Evaluation of the structure of monocrystalline Ni superalloys derived in different condi-tions ofdirectional solidification using methods of quantitative analysis of video images

Iskhodzhanova I.V., Bondarenko Yu.A., Lapteva M.A.
Iskhodzhanova I.V., Bondarenko Yu.A., Lapteva M.A. Evaluation of the structure of monocrystalline Ni superalloys derived in different condi-tions ofdirectional solidification using methods of quantitative analysis of video images // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-6-6. URL: https://www.viam-works.ru/en/journal/2015/12/6
Keywords
quantitative analysis of video images, methods to assess the geometric characteristics and volume fraction, porosity, directional solidification.
Abstract

The article presents a research on development of methods to assess the geometric characteristics and volume fraction of porosity, the geometric characteristics and volume fraction of eutectic (γ-γ)ʹ-phase, and the geometric characteristics of particles of the hardening γʹ-phase in monocrystalline Ni superalloys ZhS32U-VI. The results of investigations on proposed methods of quantitative metallographic analysis of blanks from the ZhS32U-VI superalloy, derived by directional solidification from the melt in different temperature gradient are presented.

Reference list
  1. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya [Cast blades of gas turbine engines: alloys, technologies, coverings] /Pod obshh. red. E.N. Kablova. 2-e izd. M.: Nauka. 2006. 632 s.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L. Kompyuternoe konstruirovanie zharoprochnogo nikelevogo splava IV pokoleniya dlya monokristallicheskih lopatok gazovyh turbin [Computer designing of heat resisting nickel alloy IV of generation for single-crystal blades of gas turbines] /V kn. Litejnye zharoprochnye splavy. Effekt S.T. Kishkina. M.: Nauka. 2006. S. 98–116.
  4. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  5. Bondarenko Yu.A., Kablov E.N., Morozova G.I. Vliyanie vysokogradientnoj napravlennoj kristallizacii na strukturu i fazovyj sostav zharoprochnogo splava tipa Rene N5 [Influence of the high-gradient directed crystallization on structure and phase composition of hot strength alloy of the Rene N5 type] //MiTOM. 1999. №2. S. 15–18.
  6. Bondarenko Yu.A., Kablov E.N. Napravlennaya kristallizaciya zharoprochnyh splavov s povyshennym temperaturnym gradientom [The directed crystallization of heat resisting alloys with the raised temperature gradient] //MiTOM. 2002. №7. S. 20–23.
  7. Bondarenko Yu.A., Echin A.B., Surova V.A., Narskij A.R. Vliyanie temperaturnogo gradienta na fronte rosta na strukturu zharoprochnogo splava pri napravlennoj kristallizacii [Influence of temperature gradient at the front growth on hot strength alloy structure at the directed crystallization] //Litejshhik Rossii. 2014. №5. S. 24–27.
  8. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of single crystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  9. Kablov E.N., Orlov M.R., Ospennikova O.G. Mehanizmy obrazovaniya poristosti v monokristallicheskih lopatkah turbiny i kinetika ee ustraneniya pri goryachem izostaticheskom pressovanii [Mechanisms of formation of porosity in single crystals turbine blades and kinetics of its elimination at hot isostatic pressing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 117–129.
  10. Zharoprochnyj splav na osnove nikelja [Heat resisting alloy on the basis of nickel]: pat. 2148099 Ros. Federaciya; opubl. 18.01.99. Byul. №12.
  11. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and x-ray of the structural analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
  12. Svetlov I.L., Ishodzhanova I.V., Evgenov A.G., Naprienko S.A. Issledovanie vysokotemperaturnoj polzuchesti i defektnosti struktury monokristallov nikelevogo zharoprochnogo splava posle gorjachego izostaticheskogo pressovaniya [Research of high-temperature creep and deficiency of structure of single crystals of nickel hot strength alloy after hot isostatic pressing] //Deformaciya i razrushenie materialov. 2011. №3. S. 28–32.
  13. Nejman A.V., Filonova E. V., Ishodzhanova I. V. O lokalnoj rekristallizacii v monokristallah nikelevyh zharoprochnyh splavov [About local re crystallization in monocrystals of nickel hot strength alloys] //Metallurgiya i mashinostroenie. 2013. №1. S. 19–22.
  14. Sidorov V.V., Ishodzhanova I.V., Rigin V.E., Folomejkin Yu.I. Ocenka effektivnosti filtracii pri razlivke slozhnolegirovannogo nikelevogo rasplava [Assessment of efficiency of filtering at razlivka complex-alloyed nickel rasplava] //Elektrometallurgiya. 2011. №11. S. 17–21.
  15. Klark E.R., Eberhardt K.N. Mikroskopicheskie metody issledovaniya materialov [Microscopic methods of research of materials]. M.: Tehnosfera. 2007. 376 s.
  16. Gulyaev A.I., Ishodzhanova I.V., Zhuravleva P.L. Primenenie metoda opticheskoj mikroskopii dlya kolichestvennogo analiza struktury PKM [Application of optical microscopy method for the quantitative analysis of polymer composite material structure] //Trudy VIAM. 2014. №7. St. 07 (viam-works.ru).