Investigation of phase transformations and formation of crystalline phases in materials for lining high-temperature electric furnaces

Babashov V.G., Maximov V.G., Butakov V.V., Varrik N.M.
Babashov V.G., Maximov V.G., Butakov V.V., Varrik N.M. Investigation of phase transformations and formation of crystalline phases in materials for lining high-temperature electric furnaces // Proceedings of VIAM. 2026. No. 4. DOI: 10.18577/2307-6046-2026-0-4-56-67. URL: https://www.viam-works.ru/en/journal/2026/4/6
Keywords
furnace lining, ceramic refractory, mullite, shrinkage, fibrous thermal insulation
Abstract

Use of industrial electric furnaces with operating temperatures of 1650–1800 °C required development of highly refractory materials with good thermal insulation properties. In industries where furnace temperatures exceed 1500 °C, mullite-corundum refractory materials containing crystalline fibers of high-alumina corundum and mullite are applied. The purpose of this work is to study the phase transformations and behavior of an experimental lining material produced by NRC «Kurchatov Institute» – VIAM under furnace operating conditions and to compare its properties with a similar imported material.

Reference list
  1. Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916. DOI: 10.31857/S0869587323100055.
  2. Zemlyanoy K.G. Refractory Service: a textbook and methodological manual. Ekaterinburg: Ural Univ. Publ. House, 2018, 172 p.
  3. Strelov K.K., Kashcheev I.D., Mamykin P.S. Refractory Technology: A Textbook for Secondary Specialized Educational Institutions, 4th ed., rev. and ad. Moscow: Metallurgiya, 1988, 528 p.
  4. Martynenko V.V., Dergaputskaya L.A. Effective thermal insulation lightweight and fibrous refractories. Ogneupory, 1993, no. 6, pp. 14–21.
  5. Allenstein J., Rouchka G., Wuthnau H. Refractory materials. Structure, properties, testing: a reference book: trans. from Germ. Moscow: Intermet Inzhiniring, 2010, 392 p.
  6. Sadik C., El Amranib I.-E., Albizane A. Recent advances in silica-alumina refractory: a review. Journal of Asian Ceramic Societies, 2014, vol. 2, pp. 83–96.
  7. Pletnev P.M., Tyulkin D.S. Experimental Compositions of Corundum-Mullite Refractories Based on Domestic Raw Materials. Ogneupory i tekhnicheskaya keramika, 2013, no. 3, pp. 10–14.
  8. Pletnev P.M., Tyulkin D.S. Structural and Phase Characteristics of Imported Refractory and Mullite-Corundum Compositions Using Its Crushed Material. Ogneupory i tekhnicheskaya keramika, 2013, no. 1–2, pp. 20–25.
  9. Sizov V.I., Gorokhovsky A.M., Karpets L.A. Use of Domestic Refractories for Lining Units for Melting and Processing Aluminum and Its Alloys. Novye ogneupory, 2006, no. 4, pp. 86–94.
  10. Sizov V.I., Gorokhovsky A.M., Karpets L.A. et al. Refractories for lining non-ferrous metallurgy units. Ogneupory i tekhnicheskaya keramika, 2008, no. 8, рр. 31–40.
  11. Deynega G.I., Kuzmina I.G., Bityutskaya O.N., Narsky A.R. Foam ceramic filters based on domestic refractory materials. Part 1. Trudy VIAM, 2023, no. 11 (129), pp. 17–25. Available at: http://www.viam-works.ru (accessed: August 29, 2025). DOI: 10.18577/2307-6046-2023-0-11-17-25.
  12. Deynega G.I., Kuzmina I.G., Bityutskaya O.N., Narsky A.R. Foam ceramic filters based on domestic refractory materials. Part 2. Trudy VIAM, 2024, no. 2 (132), pp. 13–22. Available at: http://www.viam-works.ru (accessed: August 29, 2025). DOI: 10.18577/2307-6046-2024-0-2-13-22.
  13. Thermal insulation product: pat. 2467877 Rus. Federation; appl. 31.05.07; publ. 10.07.10.
  14. Refractory thermal insulation material: pat. 908782 USSR; appl. 11.04.80; publ. 22.08.82.
  15. Fire-resistant thermal-insulation inorganic plate and preparation method thereof: pat. CN112521122; appl. 16.12.20; publ. 19.03.21.
  16. Krasnyy B.L., Ikonnikov K.I., Lemeshev D.O., Sizova A.S. Oxide-containing mineral fibers: types, production methods, application, and manufacturers (review). Steklo i keramika, 2022, vol. 95, no. 1 (1129), pp. 39–50. DOI: 10.14489/glc.2022.01.pp.039-050.
