The influence of variable sulfur content on the high-temperature resistance of cast heat-resistant nickel alloy VZhM200
UDC
669.018.44:669.245
DOI
10.18577/2307-6046-2025-0-9-3-18
Article PDF (Russian)
(904.73 KB)
How to cite
Min P.G., Vadeev V.E., Sankin R.V., Chemov D.A. The influence of variable sulfur content on the high-temperature resistance of cast heat-resistant nickel alloy VZhM200 // Proceedings of VIAM. 2025. No. 9. DOI: 10.18577/2307-6046-2025-0-9-3-18. URL: https://www.viam-works.ru/en/journal/2025/9/1
Keywords
gas corrosion resistance, superalloy, surface oxidation, blades, structure, sulfur, impurity
Abstract
The paper studies the influence of sulfur impurity on the high-temperature resistance at T = 1000 °C for 500 hours of cast heat-resistant hafnium-containing nickel alloy VZhM200. It has been found that with the increase of the sulfur content, the high temperature resistance of the alloy decreases, and with the increase of its content from 0,0038 to 0,0130 wt. %, a slowdown in the high-temperature oxidation process is observed. This is due to the fact that sulfur is concentrated in the composition of hafnium-containing carbides, thereby reducing its diffusion from the volume to the surface of the material, which prevents the destruction of the forming oxide layer.
Reference list
- Kablov E.N., Ospennikova O.G., Svetlov I.L. Highly efficient cooling of GTE hot section blades. Aviacionnye materialy i tehnologii, 2017, no. 2 (47), pp. 3–14. DOI: 10.18577/2071-9140-2017-0-2-3-14.
- Budinovskiy S.A., Gorlov D.S., Benklyan A.S. Deposition of protective ion-plasma coatings on largescale parts on MAP type installations. Aviation materials and technologies, 2024, no. 1 (74), paper no. 08. Available at: http://www.journal.viam.ru (accessed: July 07, 2025). DOI: 10.18577/2713-0193-2024-0-1-101-110.
- Tyunkov А.V., Аndronov А.А., Zolotukhin D.B. et al. Methods of forming heat-protective coatings of turbine blades (review). Aviation materials and technologies, 2024, no. 4 (77), paper no. 10. Available at: http://www.journal.viam.ru (accessed: July 07, 2025). DOI: 10.18577/2713-0193-2024-0-4-140-168.
- Inozemtsev A.A., Koryakovtsev A.S., Lesnikov V.P., Kuznetsov V.P. The role of materials and protective coatings of turbine blades in ensuring the reliability and efficiency of gas turbine engines. Scientific ideas of S.T. Kishkin and modern materials science: Reports Int. Sci.-Tech. Conf. Moscow: VIAM, 2006, pp. 84–87.
- Kablov E.N., Muboyadzhyan S.A. Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 60–70.
- Geddes B., Leon H., Huang X. Superalloys: Alloying and performance. Materials Park, Ohio: ASM International, 2010, 176 p.
- Reed R.C. The Superalloys Fundamentals and Applications. Cambridge: Cambridge University Press, 2006, 390 p.
- Shein E.A. Tendencies in the field of alloying and microalloying of heat resisting single-crystal alloys on the basis of nickel (review). Trudy VIAM, 2016, no. 3, paper no. 02. Available at: http://www.viam-works.ru (accessed: July 07, 2025). DOI: 10.18577/2307-6046-2016-0-3-2-2.
- Pettit F.S., Meier G.H. Oxidation and hot corrosion of superalloys. Superalloys. Warrendale, USA: The Minerals, Metals & Materials Society, 1984, pp. 651–687. DOI: 10.7449/1984/Superalloys_1984_651_687.
- Ross I.V., Sims C.T. Nickel-based alloys. Superalloys II. Heat-resistant materials for aerospace and industrial power plants: in 2 books. Ed. S.T. Sims, N.S. Stoloff, W.K. Hagel; trans. from Engl. Moscow: Metallurgiya, 1995, book 1, p. 128–172.
- Choi K., Choe B., Han S. et al. Effects of Cr and Al Contents on the Oxide Structures of Ni-based Superalloys at High Temperatures. Metals, 2025, vol. 15 (388), pp. 1–15. DOI: 10.3390/met15040388.
- Chang J., Feng W., Zhao W. et al. Investigation on Optimal Ta/Cr Ratio of a Single Crystal Ni-base Superalloy in View of the Isothermal Oxidation Behavior. Crystals, 2021, vol. 11 (1421), pp. 1–15. DOI: 10.3390/cryst11111421.
