Kashapov O.S., Kondratyeva A.R., Monin S.A., Kalashnikov V.S. Influence of macrofiber orientation on the fatigue properties of rings made of heat-resistant titanium alloy of the Ti–Al–Sn–Zr–Mo–V–Nb–Fe–Si–(O–C) system (grade VT46) // Proceedings of VIAM. 2026. No. 8 (162). С. 51-67. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-8-51-67.

Influence of macrofiber orientation on the fatigue properties of rings made of heat-resistant titanium alloy of the Ti–Al–Sn–Zr–Mo–V–Nb–Fe–Si–(O–C) system (grade VT46)

Kashapov O.S., Kondratyeva A.R., Monin S.A., Kalashnikov V.S.
Abstract

The fatigue properties and crack resistance of solid-rolled rings made of VT46 titanium alloy were investigated. The influence of macrostructure inhomogeneity and microfiber orientation on mechanical properties was established. It was shown that despite the overall stability of strength properties, anisotropy of fatigue life and crack growth parameters is observed. There were determined threshold stress intensity factors, and were estimated critical defect sizes. It is necessary to enhance the rolling technology to improve structural homogeneity.

Keywords
titanium alloys, gas turbine engine rings, hot rolling, macrostructure, fatigue life, fracture toughness, macro texture, anisotropy

