Features of non-destructive testing of silumin castings by X-ray computed tomography

Demidov A.A., Trapeznikov A.V., Kosarina E.I., Osiyanenko N.V.
Demidov A.A., Trapeznikov A.V., Kosarina E.I., Osiyanenko N.V. Features of non-destructive testing of silumin castings by X-ray computed tomography // Proceedings of VIAM. 2026. No. 4. DOI: 10.18577/2307-6046-2026-0-4-158-167. URL: https://www.viam-works.ru/en/journal/2026/4/13
Keywords
X-ray computed tomography, CAD model, X-ray porosity scale
Abstract

A special feature of non-destructive testing using X-ray computed tomography (XCT) of medium-sized aluminum alloy housing parts is that a tomogram is obtained simultaneously for two parts, CAD models of products were embedded in images for decoding tomographic images and sorting out control objects. Defect coordinates relative to the clean outline of the CAD model were used to determine their acceptability. Since X-ray computed tomography (XCT) is not feasible, porosity score assessment is selectively performed using traditional X-ray methods. 

Reference list
  1. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), pp. 24–34. Available at: http://www.journal.viam.ru (accessed: August 21, 2025). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  2. Gorbovets M.A., Nikolaev E.V., Startsev V.O. Climate testing of Arctic materials. Part 1. Requirements for materials. Aviation materials and technologies, 2024, no. 4 (77), pp. 180–188. Available at: http://www.journal.viam.ru (accessed: August 14, 2025). DOI: 10.18577/2713-0193-2024-0-4-180-188.
  3. Reshetnikov Yu.V., Trapeznikov A.V., Vlasova K.A., Leonov A.A. Different factors influence on technological properties of self-hardening phenol formaldehyde resin sands. Part 1. Aviation materials and technologies, 2024, no. 1 (74), pp. 63–77. Available at: http://www.journal.viam.ru (accessed: August 14, 2025). DOI: 10.18577/2713-0193-2024-0-1-63-77.
  4. Oglodkov M.S., Romanenko V.A., Kozhekin A.E. Directions of development melting and casting technologies of aluminum-lithium alloys (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 51–62. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2023-0-2-51-62.
  5. State Standard 1583–93. Aluminum Casting Alloys. Specifications. Minsk: Publ. House of Standards, 1993, 30 p.
  6. Kazantsev S.P., Furman E.L. Defects in Investment Castings. Ekaterinburg: UrFU, 2019, 110 p. Available at: https://study.urfu.ru/Aid/Publication/13842/1/1229_Казанцев.pdf (accessed: August 14, 2025
  7. Obodovsky A.V., Klonov V.V., Larionov I.A., Potrakhov N.N. On the Modernization of an X-ray Diagnostic Unit for Tomographic Studies. Reports of 5th All-Rus. Sci. and Pract. Conf. of X-ray Equipment Manufacturers. St. Petersburg: ETU «LETI» Publ. House, 2018, pp. 60–62.
  8. Krotova U.V., Savchenko O.A., Mitryaikin V.I., Zaitseva T.A., Zakirov R.Kh. Application of X-ray computed tomography for diagnostics of composite structures in the power industry. Problemy energetiki, 2024, vol. 26, no. 2, pp. 15–31.
  9. Becker B., Rumyantsev S. Software for visualization and analysis of computed tomography data. Reports of the 4th International Conf. «The Newest Control Technologies». Moscow: Ostek-SMT, 2016, pp. 7–9.
  10. Kosushkin P.A. Advanced technologies for quality control. Vektor vysokikh tekhnologiy, 2016, no. 5 (26), pp. 38–42.
  11. Van Aarle W., Palenstijn W.J., Cant J. et al. Fast and flexible X-ray tomography usingthe ASTRA toolbox. Optic Express, 2016, vol. 24, no. 22, pp. 25129–25147.
  12. Zubova A.V., Pikhur O.L., Bessonov V.B. et al. A case of surgical removal of lower third molars in a craniological series from the Pucara de Tilcara fortress (Jujuy Province, Argentina). Arkheologiya, etnografiya i antropologiya Evrazii, 2020, vol. 48, no. 2, pp. 149–156.
  13. Sergienko I.V., Amirova L.A., Krymova M.A., Tangatarov R.R. Digital tools in the professional activities of a specialist: a textbook for universities. St. Petersburg: Lan, 2025, 204 p.
  14. Berdnikova A.A., Verzun N.A., Kolbanev M.O. Architecture and access models in information and communication systems: a textbook for universities. St. Petersburg: Lan, 2024, 96 p.
  15. Ingacheva A.S., Sheshkus A.V., Chernov T.S. et al. X-ray computed tomography – a new tool in recognition. Trudy ISA RAN, 2018, Special issue, pp. 90–95.