvigatelej i sudov»: sb. dokladov yubilejnogo soveshhaniya, posvyashhennogo 55-letiyu titanovoj laboratorii VIAM. M.: VIAM. 2007. S. 4–8.
  5. Horev A.I. Fundamentalnye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravleniya ih razvitiya [Fundamental and applied works on structural titanium alloys and perspective directions of their development] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 04. Available at: http://www.viam-works.ru (accessed: July 14, 2015).
  6. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Ekonomnolegirovannye titanovye splavy dlya sloistyh metallopolimernyh kompozicionnyh materialov [Low-cost alloyed titanium alloys for metal-polymer laminates] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. Available at: http://www.viam-works.ru (accessed: July 14, 2015). DOI: 10.18577/2307-6046-2014-0-11-2-2.
  7. Ilin A.A., Kolachev B.A., Nosov V.K., Mamonov A.M. Vodorodnaya tehnologiya titanovyh splavov [Hydrogen technology of titanium alloys]. M.: Izdatelskij dom MISiS, 2002. 392 s.
  8. Panin P.V., Dzunovich D.A., Alekseev E.B. Sposoby opisaniya fazovogo sostava titanovyh splavov, dopolnitelno legirovannyh vodorodom (obzor) [Ways of phase areas representation in titanium alloys additionally doped with hydrogen (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 03. Available at: http://www.viam-works.ru (accessed: July 14, 2015). DOI: 10.18577/2307-6046-2015-0-3-3-3.
  9. Panin P.V., Shiryaev A.A., Dzunovich D.A. Postroenie temperaturno-koncentracionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitelno legirovannogo vodorodom [Creation of the temperature and concentration chart of phase composition of the VT6 titanium alloy which has been in addition alloyed by hydrogen] // Tehnologiya mashinostroeniya. 2014. №3. S. 5–9.
  10. Ilin A.A., Skvorcova S.V., Mamonov A.M., Kollerov M.Yu. Fazovye i strukturnye prevrashheniya v titanovyh splavah raznyh klassov pod dejstviem vodoroda [Phase and structural transformations in titanium alloys of different classes under the influence of hydrogen] // Titan. 2007. №1. S. 32–37.
  11. Skvortsova S.V., Panin P.V., Nochovnaya N.A., Grushin I.A., Mitropolskaya N.G. Vliyanie vodoroda na fazovye i strukturnye prevrashheniya v titanovom splave VT6 [Influence of hydrogen on phase and structural transformations in BT6 titanium alloy] //Tehnologiya legkih splavov. 2011. №4. S. 35–40.
  12. Skvortsova S.V., Panin P.V., Dzunovich D.A., Zasypkin V.V., German M.A. Sozdanie kompozitnoj struktury v titanovom splave Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Creation of composite structure in Ti-6Al titanium alloy by means of thermohydrogen treating] / V sb. tezisov dokladov VII Mezhdunarodnogo ajerokosm. kongressa (IAC’12). M.: MGU im. M.V. Lomonosova, 2012. S. 197–198.
  13. Panin P.V., Dzunovich D.A., Zasypkin V.V. Sozdanie dvuhfaznoj kompozitnoj struktury v alfa-splave Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Creation of diphasic composite structure in Ti–6Al alpha alloy by means of thermohydrogen treating] // Nauchnye trudy (Vestnik MATI). 2012. №19 (91). S. 33–37.
  14. Panin P.V., Lukina E.A., Dzunovich D.A., German M.A. Preobrazovanie struktury titanovogo splava Ti–6Al s pomoshhyu termovodorodnoj obrabotki [Transformation of structure of Ti-6Al titanium alloy by means of thermohydrogen treating] / V sb. materialov Vserossijskoj nauch.-tehnich. konf. «Novye materialy i tehnologii – 2012». M.: MATI. 2012. S. 83–84.
  15. Panin P.V., Grushin I.A., Mitropolkaya N.G. Issledovanie zakonomernostej izmeneniya strukturno-fazovogo sostoyaniya titanovogo splava VT6 pri dopolnitelnom legirovanii vodorodom [Research of patterns of change of structural and phase condition of BT6 titanium alloy at additional alloying hydrogen] // Nauchnye trudy (Vestnik MATI). 2013. №20 (92). S. 31–34.
  16. Ilin A.A., Skvortsova S.V., Panin P.V., Shalin A.V. Vliyanie termovodorodnoj obrabotki i plasticheskoj deformacii na strukturoobrazovanie v titanovyh splavah raznyh klassov [Influence of thermohydrogen treating and plastic strain on structurization in titanium alloys of different classes] //Aviacionnaya promyshlennost. 2009. №4. S. 31–36.
  17. Ovchinnikov A.V., Nosov V.K., Afonin V.E., Panin P.V. Osnovnye zakonomernosti deformacii splavov titan-vodorod [Main patterns of deformation of alloys titanium-hydrogen] // Tehnologiya legkih splavov. 2007. №3. S. 96–99.
  18. Panin P.V., Dzunovich D.A., Lukina E.A. Upravlenie strukturoj i svojstvami titanovyh splavov pri obratimom legirovanii vodorodom i plasticheskoj deformacii [Management of structure and properties of titanium alloys at reversible alloying hydrogen and plastic strain] / V sb. materialov XIX nauch.-tehnich. konf. molodyh uchenyh i specialistov RKK «Energiya». Ser. XII. 2012. Vyp. 1–2. S. 103–107.
  19. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] // Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33.
  20. Panin P.V. Zakonomernosti formirovaniya fazovogo sostava i struktury v titanovyh splavah pri termovodorodnoj obrabotke i plasticheskoj deformacii [Patterns of forming of phase structure and structure in titanium alloys at thermohydrogen treating and plastic strain]: avtoref. dis. … kand. tekhn. nauk. M., 2009. 24 s.