Comparative analysis of mechanical properties of heat-resistant titanium alloy VT46 in cast and forged conditions

Kashapov O.S., Makushina M.A., Kalashnikov V.S., Lavrova O.Yu.
Kashapov O.S., Makushina M.A., Kalashnikov V.S., Lavrova O.Yu. Comparative analysis of mechanical properties of heat-resistant titanium alloy VT46 in cast and forged conditions // Proceedings of VIAM. 2025. No. 9. DOI: 10.18577/2307-6046-2025-0-9-19-34. URL: https://www.viam-works.ru/en/journal/2025/9/2
Keywords
heat-resistant titanium alloys, titanium alloy VT46, forgings, castings, mechanical properties, microstructure
Abstract

The paper presents comparison of main mechanical properties of rods, forgings and castings made of heat-resistant titanium pseudo-alpha alloy VT46 (VT46L), as well as similar alloys of the same class and application in the range of operating temperatures. Values of long-term strength at 500 and 550 °С have been presented specifically. The article shows microstructure study results of the said semi-finished products material. It provides a generalized description of the technology for manufacturing semi-finished products, indicating features that distinguish VT46 alloy from serial titanium alloys. Possible application areas of VT46 alloy in relation to engine parts and aircraft equipment are discussed.

Reference list
  1. Moiseyev V.N. Titanium Alloys: Russian Aircraft and Aerospace Applications. New York: CRC Press, 2006, 214 p.
  2. Sun Z., Wu H., Ma X. et al. Dependence of Microstructure on Solution and Aging Treatment for Near-b Forged TA15 Ti-Alloy. Journal of Materials Engineering and Performance, 2016, vol. 25 (10), pp. 4549–4560. DOI: 10.1007/s11665-016-2282-2.
  3. Wu H., Sun Z., Cao J., Yin Z. Microstructure and Mechanical Behavior of Heat-Treated and Thermomechanically Processed TA15 Ti Alloy Composites. Journal of Materials Engineering and Performance, 2019, vol. 28 (2), pp. 788–799. DOI: 10.1007/s11665-019-3881-5.
  4. Sun Z., Wang X., Zhang J., Yang H. Prediction and control of equiaxed α in near-β forging of TA15 Ti-alloy based on BP neural network: For purpose of tri-modal microstructure. Materials Science & Engineering, 2014, vol. 591, pp. 18–25. DOI: 10.1016/j.msea.2013.10.080.
  5. Zhu S., Yang H., Guo L.G., Fan X.G. Effect of cooling rate on microstructure evolution during α/β heat treatment of TA15 titanium alloy. Materials characterization, 2012, vol. 70, pp. 101–110. DOI: 10.1016/j.matchar.2012.05.009.
  6. Solonin O.P., Glazunov S.G. Modern heat-resistant titanium alloys and prospects for their application in engines. Moscow: Metallurgiya, 1974, 448 p.
  7. Yashin M.S., Kapitanenko D.V. Investigation of the structure and properties of the VT3-1 alloy in relation to the technology for obtaining stampings of disks and turbine blades. Trudy VIAM, 2023, no. 8 (126), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 22, 2025). DOI: 10.18577/2307-6046-2023-0-8-52-63.
  8. Yakovlev M.M., Yarullin R.R., Shlyannikov V.N. Parameters of fracture resistance of a simulation model of a compressor disk. Vestnik Permskogo natsionalnogo issledovatelskogo politekhnicheskogo universiteta. Ser.: Mekhanika, 2020, no. 3, pp. 98–107. DOI: 10.15593/perm.mech/2020.3.10.
  9. Petrov A.P., Bespalov A.V., Sokolov A.V., Shlensky A.G. Hot hydrostatic extrusion of titanium blanks in the production of compressor blades for gas turbine engines. Tekhnologiya legkikh splavov, 2022, no. 1, pp. 58–66. DOI: 10.24412/0321-4664-2022-1-58-66.
  10. Bratan S.M., Roshchupkin S.I., Chasovitina A.S., Gupta K. Influence of relative vibrations of the abrasive tool and the workpiece during finish grinding on the probability of material removal. Obrabotka metallov (tekhnologiya, oborudovaniye, instrumenty), 2022, vol. 24, no. 1, pp. 33–47. DOI: 10.17212/1994-6309-2022-24.1-33-47.
  11. Egorova Yu.B., Davydenko L.V., Belova S.B. Statistical comparison of long-term and short-term strength of titanium alloys at operating temperatures. Tekhnologiya legkikh splavov, 2024, no. 1, pp. 13–22. DOI: 10.24412/0321-4664-2024-1-13-22.
  12. Lomakin E.V., Bragov A.M., Konstantinov A.Yu. et al. Modeling the behavior of titanium alloy VT20 under impact interaction. Vestnik Nizhegorodskogo universiteta im. N.I. Lobachevskogo, 2011, no. 1, pp. 129–132.
  13. Gadalov V.N., Kutepov S.N., Filonovich A.V. et al. Monitoring of numerical modeling of the process of surface-hardening treatment of titanium alloys VT20 and OT4. Izvestiya TulGU. Ser.: Tekhnicheskiye nauki, 2023, no. 9, pp. 354–358. DOI: 10.24412/2071-6168-2023-9-349-350.
  14. Soler Ya.I., Shi M. Improving the efficiency of using silicon carbide abrasive wheels in surface grinding of titanium alloy VT20. Mashinostroyenie i mashinovedenie, 2016, no. 8 (115), pp. 43–55.
