Study of the structure and physical and mechanical properties of reinforced composite material based on silicon carbide

Kolmogorov A.Yu., Sorokin O.Ju., Vaganova M.L., Chaynikova A.S.
Kolmogorov A.Yu., Sorokin O.Ju., Vaganova M.L., Chaynikova A.S. Study of the structure and physical and mechanical properties of reinforced composite material based on silicon carbide // Proceedings of VIAM. 2026. No. 2. DOI: 10.18577/2307-6046-2026-0-2-117-126. URL: https://www.viam-works.ru/en/journal/2026/2/11
Keywords
silicon carbide, composite material, internal stresses, dispersed composition, filler, matrix
Abstract

The structure and physical and mechanical properties of a silicon carbide–based composite material reinforced with metallic fibers were studied. The optimal content of the reinforcing phase was determined, and the fiber surface was modified to improve adhesion to the matrix. Impact toughness, three-point bending strength, and the coefficient of linear thermal expansion were measured. It was found that fiber reinforcement contributes to the redistribution of internal stresses, leading to improved resistance to impact and bending loads. A correlation was revealed between the strength characteristics and the amount  of the reinforcement.

Reference list
  1. Breede F., Hofmann S., Jain N., Jemmali R. Design, manufacture, and characterization of a carbon fiber-reinforced silicon carbide nozzle extension. International Journal of Applied Ceramic Technology, 2016, vol. 13, no. 1, pp. 3–16.
  2. Krenkel W. Carbon fibre reinforced silicon carbide composites (C/SiC, C/C‒SiC). Handbook of Ceramic Composites. Ed. N.P. Bansal. New York, USA: Springer Science+Business Media Inc., 2005, pp. 117–148.
  3. Krenkel W., Berndt F. C/C‒SiC composites for space applications and advanced friction systems. Materials Science and Engineering A, 2005, vol. 412, no. 1–2, pp. 177–181.
  4. Semeyko K.V., Malinovsky A.I., Grebenkov A.Zh. et al. Development of technologies for producing silicon carbide (review). Vestnik NYATS RK, 2021, no. 2, pp. 30–41.
  5. Khin M., Popova N.A., Lukin E.S. Composite ceramics based on silicon carbide. Novye ogneupory, 2019, no. 4, pp. 34–39.
  6. Babashov V.G., Varrik N.M., Maksimov V.G., Samorodova O.N. Oxide fiber coated with silicon carbide for producing composite materials. Aviation materials and technologies, 2021, no. 3 (64), pp. 94–104. Available at: http://www.journal.viam.ru (accessed: June 02, 2025). DOI: 10.18577/2713-0193-2021-0-3-94-104.
  7. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: June 02, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  8. Garshin A.P., Nilov A.S., Galinskaya O.O., Krasnov V.I. Prospects for development and ways to improve aircraft braking systems on the base ceramic matrix composite materials (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 104–121. Available at: http://www.journal.viam.ru (accessed: June 02, 2025). DOI: 10.18577/2713-0193-2023-0-2-104-121.
  9. Zhitnyuk S.V. Oxygen-free ceramic materials for the space technics (review). Trudy VIAM, 2018, no. 8 (68), pp. 81–88. Available at: http://www.viam-works.ru (accessed: June 02, 2025). DOI: 10.18577/2307-6046-2018-0-8-81-88.
  10. Evdokimov S.A., Shchegoleva N.E., Kachaev A.A. Methods for joining ceramic composite materials based on SiC with ceramic and metallic materials (review). Aviation materials and technologies, 2022, no. 3 (68), pp. 75–83. Available at: http://www.journal.viam.ru (accessed: June 02, 2025). DOI: 10.18577/2713-0193-2022-0-3-75-83.
  11. Tolmachev Ya.V., Zavarzin S.V., Loshchinina A.O., Knyazev A.V. High temperature oxide corrosion of ceramic materials in turbine engines. Trudy VIAM, 2023, no. 7 (125), pp. 69–83. Available at: http://www.viam-works.ru (accessed: June 02, 2025). DOI: 10.18577/2307-6046-2023-0-7-69-83.
  12. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), pp. 32–51. Available at: http://www.viam-works.ru (accessed: June 02, 2025). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  13. Perevislov S.N., Bespalov I.A., Tomkovich M.V. Effect of Modifying the Structure of Silicon Carbide-Based Materials on Their Dynamic Properties. Novye ogneupory, 2018, no. 7, pp. 39–44.
  14. Petrov V.M., Kozlov S.D. Glass-crystalline and glass-ceramic materials: a tutorial. Moscow: Bauman Moscow State Tech. Univ., 2012, 256 p.
  15. Tulin A.A. Glass-ceramics: structure, properties, application. Moscow: Nauka, 2005, 312 p.
  16. Lebedev A.N., Mikhailov V.V. Composite materials based on glass-ceramics and metals. St. Petersburg: BHV-Petersburg, 2010, 228 p.
  17. Kuznetsov V.A. Reinforcement of Reinforced Concrete Structures. Moscow: Stroyizdat, 1985, 240 p.
  18. Ivanov A.L. Influence of Reinforcement Surface Condition on the Strength of Adhesion to Concrete. Beton i zhelezobeton, 2001, no. 9, pp. 14–17.
  19. Trushnikov D.N. Behavior of Fibrous Reinforcing Elements in Composites under Dynamic Loads. Fizika prochnosti i plastichnosti materialov, 2012, vol. 24, no. 3, pp. 125–131.
  20. Briggs J. Engineering ceramics in Europe and the USA. Worcester, 2011, 331 p.
  21. Crouch I.G. Characterization, significance and detection of manufacturing defects in Reaction Sintered Silicon Carbide armour materials. Ceramics International, 2015, no. 9, pp. 11581–11591.
  22. Dyakin P.V., Pivinsky Yu.E., Prokhorenkov D.S., Doroganov V.A. Phase composition, structure and some properties of materials based on bauxite HCBS of composite composition in the Al2O3‒SiO2‒SiC system. Vestnik BGTU imeni V.G. Shukhova, 2020, no. 2, pp. 115–125.