Studying the characteristics of VPZ-25 cold-curing polymer filler and developing a technology for filling honeycomb panels for aircraft components

Kopylov A.V., Kovalenko A.V., Sidelnikov N.K., Kurnosov A.O., Slavin A.V.
Kopylov A.V., Kovalenko A.V., Sidelnikov N.K., Kurnosov A.O., Slavin A.V. Studying the characteristics of VPZ-25 cold-curing polymer filler and developing a technology for filling honeycomb panels for aircraft components // Proceedings of VIAM. 2025. No. 12. DOI: 10.18577/2307-6046-2025-0-12-37-52. URL: https://www.viam-works.ru/en/journal/2025/12/4
Keywords
aviation technique, VPZ-25 polymer filler, spheroplastic, glass microspheres, epoxy binder, honeycomb panels, polymer composite materials
Abstract

This paper presents the results of a study of the characteristics and microstructure of samples of cold-curing polymer syntactic filler grade VPZ-25. Based on the results of testing the samples, a comparative analysis of the characteristics of VPZ-25 with the characteristics of a foreign analogue of cold-curing polymer filler was performed. Based on the results of preliminary testing of VPZ-25, a technology for filling honeycomb panels with VPZ-25 polymer filler for aircraft components was developed under various conditions. 

Reference list
  1. Shershak P.V. Rational Selection of Design Solutions in Developing Aircraft Floor Structures from Polymer Composite Materials: thesis abstract, Cand. Sc. (Tech.). Moscow, 2017, 20 p.
  2. Slivinsky V.I., Tkachenko G.V., Slivinsky M.V. Efficiency of Using Honeycomb Structures in Aircraft. Vestnik Sibirskogo gosudarstvennogo aerokosmicheskogo universiteta im. akademika M.F. Reshetneva, 2005, no. 3, pp. 169–173.
  3. Alfutov N.A., Zinoviev P.A., Popov B.G. Calculation of Multilayer Plates and Shells from Composite Materials. Moscow: Mashinostroenie, 1984, 264 p.
  4. Shershak P.V., Kosarev V.A., Kurilenko N.V. The influence of the height of the polymer honeycomb core on the rigidity of three-layer honeycomb floor panels of aircraft. Aviatsionnaya promyshlennost, 2016, no. 2, pp. 49–52.
  5. Kablov E.N. The role of chemistry in the creation of new-generation materials for complex technical systems. Report of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  6. Malysheva G.V., Marakhovskiy P.S., Barinov D.Ya., Nikolaev E.V. Optimization of the curing modes of fiber-glass based on epoxy binder. Aviation materials and technologies, 2023, no. 2 (71), paper no. 08. Available at: http://www.journal.viam.ru (accessed: 28.10.2025). DOI: 10.18577/2713-0193-2023-0-2-94-103.
  7. Belinis P.G., Lukyanenko Yu.V., Rogozhnikov V.N., Tsykun R.G., Donetskiy K.I. Design research on a constructural multilayer woven preform of an integral panel fragment for aircraft. Aviation materials and technologies, 2023, no. 3 (72), paper no. 09. Available at: http://www.journal.viam.ru (accessed: October 29, 2025). DOI: 10.18577/2713-0193-2023-0-3-114-124.
  8. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: October 30, 2025). DOI: 10.18577/2713-0193-2023-0-1-82-92.
  9. Sutubalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), paper no. 10. Available at: http://www.journal.viam.ru (accessed: November 05, 2025). DOI: 10.18577/2713-0193-2024-0-1-121-135.
  10. Panin V.F., Gladkov Yu.A. Structures with Filler: Handbook. Moscow: Mashinostroenie, 1991, 272 p.
  11. Endogur A.I., Weinberg M.V., Ierusalimsky K.M. Honeycomb Structures. Selection of Parameters and Design. Moscow: Mashinostroenie, 1986, 200 p.
  12. Panin V.F. Structures with Honeycomb Filler. Moscow: Mashinostroenie, 1982, 152 p.
  13. Mikhailin Yu.M. Fibrous Polymer Composite Materials in Engineering. St. Petersburg: Scientific Foundations and Technologies, 2013, 715 p.
  14. Minakov V.T., Postnov V.I., Shvets N.I., Zastrogina O.B., Petukhov V.I., Makrushin K.V. Features of the manufacture of three-layer honeycomb panels with a hot-curing polymer filler. Aviatsionnye materialy i tekhnologii, 2009, no. 3, pp. 6–9.
  15. Shershak P.V., Shokin G.I., Egorov V.N. Technological Features of the Production of Three-Layer Honeycomb Aircraft Floor Panels. Aviatsionnaya promyshlennost, 2014, no. 3, pp. 34–42.
  16. Airworthiness standards for air-planes of the transport category: AP-25: utv. Postanovleniyem 35-y sessii Soveta po aviatsii i ispolzovaniyu vozdushnogo prostranstva 23.10.2015. 5-ye izd. s popravkami 1–8. M.: Aviaizdat, 2015, 290 р.
  17. Ilyushenkov S.F., Tsvetkov V.E., Sereduta P.I., Tsvetkova N.N. Modern design and technological developments of aircraft interior elements. Polimernye materialy, 2024, no. 12, pp. 36–42.
  18. Ilyushenkov S.F., Batizat D.V., Sereduta P.I. Development of three-layer honeycomb floor panels for passenger aircraft made of polymer composites. Polimernye materialy, 2025, no. 3 (310), pp. 14–21.
  19. Kapustianskaia M.A., Lyubimova A.S., Kovalenko A.V., Sidelnikov N.K., Tkachuk A.I., Slavin A.V. Development of a cold-curing polymer syntatic filler with enhanced physico-mechanical properties. Trudy VIAM, 2024, no. 11 (141), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 05, 2025). DOI: 10.18577/2307-6046-2024-0-11-33-43.
  20. Epocast 1618-D/B. Available at: https://freemansupply.com/products/liquid-tooling-materials/epoxy-aerospace-syntactics/epocast-1618-epoxy-syntactic (accessed: November 05, 2025).