The effect of moisture on the strength and durability of carbon fiber reinforced plastic

Startsev O.V., Dvirnaya E.V., Kornienko G.V., Petrov M.G.
Startsev O.V., Dvirnaya E.V., Kornienko G.V., Petrov M.G. The effect of moisture on the strength and durability of carbon fiber reinforced plastic // Proceedings of VIAM. 2026. No. 4. DOI: 10.18577/2307-6046-2026-0-4-68-84. URL: https://www.viam-works.ru/en/journal/2026/4/7
Keywords
carbon fiber reinforced plastic, durability, strength parameter, moisture content, glass transition temperature
Abstract

This paper presents studies on the change in the durability of carbon fiber reinforced plastic during moisture sorption. For this purpose, at different stages of material moistening and in the dried state of it, short beam shear tests at loading rates differing by 3–4 orders of magnitude, cyclic tension-compression tests with increasing loading amplitude and a dynamic mechanical analysis were carried out. The study shows that the strength properties and the glass transition temperature of the carbon fiber reinforced polymer with different moisture content conform to the temperature-humidity analogy and ramp-down with the increase of moisture content.

Reference list
  1. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: September 05, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  2. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  3. Gunyaeva A.G., Sidorina A.I., Kurnosov A.O., Klimenko O.N. Polymeric composite materials of new generation on the basis of binder VSE-1212 and the filling agents alternative to ones of Porcher Ind. and Toho Tenax. Aviacionnye materialy i tehnologii, 2018, no. 3 (52), pp. 18–26. DOI: 10.18577/2071-9140-2018-0-3-18-26.
  4. Veligodskiy I.M., Koval T.V., Gulyaev I.N. Influence of climatic conditions on CFRP VKU-39 after three year outdoor exposition in eight climatic zones. Trudy VIAM, 2023, no. 8 (126), pp. 113–128. Available at: http://www.viam-works.ru (accessed: September 09, 2025). DOI: 10.18577/2307-6046-2023-0-8-113-128.
  5. Startsev V.O., Slavin A.V. Carbon and glass reinforced polymer based on solventfree binders resistance to the impact of a moderate cold and moderate warm climate. Trudy VIAM, 2021, no. 5 (99), pp. 114–126. Available at: http://www.viam-works.ru (accessed: September 13, 2025). DOI: 10.18577/2307-6046-2021-0-5-114-126.
  6. Startsev O.V., Skirta A.A., Startsev V.O., Valevin E.O., Kogan A.M. Ageing of VKU-39 carbon plastic under moderately warm and tropical climate conditions. 1. Changes of strength indicators. Science. Series D, 2025, vol. 178, pp. 382–386. DOI: 10.1134/S1995421225700236.
  7. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Comprehensive research of the influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 3. Calculation of activation energy and thermal resource of polymeric composite materials on the basis of epoxy matrix. Trudy VIAM, 2016, no. 5 (41), pp. 100–112. Available at: http://www.viam-works.ru (accessed: September 13, 2025). DOI: 10.18577/2307-6046-2016-0-5-11-11.
  8. Startsev O.V., Kornienko G.V., Gladkikh A.V., Gorbovets M.A. Nondestructive measurements of shear modulus in a sheet plane upon aging of polymeric composites. Polymer Science. Series D, 2024, vol. 17, pp. 606–614. DOI: 10.1134/s1995421224701041.
  9. Pride R.A. Environment effects of composites for aircraft. CTOL Transport Technology: conference proceedings. Hampton, VR, 1978, pp. 239–258. Available at: https://ntrs.nasa.gov/api/citations/19780019118 (accessed: July 28, 2025).
  10. Collings T.A. The effect of observed climatic conditions on the moisture equilibrium level of fiber-reinforced plastics. Composites, 1986, vol. 17, pp. 33–41. DOI: 10.1016/0010-4361(86)90731-7.
  11. Baker D.J. Ten-Year Ground Exposure of Composite Materials Used on the Bell Model 206L Helicopter Flight Service Program. NASA, 1994. Available at: https://ntrs.nasa.gov/citations/19950005944 (accessed: July 29, 2025).
