Nitrogen removal from complex-alloyed melts based on nickel in process of decarburization
Rigin V.E., Sidorov V.V., Burtsev V.T. Nitrogen removal from complex-alloyed melts based on nickel in process of decarburization // Proceedings of VIAM. 2016. No. 1. DOI: 10.18577/2307-6046-2016-0-1-10-16. URL: https://www.viam-works.ru/en/journal/2016/1/2
Abstract
It is found that in the process of decarburization of complex-alloyed nickel melts nitrogen is released together with the carbon to form the CO compound. As a melt alloying increases the denitride effect decreales. The intensity of denitride process during melt decarboning favours transition of [С]+[О]=СОg reaction in bubble mode («carbon boiling process»), that achieved by preliminary introduction carbon in melt and correspending increase of nickel oxide quantity.
Reference list
- Kablov E.N., Logunov A.V., Sidorov V.V. Obespechenie ultravysokoj chistoty metalla – garantiya kachestva litejnyh zharoprochnyh splavov [Ensuring ultrahigh purity of metal – quality assurance of foundry hot strength alloys] // Metally. 2000. №6. S. 40–46.
- Kablov E.N., Logunov A.V., Sidorov V.V. Mikrolegirovanie RZM – sovremennaya tehnologiya povysheniya svojstv litejnyh zharoprochnyh nikelevyh splavov [RZM microalloying – modern technology of increase of properties of cast heat resisting nickel alloys] // Perspektivnye materialy. 2001. №1. S. 23–34.
- Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh) zagotovok iz sovremennyh litejnyh vysokozharoprochnyh splavov. Ekaterinburg: Izdatelskij dom «IzdatNaukaServis», 2011. S. 31–38.
- Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Features of smelting technology and razlivka of modern cast high-heat resisting nickel alloys] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 68–78.
- Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
- Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Meethman G.W. Trance elements in superalloys-an overview // Metals Technol. 1984. V. 11. №10. P. 414–418.
- Strangman T.E., Hoppin G.S., Phipps C.M. Development of exothermically cast single-crystal MAR-M247 and derivative alloys / In: Superalloys. 1980. P. 215–224.
- Durber G., Osgerby S. Effect of small amounts of nitrogen and silicon on microstructure and prepertis of MAR-M200 nickel-base superalloys // Metals Technol. 1984. V. 11. №4. P. 129–137.
- Quested P.N., Gibbon T.B., Durber G.L.R. Nickel-base superalloys: physical metallurgy of recycling // Proc. AGARD Conf. «Materials substitution and recycling». Vimerio. 1983. P. 389–402.
- Mitchel A., Tripp D.W. Higt temperature materials for power engineering 1990. Part II // Proceedings of a Conference held in Liege. Belgium. 1990. P. 1665–1673.
- Erickson G.L. The development and application of CMSX-10 / Presented at the of the Second Pacific Rum International Conference on Advanced Materials and Processing (PRJCM-2), occurring. Kyongju. 1995.
- Kablov D.E., Sidorov V.V., Min P.G. Vliyanie primesi azota na strukturu monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i razrabotka effektivnyh sposobov ego rafinirovaniya [Influence of impurity of nitrogen on structure of monocrystals of heat resisting ZhS30-VI nickel alloy and development of effective ways of its refinement] // Aviacionnye materialy i tehnologii. 2012. №2. S. 32–36.
- Kablov D.E., Chabina E.B., Sidorov V.V., Min P.G. Issledovanie vliyaniya azota na strukturu i svojstva monokristallov iz litejnogo zharoprochnogo splava ZhS30-VI [Research of influence of nitrogen on structure and properties of monocrystals from foundry ZhS30-VI hot strength alloy] // MiTOM. 2013. №8. S. 3–7.
- Kablov D.E., Sidorov V.V., Min P.G. Zakonomernosti povedeniya azota pri poluchenii monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i ego vliyanie na ekspluatacionnye svojstva [Patterns of behavior of nitrogen when receiving monocrystals of heat resisting ZhS30-VI nickel alloy and its influence on operational properties] // MiTOM. 2014. №1. S. 8–12.
- Linchevskij B.V. Vakuumnaya metallurgiya stali i splavov [Vacuum metallurgy of steel and alloys]. M.: Metallurgiya, 1970. 258 s.
- Grigoryan V.A., Belyanchikov L.N., Stomahin A.Ya. Teoreticheskie osnovy elektrostaleplavilnyh processov [Theoretical bases of electrosteel-smelting processes]. M.: Metallurgiya, 1987. 272 s.
- Sobolevskij A.L. Raskislenie i degazacija nerzhavejushhej stali pri vakuumnoj plavke [Deoxidation and decontamination of stainless steel at vacuum melting]: avtoref. dis. … kand. tehn. nauk. M.: MVMI, 1968. 16 s.
- Butskij E.V. Issledovanie povedeniya azota v zharoprochnyh splavah na nikelevoj osnove [Research of behavior of nitrogen in hot strength alloys on nickel basis]: avtoref. dis. … kand. tehn. nauk. M.: MISiS, 1975. 24 s.
- Fedorchenko V.I. Kinetika i termodinamika vzaimodejstviya azota s rasplavami na osnove zheleza i nikelya [Kinetics and thermodynamics of interaction of nitrogen with alloys on the basis of iron and nickel]: avtoref. dis. … kand. tehn. nauk. M.: IMET, 1969. 22 s.
- Belyanchikov L.N., Valen P. i dr. Opredelenie limitirujushhego zvena processa deazotacii nikelevyh rasplavov v vakuume [Definition of limiting link of process of de nitrogen nickel alloys in vacuum] // Izvestiya vuzov. Ser. «Chernaya metallurgiya». 1986. №9. S. 31–19.
- Cidorov V.V., Burcev V.T., Rigin V.E. Issledovanie processov obezuglerozhivanija slozhnolegirovannyh nikelevyh rasplavov v vakuume [Research of processes of decarbonization complex-alloyed nickel alloys in vacuum] / V sb. nauch. tr. «Fundamentalnye issledovaniya fizikohimii metallicheskih rasplavov». M.: IKC «Akademkniga». 2002. S. 364–370.
- Sidorov V.V., Rigin V.E. Issledovanie tehnologicheskogo processa obezuglerozhivanija mnogokomponentnyh rasplavov na osnove nikelya [Research of technological process of decarbonization multicomponent alloys on the basis of nickel] / V sb.: Aviacionnye materialy i tehnologii. Vyp. «Tehnologiya proizvodstva aviacionnyh metallicheskih materialov». M.: VIAM, 2002. S. 108–115.
- Averin V.V., Revjakin A.V. i dr. Vzaimodejstvie azota s metallicheskimi rasplavami [Nitrogen interaction with metal rasplavami] / V sb.: «Fiziko-himicheskie osnovy metallurgicheskih processov». M.: Nauka, 1973. S. 201–210.
- Kablov E.N. i dr. Vakuumnaya indukcionnaya plavilno-razlivochnaya ustanovka VIAM–2002 dlya polucheniya vysokokachestvennyh specsplavov [The vacuum induction VIAM-2002 melting and barreling unit for receiving high-quality special alloys ] // Elektrometallurgiya. 2004. №5. S. 24–26.