Nitrogen removal from complex-alloyed melts based on nickel in process of decarburization

Rigin V.E., Sidorov V.V., Burtsev V.T.
Rigin V.E., Sidorov V.V., Burtsev V.T. Nitrogen removal from complex-alloyed melts based on nickel in process of decarburization // Proceedings of VIAM. 2016. No. 1. DOI: 10.18577/2307-6046-2016-0-1-10-16. URL: https://www.viam-works.ru/en/journal/2016/1/2
Abstract

It is found that in the process of decarburization of complex-alloyed nickel melts nitrogen is released together with the carbon to form the CO compound. As a melt alloying increases the denitride effect decreales. The intensity of denitride process during melt decarboning favours transition of [С]+[О]=СОg reaction in bubble mode («carbon boiling process»), that achieved by preliminary introduction carbon in melt and correspending increase of nickel oxide quantity.

Reference list
  1. Kablov E.N., Logunov A.V., Sidorov V.V. Obespechenie ultravysokoj chistoty metalla – garantiya kachestva litejnyh zharoprochnyh splavov [Ensuring ultrahigh purity of metal – quality assurance of foundry hot strength alloys] // Metally. 2000. №6. S. 40–46.
  2. Kablov E.N., Logunov A.V., Sidorov V.V. Mikrolegirovanie RZM – sovremennaya tehnologiya povysheniya svojstv litejnyh zharoprochnyh nikelevyh splavov [RZM microalloying – modern technology of increase of properties of cast heat resisting nickel alloys] // Perspektivnye materialy. 2001. №1. S. 23–34.
  3. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh) zagotovok iz sovremennyh litejnyh vysokozharoprochnyh splavov. Ekaterinburg: Izdatelskij dom «IzdatNaukaServis», 2011. S. 31–38.
  4. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Features of smelting technology and razlivka of modern cast high-heat resisting nickel alloys] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 68–78.
  5. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  6. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  7. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  8. Meethman G.W. Trance elements in superalloys-an overview // Metals Technol. 1984. V. 11. №10. P. 414–418.
  9. Strangman T.E., Hoppin G.S., Phipps C.M. Development of exothermically cast single-crystal MAR-M247 and derivative alloys / In: Superalloys. 1980. P. 215–224.
  10. Durber G., Osgerby S. Effect of small amounts of nitrogen and silicon on microstructure and prepertis of MAR-M200 nickel-base superalloys // Metals Technol. 1984. V. 11. №4. P. 129–137.
  11. Quested P.N., Gibbon T.B., Durber G.L.R. Nickel-base superalloys: physical metallurgy of recycling // Proc. AGARD Conf. «Materials substitution and recycling». Vimerio. 1983. P. 389–402.
  12. Mitchel A., Tripp D.W. Higt temperature materials for power engineering 1990. Part II // Proceedings of a Conference held in Liege. Belgium. 1990. P. 1665–1673.
  13. Erickson G.L. The development and application of CMSX-10 / Presented at the of the Second Pacific Rum International Conference on Advanced Materials and Processing (PRJCM-2), occurring. Kyongju. 1995.
  14. Kablov D.E., Sidorov V.V., Min P.G. Vliyanie primesi azota na strukturu monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i razrabotka effektivnyh sposobov ego rafinirovaniya [Influence of impurity of nitrogen on structure of monocrystals of heat resisting ZhS30-VI nickel alloy and development of effective ways of its refinement] // Aviacionnye materialy i tehnologii. 2012. №2. S. 32–36.
  15. Kablov D.E., Chabina E.B., Sidorov V.V., Min P.G. Issledovanie vliyaniya azota na strukturu i svojstva monokristallov iz litejnogo zharoprochnogo splava ZhS30-VI [Research of influence of nitrogen on structure and properties of monocrystals from foundry ZhS30-VI hot strength alloy] // MiTOM. 2013. №8. S. 3–7.
  16. Kablov D.E., Sidorov V.V., Min P.G. Zakonomernosti povedeniya azota pri poluchenii monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i ego vliyanie na ekspluatacionnye svojstva [Patterns of behavior of nitrogen when receiving monocrystals of heat resisting ZhS30-VI nickel alloy and its influence on operational properties] // MiTOM. 2014. №1. S. 8–12.
  17. Linchevskij B.V. Vakuumnaya metallurgiya stali i splavov [Vacuum metallurgy of steel and alloys]. M.: Metallurgiya, 1970. 258 s.
  18. Grigoryan V.A., Belyanchikov L.N., Stomahin A.Ya. Teoreticheskie osnovy elektrostaleplavilnyh processov [Theoretical bases of electrosteel-smelting processes]. M.: Metallurgiya, 1987. 272 s.
  19. Sobolevskij A.L. Raskislenie i degazacija nerzhavejushhej stali pri vakuumnoj plavke [Deoxidation and decontamination of stainless steel at vacuum melting]: avtoref. dis. … kand. tehn. nauk. M.: MVMI, 1968. 16 s.
  20. Butskij E.V. Issledovanie povedeniya azota v zharoprochnyh splavah na nikelevoj osnove [Research of behavior of nitrogen in hot strength alloys on nickel basis]: avtoref. dis. … kand. tehn. nauk. M.: MISiS, 1975. 24 s.
  21. Fedorchenko V.I. Kinetika i termodinamika vzaimodejstviya azota s rasplavami na osnove zheleza i nikelya [Kinetics and thermodynamics of interaction of nitrogen with alloys on the basis of iron and nickel]: avtoref. dis. … kand. tehn. nauk. M.: IMET, 1969. 22 s.
  22. Belyanchikov L.N., Valen P. i dr. Opredelenie limitirujushhego zvena processa deazotacii nikelevyh rasplavov v vakuume [Definition of limiting link of process of de nitrogen nickel alloys in vacuum] // Izvestiya vuzov. Ser. «Chernaya metallurgiya». 1986. №9. S. 31–19.
  23. Cidorov V.V., Burcev V.T., Rigin V.E. Issledovanie processov obezuglerozhivanija slozhnolegirovannyh nikelevyh rasplavov v vakuume [Research of processes of decarbonization complex-alloyed nickel alloys in vacuum] / V sb. nauch. tr. «Fundamentalnye issledovaniya fizikohimii metallicheskih rasplavov». M.: IKC «Akademkniga». 2002. S. 364–370.
  24. Sidorov V.V., Rigin V.E. Issledovanie tehnologicheskogo processa obezuglerozhivanija mnogokomponentnyh rasplavov na osnove nikelya [Research of technological process of decarbonization multicomponent alloys on the basis of nickel] / V sb.: Aviacionnye materialy i tehnologii. Vyp. «Tehnologiya proizvodstva aviacionnyh metallicheskih materialov». M.: VIAM, 2002. S. 108–115.
  25. Averin V.V., Revjakin A.V. i dr. Vzaimodejstvie azota s metallicheskimi rasplavami [Nitrogen interaction with metal rasplavami] / V sb.: «Fiziko-himicheskie osnovy metallurgicheskih processov». M.: Nauka, 1973. S. 201–210.
  26. Kablov E.N. i dr. Vakuumnaya indukcionnaya plavilno-razlivochnaya ustanovka VIAM–2002 dlya polucheniya vysokokachestvennyh specsplavov [The vacuum induction VIAM-2002 melting and barreling unit for receiving high-quality special alloys ] // Elektrometallurgiya. 2004. №5. S. 24–26.