Review of polymer-derived ceramics (PDC)

Part 1. Preceramic polymers and production of PDC materials
Parashchenko N.M., Tupikov A.S., Lyzhenkov Z.A., Golovko D.S.
Parashchenko N.M., Tupikov A.S., Lyzhenkov Z.A., Golovko D.S. Review of polymer-derived ceramics (PDC). Part 1. Preceramic polymers and production of PDC materials // Proceedings of VIAM. 2025. No. 8. DOI: : 10.18577/2307-6046-2025-0-8-134-151. URL: https://www.viam-works.ru/en/journal/2025/8/12
Keywords
preceramic polymers, PDC ceramics, polymer-derived ceramic precursor, pyrolysis, silicon carbide, silicon nitride, functional ceramics
Abstract

This paper provides a review of preceramic polymers used for the production of polymer-derived ceramics. The article considers the main classes of organosilicon precursors, their chemical nature, and synthesis methods. The paper gives a detailed description of structural features of various types of preceramic polymers and their influence on the composition, morphology, and properties of the final ceramic materials. Additionally, the transformation stages of precursors into PDCs and the factors affecting this process are considered.

Reference list
  1. Pandey S.P., Singh V. The Importance of Engineering Materials in Present World. International Journal of Science and Research, 2015, vol. 6, is. 3, pp. 433–441.
  2. Yajima S., Hayashi J., Omori M. Continuous silicon carbide fiber of high tensile strength. Chemistry Letters, 1975, vol. 4, no. 9, pp. 931–934. DOI: 10.1246/cl.1975.931.
  3. Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
  4. Каблов Е.Н., Щетанов Б.В., Ивахненко Ю.А., Балинова Ю.А. Перспективные армирующие высокотемпературные волокна для металлических и керамических композиционных материалов. Aviacionnye materialy i tekhnologii, 2005, no. 2, pp. 3–5.
  5. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.S. Promising high-temperature ceramic composite materials. Rossiyskiy khimicheskiy zhurnal, 2010, vol. 54, no. 1, pp. 20–24.
  6. Colombo P., Mera G., Riedel R., Soraru G.D. Polymer‐Derived Ceramics: 40 Years of Research and Innovation in Advanced Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, no. 7, pp. 1805–1837. DOI: 10.1111/j.1551-2916.2010.03876.x.
  7. Kleebe H.-J., Blum Y.D. SiOC ceramic with high excess free carbon. Journal of the European Ceramic Society, 2008, vol. 28, no. 5, pp. 1037–1042. DOI: 10.1016/j.jeurceramsoc.2007.09.024.
  8. Miller R.D., Michl J. Polysilane high polymers. Chemical Reviews, 1989, vol. 89, no. 6, pp. 1359–1410. DOI: 10.1021/cr00096a006.
  9. Kipping F.S., Sands J.E. XCIII. – Organic derivatives of silicon. Part XXV. Saturated and unsaturated silicohydrocarbons, Si4Ph8. Journal of the Chemical Society, Transactions, 1921, vol. 119, pp. 830–847.
  10. Kipping F.S. CCCVIII. – Organic derivatives of silicon. Part XXX. Complex silicohydrocarbons [SiPh2]n. Journal of the Chemical Society, Transactions, 1924, vol. 125, pp. 2291–2297.
  11. Aitken C., Harrod J.F., Samuel E. Polymerization of primary silanes to linear polysilanes catalyzed by titanocene derivatives. Journal of Organometallic Chemistry, 1985, vol. 279, no. 1–2, pp. C11–C13. DOI: 10.1016/0022-328X(85)87029-7.
  12. Erin K.D., Sorokin O.Yu., Monin S.A., Gor-bovets M.A. Methods for measuring and improving the crack resistance of silicon carbide composite materials. Trudy VIAM, 2024, no. 11 (141), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 11, 2025). DOI: 10.18577/2307-6046-2024-0-11-44-70.
  13. Shiina K., Kumada M. Notes – Thermal Rearrangement of Hexamethyldisilane to Trimethyl(dimethylsilylmethyl)silane. The Journal of Organic Chemistry, 1958, vol. 23, no. 1, pp. 129–139. DOI: 10.1021/jo01095a635.
  14. Schilling C.L., Wesson J.P., Williams T.C. Polycarbosilane precursors for silicon carbide. Journal of Polymer Science: Polymer Symposia, 1983, vol. 70, no. 1, pp. 121–128. DOI: 10.1002/polc.5070700110.
  15. Corriu R.J.P., Guerin C., Henner B. et al. Organosilicon polymers: synthesis of poly[(silanylene)diethynylene]s with conducting properties. Chemistry of Materials, 1990, vol. 2, no. 4, pp. 351–352. DOI: 10.1021/cm00010a008.
  16. Zhang X., Zhou Q., Weber W.P. et al. Anionic ring-opening polymerization of sila- and germacyclopent-3-enes. Macromolecules, 1988, vol. 21, no. 6, pp. 1563–1566. DOI: 10.1021/ma00184a004.