  15. Zenkov E.V. Experimental studies of the strength of models of connecting rods of automobile engines made of titanium alloy VT20. Mezhdunarodnyy nauchno-issledovatelskiy zhurnal, 2021, no. 11 (113), part 1, pp. 23–28. DOI: 10.23670/IRJ.2021.113.11.006.
  16. Antipin N.A., Getsov L.B., Gnedenkov E.V. et al. Strength and crack resistance of centrifugal compressor wheels. Gazovaya promyshlennost, 2017, no. 11 (760), pp. 120–128.
  17. Tisarev A.Yu., Vasilevich N.M. Study of the influence of non-axisymmetric elements of the engine air system on flow parameters, temperature fields, and deformations of gas turbine engine parts. Vestnik SGAU, 2012, no. 3 (34), pp. 279–284.
  18. Makushina M.A., Kochetkov A.S., Nochovnaya N.A. Cast titanium alloys for aviation equipment (review). Trudy VIAM, 2021, no. 7 (101), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 22, 2025). DOI: 10.18577/2307-6046-2021-0-7-39-47.
  19. Kishalov A.E., Lipatov V.D. Automated design of the main units of a turbofan turbofan engine using the AL-31F engine family as an example. Vestnik UGATU, 2020, vol. 24, no. 4 (90), pp. 48–56.
  20. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., add. and rev. Moscow: VIAM, 2010, vol. 6: Titanium alloys, 95 p.
  21. Gunyaeva A.G., Kurnosov A.O., Slavin A.V. Experience in the use of polymer composite materials developed by NRC «Kurchatov Institute» – VIAM in engines for civil aircraft. Aviation materials and technologies, 2024, no. 4 (77), paper no. 06. Available at: http://www.journal.viam.ru (accessed: 28.07.2025). DOI: 10.18557/2713-0193-2024-0-4-82-94.
  22. Andryushkin A.Yu., Komarov K.A., Gumanenko Ya.D. Influence of operating temperature on the choice of material for the optimal design of the aircraft power strut. Aerokosmicheskaya tekhnika i tekhnologii, 2024, vol. 2, no. 4, pp. 68–79. DOI: 10.52467/2949-401X-2024-2-4-68-79.
  23. Kalashnikov V.S., Reshetilo L.P., Chuchman O.V., Naprienko S.A. Strength and reliability of rods and rotor blade stamps made of heat-resistant industrial titanium alloys and modern pseudo-α-titanium alloy. Trudy VIAM, 2022, no. 2 (108), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 19, 2025). DOI: 10.18577/2307-6046-2022-0-2-13-31.
  24. Kablov E.N. Materials and technologies of VIAM for «Aviadvigatel». Permskie aviatsionnye dvigateli, 2014, no. 31, pp. 43–47.
  25. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  26. Kashapov O.S., Reshetilo L.P., Kalashnikov V.S., Pavlova T.V. On the influence of cooling rates on the microstructure and properties of heat-resistant titanium pseudo-alpha alloy during solid solution heat treatment with air cooling. Metally, 2021, no. 6, pp. 46–61.
  27. Kashapov O.S., Pavlova T.V., Kalashnikov V.S., Kondrateva A.R. Research of influence of alloying elements content on properties of high strength near alpha heat resistance titanium alloy VT46. Trudy VIAM, 2016, no. 9, paper no. 06. Available at: http://www.viam-works.ru (accessed: July 28, 2025). DOI: 10.18577/2307-6046-2016-0-9-6-6.
  28. Karachevtsev F.N., Alekseev A.V., Letov A.F., Dvoretskov R.M. Plasma methods of nickel alloys elemental chemical composition analysis. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 483–497. DOI: 10.18577/2071-9140-2017-0-S-483-497.
  29. Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. Practical guide to metallography of titanium-based alloys and its intermetallic compounds: a tutorial. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
  30. Makushina M.A., Kochetkov A.S., Vinogradov I.D. The influence of various modes of hot isostatic pressed and heat treatment on structure and properties of castings from the VT40L alloy. Trudy VIAM, 2023, no. 10 (128), paper no. 03. Available at: http://www.viam-works.ru (accessed: July 22, 2025). DOI: 10.18577/2307-6046-2023-0-10-24-34.
  31. Rajan S., Wanjara P., Gholipour J., Kabir A. Joining of Dissimilar Alloys Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si Using Linear Friction Welding. Materials, 2020, no. 13, pp. 3664–3689. DOI: 10.3390/ma13173664/.
  32. Kim Y., Jeong H., Park J. et al. Optimizing process parameters for hot forging of Ti-6242 alloy: A machine learning and FEM simulation approach. Journal of Materials Research and Technology, 2023, no. 27, pp. 8228–8243. DOI: 10.1016/j.jmrt.2023.11.193.
  33. Li Q., Chen E., Bice D., Dunand D. Mechanical Properties of Cast Ti-6Al-2Sn-4Zr-2Mo Lattice Block Structures. Advanced engineering materials, 2008, no. 10, pp. 939–942.
  34. Bashir S., Thomas M.C. Creep and high temperature low cycle fatigue of cast Ti-6Al-2Mo-4Zr-2Sn. Titanium’ 92. Science and Technology. The Minerals, Metals and Materials Society, 1993, pp. 319–326.