Formation of microstructure, phase composition and mechanical properties of high-carbon bearing steel at various stages of processing

Sevalnev G.S., Dulnev K.V., Korobova E.N., Sevalneva T.G.
Sevalnev G.S., Dulnev K.V., Korobova E.N., Sevalneva T.G. Formation of microstructure, phase composition and mechanical properties of high-carbon bearing steel at various stages of processing // Proceedings of VIAM. 2026. No. 5. DOI: 10.18577/2307-6046-2026-0-5-3-12. URL: https://www.viam-works.ru/en/journal/2026/5/1
Keywords
high carbon bearing steel, microstructure, phase composition, mechanical properties, martensite, austenite, cold treatment
Abstract

The paper investigates the microstructure, phase composition and mechanical properties of high-carbon bearing steel of the С–Cr–Mo–W–V–Nb alloying system under various heat treatment regimes. It has been established that the application of multi-stage tempering (up to 5 cycles) and cold treatment allows for effective control of the steel’s phase composition, achieving a martensite content up to 90 %. With optimal heat treatment, the steel demonstrates tensile strength up to 2620 MPa, yield strength of 2160 MPa, relative elongation of 6 %, and reduction of area of 8 %.

Reference list
  1. Sprishevsky A.I. Rolling bearings. Moscow: Mashinostroenie, 1968, 632 p.
  2. Morozova L.V., Grigorenko V.B., Konyshev D.V., Vlasov A.I. Reasons for the destruction of separators single-row radial rolling bearing study. Trudy VIAM, 2019, no. 10 (82), pp. 84–94. Available at: http://www.viam-works.ru (accessed: November 27, 2025). DOI: 10.18577/2307-6046-2019-0-10-84-94.
  3. Trojahn W., Streit E., Chin H., Ehlert D. Progress in bearing performance of advanced nitrogen alloys stainless steel, Cronidur 30. Materialwissenschaft und Werkstofftechnik: Entiwicklung, Fertigung, Prüfung, Eigenschaften und Anwendungen technischer Werkstoffe, 1999, vol. 30, no. 10, pp. 605–611.
  4. Bakradze M.M., Voznesenskaya N.M., Leonov A.V., Krylov S.A., Tonysheva O.A. Development and research of high-strength corrosion-resistant steel for bearing parts. Metallurg, 2019, no. 11, pp. 39–44.
  5. Nozhnitsky Yu.A., Petrov N.I., Lavrentyev Yu.L. Hybrid rolling bearings for aircraft engines (review). Aviatsionnye dvigateli, 2019, no. 2 (3), pp. 63–76.
  6. Kim S.S., Kato K., Hokkirigawa K., Abe H. Wear Mechanism of Ceramic Materials in Dry rolling Friction. Transaction of the ASME, 1986, vol. 108, pp. 522–526.
  7. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  8. Ooi S., Bhadeshia H.K.D.H. Duplex Hardening of steels for Aeroengine Bearings. ISIJ International, 2012, vol. 52, no. 11, pp. 1927–1934.
  9. Berns H., Ehrhardt R. Carbon or nitrogen alloyed quenched and tempered stainless steel – comparative study. Steel research 67, 1996, no. 8, pp. 343–349.
  10. Berns H., Escher C., Streich W.D. Martensitic high nitrogen steel for applications at elevated temperature. Materials science forum. Trans. Tech. Publications Ltd, 1999, vol. 318, pp. 443–448.
  11. Gromov V.I., Yakusheva N.A., Vostrikov A.V., Cherkashneva N.N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021, no. 1 (62), pp. 3‒12. Available at: http://www.journal.viam.ru (accessed: November 27, 2025). DOI: 10.18577/2713-0193-2021-0-1-3-12.
  12. Eliseev E.A., Karpukhin S.D., Druzhinina M.E. The effect of nickel on the structure of the nitrided layer of low-carbon martensitic steels. Aviation materials and technologies, 2025, no. 1 (78), pp. 18–27. Available at: http://www.journal.viam.ru (accessed: November 27, 2025). DOI: 10.18577/2713-0193-2025-0-1-18-27.
  13. Korobova E.N., Sevalnev G.S., Gromov V.I., Leonov A.V. Steels for the manufacture of roller bearings for special purposes (review). Trudy VIAM, 2021, no. 11 (105), pp. 3–11. Available at: http://www.viam-works.ru (accessed: November 27, 2025). DOI: 10.18577/2307-6046-2021-0-11-3-11.
  14. Rabitsch R., Koch F., Würzinger P. M50 (AMS 6191) and M50NiL (AMS 6278) High-Performance VIM-VAR Melted Bearing Steels for the Aviation Industry. Proceedings of the 2005 International Symposium on Liquid Metal Processing and Casting, 2005, vol. 5, pp. 57–64.
  15. Spektor A.G., Zelbet B.M., Kiseleva S.A. Structure and properties of bearing steels. Moscow: Metallurgiya, 1980, 264 p.
  16. Stein G., Hucklenbroich I., Wagner M. P 2000-A new austenitic high nitrogen steel for power generating equipment. Materials science forum. Trans Tech Publications Ltd, 1999, vol. 318, pp. 167–174.
  17. Ageeva E.V., Khardikov S.V., Pikalov S.V., Ageev E.V. X-ray structural analysis of powder ball bearing steel obtained by electrical discharge dispersion. Izvestiya Yugo-Zapadnogo gosudarstvennogo universiteta, 2015, vol. 1, no. 3, p. 35.
  18. Sevalnev G.S., Sevalneva T.G., Kolmakov A.G., Dulnev K.V., Krylov S.A. Study of the tribo-technical characteristics of corrosion-resistant steels with different mechanisms of volumetric hardening. Trudy VIAM, 2021, no. 10 (104), pp. 3–11. Available at: http://www.viam-works.ru (accessed: November 27, 2025). DOI: 10.18577/2307-6046-2021-0-10-3-11.