Evaluation of the structure of monocrystalline Ni superalloys derived in different condi-tions ofdirectional solidification using methods of quantitative analysis of video images
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2015-0-12-6-6
Article PDF (Russian)
(1.8 MB)
How to cite
Iskhodzhanova I.V., Bondarenko Yu.A., Lapteva M.A. Evaluation of the structure of monocrystalline Ni superalloys derived in different condi-tions ofdirectional solidification using methods of quantitative analysis of video images // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-6-6. URL: https://www.viam-works.ru/en/journal/2015/12/6
Keywords
quantitative analysis of video images, methods to assess the geometric characteristics and volume fraction, porosity, directional solidification.
Abstract
The article presents a research on development of methods to assess the geometric characteristics and volume fraction of porosity, the geometric characteristics and volume fraction of eutectic (γ-γ)ʹ-phase, and the geometric characteristics of particles of the hardening γʹ-phase in monocrystalline Ni superalloys ZhS32U-VI. The results of investigations on proposed methods of quantitative metallographic analysis of blanks from the ZhS32U-VI superalloy, derived by directional solidification from the melt in different temperature gradient are presented.
Reference list
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya [Cast blades of gas turbine engines: alloys, technologies, coverings] /Pod obshh. red. E.N. Kablova. 2-e izd. M.: Nauka. 2006. 632 s.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N., Petrushin N.V., Svetlov I.L. Kompyuternoe konstruirovanie zharoprochnogo nikelevogo splava IV pokoleniya dlya monokristallicheskih lopatok gazovyh turbin [Computer designing of heat resisting nickel alloy IV of generation for single-crystal blades of gas turbines] /V kn. Litejnye zharoprochnye splavy. Effekt S.T. Kishkina. M.: Nauka. 2006. S. 98–116.
- Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
- Bondarenko Yu.A., Kablov E.N., Morozova G.I. Vliyanie vysokogradientnoj napravlennoj kristallizacii na strukturu i fazovyj sostav zharoprochnogo splava tipa Rene N5 [Influence of the high-gradient directed crystallization on structure and phase composition of hot strength alloy of the Rene N5 type] //MiTOM. 1999. №2. S. 15–18.
- Bondarenko Yu.A., Kablov E.N. Napravlennaya kristallizaciya zharoprochnyh splavov s povyshennym temperaturnym gradientom [The directed crystallization of heat resisting alloys with the raised temperature gradient] //MiTOM. 2002. №7. S. 20–23.
- Bondarenko Yu.A., Echin A.B., Surova V.A., Narskij A.R. Vliyanie temperaturnogo gradienta na fronte rosta na strukturu zharoprochnogo splava pri napravlennoj kristallizacii [Influence of temperature gradient at the front growth on hot strength alloy structure at the directed crystallization] //Litejshhik Rossii. 2014. №5. S. 24–27.
- Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of single crystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
- Kablov E.N., Orlov M.R., Ospennikova O.G. Mehanizmy obrazovaniya poristosti v monokristallicheskih lopatkah turbiny i kinetika ee ustraneniya pri goryachem izostaticheskom pressovanii [Mechanisms of formation of porosity in single crystals turbine blades and kinetics of its elimination at hot isostatic pressing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 117–129.
- Zharoprochnyj splav na osnove nikelja [Heat resisting alloy on the basis of nickel]: pat. 2148099 Ros. Federaciya; opubl. 18.01.99. Byul. №12.
- Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and x-ray of the structural analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
- Svetlov I.L., Ishodzhanova I.V., Evgenov A.G., Naprienko S.A. Issledovanie vysokotemperaturnoj polzuchesti i defektnosti struktury monokristallov nikelevogo zharoprochnogo splava posle gorjachego izostaticheskogo pressovaniya [Research of high-temperature creep and deficiency of structure of single crystals of nickel hot strength alloy after hot isostatic pressing] //Deformaciya i razrushenie materialov. 2011. №3. S. 28–32.
- Nejman A.V., Filonova E. V., Ishodzhanova I. V. O lokalnoj rekristallizacii v monokristallah nikelevyh zharoprochnyh splavov [About local re crystallization in monocrystals of nickel hot strength alloys] //Metallurgiya i mashinostroenie. 2013. №1. S. 19–22.
- Sidorov V.V., Ishodzhanova I.V., Rigin V.E., Folomejkin Yu.I. Ocenka effektivnosti filtracii pri razlivke slozhnolegirovannogo nikelevogo rasplava [Assessment of efficiency of filtering at razlivka complex-alloyed nickel rasplava] //Elektrometallurgiya. 2011. №11. S. 17–21.
- Klark E.R., Eberhardt K.N. Mikroskopicheskie metody issledovaniya materialov [Microscopic methods of research of materials]. M.: Tehnosfera. 2007. 376 s.
- Gulyaev A.I., Ishodzhanova I.V., Zhuravleva P.L. Primenenie metoda opticheskoj mikroskopii dlya kolichestvennogo analiza struktury PKM [Application of optical microscopy method for the quantitative analysis of polymer composite material structure] //Trudy VIAM. 2014. №7. St. 07 (viam-works.ru).