Investigation of deformation welding processes of semi-finished product made of alloy type EP718-ID

Yashin M.S., Kapitanenko D.V., Afanasiev-Khodykin A.N.
Yashin M.S., Kapitanenko D.V., Afanasiev-Khodykin A.N. Investigation of deformation welding processes of semi-finished product made of alloy type EP718-ID // Proceedings of VIAM. 2026. No. 2. DOI: 10.18577/2307-6046-2026-0-2-27-36. URL: https://www.viam-works.ru/en/journal/2026/2/3
Keywords
pressure welding, isothermal deformation, heat-resistant nickel alloys, heat treatment, soldering, computer modeling
Abstract

The article presents the results of a study of deformation welding processes of blanks made of EP718-ID alloy. Before upsetting, the blanks were soldered to protect the mating surfaces from oxidation and to improve the quality of the weld. Soldering was performed according to two methods: over the entire area of the mating surfaces and along the contour. After plastic deformation and heat treatment of the composite blanks, the weld on the stamping, pre-soldered along the contour of the mating surfaces, was destroyed after cooling. The welded joint on the stamping with soldering over the entire area remained inseparable.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Gelman A.S. Fundamentals of Pressure Welding. Moscow: Mashinostroenie, 1970, 311 p.
  3. Akhunova A.Kh., Galieva E.V., Povarova K.B., Bazyleva O.A., Valitov V.A., Dmitriev S.V., Drozdov A.A., Arginbaeva E.G. Modeling of Pressure Welding of Dissimilar Cast and Wrought Nickel-Based Alloys under Bulk Plastic Flow Conditions. Fundamentalnye problemy sovremennogo materialovedenia, 2016, vol. 13, no. 1, pp. 131–135.
  4. Galieva E.V., Povarova K.B., Drozdov A.A., Valitov V.A. Structure and properties of solid-phase joints of deformable nickel alloy EP975 and single-crystal intermetallic alloy VKNA-25 obtained by pressure welding with a degree of deformation of 24% under conditions of superplasticity of alloy EP975. Metally, 2018, no. 6, pp. 64–72.
  5. Valitov V.A., Povarova K.B., Bazyleva O.A., Drozdov A.A., Ovsepyan S.V., Galieva E.V. Research of solid compound formation during thermal deformation effect on intermetallic Ni3Al-alloy with a heat-resistant alloy EP975 and influence on the physical, mechanical and performance properties. Materials Science Forum, 2016, vol. 838–839, pp. 523–527. DOI: 10.4028/www.scientific.net/MSF.838-839.523.
  6. Galieva E.V., Klassma E.Y., Valitov V.A. Еffect of the pressure welding scheme on the microstructure of solid-state joints from nickel-based superalloys ek61 and EP975 with different phase compositions. Materials Technologies Design, 2024, vol. 6, no. 2 (17), pp. 59–66. DOI: 10.54708/26587572_2024_621759.
  7. Aviation Materials: in 9 vol. Handbook. Ed. R.E. Shalin. 7th ed., rev. and add. Moscow: ONTI, 1989, Vol. 3: Heat-Resistant Steels and Alloys. Alloys Based on Refractory Metals, part 1: Wrought Heat-Resistant Steels and Alloys, 567 p.
  8. Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), pp. 30–40. Available at: http://www.journal.viam.ru (accessed: May 30, 2025). DOI: 10.18577/2713-0193-2022-0-1-30-40.
  9. Krokhina V.A., Arislanov А.A., Putyrskiy S.V., Anisimova A.Yu. Investigation of the regularities of the formation of the structure of rods made of titanium alloy VT6 depending on various technological schemes of manufacture. Aviation materials and technologies, 2023, no. 4 (73), pp. 36–44. Available at: http://www.journal.viam.ru (accessed: May 30, 2025). DOI: 10.18577/2713-0193-2023-0-4-36-44.
  10. Method for manufacturing composite blanks of the «disk-disk» and «disk-shaft» types from heat-resistant titanium and nickel alloys: pat. RU 2610658C2 Rus. Federation; appl. 05.08.15; publ. 14.02.17.
  11. Doronin O.N., Gorlov D.S., Azarovsky E.N., Kochetkov A.S. Study of the structure and properties of a heat-resistant coating at high-temperature deformation of samples from titanium intermetallic alloy. Aviation materials and technology, 2021, no. 1 (62), pp. 61–70. Available at: http://www.journal.viam.ru (accessed: May 30, 2025). DOI: 10.18577/2713-0193-2021-0-1-61-70.
  12. Sirotinskiy A.A. Production Technology and industrial publication of silicate enamel coatings. Ekspozitsiya Neft i Gaz, 2007, no. 42, pp. 36–38.
  13. Tsepin M.A., Begnarsky V.V., Lisunets N.L. et al. Using specialized programs in the development of technological processes for metal forming. Tsvetnye metally, 2007, no. 5, pp. 98–101.
  14. Stebunov S.A., Biba N.V. Qform – a program created for technologists. Kuznechno-shtampovoye proizvodstvo, 2004, no. 9, pp. 38–43.
  15. Naprienko S.A., Erak A.D., Afanasev-Khodykin A.N., Davidenko A.N. Structure variation and properties of soldered joints VPr16 under various temperature exposures. Aviation materials and technologies, 2023, no. 1 (70), pp. 115–125. Available at: http://www.journal.viam.ru (accessed: May 30, 2025). DOI: 10.18577/2713-0193-2023-0-1-115-125.