  17. Zeldin M., Wynne K.J., Allcock H.R. Inorganic and Organometallic Polymers: Macromolecules Containing Silicon, Phosphorus, and Other Inorganic Elements. American Chemical Society, 1988, vol. 360, p. 536. DOI: 10.1021/bk-1988-0360.
  18. Seyferth D., Prud'homme C., Wiseman G.H. Cyclic polysiloxanes from the hydrolysis of dichlorosilane. Inorganic Chemistry, 1983, vol. 22, no. 15, pp. 2163–2167. DOI: 10.1021/ic00157a014.
  19. Polysilane-siloxane oligomers and copolymers and methods of making the same: pat. US4626583A; appl. 11.07.85; publ. 21.01.87.
  20. Chojnowski J., Kurjata J., Rubinsztajn S. Poly(oxymultisilane)s by ring‐opening polymerization. Fully methylated silicon analogues of oxirane and THF polymers. Macromolecular Rapid Communications, 1988, vol. 9, no. 7, pp. 469–475. DOI: 10.1002/marc.1988.030090704.
  21. Zhang H., Pantano C.G. Synthesis and Characterization of Silicon Oxycarbide Glasses. Journal of the American Ceramic Society, 1990, vol. 73, no. 4, pp. 958–963. DOI: 10.1111/j.1151-2916.1990.tb05143.x.
  22. Sorarù G.D., D'Andrea G., Campostrini R. et al. Structural Characterization and High‐Temperature Behavior of Silicon Oxycarbide Glasses Prepared from Sol‐Gel Precursors Containing Si–H Bonds. Journal of the American Ceramic Society, 1995, vol. 78, no. 2, pp. 379–387. DOI: 10.1111/j.1151-2916.1995.tb08811.x.
  23. Gervais C., Babonneau F., Dallabonna N. et al. Sol‐Gel‐Derived Silicon‐Boron Oxycarbide Glasses Containing Mixed Silicon Oxycarbide (SiCxO4−x) and Boron Oxycarbide (BCyO3−y) Units. Journal of the American Ceramic Society, 2001, vol. 84, no. 10, pp. 2160–2164. DOI: 10.1111/j.1151-2916.2001.tb00981.x.
  24. Mir F.A., Khan N.Z., Parvez S. Recent advances and development in joining ceramics to metals. Materials Today: Proceedings, 2021, vol. 46, pp. 6570–6575. DOI: 10.1016/j.matpr.2021.04.047.
  25. Shestakov A.M. Ceramics based on organo-silicon polymers-precursors: properties and applications (review). Trudy VIAM, 2023, no. 2 (120), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 11, 2025). DOI: 10.18577/2307-6046-2023-0-2-113-131.
  26. Nicholas J.R. Processing of continuous fiber reinforced ceramic composites for ultra high temperature applications using organosilicon polymer precursors. Missouri University of Science and Technology, 2013, 59 p.
  27. Seyferth D., Wiseman G.H., Prud'homme C. A Liquid Silazane Precursor to Silicon Nitride. Journal of the American Ceramic Society, 1983, vol. 66, no. 1, pp. C13–C14. DOI: 10.1111/j.1151-2916.1983.tb09979.x.
  28. Hörz M., Zern A., Berger F. et al. Novel polysilazanes as precursors for silicon nitride/silicon carbide composites without «free» carbon. Journal of the European Ceramic Society, 2005, vol. 25, no. 2–3, pp. 99–110. DOI: 10.1016/j.jeurceramsoc.2004.07.020.
  29. Seyferth D., Wiseman G.H. High‐Yield Synthesis of Si3N4/SiC Ceramic Materials by Pyrolysis of a Novel Polyorganosilazane. Journal of the American Ceramic Society, 1984, vol. 67, no. 7, pp. C132–C133. DOI: 10.1111/j.1151-2916.1984.tb19620.x.
  30. Blum Y., Laine R.M. Catalytic methods for the synthesis of oligosilazanes. Organometallics, 1986, vol. 5, no. 10, pp. 2081–2086. DOI: 10.1021/om00141a026.
  31. Seyferth D., Strohmann C., Dando N.R., Perrotta A.J. Poly(ureidosilazanes): Preceramic Polymeric Precursors for Silicon Carbonitride and Silicon Nitride. Synthesis, Characterization, and Pyrolytic Conversion to Si3N4/SiC Ceramics. Chemistry of Materials, 1995, vol. 7, no. 11, pp. 2058–2066. DOI: 10.1021/om00141a026.
  32. Schwark J.M., Sullivan M.J. Isocyanate-Modified Polysilazanes: Conversion to Ceramic Materials. MRS Proceedings, 1992, vol. 271, p. 807. DOI: 10.1557/PROC-271-807.
  33. Pump J., Rochow E.G. Silylcarbodiimide. IV. Sila‐polycarbodiimide. Zeitschrift anorg allge chemie, 1964, vol. 330, no. 1–2, pp. 101–106. DOI: 10.1002/zaac.19643300114.
