Early stages of environmental degradation investigated by moisture transfer parameters of CFRP used for aerospace applications
UDC
539.217.3:539.219.3
DOI
10.18577/2307-6046-2014-0-7-8-8
Article PDF (Russian)
(591.63 KB)
How to cite
Frolov A.S., Panin S.V. Early stages of environmental degradation investigated by moisture transfer parameters of CFRP used for aerospace applications // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-8-8. URL: https://www.viam-works.ru/en/journal/2014/7/8
Abstract
Moisture transfer parameters were evaluated for Hexcel CFRP, used in aerospace applications. The additive moisture transfer model was used to investigate the early stages of environmental degradation. After 6 month of outdoor exposure in warm tem-perate maritime climate initial stages of polymer degradation were discovered in surface layer less than 10 µm. Influence of CFRP degradation on the moisture transfer pa-rameters was evaluated.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Guljaev I.N., Gunjaev G.M., Raskutin A.E. Polimernye kompozicionnye materialy s funkcijami adaptacii i diagnostiki sostojanija [Polymer composite materials with features of adaptation and diagnosis of the condition] //Aviacionnye materialy i tehnologii. 2012. №S. S. 242–253.
- Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of the PCM] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
- Kirillov V.N., Vapirov Ju.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v uslovijah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Study of atmospheric resistance of polymer composite materials in the atmosphere warm, moist and moderately warm climate] //Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
- Starcev O.V., Kuznecov A.A., Krotov A.S., Anihovskaja L.I., Senatorova O.G. Modelirovanie vlagoperenosa v sloistyh plastikah i stekloplastikah [Modelling of moisture transfer in layered plastic and fiberglass] //Fizicheskaja mezomehanika. 2002. T. 5. №2. S. 109–114.
- Starcev O.V., Krotov A.S., Senatorova O.G., Anihovskaja L.I., Antipov V.V., Grashhenkov D.V. Sorbcija i diffuzija vlagi v sloistyh metallopolimernyh kompozicionnyh materialah tipa «SIAL» [Sorption and diffusion of moisture in layered metal-polymer composite materials such as «SIAL»] //Materialovedenie. 2011. №12. S. 38–44.
- Meljohina M.I., Kavun N.S., Rakitina V.P. Jepoksidnye stekloplastiki s uluchshennoj vlago- i vodostojkost'ju [Epoxy fiberglass with improved moisture resistance and water resistance] //Aviacionnye materialy i tehnologii. 2013. №2. S. 29–31.
- Starcev O.V., Anihovskaja L.I., Litvinov A.A., Krotov A.S. Povyshenie dostovernosti prognozirovanija svojstv polimernyh kompozitnyh materialov pri termovlazhnostnom starenii [Increasing the reliability of predicting the properties of polymeric composite materials under Hygrothermal aging] //DAN. 2009. T. 428. №1. S. 56–60.
- Starcev O.V., Filistovich D.V., Kuznecov A.A., Krotov A.S., Anihovskaja L.I., Dement'eva L.A. Deformiruemost' listovyh stekloplastikov na osnove kleevyh prepregov pri sdvigovyh nagruzkah vo vlazhnoj srede [Deformability sheet GRP based adhesive prepreg under shear stress in a wet environment] //Perspektivnye materialy. 2004. №1. S. 20–26.
- Stapcev O.V., Prokopenko K.O., Litvinov A.A., Kpotov A.S., Anihovskaja L.I., Dement'eva L.A. Issledovanie tepmovlazhnostnogo stapenija aviacionnogo stekloplastika [Study tepmovlazhnostnogo stapeniya aircraft fiberglass] //Germetiki. Klei. Tehnologii. 2009. №8. S. 18–22.
- Antipov V.V., Starcev O.V., Senatorova O.G. Zakonomernosti vlagoperenosa v SIA-Lah [Laws of moisture transfer in SIAL] //Korrozija: materialy, zashhita. 2012. №3. S. 13–18.
- Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniju kojefficienta dif-fuzii i predel'nogo vlagosoderzhanija dlja ocenki mehanicheskih svojstv ugleplastikov [Study patterns of moisture transfer and development of a standard to determine the diffusion coefficient and moisture content limit to evaluate the mechanical properties of carbon fiber reinforced plastics] //Aviacionnye materialy i tehnologii. 2013. №3. S. 44–48.
- Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging aviation applications of composite materials. I. Mechanisms of aging] //Deformacija i razrushenie materialov. 2010. №11. S. 19–26.
- Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. II. Relaksacija ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging aviation ap-plications of composite materials. II. Relaxation of the initial disequilibrium and structural properties of the gradient across the thickness] //Deformacija i razrushenie materialov. 2010. №12. S. 40–46.
- Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging aviation applications of composite materials. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
- Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. C. 16–21