Prospects for application of europium to improve the performance properties of casting aluminum alloys
UDC
669.715:546.661
DOI
10.18577/2307-6046-2026-0-3-66-84
Article PDF (Russian)
(1.73 MB)
How to cite
Petrov I.A., Trapeznikov A.V., Reshetnikov Yu.V., Vorobyova E.I. Prospects for application of europium to improve the performance properties of casting aluminum alloys // Proceedings of VIAM. 2026. No. 3. DOI: 10.18577/2307-6046-2026-0-3-66-84. URL: https://www.viam-works.ru/en/journal/2026/3/6
Keywords
rare earth elements, europium, cast aluminum alloys, modification, adsorption mechanisms, mechanical properties, microstructure
Abstract
This review examines various aspects of the application of the rare earth element europium. The main areas of its application in various industries are described. The historical aspect of the discovery of europium is shown. The results of studies on the effect of europium on the structure and mechanical properties of various cast aluminum alloys (silumins) are presented. Various theories and adsorption mechanisms explaining the processes of modification of eutectic and primary silicon with europium are considered.
Reference list
- Baranovskaya V.B., Karpov Yu.A., Petrova K.V., Korotkova N.A. Modern trends in the use of rare earth metals and their compounds in metallurgy and the production of optical materials. Tsvetnye metally, 2020, no. 11, pp. 54–62.
- Volkov A.I., Stulov P.E., Leontyev L.I., Uglov V.A. Analysis of the use of rare earth metals in the ferrous metallurgy of Russia and the world. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya, 2020, vol. 63, no. 6, pp. 405–418.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare earth elements – materials of modern and future high technologies. Trudy VIAM, 2013, no. 2, pp. 3–13. Available at: http://www.viam-works.ru (accessed: August 15, 2025).
- Nochovnaya N.A., Khorev A.L., Yakovlev A.I. Prospects for alloying titanium alloys with rare earth elements. Metallovedenie i termicheskaya obrabotka metallov, 2013, no. 8, pp. 18–23.
- Skupov A.A., Panteleev M.D., Ioda E.N., Movenko D.A. The efficiency of rare earth metals for filler materials alloying. Aviacionnye materialy i tehnologii, 2017, no. 3 (48), pp. 14–19. DOI: 10.18577/2071-9140-2017-0-3-14-19.
- Volkova E.F., Mostyaev I.V., Akinina M.V., Alikhanyan A.A. Impact study of the full cycle of the heat treatment on the structure and mechanical properties of forgings made of heat-resistant magnesium alloy of the Mg–Zn–Zr‒REE system. Aviation materials and technologies, 2025, no. 1 (78), pp. 88–98. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2025-0-1-88-98.
- Mostyaev I.V. REE – quality factor increase properties of magnesium alloy (review). Trudy VIAM, 2015, no. 7, pp. 8–12. Available at: http://www.viam-works.ru (accessed: August 15, 2025). DOI: 10.18577/2307-6046-2015-0-7-2-2.
- Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 3 (68), pp. 108–119. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2022-0-3-108-119.
- Sudzhanskaya I.V., Lebedeva Yu.E., Vaganova M.L., Shchegoleva N.E. Effect of co-doped of CeO2, Y2O3 on microstructure and mechanical properties of ceramic spinel MgAl2O4. Aviation materials and technologies, 2025, no. 2 (79), pp. 91–102. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2025-0-2-91-102.
- Varfolomeev M.S., Shcherbakova G.I. Refractory compositions designed for highly heat-resistant ceramic molds in foundry practice. Refractories and Industrial Ceramics, 2018, vol. 59, no. 3, pp. 290–295.
- Sokolov A.V., Deynega G.I., Kuzmina N.A. Influence of Sc2O3 additive on sintering temperature and properties of ZrO2–Y2O3 system oxide ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 64–69. DOI: 10.18577/2071-9140-2020-0-1-64-69.
- Shlyaptseva A.D., Petrov I.A., Ryakhovsky A.P., Moiseev V.S. Development of a complex modifying flux for cast aluminum alloys. Liteyshchik Rossii, 2020, no. 4, pp. 13–17.
- Trapeznikov A.V., Vlasova K.A., Reshetnikov Yu.V. Tableted modifiers for cast aluminum alloys. Aviation materials and technologies, 2024, no. 3 (76), pp. 14–24. Available at: http://www.journal.viam.ru (accessed: August 15, 2025). DOI: 10.18577/2713-0193-2024-0-3-14-24.
- Duyunova V.A., Trapeznikov A.V., Leonov A.A., Koreneva E.A. Modifying of cast aluminum alloys (review). Trudy VIAM, 2023, no. 4 (122), pp. 14–26. Available at: http://www.viam-works.ru (accessed: August 15, 2025). DOI: 10.18577/2307-6046-2023-0-4-14-26.
- Demarçay E. Sur un nouvel élément, l‘europium. Comptes Rendus Hebdomadaires des Séances de l’Académie des Science, 1901, vol. 132, pp. 1484–1486.
- Detkov P.G., Drobot D.V. History of the discovery of rare earth elements. Samarium, europium and gadolinium. Tsvetnye metally, 2024, no. 5, pp. 84–90.
- Encyclopedia of Technologies 2.0: Rare Earth Elements. Ed. D.O. Skobelev. Moscow; St. Petersburg: Renome, 2024, 340 p.
- Edwards J.D., Archer R.S. The new aluminum-silicon alloys – an important process of «modification» and the remarkable improvement in properties it brings about. Chemical and Metallurgical Engineering, 1924, vol. 31, pp. 504–508.
- Stroganov G.B., Rotenberg V.A., Gershman G.B. Aluminum-silicon alloys. Moscow: Metallurgiya, 1977, 272 p.
