Optimization of the solder composition for joining dissimilar EP975 and VKNA-25 alloys using modern computational systems

Galushka I.A., Afanasiev-Khodykin A.N., Panteleev M.D., Zotov S.D.
Galushka I.A., Afanasiev-Khodykin A.N., Panteleev M.D., Zotov S.D. Optimization of the solder composition for joining dissimilar EP975 and VKNA-25 alloys using modern computational systems // Proceedings of VIAM. 2026. No. 2. DOI: 10.18577/2307-6046-2026-0-2-37-48. URL: https://www.viam-works.ru/en/journal/2026/2/4
Keywords
brazing, a diffusive brazing, brazing alloy, nickel super alloys, rotor design GTE
Abstract

A nickel-based brazing metal designated VPr56 was developed for high-temperature diffusion brazing of bimetallic blisk-type components made from heat-resistant nickel alloys EP975 (disk) and VKNA-25 (blade). The study examined the influence of alloying elements (Ti, Nb, B) on the brazing metal’s key processing characteristics: melting temperature, wettability, joint uniformity, and susceptibility to erosion of the base metal. Experimental design and regression analysis were applied to optimize the composition. It was shown that VPr56 meets the requirements for joints of gas turbine engines (GTE) joints.

Reference list
  1. Inozemtsev A.A., Nikhamkin M.A., Sandratsky V.L. Gas turbine engines. Fundamentals of designing aircraft engines and power plants: in 5 vols. Moscow: Mashinostroenie, 2007, vol. 1: General information. Main parameters and requirements. Design and power schemes, pp. 7–17.
  2. Reed R.C. The superalloys: fundamentals and applications. Cambridge; New York: Cambridge University Press, 2006, pp. 363–372.
  3. Furrer D., Fecht H. Ni-Based Superalloys for Turbine Discs. JOM, 1999, vol. 51, pp. 14–17. DOI: s11837-999-0005-y.
  4. Klocke F., Schmitt R., Zeis M. et al. Technological and Economical Assessment of Alternative Process Chains for Blisk Manufacture. Procedia CIRP, 2015, vol. 35, pp. 67–72. DOI: 10.1016/j.procir.2015.08.052.
  5. Inozemtsev A.A., Nikhamkin M.A., Sandratsky V.L. Gas Turbine Engines. Fundamentals of Designing Aircraft Engines and Power Plants: in 5 vols. Moscow: Mashinostroenie, 2007, vol. 2: Compressors. Combustion Chambers. Afterburners. Turbines. Exhaust Devices, 368 p.
  6. Lunev A.N., Kurylev D.V. Review of Progressive Methods for Manufacturing Axial Monowheels of Aircraft Gas Turbine Engines. Fundamentalnye issledovaniya, 2016, no. 6-1, pp. 78–82. Available at: http://www.fundamental-research.ru/ru/article/view?id=40375 (accessed: June 20, 2025).
  7. Magerramova L.A., Vasiliev B.E. Bimetallic turbine blades with banded blades for gas turbine engines. Nauka i obrazovaniye: nauchnoye izdaniye MGTU im. N.E. Baumana, 2015, no. 6, pp. 143–156.
  8. Yuan J., Scarpa F., Titurus B. et al. Efficient computational techniques for mistuning analysis of bladed discs: A review. Mechanical Systems and Signal Processing, 2017, vol. 87, part A, pp. 71–90.
  9. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: June 20, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  10. Kolyadov E.V., Visik E.M., Gerasimov V.V., Bityutskaya O.N. Features of the morphology of the structure of nickel superalloy depending on the values of the axial and radial temperature gradients at the crystallization front. Aviation materials and technologies, 2024, no. 2 (75), pp. 15–24. Available at: http://www.journal.viam.ru (accessed: June 20, 2025). DOI: 10.18577/2713-0193-2024-0-2-15-24.
  11. Lashko N.F., Lashko S.V. Questions of theory and technology of soldering. Saratov: Publ. house Saratovsk. Univ., 1974, 248 p.
  12. Petrunin I.E., Markova I.Yu., Ekatova A.S. Metallurgy of soldering. Moscow: Metallurgiya, 1976, 264 p.
  13. Ospennikova O.G., Lukin V.I., Afanasyev-Khodykin A.N., Galushka I.A. Technology of the high temperature diffusive brazing of a bimetallic «blisk» design. Trudy VIAM, 2019, no. 9 (81), pp. 26–37. Available at: http://www.viam-works.ru (accessed: June 20, 2025). DOI: 10.18577/2307-6046-2019-0-9-26-37.
  14. Ospennikova O.G., Afanasyev-Khodykin A.N., Galushka I.A. Investigation of a brazed joint microstructure formation, made of dissimilar nickel super alloys and the complex brazing alloy. Trudy VIAM, 2021, no. 1 (95), pp. 3‒12. Available at: http://www.viam-works.ru (accessed: June 20, 2025). DOI: 10.18577/2307-6046-2021-0-1-3-12.
  15. Zhou X., Huang Y., Chen Y. et al. Brazing of Ni-based single crystal superalloy with high carbon content γ layer. Applied Surface Science, 2020, vol. 514, art. 145936. DOI: 10.1016/j.apsusc.2020.145936.
  16. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  17. Kendall M.J., Stewart A. Multivariate Statistical Analysis and Time Series. Moscow: Nauka, 1976, 736 p.
  18. Nalimov V.V., Chernova N.A. Statistical Methods for Designing Extreme Experiments. Moscow: Nauka, 1965, 339 p.
  19. Ivchenko G.I., Medvedev Yu.I. Mathematical Statistics. Moscow: Vysshaya Shkola, 1984, 248 p.
  20. Petrushin N.V., Visik E.M., Elyutin E.S. Improvement of the chemical composition and structure of castable nickel-base superalloy with low density. Part 2. Trudy VIAM, 2021, no. 4 (98), pp. 3–15. Available at: http://www.viam-works.ru (accessed: June 20, 2025). DOI: 10.18577/2307-6046-2021-0-4-3-15.