Optimization of heat treatment for high-strength corrosion-resistant nitrogen-containing steel to produce seamless thin-walled tubes

Sevalnev G.S., Dulnev K.V., Ryzhkov P.V., Leonov A.V., Voznesenskaya N.M.
Sevalnev G.S., Dulnev K.V., Ryzhkov P.V., Leonov A.V., Voznesenskaya N.M. Optimization of heat treatment for high-strength corrosion-resistant nitrogen-containing steel to produce seamless thin-walled tubes // Proceedings of VIAM. 2025. No. 8. DOI: 10.18577/2307-6046-2025-0-8-41-52. URL: https://www.viam-works.ru/en/journal/2025/8/4
Keywords
high-strength corrosion-resistant steel, high-nitrogen steel, thin-walled pipes, phase composition, mechanical properties, manufacturability
Abstract

The article examines the optimization of heat treatment for producing thin-walled pipes via cold rolling from high-strength corrosion-resistant steel 15Kh15N4AGM-Sh. The high strength of this steel after quenching (σв > 1700 MPa) makes deformation difficult. It was established that annealing the steel leads to significant embrittlement. Tempering at 600–700 °C forms a highly tempered martensite structure, reducing strength (σ0,2 ≈ 990 MPa at 600 °C) while maintaining ductility (δ5 ≈ 19 %). Based on the research results, it was determined that the best reduction in strength characteristics without a significant decrease in ductility occurs in temperature range 630–660 °С.