- Day M.G., Hellawell A. The Microstructure and Crystallography of Aluminium-Silicon Eutectic Alloys. Proceedings of the Royal Society of London. Series A, Mathematical and Physical Sciences, 1968, vol. 305, no. 1483, pp. 473–491.
- Lu S.Z., Hellawell A. The mechanism of silicon modification in aluminum-silicon alloys: Impurity induced twinning. Metallurgical and Materials Transactions A, 1987, vol. 18, pp. 1721–1733.
- Nogita K., Yasuda H., Yoshiya M. et al. The role of trace element segregation in the eutectic modification of hypoeutectic Al–Si alloys. Journal of Alloys and Compounds, 2010, vol. 489, is. 2, pp. 415–420.
- Petrov I.A., Shlyaptseva A.D. Effect of REE on the crystallization process of eutectic silumin. Metally, 2022, no. 2, pp. 19–27.
- Veryatin U.D., Mashirev V.P., Ryabtsev N.G. et al. Thermodynamic properties of inorganic substances: a handbook. Ed. A.P. Zefirov. Moscow: Atomizdat, 1965, 460 p.
- Gursoy O., Timelli G. Lanthanides: a focused review of eutectic modification in hypoeutectic Al–Si alloys. Journal of Materials Research and Technology, 2020, vol. 9, is. 4, pp. 8652–8666.
- CRC Handbook of Chemistry and Physics. Eds. W.M. Haynes, D.R. Lide. 95th ed. CRC Press: Boca Raton, 2014, 2704 p.
- Smithells Metals Reference Book. Eds. W.F. Gale, T.C. Totemeier. 8th ed. Oxford: Totemeier Imprint, 2003, 2080 p.
- Petrov I.A., Telitsyna O.V. Study of the influence of some rare earth elements on the properties of eutectic silumin. Tekhnologiya legkikh splavov, 2021, no. 1, pp. 54–59.
- Li J.H., Wangb X.D., Ludwig T.H. et al. Modification of eutectic Si in Al–Si alloys with Eu addition. Acta Materialia, 2015, vol. 84, pp. 153–163.
- Mao F., Qiao Y., Zhang P. et al. Modification Mechanism of Rare Earth Eu on Eutectic Si in Hypoeutectic Al–Si Alloy. International Journal of Metalcasting, 2022, vol. 16, pp. 634–645.
- Nogita K., McDonald S.D., Dahle A.K. Eutectic Modification of Al–Si Alloys with Rare Earth Metals. Materials Transactions, 2004, vol. 45, is. 2, pp. 323–326.
- Li J.H., Ludwig T.H., Oberdorfer B., Schumacher P. Solidification behaviour of Al–Si based alloys with controlled additions of Eu and P. International Journal of Cast Metals Research, 2018, vol. 31 (6), pp. 319–331. DOI: 10.1080/13640461.2018.1480891.
- Barrirero J., Pauly C., Engstler M. et al. Eutectic modification by ternary compound cluster formation in Al–Si alloys. Scientific Reports, 2019, vol. 9, p. 5506. DOI: 10.1038/s41598-019-41919-2.
- Mao F., Yan G., Xuan Z. et al. Effect of Eu addition on the microstructures and mechanical properties of A356 aluminum alloys. Journal of Alloys and Compounds, 2015, vol. 650, pp. 896–906. DOI: 10.1016/j.jallcom.2015.06.266.
- Li J., Fredrik H., Manfred W. et al. The roles of Eu during the growth of eutectic Si in Al–Si alloys. Scientific Reports, 2015, vol. 5 (1), p. 13802. DOI: 10.1038/srep13802.
- Spacil I., Gehringer D., Holec D. et al. Elucidating effects of Eu and P on solidification and precipitation of Al–7Si–0,3Mg based alloys refined by Ta and TiB2. Journal of Alloys and Compounds, 2024, vol. 978, p. 173343. DOI: 10.1016/j.jallcom.2023.173343.
- Sahin H., Dispinar D. Effect of Rare Earth Elements Erbium and Europium Addition on Microstructure and Mechanical Properties of A356 (Al–7Si–0,3Mg) Alloy. International Journal of Metalcasting, 2023, vol. 17, pp. 2612–2621. DOI: 10.1007/s40962-023-01060-3.
- Ou C., Xiao C., Tang S. et al. Effect of the co-addition of Eu and Er on the microstructure and mechanical properties of Al–9,5Si–2Cu–0,6Mg alloy. Materials Letters, 2025, vol. 382, p. 137848. DOI: 10.1016/j.matlet.2024.137848.
- Mao F., Wei S., Ou L. et al. Different Influences of Rare Earth Eu Addition on Primary Si Refinement in Hypereutectic Al–Si Alloys with Varied Purity. Materials, 2019, vol. 12 (21), p. 3505. DOI: 10.3390/ma12213505.
- Guo J., Mao F., Zhang G. et al. Dual Modification of Hypereutectic Al–Si Alloy and Spheroidization Mechanism of Primary Silicon with Eu Addition. International Journal of Metalcasting, 2024, vol. 18, pp. 2562–2578. DOI: 10.1007/s40962-023-01198-0.
- Mao F., Zhang L., Guo J. et al. The Effect of Eu and T6 heat treatment on Microstructure of A390 Alloys. International Journal of Metalcasting, 2025. Available at: https://link.springer.com/article/10.1007/s40962-025-01649-w (accessed: August 15, 2025). DOI: 10.1007/s40962-025-01649-w.
- Mao F., Guo J.L., Liu S.H. et al. Spheroidization mechanism of primary silicon in hypereutectic Al–Si alloys with Eu addition. Rare Metals, 2025, vol. 44, pp. 7940–7955. DOI: 10.1007/s12598-025-03504-7.