Study of the impact of technological parameters on coating deposition using the UMP-500 unit
UDC
629.7.023.224
DOI
10.18577/2307-6046-2026-0-2-139-153
Article PDF (Russian)
(1.71 MB)
How to cite
Kashin D.S., Stekhov P.A. Study of the impact of technological parameters on coating deposition using the UMP-500 unit // Proceedings of VIAM. 2026. No. 2. DOI: 10.18577/2307-6046-2026-0-2-139-153. URL: https://www.viam-works.ru/en/journal/2026/2/13
Keywords
nickel alloys, aluminium layer, chemical vapor depostion, heat resistant, diffusion coating, aluminizing
Abstract
This article investigates the influence of process parameters, such as process temperature, aluminide coating application time, and the vacuum annealing temperature of the formed coating. At high temperatures uniform aluminide coating layer forms across the entire specimen surface. This finding opens up opportunities for applying these coatings to high-tech components with complex external and internal geometries manufactured via additive manufacturing. Such an approach will ultimately enhance the efficiency and reliability of modern gas turbine engines.
Reference list
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New-generation materials and digital additive technologies for the production of resource parts at FSUE VIAM. Part 1. Materials and synthesis technologies. Elektrometallurgiya, 2022, no. 1, pp. 2–12. DOI: 10.31044/1684-5781-2022-0-1-2-12.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S., Dynin N.V. New-generation materials and digital additive technologies for the production of resource parts at FSUE VIAM. Part 3. Adaptation and creation of materials. Elektrometallurgiya, 2022, no. 4, pp. 15–25. DOI: 10.31044/1684-5781-2022-0-4-15-25.
- Kablov E.N., Evgenov A.G., Petrushin N.V., Bazyleva O.A., Mazalov I.S. New-generation materials and digital additive technologies for the production of resource parts at VIAM. Part 4. Development of heat-resistant materials. Elektrometallurgiya, 2022, no. 5, pp. 8–19. DOI: 10.31044/1684-5781-2022-0-5-8-19.
- Shchetinina N.D., Kuznetsova P.E., Dynin N.V., Selivanov A.A. Aluminum alloys with additions of Sc and Zr in additive manufacturing (review). Aviation materials and technologies, 2021, no. 3 (64), pp. 19–34. Available at: http://www.journal.viam.ru (accessed: June 23, 2025). DOI: 10.18577/2713-0193-2021-0-3-19-34.
- Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: June 23, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.
- Nerush S.V., Sviridov A.V., Afansiev-Khodykin A.N., Galushka I.A., Tarasov S.A. Development of brazing technology for parts obtained by additive technologies from cobalt based metal powder composition. Aviation materials and technologies, 2022, no. 2 (67), pp. 18–29. Available at: http://www.journal.viam.ru (accessed: June 23, 2025). DOI: 10.18577/2713-0193-2022-0-2-18-29.
- Marakhovskij P.S., Barinov D.Ya., Shorstov S.Yu., Vorobev N.N. On creation of physical and mathematical models of heat and mass transfer during manufacturing by additive technologies (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 111–119. Available at: http://www.journal.viam.ru (accessed: June 23, 2025). DOI: 10.18577/2713-0193-2022-0-2-111-119.
- Khasanova L.A., Drevnyak V.V., Zhukov A.A., Saadatibai M. Analysis of defects in protective coatings during their application. Nauchniy vestnik MGTU GA, 2015, no. 222, pp. 207–212.
- Simonov V.N., Unchikova M.V., Pakhomova S.A. Improving the Quality of Chrome-Aluminized Coatings Obtained by the Gas Circulation Method. Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyenie, 2016, no. 2, pp. 134–145. DOI: 10.18698/0236-3941-2016-2-134-145.
- Lesnikov V.P., Kuznetsov V.P., Konakova I.P., Moroz E.V. Design of Complex Protective Coatings for Single-Crystal Cooled Turbine Blades of Modern GTEs. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2012, no. 3 (34), pp. 211–216.
- Bakhrunov K.K. Mechanical properties of coatings on nickel-based heat-resistant alloys obtained by circulation chromium aluminizing. Izvestiya vysshikh uchebnykh zavedeniy. Mashinostroyenie, 2011, no. 7, pp. 63–68.
- Method of diffusion chromium aluminizing of a part surface: pat. 2270880 Rus. Federation; appl. 29.09.04; publ. 27.02.06.
- Method of applying two-component chromium-aluminum coatings to the internal cavities of cooled working blades of gas turbines and device for implementing the method: pat. 2520237 Rus. Federation; appl. 28.02.12; publ. 20.06.14.
- Peng X. Metallic Coatings for high-temperature oxidation resistance. Thermal Barrier Coatings: Woodhead Publishing Series in Metals and Surface Engineering. Woodhead Publishing, 2011, pp. 53–74. DOI: 10.1533/9780857090829.1.53.
- Method of protecting surface areas of a part: pat. 2232205 Rus. Federation; appl. 06.09.02; publ. 10.07.04.
- Method of protecting the blade surface: pat. 2252110 Rus. Federation; appl. 09.10.03; publ. 20.05.05.
- Diffusion Coating Mixtures: pat. US 4617202; appl. 09.10.81; publ. 14.10.86.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.