Hard magnetic materials for aviation navigation devices made on the basis of a mixture of neodymium and praseodymium

Piskorsky V.P., Potapov M.V., Valeev R.A., Buzenkov A.V., Morgunov R.B.
Piskorsky V.P., Potapov M.V., Valeev R.A., Buzenkov A.V., Morgunov R.B. Hard magnetic materials for aviation navigation devices made on the basis of a mixture of neodymium and praseodymium // Proceedings of VIAM. 2026. No. 5. DOI: 10.18577/2307-6046-2026-0-5-123-132. URL: https://www.viam-works.ru/en/journal/2026/5/10
Keywords
rare-earth magnets, saturation magnetization, residual induction, coercive force, sintering temperature, annealing temperature, demagnetization curve
Abstract

The work studies sintered materials for aviation navigation devices based on praseodymium with an impurity of neodymium. It has been established that at a high content of cobalt, which is necessary to increase the temperature stability, the impurity of neodymium is acceptable only in minimal quantities. In neodymium-based materials, the content of the main magnetic phase R2(Fe, Co)14B decreases sharply with an increase in the content of cobalt. It had been established that a material with a minimum content of cerium has optimal magnetic properties.

Reference list
  1. Topilskaya S.V., Borodulin D.S., Kornyukhin A.V. Experimental assessment of permissible mechanical effects on a dynamically tuned gyroscope. Vestnik MGTU im. N.E. Baumana. Ser.: Priborostroenie, 2018, no. 4, pp. 69–79. DOI: 10.18698/0236-3933-2018-4-69-79.
  2. Litvin M.A., Malyugina A.A., Miller A.B. et al. Types of errors in inertial navigation systems and methods of their approximation. Informatsionnye protsessy, 2014, vol. 14, no. 4. pp. 326–339.
  3. Smirnov V.A., Snedkov A.B. Adaptive Calibration of a Gyroscope Angle Sensor. Omskiy nauchnyy vestnik, 2021, no. 3 (177), pp. 85–88. DOI: 10.25206/1813-8225-2021-177-85-88.
  4. Peshekhonov V.G. Gyroscopy Development Prospects. Giroskopiya i navigatsiya, 2020, vol. 28, no. 2, pp. 3–10. DOI: 10.17285/0869-7035.0028.
  5. Umarkhodzhaev R.M., Pavlov Yu.V., Vasilyeva A.N. History of the Development of a Gyroscope Based on Nuclear Magnetic Resonance in Russia in the 1960s–2000s. Giroskopiya i navigatsiya, 2018, vol. 26, no. 1, pp. 3–27. DOI: 10.17285/0869-7035.2018.26.1.003-027.
  6. Vershovsky A.K., Litmanovich Yu.A., Pazgalev A.S., Peshekhonov V.G. Nuclear Magnetic Resonance Gyroscope: Limiting Characteristics. Giroskopiya i navigatsiya, 2018, vol. 26, no. 1, pp. 55–80. DOI: 10.17285/0869-7035.2018.26.1.055-080.
  7. Pomerantsev N.M., Skrotsky G.V. Physical Foundations of Quantum Gyroscopy. Uspekhi fizicheskikh nauk, 1970, vol. 100, is. 3, pp. 361–394.
  8. Martynenko Yu.G. Trends in the Development of Modern Gyroscopy. Sorosovskiy obrazovatelniy zhurnal, 1997, no. 11, pp. 120–127.
  9. Korolev M.N. Study of Technical Characteristics of Modern Types of Angular Rate Sensors. 12th Int. Sc. and Tech. Conf. «Instrument Engineering–2019». Moscow, 2019, pp. 21–23.
  10. Xinyuan T., Podchezertsev V.P. Algorithms for Certification of a Dynamically Tuned Gyroscope under Conditions of Real Orientation Relative to a Geographic Coordinate System. Inzhenerniy zhurnal: nauka i innovatsii, 2017, is. 10, pp. 1–15. DOI: 10.18698/2308-6033-2017-10-1691.
  11. Korolev M.N., Malyutin D.M. Analysis of technical characteristics of sensitive elements of indicator gyroscopic stabilizers. Izvestiya Tulskogo gosudarstvennogo universiteta. Tekhnicheskie nauki, 2019, is. 8, pp. 30–46.