  12. Ramesh C., Arumugam V., Stanley J., Kumar V. Effects of hydrolytic aging on glass/epoxy, kevlar/epoxy, and hybrid (glass/kevlar/epoxy) composites. International Journal of Engineering Research & Technology (IJERT), 2013, vol. 2, pp. 1589–1596. DOI: 10.17577/IJERTV2IS50859.
  13. Bone J.E., Sims G.D., Maxwell A.S. et al. On the relationship between moisture uptake and mechanical property changes in a carbon fibre/epoxy composite. Journal of Composite Materials, 2022, vol. 65, pp. 2189–2199. DOI: 10.1177/00219983221091465.
  14. Anderson E., Gunawan B., Nicholas J. et al. A multicontinuum theory based approach to the analysis of fiber-reinforced polymer composites with degraded stiffness and strength properties due to moisture absorption. Journal of Marine Science and Engineering, 2023, vol. 11, art. 421. DOI: 10.3390/jmse11020421.
  15. Pritchard G., Speake S.D. The use of water absorption kinetic data to predict laminate property changes. Composites, 1987, vol. 18, pp. 227–232. DOI: 10.1590/0104-1428.2106.
  16. Nandagopal R.A., Boay C.G., Narasimalu S. An empirical model to predict the strength degradation of the hygrothermal aged CFRP material. Composite Structures, 2020, vol. 236, art. 111876.
  17. Urzhumtsev Yu.S. Time-temperature superposition. Review. Mechanics of Composite Materials, 1976, vol. 11, pp. 57–72. DOI: 10.1007/bf00855426.
  18. Cha J.Y., Yoon S.B. Determination of shift factor for long-term life prediction of carbon/fiber epoxy composites using the time-temperature superposition principle. Functional Composites and Structures, 2022, vol. 4, art. 015003. DOI: 10.1088/2631-6331/ac529e.
  19. Maksimov R.D., Sokolov E.A., Mochalov V.P. Effect of temperature and moisture on the creep of polymeric materials. 1. One-dimensional extension under stationary temperature-moisture conditions. Polymer Mechanics, 1975, vol. 11, pp. 334–339. DOI: 10.1007/BF00863977.
  20. Maksimov R.D., Sokolov E.A., Mochalov V.P. Effect of temperature and humidity on the creep of polymer materials. 2. Uniaxial elongation under variable temperature-humidity conditions. Polymer Mechanics, 1975, vol. 11, pp. 834–839. DOI: 10.1007/BF00857602.
  21. Maksimov R.D., Mochalov V.P., Sokolov E.A. Influence of temperature and humidity on the creep of polymer materials. 3. Shear, and shear and tensile strain acting together. Polymer Mechanics, 1976, vol. 12, pp. 562–567. DOI: 10.1007/BF00857006.
  22. Hafiz T.A. Life prediction of carbon fiber reinforced polymers using time temperature shift factor. International Journal of Engineering Transactions A: Basics, 2020, vol. 33, pp. 1340–1346. DOI: 10.5829/ije.2020.33.07a.21.
  23. Petrov M.G., Startsev O.V., Lebedev M.P. Study of the strength of structural carbon fiber reinforced plastics under tension, compression and interlayer shear. Deformatsiya i razrusheniye materialov, 2025, no. 3, pp. 19–27. DOI: 10.31044/1814-4632-2025-3-19-27.
  24. Gulyaev I.N., Safronov A.M., Satdinov R.A. Comparison online and offline of prepregs manufacturing technologies and properties of carbon fiber plastics. Trudy VIAM, 2022, no. 6 (112), pp. 49–57. Available at: http://www.viam-works.ru (accessed: September 15, 2025). DOI: 10.18577/2307-6046-2022-0-6-49-57.
  25. State Standard 32659–2014 (ISO 14130:1997). Polymer composites. Test methods. Determination of apparent interlaminar shear strength by the short beam test method. Moscow: Standartinform, 2014, 16 p.
  26. ISO 6721-11. Plastics – Determination of dynamic mechanical properties – Part 11: Glass transition temperature. ISO, 2012, 22 p.
  27. Isupov V.V., Startsev O.V. Numerical methods in dynamic mechanical spectroscopy of polymers. Reports of the Int. Conf. «Mathematical Models and Numerical Methods of Continuum Mechanics». Ed. Yu.I. Shokin. Novosibirsk, 1996, pp. 293–294.