Properties of coating systems with a universal cold-curing putty with fluoroplastic, fluoro-rubber and polyurethane enamels after exposure to various performance factors

Marchenko S.A., Skivko P.V., Kuznetsova V.A.
Marchenko S.A., Skivko P.V., Kuznetsova V.A. Properties of coating systems with a universal cold-curing putty with fluoroplastic, fluoro-rubber and polyurethane enamels after exposure to various performance factors // Proceedings of VIAM. 2025. No. 9. DOI: 10.18577/2307-6046-2025-0-9-135-148. URL: https://www.viam-works.ru/en/journal/2025/9/11
Keywords
universal cold-curing putty, coating systems, adhesion, impact strength, water absorption, artificial aging, fungus resistance
Abstract

This study examines the properties of paint coatings based on a universal cold-curing putty with fluoroplastic, fluoro-rubber and polyurethane enamels in their initial state and after exposure to various operational factors. The results show that the use of putty in systems with different enamels does not affect the appearance, fungal growth and adhesion of paint coatings. The impact resistance of coating systems containing this putty shows no deterioration after testing (compared to systems with the putty in its initial state).

Reference list
  1. Kablov E.N. Aviation Materials Science: Results and Prospects. Vestnik Rossiyskoy akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
  2. Kablov E.N. Structural and Functional Materials – the Basis of Economic and Scientific-Technical Development of Russia. Voprosy materialovedeniya, 2006, no. 1, pp. 64–67.
  3. Kablov E.N. Aviation Materials Science in the 21st Century. Prospects and Tasks. Aviation Materials. Selected Works of VIAM 1932–2002. Moscow: MISiS–VIAM, 2002, pp. 23–47.
  4. Barannikov A.A., Veshkin E.A., Sudyin Yu.I., Mishunin N.N. Materials, technologies and equipment developed by the National Research Center «Kurchatov Institute» – VIAM for repairing products made of polymer composite materials for various purposes. Aerokosmicheskaya tekhnika i tekhnologii, 2025, vol. 3, no. 1, pp. 82–96.
  5. Kablov E.N. New generation materials – the basis of innovations, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  6. Pegov I.L. Comparative analysis of modern paints and varnishes. Vestnik NGIEI, 2014, no. 10, pp. 98–103.
  7. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  8. Semenova L.V., Karimova S.A., Polyakova A.V. Modern integrated protection systems for structures made of metal, polymer composite materials and their compounds. Novosti materialovedeniya. Nauka i tekhnika, 2014, no. 3, paper no. 02. Available at: http://materialsnews.ru (accessed: July 16, 2025).
  9. Andryushkin A.Yu., Vedernikov A.Yu., Khmelevskoy N.Yu. Technological features of applying paint and varnish coatings to the external surfaces of aircraft and helicopters. Aerokosmicheskaya tekhnika i tekhnologii, 2023, vol. 1, no. 4, pp. 103–115.
  10. Kucherenko E.V., Shcherbakov A.S., Arzamascev S.V. Composite materials based on polyester resin. Sovremennye innovatsii, 2016, no. 3 (5), pp. 5–7.
  11. Shmoilov E.E., Fedotov M.Yu., Sharutin I.A. et al. Polymer composites for external reinforcement of building structures. International Journal for Computational Civil and Structural Engineering, 2024, vol. 20 (1), pp. 21–34.
  12. Brock T. Unsaturated polyesters. European Guide to Paints and Coatings. Moscow: Paint-Media, 2007, pp. 73–78.
  13. Marchenko S.A., Skivko P.V. Effect of temperature on drying time and viability of epoxyvinyl ether resin putty. Trudy VIAM, 2024, no. 10 (140), paper no. 08. Available at: http://www.viam-works.ru (accessed: July 16, 2025). DOI: 10.18577/2307-6046-2024-0-10-84-93.
  14. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  15. Zheleznyak V.G., Serdcelyubova A.S., Merkulova Yu.I., Skivko P.V. Paint coating system based on polyurethane enamel for protecting heated frontal surfaces of aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 10. Available at: http://www.journal.viam.ru (ассеssed: July 16, 2025). DOI: 10.18577/2713-0193-2022-0-1-120-128.
  16. Zubarev P.A., Lakhno A.V. Wear-resistant polyurethane coatings. Molodoy ucheny, 2014, no. 20, pp. 143–146.
  17. Kozlova A.A., Kondrashov E.K. Influence of molecular weight and elemental composition of isocyanates on the properties of fluoropolyurethane enamels. Aviation materials and technologies, 2023, no. 4 (73), paper no. 09. Available at: http://www.journal.viam.ru (accessed: July 16, 2025). DOI: 10.18577/2713-0193-2023-0-4-92-100.
  18. Kuznetsova V.A., Yemelyanov V.V., Marchenko S.A., Kovrizhkina N.A. The influence of artificial aging on the properties of coating systems based onchromate-free primer VG-44 using epoxy, polyurethane, acrylic urethane and fluoropolyurethane enamels. Trudy VIAM, 2023, no. 10 (128), paper no. 11. Available at: http://www.viam-works.ru (accessed: July 16, 2025). DOI: 10.18577/2307-6046-2023-0-10-119-131.
  19. Kochetkova G.V., Loginov B.A. New brands of domestic fluororubbers. Rossiyskiy khimicheskiy zhurnal, 2008, vol. LII, no. 3, pp. 23–25.
  20. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.