Lighting protection coating based on polymer composite film with integrated metal mesh

Gunyaeva A.G., Klimenko O.N.
Gunyaeva A.G., Klimenko O.N. Lighting protection coating based on polymer composite film with integrated metal mesh // Proceedings of VIAM. 2025. No. 8. DOI: 10.18577/2307-6046-2025-0-8-100-111. URL: https://www.viam-works.ru/en/journal/2025/8/9
Keywords
polymer composite materials, lightning protection, metal perforated foils, metal knitted wire mesh, composite leveling films
Abstract

The article considers modern approaches to lightning protection of structures from PCM that extending to the outer circuit of aircrafts. A The lightning protection coating named VMPZ-1 is new development of the NRC «Kurchatov Institute» – VIAM , which is a leveling composite film with an integrated metal layer that can be used as metal perforated foils or metal knitted wire nets of various surface densities. The basic properties of the developed lightning coating VMZP-1 and the results of testing elementary samples for lightning resistance are given here.

Reference list
  1. Kablov E.N. The role of state scientific centers of the Russian Federation in ensuring the national security of the country. Perspektivnyye tekhnologii dlya sistem bezopasnosti, 2023, no. 1, pp. 4–9.
  2. Kablov E.N. Quality control of materials – a guarantee of the safe operation of aviation equipment. Aviacionnye materialy i tehnologii, 2001, no. 1, pp. 3–8.
  3. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  4. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: June 04, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  5. Sazhenkov N.A., Sazhenkov A.N. Lightning protection coatings of engine nacelles made of polymer composite materials. Part 1. Analysis of existing types of lightning protection. Vestnik PNIPU. Aerokosmicheskaya tekhnika, 2021, no. 67, pp. 43–55.
  6. Chursova L.V., Panina N.N., Grebeneva T.A., Vishnyakov L.R. Materials for lightning protection systems of polymer composite materials. Manufacturing features (review, part I). Vse materialy. Entsiklopedicheskiy spravochnik, 2023, no. 9, pp. 25–33.
  7. Mishkin S.I., Klimenko O.N., Gunyaeva A.G. Materials for the lightnings protection of aviation engineering. Trudy VIAM, 2023, no. 7 (125), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 24, 2025). DOI: 10.18577/2307-6046-2023-0-7-84-92.
  8. Chernyshev B.D., Kovalev A.D., Siluk N.P., Rojkov S.S., Shustov V.S., Ryzhkova G.S., Melnikov S.A. Microstructure and functional properties of bulk samples made from W–Ni–Cu pseudoalloy by cold isostatic pressure. Aviation materials and technologies, 2025, no. 2 (79), paper no. 06. Available at: http://www.journal.viam.ru (accessed: June 01, 2025). DOI: 10.18577/2713-0193-2025-0-2-59-71.
  9. Gunyaeva A.G., Kurnosov A.O., Slavin A.V. Experience in the use of polymer composite materials developed by NRC «Kurchatov Institute» – VIAM in engines for civil aircraft. Aviation materials and technologies, 2024, no. 4 (77), paper no. 06. Available at: http://www.journal.viam.ru (accessed: May 25, 2025). DOI: 10.18577/2713-0193-2024-0-4-82-94.
  10. Chursova L.V., Panina N.N., Grebeneva T.A., Vishnyakov L.R. Features of the use of conductive knitted wire meshes and perforated foils in the creation of lightning protection systems for polymer carbon composite structures (review, part II). Vse materialy. Entsiklopedicheskiy spravochnik, 2023, no. 10, pp. 18–26.
  11. Tkachenko A.N., Vishnyakov L.R., Gogaev K.A. et al. Copper microwires for knitted lightning protection meshes. Tekhnologicheskiye sistemy, 2009, no. 4, pp. 40–44.
  12. Conductive layer of lightning protection coating for polymer composites: pat. 2764853 Rus. Federation; appl. 26.05.21; publ. 21.01.22.
  13. Boytsov B.V., Vishnyakov L.R., Kazakov M.E., Krivonos V.V. Innovative design and technological solutions for lightning protection of aircraft structures made of polymer composite materials. Kachestvo i zhizn, 2020, no. 2 (26), pp. 74–81.
  14. Polymer film coating with an integrated metal layer based on a heat-resistant binder: pat. 2839081 Rus. Federation; appl. 17.07.24; publ. 28.04.25.
  15. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://www.journal.viam.ru (accessed: May 25, 2025). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  16. Bukharov S.V., Gunyaeva A.G., Raskutin A.E. Research of the zone of damage of lightning protection coating made of carbon fiber reinforced plastics by high-voltage discharges simulating lightning currents. Nauchnye trudy (Vestnik «MATI»), 2014, no. 22 (94), pp. 4–14.
  17. Murashov V.V., Kosarina E.I., Generalov A.S. Quality control of aviation parts made from polymer composite materials and multilayers adhered constructions. Aviacionnye materialy i tehnologii, 2013, no. 3, pp. 65–70.