Influence of amodified film-forming agent on the properties of anti-wear matte coating used to protect cabin and dashboard components in aircraft

Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Kurshev E.V.
Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Kurshev E.V. Influence of amodified film-forming agent on the properties of anti-wear matte coating used to protect cabin and dashboard components in aircraft // Proceedings of VIAM. 2025. No. 9. DOI: 10.18577/2307-6046-2025-0-9-90-101. URL: https://www.viam-works.ru/en/journal/2025/9/7
Keywords
polymer film-forming agent, modifier, hardener, coating, structure, wear resistance, adhesion, water resistance, coating gloss, elasticity
Abstract

Currently, special requirements are imposed to the quality and appearance of the coverings used to protect elements of cabin and dashboards in aircraft. These requirements are associated with the need of providing high level of visual and overall performance of the pilot both under natural and artificial lighting, as well as with fire safety. This work is devoted to studying the properties of the decorative, fireproof, wear-resistant matte paint coatings obtained using a two-phase polymer system: polyester – fluoropolyurethane oligomer.

Reference list
  1. Zhitomirsky G.I. Aircraft design. Moscow: Mashinostroenie, 1991, 400 p.
  2. Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
  3. Kablov E.N. Aviation Materials Science in the 21st Century. Prospects and Objectives. Aviation Materials. Selected Works of VIAM 1932–2002. Moscow: MISIS–VIAM, 2002, pp. 23–47.
  4. Kablov E.N. New-Generation Materials – the Basis for Innovation, Technological Leadership, and National Security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  5. Kablov E.N. New-Generation Materials. Zashchita i bezopasnost, 2014, no. 4, pp. 28–29.
  6. Kablov E.N. Main Results and Directions of Development of Materials for Advanced Aviation Technology. 75 Years. Aviation Materials. Moscow: VIAM, 2007, pp. 20–26.
  7. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: July 14, 2025). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  8. Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Zheleznyak V.G. Trends in the development of matte wear-resistant paint coatings. Trudy VIAM, 2023, no. 10 (128), paper no. 12. Available at: http://www.viam-works.ru (accessed: July 14, 2025). DOI: 10.18577/2307-6046-2023-0-10-132-144.
  9. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  10. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (ассеssed: July 07, 2025). DOI:10.18577/2713-0193-2022-0-1-110-119.
  11. Kozlova A.A., Kondrashov E.K. Influence of molecular weight and elemental composition of isocyanates on the properties of fluoropolyurethane enamels. Aviation materials and technologies, 2023, no. 4 (73), paper no. 09. Available at: http://www.journal.viam.ru (accessed: July 28, 2025). DOI: 10.18577/2713-0293-2023-0-4-92-100.
  12. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  13. Makushchenko I.S., Kozlov I.А., Smirnov D.N., Kurshev E.V., Lonskii S.L. Study of the microstructure and distribution of corrosion inhibitors in polysulfide sealant. Aviation materials and technologies, 2025, no. 2 (79), paper no. 10. Available at: http://www.journal.viam.ru (accessed: July 24, 2025). DOI: 10.18577/2713-0193-2025-0-2-128-136.
  14. Zhelezina G.F., Kulagina G.S., Soloveva N.A., Barbotko S.L. Influence of composition and structure on the fire resistance of aramid organoplastics. Aviation materials and technologies, 2024, no. 3 (76), paper no. 07. Available at: http://www.journal.viam.ru (accessed: 24.07.2025). DOI: 10.18577/2713-0193-2024-0-3-81-89.
  15. Yulovskaya V.D. Oligomers. Rubber – oligomeric compositions, structure and properties: textbook. Moscow, 2008, 46 p.
  16. Petrov G.N., Sinaisky A.G., Dahlgren I.V. Liquid hydrocarbon rubbers and their application areas. Klei. Germetiki. Tekhnologii, 2009, no. 10, pp. 24–27.
  17. Semenova L.V., Nefedov N.I., Belova M.V., Laptev A.B. Systems of paint coatings for helicopter equipment. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 56–61. DOI: 10.18577/2071-9140-2017-0-4-56-61.
  18. Sukhareva L.A. Polyester Coatings. Structure and Properties. Moscow: Khimiya, 1987, 191 p.
  19. Berlin A.A., Basin V.E. Basics of Polymer Adhesion. Moscow: Khimiya, 1969, 319 p.
  20. Yakovlev A.D., Yakovlev S.A. Functional-Purpose Paint and Varnish Coatings. St. Petersburg: Khimizdat, 2016, 272 p.
  21. Noskov A.M., Novikov N.I. Curing of Glycidyl Ethers with Amines in the Presence of Hydroxyl Groups. Zhurnal prikladnoy khimii, 2008, vol. LW, no. 12, pp. 2733–2737.
  22. Chalykh A.E. Diffusion in Polymer Systems. Moscow: Khimiya, 1987, pp. 252–266.
  23. Zinoviev V.E. On the issue of the relationship between adhesion and the quality of the surface layer of the substrate of the adhesive joint. Vestnik RGUPS, 2010, no. 4, pp. 5–9.
  24. Kuznetsova V.A., Shapovalov G.G., Marchenko S.A., Kovrizhkina N.A., Silaeva A.A. Paint coatings on the basis of epoxy and acrylic diphasic polymeric system for coloring of elements of cabin of pilots and dashboards. Trudy VIAM, 2020, no. 12 (94), paper no. 09. Available at: http://www.viam-works.ru (accessed: July 07, 2025). DOI: 10.18577/2307-6046-2020-0-12-87-95.
  25. Kondrashov E.K., Kozlova A.A. Paint coatings with special optical properties. Trudy VIAM, 2023, no. 9 (127), paper no. 09. Available at: http://www.viam-works.ru (accessed: July 04, 2025). DOI: 10.18577/2307-6046-2023-0-9-101-109.
  26. Semenova L.V., Rodina N.D., Nefedov N.I. An effect of roughness of paint and varnish coating systems on service properties of aircraft. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 37–40.
  27. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.