  17. Kosenko N.F., Pimkov Yu.V., Filatova N.V. Influence of Mechanical Treatment on the Devitrification Process in Mullite-Siliceous Fibers. Ogneupory i tekhnicheskaya keramika, 2013, no. 4–5, pp. 3–9.
  18. Meshkov V.I. High-Temperature Fibrous Thermal Insulation by Unifrax, Presented by Izomat. Novye ogneupory, 2006, no. 4, pp. 115–117.
  19. Zapolskikh I.V. Application of products of JSC SOZ and MTK SL in various industries. Ogneupory i tekhnicheskaya keramika, 2008, no. 10, pp. 22–29.
  20. Soshkin V.E., Baizdrenko V.S. Fibrous refractories for thermal insulation of covers and dampers of heating units. Liteynoe proizvodstvo, 2013, no. 4, pp. 27–29.
  21. Pavlov M.D., Okunkova A.A., Smurov I.Yu. Production of fibrous thermal insulation material based on aluminosilicate ceramics by laser processing. Perspektivnye materialy, 2013, no. 8, pp. 80–84.
  22. Zubashchenko R.V. Experience in the use of heat-resistant thermal insulation products based on aluminosilicate fiber in the lining of heating units in the ceramic industry. Steklo i keramika, 2017, no. 6, pp. 21–23.
  23. Abyzov A.N., Podkopaev V.N., Abyzov V.A., Pak Ch.G. Development and study of refractory fibrous material on a magnesia binder. Ogneupory i tekhnicheskaya keramika, 2010, no. 1–2, pp. 3–7.
  24. Kovylov V.M., Tomilin Yu.I., Lebedev Yu.N., Klinov O.A. Efficiency of using fibrous materials and products in furnace thermal barriers. Novye ogneupory, 2003, no. 4, pp. 22–25.
  25. Popov R.Yu., Dyatlova E.M., Sergievich O.A., Pogrebenkov V.M. Influence of modifying refractory and high-strength additives on the physical and technical characteristics of mullite-cordierite ceramics. Trudy Kolskogo nauchnogo tsentra RAN, 2018, vol. 9, no. 2-2, pp. 889–894. DOI: 10.25702/KSC.2307-5252.2018.9.1.889-894.
  26. Ceramic fiber insulation boards up to 1900 °C. Available at: https://thermocomponents.ru/catalog/vysokotemperaturnaya-teploizolyatsiya/keramicheskie-voloknistye-teploizolyatsionnye-plity/ (accessed: August 29, 2025).
  27. Kondratenko A.P., Kuzmina M.Yu. Improving the lining of electric crucible resistance furnaces through the use of modern fibrous refractory materials. Molodezhnyy vestnik IrGTU, 2023, vol. 13, no. 2, pp. 546–556.
  28. Pashkov E.I., Permyakov M.B., Krasnova T.V. Protection of heating units in an aggressive high-temperature environment with building thermal insulation materials. Vestnik evraziyskoy nauki, 2021, vol. 13, no. 2, art. 14.
  29. Moizis E.S., Kapustin R.D., Ilyukhin M.A. Development and application of new highly efficient structural refractory materials. Ogneupory i tekhnicheskaya keramika, 2015, no. 11–12, pp. 34–37.
  30. Akselrod L.M., Anikievich I.G., Smertin V.V., Nazmiev M.I. Features of New Developments in the Field of Basic Refractories. Novye ogneupory, 2008, no. 9, pp. 23–28.
  31. Grashchenkov D.V., Balinova Yu.A., Tinyakova E.V. Ceramic Aluminum Oxide Fibers and Materials Based on Them. Steklo i keramika, 2012, no. 4, pp. 32–35.
  32. Varrik N.M., Maksimov V.G. Study of Structural Changes in Oxide Ceramics by Polarization Microscopy. Zavodskaya laboratoriya. Diagnostika materialov, 2022, vol. 88, no. 7, pp. 29–35. DOI: 10.26896/1028-6861-2022-88-7-29-35.
  33. Antipov V.V., Varrik N.M., Maksimov V.G., Lugovoy A.A., Babashov V.G., Shavnev A.A. Study of mechanical and thermal characteristics of a porous ceramic material based on mullite. Trudy VIAM, 2023, no. 6 (124), pp. 38–45. Available at: http://www.viam-works.ru (accessed: August 29, 2025). DOI: 10.18577/2307-6046-2023-0-6-38-45.
  34. Butakov V.V., Lugovoy A.A., Varrik N.M., Babashov V.G. Assessment of thermal conductivity of a layered highly porous thermal insulation material. Aviation materials and technologies, 2022, no. 3 (68), pp. 120–129. Available at: http://www.journal.viam.ru (accessed: August 29, 2025). DOI: 10.18577/2713-0193-2022-0-3-120-129.