Early stages of environmental degradation investigated by moisture transfer parameters of CFRP used for aerospace applications

Frolov A.S., Panin S.V.
Frolov A.S., Panin S.V. Early stages of environmental degradation investigated by moisture transfer parameters of CFRP used for aerospace applications // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-8-8. URL: https://www.viam-works.ru/en/journal/2014/7/8
Abstract

Moisture transfer parameters were evaluated for Hexcel CFRP, used in aerospace applications. The additive moisture transfer model was used to investigate the early stages of environmental degradation. After 6 month of outdoor exposure in warm tem-perate maritime climate initial stages of polymer degradation were discovered in surface layer less than 10 µm. Influence of CFRP degradation on the moisture transfer pa-rameters was evaluated.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Guljaev I.N., Gunjaev G.M., Raskutin A.E. Polimernye kompozicionnye materialy s funkcijami adaptacii i diagnostiki sostojanija [Polymer composite materials with features of adaptation and diagnosis of the condition] //Aviacionnye materialy i tehnologii. 2012. №S. S. 242–253.
  3. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vlijanija klimaticheskih faktorov i mehanicheskogo nagruzhenija na strukturu i mehanicheskie svojstva PKM [Investigation of the influence of climatic factors and mechanical loading on the structure and mechanical properties of the PCM] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  4. Kirillov V.N., Vapirov Ju.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v uslovijah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Study of atmospheric resistance of polymer composite materials in the atmosphere warm, moist and moderately warm climate] //Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  5. Starcev O.V., Kuznecov A.A., Krotov A.S., Anihovskaja L.I., Senatorova O.G. Modelirovanie vlagoperenosa v sloistyh plastikah i stekloplastikah [Modelling of moisture transfer in layered plastic and fiberglass] //Fizicheskaja mezomehanika. 2002. T. 5. №2. S. 109–114.
  6. Starcev O.V., Krotov A.S., Senatorova O.G., Anihovskaja L.I., Antipov V.V., Grashhenkov D.V. Sorbcija i diffuzija vlagi v sloistyh metallopolimernyh kompozicionnyh materialah tipa «SIAL» [Sorption and diffusion of moisture in layered metal-polymer composite materials such as «SIAL»] //Materialovedenie. 2011. №12. S. 38–44.
  7. Meljohina M.I., Kavun N.S., Rakitina V.P. Jepoksidnye stekloplastiki s uluchshennoj vlago- i vodostojkost'ju [Epoxy fiberglass with improved moisture resistance and water resistance] //Aviacionnye materialy i tehnologii. 2013. №2. S. 29–31.
  8. Starcev O.V., Anihovskaja L.I., Litvinov A.A., Krotov A.S. Povyshenie dostovernosti prognozirovanija svojstv polimernyh kompozitnyh materialov pri termovlazhnostnom starenii [Increasing the reliability of predicting the properties of polymeric composite materials under Hygrothermal aging] //DAN. 2009. T. 428. №1. S. 56–60.
  9. Starcev O.V., Filistovich D.V., Kuznecov A.A., Krotov A.S., Anihovskaja L.I., Dement'eva L.A. Deformiruemost' listovyh stekloplastikov na osnove kleevyh prepregov pri sdvigovyh nagruzkah vo vlazhnoj srede [Deformability sheet GRP based adhesive prepreg under shear stress in a wet environment] //Perspektivnye materialy. 2004. №1. S. 20–26.
  10. Stapcev O.V., Prokopenko K.O., Litvinov A.A., Kpotov A.S., Anihovskaja L.I., Dement'eva L.A. Issledovanie tepmovlazhnostnogo stapenija aviacionnogo stekloplastika [Study tepmovlazhnostnogo stapeniya aircraft fiberglass] //Germetiki. Klei. Tehnologii. 2009. №8. S. 18–22.
  11. Antipov V.V., Starcev O.V., Senatorova O.G. Zakonomernosti vlagoperenosa v SIA-Lah [Laws of moisture transfer in SIAL] //Korrozija: materialy, zashhita. 2012. №3. S. 13–18.
  12. Nikolaev E.V., Kirillov V.N., Skirta A.A., Grashhenkov D.V. Issledovanie zakonomernostej vlagoperenosa i razrabotka standarta po opredeleniju kojefficienta dif-fuzii i predel'nogo vlagosoderzhanija dlja ocenki mehanicheskih svojstv ugleplastikov [Study patterns of moisture transfer and development of a standard to determine the diffusion coefficient and moisture content limit to evaluate the mechanical properties of carbon fiber reinforced plastics] //Aviacionnye materialy i tehnologii. 2013. №3. S. 44–48.
  13. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging aviation applications of composite materials. I. Mechanisms of aging] //Deformacija i razrushenie materialov. 2010. №11. S. 19–26.
  14. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. II. Relaksacija ishodnoj strukturnoj neravnovesnosti i gradient svojstv po tolshhine [Climatic aging aviation ap-plications of composite materials. II. Relaxation of the initial disequilibrium and structural properties of the gradient across the thickness] //Deformacija i razrushenie materialov. 2010. №12. S. 40–46.
  15. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging aviation applications of composite materials. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  16. Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. C. 16–21