Reference list
  1. Loginov Yu.N., Shimov G.V., Bushueva N.I. On the forecast of the development of martensitic transformation during mandrel-free drawing of pipes made of austenitic steel. Chernye metally, 2021, no. 4, pp. 25–31. DOI: 10.17580/chm.2021.04.05.
  2. Frolov A.V., Kravchenko A.S. Development of a technology for welding thin-walled pipes with a pulsed arc. Reports II Int. Sci. and Pract. Conf. of young scientists «Science, innovation and technology: from ideas to implementation»: in 2 parts. Komsomolsk-on-Amur: Komsomolsk-on-Amur State Univ., 2022, part 2, pp. 181–185.
  3. Smertin S.A., Zemtsov M.I. Analysis of the possibility of manufacturing semi-finished products – thin-walled pipes bent to the required angle. Coll. of materials of the All-Rus. Annual Sci.-Pract. Conf. «Society, science, innovation (NPK-2014)». Kirov: Vyatka State Univ., 2014, pp. 1387–1391.
  4. Zhitelev D.A., Pozdnyakov T.D., Sulegin D.A., Naumov V.N. Study of experimental and numerical behavior of thin-walled pipes under quasi-static loading mode. Proceedings of NSTU named after R.E. Alekseev, 2022, no. 4 (139), pp. 85–96.
  5. Priymak E.Yu., Stepanchukova A.V. Formation of the structure of steels for the production of drill pipes by friction welding. XIII Int. Sci.-Tech. Ural school-seminar of young scientists-metallologists. II Int. Sci. school for youth «Materials science and metallophysics of light alloys». Ekaterinburg, 2012, pp. 3–4.
  6. Pugacheva T.M., Mikheev D.A. Materials science study of drill pipe lock joints after surfacing using various fluxes. Bulletin of the Belgorod State Technological University named after V.G. Shukhov, 2018, no. 6, pp. 97–102.
  7. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  8. Bannykh I.O., Ashmarin A.A., Betzofen S.Ya. et al. Optimization of chemical composition and parameters of thermomechanical processing of TRIP steels based on new methods of X-ray tensometry, texture and phase analysis. Metally, 2022, no. 6, pp. 66–72.
  9. Udod K.A., Trofimenko N.N., Romanenko D.N., Sevalnev G.S. Prospects for the development of constructional aluminium-doped steels. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 9–13. DOI: 10.18577/2071-9140-2019-0-3-9-13.
  10. Serebryakov A.V. Research, development of technology and mastering the production of precision pipes made of corrosion-resistant steel: thesis, Cand. Sc. (Tech.). Ekaterinburg: Ural State Tech. Univ. - UPI, 2007, 160 p.
  11. Atanasov V.R., Panchenko S.A. Development of scientific foundations and technological methods for increasing the corrosion resistance of pipes made of duplex steels. Stroitelstvo. Materialovedenie. Mashinostroenie. Ser.: Starodubovskie chteniya, 2015, no. 80, pp. 18–26.
  12. Bolshakov V.I., Dergach T.A., Sukhomlin G.D., Panchenko S.A. Application of grain boundary design to increase the corrosion resistance of pipes made of ferritic-austenitic steels. Korroziya: materialy, zashchita, 2014, no. 7, pp. 20–26.
  13. Filisteev V.G., Steklova E.O., Berezovsky A.V. Weldability of Duplex Steels for Transporting Aggressive Environments Containing Hydrogen Sulfide and Carbon Dioxide. Expositsiya Neft Gaz, 2023, no. 2, pp. 70–75.
  14. Kondratenko L.A., Terekhov V.M., Mironova L.I. Analysis of Some Problems of Mechanical Fastening of Bimetallic Heat Exchange Tubes in Power Plants. Problemy mashinostroyeniya i avtomatizatsii, 2017, no. 3, pp. 83–88.
  15. Nikitin K.N., Osadchiy V.Ya., Safyanov A.V. еt al. Development and mastering of import-substituting technology for the production of seamless bimetallic pipes for nuclear power engineering. Stal, 2017, no. 7, pp. 44–50.
  16. Komarov A.I., Nikitin K.N., Safyanov A.V. et al. Improving the technology for the production of seamless bimetallic pipes for pipelines of nuclear power plants. Chernye metally, 2017, no. 9, pp. 68–73.
  17. Krasnykh V.I., Zhdanova A.S., Garanzha T.V. Precision alloys with specified elastic properties: the need for a new life. Stal, 2015, no. 7, pp. 60–66.
  18. Korol R.M., Mironenko A.Yu., Mironenko M.A. Features of the manufacturing technology of high-quality precision tubes from a foreign analogue of the molybdenum alloy MChVP. Metallurgicheskaya i gornorudnaya promyshlennost, 2017, no. 3, pp. 43–47.
  19. Kravchenko O.V. Features of the main technological and design parameters of the stationary stand of the HPTR mill for rolling precision heat exchange tubes. HERALD of the Donbass State Engineering Academy, 2019, no. 2 (46), pp. 64–67.
  20. Ushakov A.S., Kondratov L.A. On the production of steel pipes. Stal, 2018, no. 7, pp. 33–43.
  21. Sevalnev G.S., Klimov V.S., Vlasov I.I., Mazalova T.A. Study of mechanical properties of Fe–Cr–Ni–Co–Mo steel 3D-printed samples after various types of processing. Trudy VIAM, 2025, no. 6 (148), paper no. 01. Available at: http://www.viam-works.ru (accessed: June 22, 2025). DOI: 10.18577/2307-6046-2025-0-6-3-12.
  22. Eliseev E.A., Karpukhin S.D., Druzhinina M.E. The effect of nickel on the structure of the nitrided layer of low-carbon martensitic steels. Aviation materials and technologies, 2025, no. 1 (78), paper no. 02. Available at: http://www.journal.viam.ru (accessed: July 01, 2025). DOI: 10.18577/2713-0193-2025-0-1-18-27.
  23. Zakalashnyy A.V., Denisova V.S., Vlasova O.V., Solntsev S.S. Technological aspects of obtaining frit of heat-resistant enamel for the protection of corrosion-resistant steels. Trudy VIAM, 2021, no. 8 (102), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 01, 2025). DOI: 10.18577/2307-6046-2021-0-8-43-49.
  24. Alekseeva M.S., Slobodskoy P.A., Lukina Е.А., Yakusheva N.A. Patterns of structure formation for open-hearth steel of the Fe–Cr–Ni–Mo–Ti system during heat treatment. Trudy VIAM, 2024, no. 2 (132), paper no. 01. Available at: http://www.viam-works.ru (accessed: July 01, 2025). DOI: 10.18577/2307-6046-2024-0-2-3-12.