Water-based enamel for coating aircraft interior elements
UDC
629.7.023.222
DOI
10.18577/2307-6046-2025-0-9-102-110
Article PDF (Russian)
(572.28 KB)
How to cite
Kozlova A.A., Shunina M.A., Kozlov I.A. Water-based enamel for coating aircraft interior elements // Proceedings of VIAM. 2025. No. 9. DOI: 10.18577/2307-6046-2025-0-9-102-110. URL: https://www.viam-works.ru/en/journal/2025/9/8
Keywords
paint materials, fire safety, styrene-acrylic dispersion, adhesion, hardness, scratch resistance, passenger cabin
Abstract
This paper examines the properties of a water-based enamel designed for coating interior structural elements of aircraft. We have performed a comparative analysis of the properties of the developed enamel with existing domestic and imported analogues. It is shown that the developed enamel meets modern fire safety requirements. The use of an aqueous styrene-(met) acrylates copolymer dispersion ensures environmental friendliness and safety by eliminating toxic solvents and enabling a high level of physical and mechanical properties.
Reference list
- Kondrashov E.K. Paints and varnishes and coatings based on them in mechanical engineering. Moscow: Paint-Media, 2021, р. 141.
- Water-based composition for paint and varnish coating: pat. 2338766 Rus. Federation; appl. 27.08.07; publ. 20.11.08.
- Kondrashov E.K., Semenova L.V., Kuznetsova V.A., Malova N.E., Lebedeva T.A. Development of aviation paints and varnishes. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 5, pp. 49–54.
- Kondrashov E.K., Kuznetsova V.A., Lebedeva T.A., Semenova L.V. Main directions for improving the operational, technological and environmental characteristics of paint and varnish coatings for aviation equipment. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 96–102.
- Barbotko S.L., Volny O.S., Kiriyenko O.A., Shurkova E.N. Fire safety assessment of polymeric materials for aviation purposes: analysis of the state, testing methods, development prospects, methodological features. Ed. E.N. Kablov. Moscow: VIAM, 2018, 408 p.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Starkov A.I., Kutsevich K.E., Isaev A.Yu., Barbotko S.L. Study of flammability, smoke formation and toxicity in the process of combustion of polymer composite materials and three-layer honeycomb structures based on them. Trudy VIAM, 2025, no. 6 (148), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 24, 2025). DOI: 10.18577/2307-6046-2025-0-6-73-85.
- Kurnosov A.O., Melnikov D.A., Sokolov I.I. Structural glass-reinforced plastics purposed for aviation industry. Trudy VIAM, 2015, no. 8, paper no. 08. Available at: http://viam-works.ru (accessed: July 24, 2025). DOI: 10.18577/2307-6046-2015-0-8-8-8.
- Davydova I.F., Kavun N.S. Fibreglasses ‒ multipurpose composite materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 253–260.
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: July 24, 2025). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Garashchenko A.N., Kulkov A.A., Strakhov V.L. The effect of the service life on the flame-retardant efficiency of the bulging coatings and the fire resistance of structures. Aviation materials and technologies, 2022, no. 2 (67), paper no. 09. Available at: http://www.journal.viam.ru (accessed: 28.03.2025). DOI: 10.18577/2713-0193-2022-0-2-97-110.
- Kuznetsova V.А., Zheleznyak V.G., Kurshev E.V., Yemelyanov V.V. Research of fuel- and water resistance of coatings based on the filled epoxy-thiokol polymeric compositions. Aviation materials and technologies, 2021, no. 2 (63), paper no. 10. Available at: http://www.journal.viam.ru (accessed: July 24, 2025). DOI: 10.18577/2713-0193-2021-0-2-93-102.
- Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
- Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Report of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: UB of RAS, 2016, pp. 25–26.
- Barbotko S.L., Petrova A.P., Volny O.S., Bochenkov M.M. Methods used to assess the fire safety of polymer binders (review). Vse materialy. Entsiklopedicheskiy spravochnik, 2019, no. 12 pp. 21–29.
- Barbotko S.L. Development of the fire safety test methods for aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 516–526. DOI: 10.18577/2071-9140-2017-0-S-516-526.