Studying the characteristics of VPZ-25 cold-curing polymer filler and developing a technology for filling honeycomb panels for aircraft components
Kopylov A.V., Kovalenko A.V., Sidelnikov N.K., Kurnosov A.O., Slavin A.V. Studying the characteristics of VPZ-25 cold-curing polymer filler and developing a technology for filling honeycomb panels for aircraft components // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-37-52. URL: https://www.viam-works.ru/en/journal/2025/12/4
Keywords
aviation technique, VPZ-25 polymer filler, spheroplastic, glass microspheres, epoxy binder, honeycomb panels, polymer composite materials
Abstract
This paper presents the results of a study of the characteristics and microstructure of samples of cold-curing polymer syntactic filler grade VPZ-25. Based on the results of testing the samples, a comparative analysis of the characteristics of VPZ-25 with the characteristics of a foreign analogue of cold-curing polymer filler was performed. Based on the results of preliminary testing of VPZ-25, a technology for filling honeycomb panels with VPZ-25 polymer filler for aircraft components was developed under various conditions.
Reference list
- Shershak P.V. Rational Selection of Design Solutions in Developing Aircraft Floor Structures from Polymer Composite Materials: thesis abstract, Cand. Sc. (Tech.). Moscow, 2017, 20 p.
- Slivinsky V.I., Tkachenko G.V., Slivinsky M.V. Efficiency of Using Honeycomb Structures in Aircraft. Vestnik Sibirskogo gosudarstvennogo aerokosmicheskogo universiteta im. akademika M.F. Reshetneva, 2005, no. 3, pp. 169–173.
- Alfutov N.A., Zinoviev P.A., Popov B.G. Calculation of Multilayer Plates and Shells from Composite Materials. Moscow: Mashinostroenie, 1984, 264 p.
- Shershak P.V., Kosarev V.A., Kurilenko N.V. The influence of the height of the polymer honeycomb core on the rigidity of three-layer honeycomb floor panels of aircraft. Aviatsionnaya promyshlennost, 2016, no. 2, pp. 49–52.
- Kablov E.N. The role of chemistry in the creation of new-generation materials for complex technical systems. Report of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
- Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: 28.10.2025). DOI: 10.18577/2713-0193-2023-0-2-94-103.
- Belinis P.G., Lukyanenko Yu.V., Rogozhnikov V.N., Tsykun R.G., Donetskiy K.I. Design research on a constructural multilayer woven preform of an integral panel fragment for aircraft. Aviation materials and technologies, 2023, no. 3 (72), paper no. 09. Available at: http://www.journal.viam.ru (accessed: October 29, 2025). DOI: 10.18577/2713-0193-2023-0-3-114-124.
- Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: October 30, 2025). DOI: 10.18577/2713-0193-2023-0-1-82-92.
- Sutubalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 05, 2025). DOI: 10.18577/2713-0193-2024-0-1-121-135.
- Panin V.F., Gladkov Yu.A. Structures with Filler: Handbook. Moscow: Mashinostroenie, 1991, 272 p.
- Endogur A.I., Weinberg M.V., Ierusalimsky K.M. Honeycomb Structures. Selection of Parameters and Design. Moscow: Mashinostroenie, 1986, 200 p.
- Panin V.F. Structures with Honeycomb Filler. Moscow: Mashinostroenie, 1982, 152 p.
- Mikhailin Yu.M. Fibrous Polymer Composite Materials in Engineering. St. Petersburg: Scientific Foundations and Technologies, 2013, 715 p.
- Minakov V.T., Postnov V.I., Shvets N.I., Zastrogina O.B., Petukhov V.I., Makrushin K.V. Features of the manufacture of three-layer honeycomb panels with a hot-curing polymer filler. Aviatsionnye materialy i tekhnologii, 2009, no. 3, pp. 6–9.
- Shershak P.V., Shokin G.I., Egorov V.N. Technological Features of the Production of Three-Layer Honeycomb Aircraft Floor Panels. Aviatsionnaya promyshlennost, 2014, no. 3, pp. 34–42.
- Airworthiness standards for air-planes of the transport category: AP-25: utv. Postanovleniyem 35-y sessii Soveta po aviatsii i ispolzovaniyu vozdushnogo prostranstva 23.10.2015. 5-ye izd. s popravkami 1–8. M.: Aviaizdat, 2015, 290 р.
- Ilyushenkov S.F., Tsvetkov V.E., Sereduta P.I., Tsvetkova N.N. Modern design and technological developments of aircraft interior elements. Polimernye materialy, 2024, no. 12, pp. 36–42.
- Ilyushenkov S.F., Batizat D.V., Sereduta P.I. Development of three-layer honeycomb floor panels for passenger aircraft made of polymer composites. Polimernye materialy, 2025, no. 3 (310), pp. 14–21.
- Kapustianskaia M.A., Lyubimova A.S., Kovalenko A.V., Sidelnikov N.K., Tkachuk A.I., Slavin A.V. Development of a cold-curing polymer syntatic filler with enhanced physico-mechanical properties. Trudy VIAM, 2024, no. 11 (141), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 05, 2025). DOI: 10.18577/2307-6046-2024-0-11-33-43.
- Epocast 1618-D/B. Available at: https://freemansupply.com/products/liquid-tooling-materials/epoxy-aerospace-syntactics/epocast-1618-epoxy-syntactic (accessed: November 05, 2025).