Study of the hydrogenation process of VT5, VT14, VT22 titanium alloys for the production of standard samples of hydrogen content
UDC
543.42:546.11
DOI
10.18577/2307-6046-2025-0-8-76-84
Article PDF (Russian)
(768.47 KB)
How to cite
Shvetsova A.N., Eroshkin S.G. Study of the hydrogenation process of VT5, VT14, VT22 titanium alloys for the production of standard samples of hydrogen content // Proceedings of VIAM. 2025. No. 8. DOI: 10.18577/2307-6046-2025-0-8-76-84. URL: https://www.viam-works.ru/en/journal/2025/8/7
Keywords
hydrogen determination, cathodic hydrogenation, spectral analysis method, standard samples, hydrogen in titanium
Abstract
Ensuring high quality of titanium alloy production dictates the development of new standard samples for hydrogen content, selection of the grade of material for their manufacture and the method of hydrogenation. In this work, the processes of hydrogen saturation of VT5, VT14 and VT22 titanium alloy samples by the electrochemical method (cathodic hydrogenation) have been studied. The paper provides the results of analysis of the degree of hydrogen saturation of the VT5, VT14 and VT22 samples, as well as the effect of the leveling annealing on the content of the β-phase fraction in the VT14 alloy samples. Hydrogen content has been measured using the emission spectral analysis.
Reference list
- Kablov E.N. Main directions of development of materials for aerospace engineering of the 21st century. Perspektivnye materialy, 2000, no. 3, pp. 27–36.
- Kablov E.N. Aviation materials science in the 21st century. Prospects and tasks. Aviation materials. Selected works of VIAM 1932–2002. Ed. E.N. Kablov. Moscow: MISiS–VIAM, 2002, pp. 23–47.
- Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), paper no. 12. Available at: https://www.journal.viam.ru (accessed: December 12, 2024). DOI: 10.18577/2713-0193-2021-0-2-115-122.
- Duyunova V.A., Pavlova T.V., Kashapov O.S., Chuchman O.V. Fatigue strength of forgings from VT6 alloy for parts of gas turbine engines and aircrafts. Aviation materials and technologies, 2023, no. 2 (71), paper no. 02. Available at: http://www.journal.viam.ru (accessed: December 12, 2024). DOI: 10.18577/2713-0193-2023-0-2-23-35.
- Oglodkov M.S., Kashapov O.S., Kalashnikov V.S., Kondratieva A.R. Comparative analysis of the characteristics of domestic alloys VT8, VT8M, VT8M-1, VT9 and Ti6242S alloy (USA) as applied to high-pressure compressor blades of aircraft gas turbine engines. Aviation materials and technologies, 2024, no. 3 (76), paper no. 04. Available at: http://www.journal.viam.ru (accessed: December 12, 2024). DOI: 10.18577/2713-0193-2024-0-3-35-50.
- Duyunova V.A., Oglodkov M.S., Putyrskiy S.V., Kochetkov A.S., Zueva O.V. Modern technologies for melting titanium alloy ingots (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 03. Available at: http://www.journal.viam.ru (accessed: December 12, 2024). DOI: 10.18577/2713-0193-2022-0-1-30-40.
- Panin P.V., Nochovnaya N.A., Kablov D.E., Alekseev E.B., Shiryaev A.A., Novak A.V. Practical guide to metallography of titanium-based alloys and its intermetallic compounds: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2020, 200 p.
- Matyugina I.V., Shubina S.B. Certified reference materials for determining gases in metals. Methodological issues of producing certified reference materials. Sverdlovsk: VNIISO Publ. House, 1973, pp.114–122.
- Wu T.-I., Wu J.-K. Effects of cathodic charging and subsequent solution treating parameters on the hydrogen redistribution and surface hardening of Ti–6Al–4V alloy. Journal of Alloys and Compounds, 2008, vol. 466, pp. 153–159.
- Huang Ch.-L., Gao Y.-J., Chuang T.-L. et al. Study of the behavior of titanium alloys as the cathode for photovoltaic hydrogen production. International Journal of Photoenergy, 2013, vol. 3, art. 857491.
- Pivovarova L.N., Zakharova L.V., Fadeev A.V. Chemical treatment of titanium alloy surfaces. Modern titanium alloys and problems of their development. Moscow: VIAM, 2010, pp. 75–80.
- Barasheva T.V., Bezgina V.I., Guskova E.I., Ermolova M.I., Lashko N.F. Study of hydrogenation of titanium alloys during etching. Tekhnologiya legkikh splavov, 1974, no. 6, рp. 43–48.
- Usova V.V., Plotnikova T.P., Kushakevich S.A. Etching of titanium and its alloys. Moscow: Metallurgy, 1984, 128 p.
- Matyugina I.V., Pliner Yu.L., Shikhaleeva T.V., Usov V.N. Saturation of standard samples for spectral analysis of VT14 alloy with hydrogen. Trudy VNIISO, 1970, is. VI, pp. 62–66.
- Industry Standard 1 90013–81. Titanium alloys. Brands. Moscow: Publ. house of standards, 1981, pp. 1–5.
- Matyugina I.V., Pliner Yu.L., Usov V.N. Standard samples for spectral determination of hydrogen in titanium alloys. Zhurnal prikladnoy spektroskopii, 1972, vol. XVII, is. 1, pp. 13–16.
- Kaganovich N.N., Shikhaleeva T.V. Hydrogenation of titanium alloys during etching. Metallovedenie i termicheskaya obrabotka, 1963, no. 3, pp. 39–44.