Reference list
  1. Kablov E.N. Materials and technology VIAM for «Aviadvigatel». Permskie aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  2. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  3. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), pp. 30–40. Available at: http://www.journal.viam.ru (accessed: April 30, 2026). DOI: 10.18577/2713-0193-2022-0-1-30-40
  4. Inozemtsev A.A., Popova D.D., Abramchuk T.V. et al. Study of the stability of the PD-14 aircraft engine to the effects of volcanic ash. Vestnik UGATU, 2022, vol. 26, no 2 (96), pp. 60-70. DOI: 10.54708/19926502_2022_2629660.
  5. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Za-vodov A.V. Prerequisites for the development of new low-alloyed technological medium strength titanium alloy with operating temperature up to 400-450 °C, capable of strengthening. Aviation materials and technologies, 2024, no. 1 (74), pp. 33-50. Available at: http://www.journal.viam.ru (accessed: April 30, 2026). DOI: 10.18577/2713-0193-2024-0-1-33-50.
  6. Chen X., Wang Y. Analysis of fatigue life in high temperature of W pattern sealing rings used in aircraft engine. Applied Mechanics and Materials, 2014, vol. 496-500, pp. 571-574. DOI: 10.4028/www.scientific.net/AMM.496-500.571.
  7. Ding X.Y., Yu Q. The influence of performance of W-type metallic sealing ring with different outer arms open angle. Advanced Materials Research, 2014, vol. 971-973, pp. 806-810. DOI: 10.4028/www.scientific.net/AMR.971-973.806.
  8. England R. Development of a thin gauge metallic seal for gas turbine engine applications to 1700 F. 33rd Joint Propulsion Conference and Exhibit, 1997. DOI: 10.2514/6.1997-2871.
  9. Honnorat Y. Issues and breakthrough in the manufacture of turboengine titanium parts. Materials Science and Engineering: A, 1996, vol. 213, no. 1-2, pp. 115-123. DOI: 10.1016/0921-5093(96)10229-X.
  10. Weaver M.J. Mechanical property requirements for aero gas turbine materials. Materials Science and Technology, 1987, vol. 3, no. 9, pp. 695-701. DOI: 10.1179/mst.1987.3.9.695.
  11. Kear B.H., Thompson E.R. Aircraft gas turbine materials and processes. Science, 1980, vol. 208, no. 4446, pp. 847-856. DOI: 10.1126/science.208.4446.847.
  12. Eylon D., Fujishiro S., Postans P.J., Froes F.H. High-temperature titanium alloys - a review. JOM, 1984, vol. 36, no. 11, pp. 55-62. DOI: 10.1007/BF03338617.
  13. Kitashima T., Suresh K.S., Yamabe-Mitarai Y. Present stage and future prospects of development of compressor material. Crystal Research and Technology, 2015, vol. 50, no. 1, pp. 28-37. DOI: 10.1002/crat.201400156.
  14. Saha B., Jana B., Yadav J.S. et al. Development and certification of Ti-8Al-1Mo-1V alloy for HP compressor blades for Adour engine applications. Bulletin of Materials Science, 1996, vol. 19, no. 4, pp. 661-669. DOI: 10.1007/BF02745158.
  15. Max B., Alexis J., Larginon C., Perusin S. Titanium alloy Ti-6242 for high temperature structural application. Static and dynamic mechanical properties and impact of ageing. MATEC Web of Conferences, 2020, vol. 321, art. 11089. DOI: 10.1051/matecconf/202032111089.
  16. Nishikiori S., Hattori H., Noda T., Okabe M., Isobe S. Application of heat-resistant titanium-based compressor disk with dual structure. Materials Science and Engineering: A, 1996, vol. 213, no. 1-2, pp. 124-127. DOI: 10.1016/0921-5093(96)10257-4.
  17. Matsumoto T. Development of near-β high strength Ti alloy Ti-5Al-2Sn-4Zr-3Cr-3Mo with superior fatigue crack growth properties. Materials Science and Engineering: A, 1996, vol. 213, no. 1-2, pp. 154-156. DOI: 10.1016/0921-5093(96)10238-0.
  18. Elrod C.W. Review of titanium application in gas turbine engines. Turbo Expo, 2003, vol. 3, pp. 649-656. DOI: 10.1115/GT2003-38862.
  19. Szkliniarz W., Szkliniarz A. Fundamentals of manufacturing technologies for aircraft engine parts made of TiAl based alloys. Archives of Metallurgy and Materials, 2016, vol. 61, no. 3, pp. 1385-1390. DOI: 10.1515/amm-2016-0227.
  20. Brotzu A., Felli F., Marra F. et al. Mechanical properties of a TiAl-based alloy at room and high temperatures. Materials Science and Technology, 2018, vol. 34, no. 15, pp. 1847-1853. DOI: 10.1080/02670836.2018.1491931.
  21. Rugg D., Dixon M., Burrows J. High-temperature application of titanium alloys in gas turbines. Material life cycle opportunities and threats - an industrial perspective. Materials at High Temperatures, 2016, vol. 33, no. 4-5, pp. 536-541. DOI: 10.1080/09603409.2016.1184423.
  22. Tru-Form - a breakthrough in aero engine ring technology. Aircraft Engineering and Aerospace Technology, 1987, vol. 59, no. 8, pp. 18-20. DOI: 10.1108/eb036488.
  23. Gebisa A.W., Lemu H.G. Additive manufacturing for gas turbine engine components. ASME Turbo Expo 2018: Turbomachinery Technical Conference and Exposition, 2018. DOI: 10.1115/GT2018- 76686.