- Mc Vay R.V., William P., Meier G.H., Pettit F.S. Oxidation of Low Sulfur Single Crystal Nickel-base Superalloys. Superalloys. Warrendale, USA: The Minerals, Metals & Materials Society, 1992, pp. 807–816.
- Sarioglu C., Stinner C., Blanchere J.R. et al. The control of sulfur content in nickel-base, single crystal superalloys and its effect on cyclic oxidation resistance. Superalloys. Warrendale, USA: The Minerals, Metals & Materials Society, 1996, pp. 71–80.
- Simpson T.M., Price A.R. Oxidation improvements of low sulfur processed superalloys. Superalloys. Warrendale, USA: The Minerals, Metals & Materials Society, 2000, pp. 387–392.
- Ultra low sulfur superalloy casting and method of making: pat. 5922148А US; appl. 25.02.97; publ. 13.07.99.
- Improved low sulfur nickel-base single crystal superalloy with ppm additions of lanthanum and yttrium: pat. 2415888 EU; appl. 14.10.10; publ. 27.06.12.
- Zhan X., Wang D., Zhang Z.-P., Zhang J. Effect of trace sulfur on the hot corrosion resistance of Ni-base single crystal superalloy. Corrosion Science, 2023, vol. 224, p. 111528. DOI: 10.1016/j.corsci.2023.111528.
- Harris K., Wahl J.B. Developments in superalloy castability and new applications for advanced superalloys. Material Science and Technology, 2009, vol. 25, no. 2. DOI: 10.1179/174328408x355442.
- Cao S., Yang Y., Chen B. et al. Influence of yttrium on purification and carbide precipitation of superalloy K4169. Journal of Materials Science & Technology, 2021, vol. 86, pp. 260–270. DOI: 10.1016/j.jmst.2021.01.049.
- Harris K., Wahl J.B. Improved single crystal superalloys, CMSX-4 (SLS) [La+Y] and CMSX-486. Superalloys. Warrendale, USA: The Minerals, Metals & Materials Society, 2004, pp. 45–52.
- Yun D.W., Seo S.M., Jeong H.W., Yoo Y.S. The cyclic oxidation behaviour of Ni-based superalloy GTD-111 with sulphur impurities at 1100 °C. Corrosion Science, 2015, vol. 90, pp. 392–401. DOI: 10.1016/j.corsci.2014.10.030.
- Peruse E., Diomande D., Dufour G. et al. Type I and Type II Hot Corrosion of Ni-based alloys without an incubation period. High Temperature Corrosion of Materials, 2025, vol. 102, pp. 1–15. DOI: 10.1007/s11085-025-10341-7.
- Min P.G., Sidorov V.V., Budinovsky S.A., Vadeev V.E. Effect of sulfur on heat resistance of single crystals of heat-resistant nickel alloy of the Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr system. Materialovedenie, 2016, no. 7, pp. 9–12.
- Kablov D.E., Sidorov V.V., Budinovskij S.A., Min P.G. The influence of sulfur impurity on heat resistance of single crystals of ZhS36-VI alloy with protective coating. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 20–23. DOI: 10.18577/2071-9140-2016-0-1-20-23.
- Min P.G., Vadeev V.E., Kolesnikov S.I., Chemov D.A. The effect of impurities on mechanical and operational properties of the cast nickel-base superalloy VZhM200. Trudy VIAM, 2024, no. 10 (140), paper no. 02. Available at: http://www.viam-works.ru (accessed: July 07, 2025). DOI: 10.18577/2307-6046-2024-0-10-13-23.
- Min P.G., Kablov D.E., Sidorov V.V., Vadeev V.E. Influence of sulfur, phosphorus and silicon impurities on the structure and properties of single crystals of nickel heat-resistant alloys Materialovedenie, 2018, no. 8, pp. 13–18. DOI: 10.31044/1684-579Х-2018-0-8-13-18.
- Kablov D.E., Sidorov V.V., Puchkov Yu.A. Diffusion behavior features of impurities and microalloying additives in nickel and single crystal superalloys. Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 24–31. DOI: 10.18577/2071-9140-2016-0-1-24-31.
- Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines’ blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), paper no. 02. Available at: http://www.journal.viam.ru (accessed: July 07, 2025). DOI: 10.18577/2713-0193-2021-0-3-11-18.
- Mataveli Suave L., Cormier J., Villechaise P. et al. Anisotropy in creep properties of DS200 + Hf alloy. Materials at High Temperatures, 2016, no. 33, pp. 361–371. DOI: 10.1080/09603409.2016.1159836.
