Effect of gas-dynamic spraying of powder materials on the adhesion of paint coatings, corrosion, and mechanical properties of magnesium alloys

Duyunova V.A., Leonov A.A., Trofimov N.V., Mukhina I.Y., Uridiya Z.P., Tokarev M.S.
Duyunova V.A., Leonov A.A., Trofimov N.V., Mukhina I.Y., Uridiya Z.P., Tokarev M.S. Effect of gas-dynamic spraying of powder materials on the adhesion of paint coatings, corrosion, and mechanical properties of magnesium alloys // Proceedings of VIAM. 2026. No. 3. DOI: 10.18577/2307-6046-2026-0-3-54-65. URL: https://www.viam-works.ru/en/journal/2026/3/5
Keywords
magnesium alloys, powder compositions, gas dynamic spraying, defect elimination, adhesion, mechanical properties
Abstract

Foundry magnesium alloys are used for the manufacture of complex-contoured castings of variable cross-section, during the production of which metallurgical defects may occur, such as underflows, small cracks, tears, shells, and microporosity. The use of gas-dynamic spraying of special powder compositions without heating is the most economical modern technological method to eliminate these defects. The article presents the results of scientific and technical research on the development ofpowder compositions for casting magnesium alloys of Mg–Al–Zn, Mg–Zn–Zr, Mg–REM–Zr systems.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N., Antipov V.V., Chesnokov D.V., Kutyrev A.E. Application of Al–Mg–Si–Cu system aluminum alloy combined anodic dissolution for prognosis of tensile strength loss during natural exposure testing. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 63–73. DOI: 10.18577/2071-9140-2020-0-2-63-73.
  3. Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), pp. 24–34. Available at: http://www.journal.viam.ru (accessed: June 26, 2025). DOI: 10.18577/2713-0193-2021-0-2-24-34.
  4. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), pp. 32–51. Available at: http://www.viam-works.ru (accessed: June 20, 2025). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  5. Kechin V.A. Ways to improve the efficiency of magnesium alloys. Liteyshchik Rossii, 2008, no. 7, pp. 17–20.
  6. Trofimov N.V., Leonov A.A., Duyunova V.A., Tokarev M.S. Modern approaches to improving the quality of casting and local repairs of products made of magnesium alloys. Trudy VIAM, 2025, no. 4 (146), pp. 57–69. Available at: http://www.viam-works.ru (accessed: June 20, 2025). DOI: 10.18577/2307-6046-2025-0-4-57-69.
  7. Du Z., Peng Y., Teng H. et al. Formation and growth of precipitates in a Mg–7Gd–5Y–1Nd–2Zn–0,5Zr alloy aged at 200 °C. Journal of Magnesium Alloys, 2022, vol. 13 (3), pp. 1–14. DOI: 10.1016/j.jma.2022.10.012.
  8. Rokhlin L.L. Patterns of influence of various rare earth metals in magnesium alloys on their strength properties. Vestnik Kontserna VKO «Almaz-Antey», 2020, no. 3 (34), pp. 38–44.
  9. Mukhina I.Yu., Trofimov N.V., Leonov A.A., Rostovtseva A.S. Development of resource-saving technological processes in magnesium metallurgy. Metally, 2021, no. 6, pp. 16–24.
  10. Istomin A.V. Study of the distribution of aluminum oxide nanopowder in a polymer solution. Aviation materials and technologies, 2024, no. 1 (74), pp. 78–88. Available at: http://www.journal.viam.ru (accessed: June 20, 2025). DOI: 10.18577/2713-0193-2024-0-1-78-88.
  11. Salehi M., Maleksaeedi S., Sapari M.A.B. et al. Additive manufacturing of magnesium–zinc–zirconium (ZK) alloys via capillary-mediated binderless three-dimensional printing. Materials Desing, 2019, no. 169, pp. 115–124.
  12. Takagi H., Sasahara H., Abe T. et al. Material-property evaluation of magnesium alloys fabricated using wire-and-arcbased additive manufacturing. Additive Manufacturing, 2018, no. 24, pp. 498–507.
  13. Knezovis N., Topis A. Additive production of wire and arc – new achievement in production. Cham: Springer international publishing, 2019, pp. 65–71.
  14. Bachurin N., Stepakin V., Buryak E. Gas-Dynamic spraying in the restoration of machine parts. Proceeding of the Donbas National Academy of Civil Engineering and Architecture, 2024, no. 4 (168), pp. 42–45.
  15. Chavdarov A.V., Tolkachev A.A. Restoration of internal surfaces of small-diameter cylindrical parts by cold gas-dynamic spraying. Tekhnicheskiy servis mashin, 2020, no. 3 (140), pp. 128–136.
  16. Nefedov N.I., Guseva M.A., Khaskov M.A. et al. Peculiarities of temperature behavior of low-molecular fluorooligomers. Polymer Sciences. Series A, 2017, vol. 59, pp. 496–505. DOI: 10/1134/ S0965545X17040034.
  17. Javaid A., Czerwinski F. Progress in twin roll casting of magnesium alloys: A review. Journal of Magnesium and Alloys, 2021, no. 9, pp. 362–391.
  18. Bobryshev B.L., Moiseev V.S., Aleksandrova Yu.P. Improvement of complex processing of magnesium alloys during melting. Tekhnologii legkikh splavov, 2021, no. 3, pp. 35–44.
  19. Kipouros G.J., Sadoway D.R. Removal of Ca from Magnesium melt by Flux Refining. Materials Transactions, 2016, vol. 57, pp. 1156–1164. DOI: 10.1016/S1471-5317(01)00004-9.