  24. Wang H., Chao Q., Yang L. et al. Introducing transformation twins in titanium alloys: an evolution of \(\alpha\) -variants during additive manufacturing. Materials Research Letters, 2021, vol. 9, no. 3, pp. 119-126. DOI: 10.1080/21663831.2020.1850536.
  25. Sun M., Xu B., Xie B. et al. Leading manufacture of the large-scale weldedess stainless steel forging ring: innovative approach by the multilayer hot-compression bonding technology. Journal of Materials Science & Technology, 2021, vol. 71, pp. 84-86. DOI: 10.1016/j.jmst.2020.08.055.
  26. Wang K., Wang L., Zheng K. et al. High-efficiency forming processes for complex thin-walled titanium alloys components: state-of-the-art and perspectives. International Journal of Extreme Manufacturing, 2020, vol. 2, no. 3, art. 032001. DOI: 10.1088/2631- 7990/ab949b.
  27. Imamura Y., Ikawa K., Motoyama K. et al. An experimental study for the development of mandrel-free hot-spinning for large size titanium alloy plate forming. Journal of Engineering for Gas Turbines and Power, 2019, vol. 141, no. 3, art. 032501. DOI: 10.1115/1.4041161.
  28. Denisov L.V., Boytsov A.G., Siluyanova M.V. Providing of operational properties for gas-turbine engine parts and assemblies using electrospark deposition. Materials Science Forum, 2020, vol. 992, pp. 574-579. DOI: 10.4028/www.scientific.net/MSF.992.574.
  29. Yeom J.T., Kim J.H., Park N.K. et al. Ring-rolling design for a large-scale ring product of Ti-6Al-4V alloy. Journal of Materials Processing Technology, 2007, vol. 187-188, pp. 747-751. DOI: 10.1016/j.jmatprotec.2006.11.042.
  30. Kim K.J., Choi S.S., Hwang C.Y. et al. Ring-rolling process for manufacturing Ti-6Al-4V plane and profiled ring-products. Advanced Materials Research, 2007, vol. 26-28, pp. 429-432. DOI: 10.4028/www.scientific.net/AMR.26-28.429.
  31. Chen D.C., You C.S., Guo M.W., Lai B.Y. Robust design of ring rolling process for titanium alloy using the Taguchi method and the finite element method. Key Engineering Materials, 2010, vol. 450, pp. 177-180. DOI: 10.4028/www.scientific.net/KEM.450.177.
  32. Whittaker R., Fox K., Walker A. Texture variations in titanium alloys for aeroengine applications. Materials Science and Technology, 2010, vol. 26, no. 6, pp. 676-684. DOI: 10.1179/026708310X12635619988186.
  33. Bache M.R., Evans W.J. Impact of texture on mechanical properties in an advanced titanium alloy. Materials Science and Engineering: A, 2001, vol. 319-321, pp. 409-414. DOI: 10.1016/S0921- 5093(00)02034-7.
  34. Won J.W., Kim D., Hong S.-G., Lee C.S. Anisotropy in twinning characteristics and texture evolution of rolling textured high purity alpha titanium. Journal of Alloys and Compounds, 2016, vol. 683, pp. 92-99. DOI: 10.1016/j.jallcom.2016.05.029.
  35. Chouhan D.K., Biswas S. Microstructure and texture evolution during multi-direction forging of titanium. Materials Today: Proceedings, 2021, vol. 44, pp. 3102-3105. DOI: 10.1016/j.matpr.2021.02.490.
  36. Krokhina V.A., Arislanov A.A., Putyrskiy S.V., Anisimova A.Yu. Investigation of the regularities of the formation of the structure of rods made of titanium alloy VT6 depending on various technological schemes of manufacture. Aviation materials and technologies, 2023, no. 4 (73), pp. 36-44. Available at: http://www.journal.viam.ru (accessed: April 30, 2026). DOI: 10.18577/2071-9140-2023-0-4-36-44.
  37. Li W., Chen Z., Liu J. et al. Rolling texture and its effect on tensile property of a near-α titanium alloy Ti60 plate. Journal of Materials Science & Technology, 2019, vol. 35, no. 5, pp. 790-798. DOI: 10.1016/j.jmst.2018.10.032.
  38. Shi X.-H., Zeng W.-D., Shi C.-L. et al. The effects of colony microstructure on the fatigue crack growth behavior for Ti-6Al-2Zr-2Sn-3Mo-1Cr-2Nb titanium alloy. Materials Science and Engineering: A, 2015, vol. 618, pp. 247-253. DOI: 10.1016/j.msea.2014.09.112.
  39. Mendia L., Estensoro F.J., Mary C., Vogel F. Effect of combined cycle fatigue on Ti6242 fatigue strength. Procedia Engineering, 2011, vol. 10, pp. 1809-1814. DOI: 10.1016/j.proeng.2011.04.301.
  40. Evans W.J., Jones J.P., Bache M.R. High-temperature fatigue/creep/environment interactions in compressor alloys. Journal of Engineering for Gas Turbines and Power, 2003, vol. 125, no. 1, pp. 246–251. DOI: 10.1115/1.1498272.
  41. Wang M. Comparison of evolution laws of stress and strain fields in hot rolling of titanium alloy large rings with different sizes. Transactions of Nonferrous Metals Society of China, 2011, vol. 21, no. 7, pp. 1611–1619. DOI: 10.1016/S1003-6326(11)60904-7.
  42. Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), pp. 115–122. Available at: https: //journal.viam.ru (accessed: April 04, 2026). DOI: 10.18577/2713-0193-2021-0-2-115-122.
  43. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  44. Murakami Y., Endo M. Effects of defects, inclusions and inhomogeneities on fatigue strength. International Journal of Fatigue, 1994, vol. 16, no. 3, pp. 163–182. DOI: 10.1016/0142- 1123(94)90001-9.