  12. Chirkin D.S., Roslovets P.V., Tatarinov F.V., Novikov L.Z. Reducing the drift of a dynamically tuned gyroscope from launch to launch. Inzhenerniy zhurnal: nauka i innovatsii, 2017, is. 1, pp. 1–11. DOI: 10.18698/2308-6033-2017-01-1579.
  13. Tian J., Pan D., Zhou H. et al. Radial cracks and fracture mechanism of radially oriented ring 2:17 type Sm–Co magnets. Journal of Alloys and Compounds, 2009, vol. 476, pp. 98–101.
  14. Tian J., Qu X., Zhang S. Influence of heat treatment on fracture and magnetic properties of radially oriented Sm2Co17 permanent magnets. Transaction Nonferrous Metallic Society China, 2007, vol. 17, pp. 491–495.
  15. Tian J., Qu X., Zhang S. et al. Magnetic properties and microstructure of radially oriented Sm(Co, Fe, Cu, Zr)Z ring magnets. Materials Letters, 2007, vol. 61, pp. 5271–5274.
  16. Matusevich V.A., Getya A.N., Sharaban Yu.V. Application of high-coercivity permanent magnets in aircraft units. Elektrotekhnika i elektromekhanika, 2006, no. 1, pp. 33–35.
  17. Li A., Li W., Wang H. et al. The study on thermal expansion of sintered Sm2Co17 magnets. IEEE Transactions on Magnetics, 2009, vol. 45, no. 10, pp. 4402–4403.
  18. Potapov M.V., Valeev R.A., Morgunov R.B., Piskorsky V.P. Properties of sintered magnets (Pr, Nd, Ce, Dy)(Fe, Co)B obtained from unrefined rare earth metals. Trudy VIAM, 2025, no. 2 (144), pp. 65–74. Available at: http://www.viam-works.ru (accessed: October 12, 2025). DOI: 10.18577/2307-6046-2025-0-2-65-74.
  19. Buzenkov A.V., Burkanov M.V., Valeev R.A., Piskorsky V.P. Influence of alloying elements and production technology on the properties of sintered magnets Pr(Nd)–Dy(M)–Fe–Co–B (M: Tb, Ce, Sm). Trudy VIAM, 2024, no. 6 (136), pp. 69–79. Available at: http://www.viam-works.ru (accessed: October 12, 2025). DOI: 10.18577/2307-6046-2024-0-6-69-79.
  20. Determination of the density of bodies by hydrostatic weighing: methodological recommendations. Irkutsk: Irkutsk State Univ., 2003, 15 p.
  21. Valeev R.A., Piskorsky V.P., Korolev D.V., Morgunov R.B. Optimization of the cobalt content as a way of temperature stabilization of rare earth magnets. Trudy VIAM, 2023, no. 3 (121), рр. 58–66. Available at: http://www.viam-works.ru (accessed: October 17, 2025). DOI: 10.18577/2307-6046-2023-0-3-58-66.
  22. Valeev R.A., Piskorsky V.P., Korolev D.V., Morgunov R.B. Optimization of the cobalt content as a way of temperature stabilization of rare earth magnets. Trudy VIAM, 2022, no. 11 (117), pp. 60–68. Available at: http://www.viam-works.ru (accessed: October 17, 2025). DOI: 10.18577/2307-6046-2022-0-11-60-68.
  23. Herbst J.F. R2Fe14B materials: intrinsic properties and technological properties and technological aspects. Reviews of Modern Physics, 1991, vol. 63, no. 4, pp. 819–898.
  24. Faria R.N., Davies B.E., Brown D.N. et al. Microstructural and magnetic studies of cast and annealed Nd and PrFeCoBZr alloys and HDDR materials. Journal of Alloys and Compounds, 2000, vol. 296, pp. 223–228.
  25. Taylor M.G., Davies B.E., Harris I.R. A comparative study of the sintering behavior of NdFeB and PrFeB for permanent magnet applications. Journal of Magnetism and Magnetic Materials, 2002, vol. 242–245, pp. 1375–1377.
  26. Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  27. Kryukov Ya.V., Samsonov N.Yu., Yatsenko V.A. Russian Rare Earth Industry: Should We Learn from China’s Experience? ECO, 2018, no. 10 (532), pp.138–152. DOI: 10.30680/ЭСО0131-7652-2018-10-138-152.