  34. Dressler W., Riedel R. Progress in silicon-based non-oxide structural ceramics. International Journal of Refractory Metals and Hard Materials, 1997, vol. 15, no. 1–3, pp. 13–47. DOI: 10.1016/S0263-4368(96)00046-7.
  35. Nahar-Borchert S., Kroke E., Riedel R. et al. Synthesis and characterization of alkylene-bridged silsesquicarbodiimide hybrid xerogels. Journal of Organometallic Chemistry, 2003, vol. 686, no. 1–2, pp. 127–133. DOI: 10.1016/S0022-328X(03)00440-6.
  36. Mera G., Riedel R., Poli F., Müller K. Carbon-rich SiCN ceramics derived from phenyl-containing poly(silylcarbodiimides). Journal of the European Ceramic Society, 2009, vol. 29, no. 13, pp. 2873–2883. DOI: 10.1016/j.jeurceramsoc.2009.03.026.
  37. Greil P. Polymer derived engineering ceramics. Advanced engineering materials, 2000, vol. 2, no. 6, pp. 339–348. DOI: 10.1002/1527-2648(200006)2.
  38. Konegger T., Agarwal A.K., Pandey A. et al. Ceramics for Sustainable Energy Technologies with a Focus on Polymer-Derived Ceramics. Novel Combustion Concepts for Sustainable Energy Development. Springer, 2014, pp. 501–533. DOI: 10.1007/978-81-322-2211-8_22.
  39. Haug R., Weinmann M., Bill J., Aldinger F. Plastic forming of preceramic polymers. Journal of the European Ceramic Society, 1999, vol. 19, no. 1, pp. 1–6. DOI: 10.1016/S0955-2219(98)00167-8.
  40. Turchenko M.V., Lebedeva Yu.E., Kolmogorov A.Yu., Gurov D.A., Chainikova A.S. Possibility of using layer-by-layer deposition technology (FDM) to produce ceramic products. Trudy VIAM, 2024, no. 8 (138), paper no. 06. Available at: http://www.viam-works.ru (accessed: May 11, 2025). DOI: 10.18577/2307- 6046-2024-0-8-64-76.
  41. Idesaki A., Narisawa M., Okamura K. et al. Application of electron beam curing for silicon carbide fiber synthesis from blend polymer of polycarbosilane and polyvinylsilane. Radiation Physics and Chemistry, 2001, vol. 60, no. 4–5, pp. 483–487. DOI: 10.1016/S0969-806X(00)00394-7.
  42. Liew L.-A., Liu Y., Luo R. et al. Fabrication of SiCN MEMS by photopolymerization of pre-ceramic polymer. Sensors and Actuators A: Physical, 2002, vol. 95, no. 2–3, pp. 120–134. DOI: 10.1016/S0924-4247(01)00723-3.
  43. Infusible preceramic polymers via plasma treatment: pat. US4743662A; appl. 03.11.86; publ. 10.05.88.
  44. Balan C., Riedel R. Rheological investigations of a polymeric precursor for ceramic materials: experiments and theoretical modeling. Journal of Optoelectronics and Advanced Materials, 2006, vol. 8, no. 2, pp. 561.
  45. Konetschny C., Galusek D., Reschke S. et al. Dense silicon carbonitride ceramics by pyrolysis of cross-linked and warm pressed polysilazane powders. Journal of the European Ceramic Society, 1999, vol. 19, no. 16, pp. 2789–2796. DOI: 10.1016/S0955-2219(99)00070-9.
  46. Zhitnyuk S.V., Medvedev P.N., Sorokin O.Yu., Kachaev A.A. Formation of crystallographic texture in polycryctalline ceramics as a way to enhance properties (review). Trudy VIAM, 2022, no. 5 (111), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 11, 2025). DOI: 10.18577/2307- 6046-2022-0-5-74-86.
  47. Yu S.H., Riman R.E., Danforth S.C., Leung R.Y. Pyrolysis of Titanium‐Metal‐Filled Poly(siloxane) Preceramic Polymers: Effect of Atmosphere on Pyrolysis Product Chemistry. Journal of the American Ceramic Society, 1995, vol. 78, no. 7, pp. 1818–1824. DOI: 10.1111/j.1151-2916.1995.tb08894.x.
  48. Esfehanian M., Oberacker R., Fett T., Hoffmann M.J. Development of Dense Filler‐Free Polymer‐Derived SiOC Ceramics by Field‐Assisted Sintering. Journal of the American Ceramic Society, 2008, vol. 91, no. 11, pp. 3803–3805. DOI: 10.1111/j.1551-2916.2008.02730.x.
  49. Butuzov A.V., Semina A.V. Preceramic polymers for the production of ceramic products by vat photopolymerization. Part 1. Methods of production and properties. Trudy VIAM, 2025, no. 3 (145), paper no. 07. Available at: http://www.viam-works.ru (accessed: May 11, 2025). DOI: 10.18577/2307-6046-2025-0-3-70-88.