- Mataveli Suave L., Cormier J., Villechaise P. et al. High temperature creep damage mechanisms in a directionally solidified alloy: impact of crystallography and environment. Superalloys. Warrendale, USA: The Minerals, Metals & Materials Society, 2016, pp. 747–756. DOI: 10.7449/Superalloys/2016/Superalloys_2016_747_756.
- Baldan A. Electron microprobe investigation of lower melting regions in the as-cast structure of DS200 + Hf single crystal. Journal of Materials Science, 1990, vol. 25, pp. 4341–4348.
- Tikhonov A.I., Kraev V.M., Siluyanova M.V. Prospects for the Development of Russian Aircraft Engine Manufacturing Based on a Unified Gas Generator. STIN, 2023, no. 6, pp. 71–74.
- Konstantinov I.V. Ensuring Technological Sovereignty of the Aviation Industry Using the Example of the SUKHOI SUPERJET NEW Aircraft. Scientific Achievements and Innovative Approaches: Theory, Methodology, Practice: Scientific Reports on Materials. VIII Int. Scientific and Practical Conf. Anapa, 2022, pр. 99–103.
- More than 40 PD-8 Engines to Be Produced in 2024. Available at: https://tass-ru/ekonomika/18995881 (accessed: July 07, 2025).
- Tolboev M.O. Civil aviation of Russia: before and after the Superjet. Standarty i kachestvo, 2019, no. 7, pp. 80–82.
- Bazikova I.V. Main problems of the implementation of the Sukhoi Superjet 100 project. Vestnik universiteta, 2018, no. 6, pp. 48–54.
- Tikhonov A.I., Sazonov A.A. Innovative Russian aircraft Sukhoi Superjet 100 as a vector of development of the aircraft industry of the future. Ekonomika i predprinimatelstvo, 2018, no. 7 (96), pp. 289–292.
- Mayorov A.V., Borisoglebskaya L.N., Bulatnikov D.V., Dudina K.E. Features of import substitution in the aircraft industry. Innovatsii, 2023, no. 1 (291), pp. 45–50. DOI: 10.26310/2071-3010.2023.291.1.004.
- Min P.G., Vadeev V.E., Min M.G. Development and implementation in production of the new single-crystal high-temperature nickel alloy for casting of gas turbine blades for the prospective engine PD-8. Aviation materials and technologies, 2025, no. 1 (78), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 07, 2025). DOI: 10.18577/2713-0193-2025-0-1-3-17.
- Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), paper no. 01. Available at: http://www.journal.viam.ru (accessed: July 07, 2025). DOI: 10.18577/2713-0193-2023-0-1-3-16.
- Heat-resistant nickel-based casting alloy and a product made from it: pat. 2740929 Rus. Federation; appl. 20.04.20; publ. 21.01.21.
- Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 07, 2025). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Kablov E.N., Bondarenko Yu.A., Echin A.B. Development of technology of cast superalloys directional solidification with variable controlled temperature gradient. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
- Gerasimov V.V., Visik E.M., Kolyadov E.V. On directional crystallization of large-sized castings on the UVNK-15 unit. Liteynoe proizvodstvo, 2013, no. 3, pp. 22–24.
- Gerasimov V.V., Kolyadov E.V. Technical characteristics and technological capabilities of the UVNK-9A and VIP-NK units for producing single-crystal castings from heat-resistant alloys. Liteshchik Rossii, 2012, no. 11, pp. 33–37.
- Kablov E.N., Gerasimov V.V., Visik E.M. Control of the structure of heat-resistant nickel alloys in the manufacture of gas turbine engine blades by directional crystallization. Aviatsionnaya promyshlennost, 1999, no. 2, pp. 12–18.
- Mehanik E.A., Min P.G., Gundobin N.V., Rastegaeva G.Yu. Determination of sulfur mass fraction in heat-resistant nickel alloy and steels within the concentration range from 0,0001 to 0,0009% wt. Trudy VIAM, 2014, no. 9, paper no. 12. Available at: http://www.viam-works.ru (accessed: July 07, 2025). DOI: 10.18577/2307-6046-2014-0-9-12-12.
- Sidorov V.V., Kablov D.E., Chabina E.B., Ospennikova O.G., Simonov V.N., Puchkov Yu.A. The influence of impurities and microalloying on the structure and performance properties of single crystals of heat-resistant nickel alloys: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2020, pp. 232–233.