Approaches to creation of adhesives for gluing of non-polar rubbers based on natural rubber with metals in curing process

Manzhosova Е.N., Lukina N.F., Isayev A.Yu., Smirnov O.I.
Manzhosova Е.N., Lukina N.F., Isayev A.Yu., Smirnov O.I. Approaches to creation of adhesives for gluing of non-polar rubbers based on natural rubber with metals in curing process // Proceedings of VIAM. 2026. No. 4. DOI: 10.18577/2307-6046-2026-0-4-45-55. URL: https://www.viam-works.ru/en/journal/2026/4/5
Keywords
glue system, elastic glue, glue intermediate layer, rubber on basis natural rubber, durability at rubber separation from metal
Abstract

The basic components which are applying at creation of elastic adhesives for gluing of non-polar rubbers on the basis of natural rubber during vulcanization are considered. Information on some domestic developmed adhesive systems with characteristics is presented comparable to the international adhesive system Hemosil 211/411. The results of researches of adhesive joints of non-polar rubber on the basis of natural rubber with metal, executed with use of experimental adhesive system « adhesive ‒ adhesive intermediate layer» in initial condition and after influence of the factors simulating operational are provided.

Reference list
  1. Petrova A.P. Rubber adhesives. The Big Handbook of the Rubber Manufacturer: in 2 parts. Moscow: Tekhinform, 2012, part 2, pp. 138–145.
  2. Kozlov V.A., Lyakin Yu.I., Kiselev V.Ya. The Effect of Surface Modification of Vulcanized Rubbers on Adhesive Strength. Klei. Germetiki. Tekhnologii, 2006, no. 12, pp. 11–15.
  3. Glue for rubber and metal. Available at: https://chemosil.ru/catalog/adhesives-and-adhesive/glue-rubber-metal/ (accessed: July 02, 2025).
  4. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  5. Petrova A.P., Malysheva G.V. Adhesives, adhesive binders, and adhesive prepregs: a textbook. Moscow: VIAM, 2017, 472 p.
  6. Petrova A.P. Adhesives: Handbook. Eds. E.N. Kablov, S.V. Reznicenko. Moscow: Redaktsiya zhurnala «Kauchuk i rezina», 2002, 196 p.
  7. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. (accessed: July 02, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  8. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubbers, hydraulic fluids, part 1: Adhesives, adhesive prepregs, 276 p.
  9. Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
  10. Kuznetsova V.А. Influence of the elastomeric modifier on mechanical and viscoelastic properties of epoxy and rubber compositions for erosion resistant coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 56–62. DOI: 10.18577/2071-9140-2020-0-2-56-62.
  11. Abramova M.G., Lutsenko A.N., Varchenko E.A. Concerning the aspects of validation of climate resistance of airborne materials at all life cycle stages (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 86–94. DOI: 10.18577/2071-9140-2020-0-1-86-94.
  12. Adhesives for bonding rubber to metal during vulcanization. Available at: http://www.elad-germes.ru/kley.htm#1 (accessed: July 02, 2025).
  13. Adhesive composition: pat. 1008229А1 Rus. Federation; appl. 10.11.81; publ. 30.03.83.
  14. Method of bonding rubber to metal: pat. 2400512С1 Rus. Federation; appl. 16.03.09; publ. 27.09.10.
  15. Keibal N.V., Bondarenko S.N., Kablov V.F. Modification of polychloroprene-based adhesive compositions with element-containing adhesion promoters. Klei. Germetiki. Tekhnologii, 2011, no. 2, pp. 6–13.
  16. Zuev A.A., Lyusova L.R., Boreiko N.P. Chlorinated isoprene rubbers in adhesive compositions. Kauchuk i rezina, 2016, no. 4, pp. 24–26.
  17. Alekhine A.K., Lyusova L.R., Naumova Yu.A. et al. Improving the adhesive properties of adhesives based on a mixture of nitrile butadiene and chlorinated rubbers with metal chelates. Klei. Germetiki. Tekhnologii, 2019, no. 6, pp. 2–8.
  18. Malysheva M.A., Lyusova L.R., Zuev A.A., Bryk Ya.A., Chaykun A.M. Adhesive compositions based on chlorinated polyisoprenes. Klei. Germetiki. Tekhnologii, 2019, no. 8, pp. 7–12.
  19. Tyumeneva T.Yu., Zhadova N.S., Lukina N.F. Development of VIAM Federal State Unitary Enterprise in the field of adhesives of industrial rubber assignment and being self-glued materials. Trudy VIAM, 2014, no. 7, pp. 23‒28. Available at: http://www.viam-works.ru (accessed: July 02, 2025). DOI: 10.18577/2307-6046-2014-0-7-23-28.
  20. Isaev A.Yu., Smirnov O.I., Rubtsova E.V., Petrova A.P. Properties and applications areas of the adhesive VKR-85. Trudy VIAM, 2021, no. 5 (99), pp. 48‒55. Available at: http://www.viam-works.ru (accessed: July 02, 2025). DOI: 10.18577/2307-6046-2021-0-5-48-55.
  21. Tyumeneva T.Yu., Lukina N.F. Development in the field of elastomeric adhesives for aviation. Trudy VIAM, 2016, no. 8, pp. 67‒71. Available at: http://www.viam-works.ru (accessed: July 02, 2025). DOI: 10.18577/2307-6046-2016-0-8-67-71.