Abstract

The article analyzes the scientific and technical literature data concerning the main methods of removing moisture-proof electrical insulation coatings from printed circuit boards and assemblies during their repair and modification. Characteristics, advantages and disadvantages of the removal of electrical insulation coatings by dissolution, peeling, mechanical, thermal and micro-jet methods are presented. The above methods mentioned for polyurethane, epoxy, acrylic, organosilicon and parylene electrical insulation coatings are considered and the most optimal methods depending on the nature of the material are determined.

Reference list
  1. Itzko E.F. Removal of paint and varnish coatings. Leningrad: Khimiya, 1991, 96 p.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. State Standard R 55491–2013. Printed circuit boards. Rules for restoration and repair. Moscow: Standartinform, 2014, 43 p.
  4. Brusnitsyna L.A., Stepanovskikh E.I. Printed circuit board manufacturing technology. Ekaterinburg: Ural University, 2015, 200 p.
  5. Hansen C. Hansen solubility parameters: a user’s handbook. 2nd ed. Boca Raton: CRC Press, 2007, 520 р.
  6. Fomina M.A., Zakharov K.E., Volkov I.A., Ivanov A.L. Research of the corrosion aggressiveness of strippers of native and foreign production used for removal of paint coatings. Trudy VIAM, 2021, no. 12 (106), paper no. 09. Available at: http://www.viam-works.ru (accessed: March 03, 2025). DOI: 10.18577/2307-6046-2021-0-12-73-85.
  7. Kireev V.V. High-molecular compounds: in 2 parts. Moscow: Yurait, 2020, part 1, 365 p.
  8. Sorokin M.F., Kochnova Z.A., Shode L.G. Chemistry and technology of film-forming substances: textbook for universities. Moscow: Khimiya, 1989, 480 p.
  9. US EPA. Scope of the Risk Evaluation for Methylene Chloride. United States Environmental Protection Agency, 2017, 72 p.
  10. Roelofs C.R., Ellenbecker M.J. Source reduction for prevention of methylene chloride hazards: Cases from four industrial sectors. Environmental Health, 2003, vol. 2, pp. 1–15. DOI: 10.1186/1476-069X-2-9.
  11. Semenova L.V., Novikova T.A., Nefedov N.I. Study of removing ability of removers for paint systems removal. Aviacionnye materialy i tehnologii, 2017, no. 1 (46), pp. 32–37. DOI: 10.18577/2071-9140-2017-0-1-32-37.
  12. Horrocks H. Conformal coating removal techniques. Circuit World, 1997, vol. 24, no. 1, pp. 13–19. DOI: 10.1108/030561201998000002.
  13. Yakovlev A.D., Yakovlev S.A. Functional paint and varnish coatings. St. Petersburg: Khimizdat, 2016, 272 p.
  14. Polukhin O. Integrated solutions for removing moisture-protective coatings. Tekhnologii v elektronnoy promyshlennosti, 2015, no. 1, pp. 62–63.
  15. Potseluev D. Abrasive to the rescue. Part 2. The first Russian installation for micro-abrasive removal of moisture-protective coatings «Borey». Vektor vysokikh tekhnologiy, 2017, no. 1, pp. 48–52.
  16. Installation «Borey» for micro-abrasive removal of moisture-protective coatings and surface treatment. Available at: https://borey-ostec.ru/ (accessed: February 27, 2025).
  17. Swam Blaster Micro-Abrasive Coating Removal Unit Models. Available at: https://www.crystalmarkinc.com/all-products/swam-blaster-micro-abrasive-blasters/ (accessed: February 27, 2025).
  18. Cummings R., Parekh N., Clatterbuck C., Frades F. Evaluation of ESD Effects During Removal of Conformal Coatings Using Micro Abrasive Blasting, 1997. Available at: https://nepp.nasa.gov/docuploads/3CBC367A-90B1-4A89-B96813B68AA399B2/microabr.pdf (accessed: February 28, 2025)
  19. AccuFlo Micro-Abrasive Removal Units. Available at: https://comcoinc.com/equipment/accuflo/# (accessed: February 27, 2025).
  20. Brock T., Groteklaus M., Mischke P. European Paints and Coatings Guide. Moscow: Paint-Media, 2013, 276 p.
  21. CHASE Corp. HumiSeal 1A33. Urethane Conformal Coating Technical Data Sheet. Available at: https://chasecorp.com/humiseal1/wp-content/uploads/sites/12/2018/10/1A33-TDS.pdf (accessed: March 03, 2025).
  22. Humiseal Stripper 1063. Safety Data Sheet. CHASE Corp., 2015. Available at: https://assets.testequity.com/te1/Documents/pdf/HumiSeal/Humiseal_S1063-QUART_Stripper_Coat_Datasheet.pdf (accessed: March 03, 2025).
  23. Potseluev D. Abrasive rushes to the rescue. Technological solution for removing moisture-protective coatings UR-231, E-30, ED-20 and parylene. Vektor vysokikh tekhnologiy, 2014, no. 7, pp. 60–64.
  24. Lu T., Reimonn G., Morose G. et al. Removing Acrylic Conformal Coating with Safer Solvents for Re-Manufacturing Electronics. Polymers, 2021, no. 13, pp. 1–14.
  25. Kochnova Z.A., Zhavoronok E.S., Chalykh A.E. Epoxy resins and hardeners: industrial products. Moscow: Paint-Media, 2006, 200 p.
  26. Kuznetsova V.A., Marchenko S.A., Emelyanov V.V., Zheleznyak V.G. Study of the influence of molecular mass of epoxy oligomers and hardeners on the operational properties of paint coatings. Aviation materials and technology, 2021, no. 1 (62), paper no. 07. Available at: http://www.journal.viam.ru (accessed: March 06, 2025). DOI: 10.18577/2713-0193-2021-0-1-71-79.
  27. Nefyodov N.I., Semyonova L.V. Development tendencies in the field on conformal coating for the moisture protection and electrical insulation of printed-circuit boards and electronic elements. Aviacionnye materialy i tehnologii, 2013, no. 1, pp. 50–52.
  28. Borisova L.N., Shestakov A.K., Tarasov A.I. Foiled materials for the manufacture of printed circuit boards. Elektronnye komponenty, 2001, no. 5, pp. 51–54.
  29. Díaz de los Ríos M., Hernández Ramos E. Determination of the Hansen solubility parameters and the Hansen sphere radius with the aid of the solver add-in of Microsoft Excel. SN Applied Science, 2020, vol. 2, pp. 1–7. DOI: 10.1007/s42452-020-2512-y.
  30. Livshits M.L., Pshiyalkovskiy B.I. Paints and varnishes: a reference manual. Moscow: Khimiya, 1982, 360 p.
  31. Kablov E.N. No future without new materials. Metallurg, 2013, no. 12, pp. 4–8.
  32. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  33. Ospennikova O.G., Kozlova A.A., Kozlov I.A. Laser technology to remove paint coatings in the process of repair and maintenance of aircraft (review). Trudy VIAM, 2021, no. 4 (98), paper no. 09. Available at: http://www.viam-works.ru (accessed: March 03, 2025). DOI: 10.18577/2307-6046-2021-0-4-110-123.
  34. Kozlova A.A., Kondrateva O.V., Kuznetsova V.A. The main problems of using domestically produced moisture-proof electrical insulating materials for automated selective application on printed assemblies (review). Aviation materials and technologies, 2022, no. 4 (69), paper no. 07. Available at: http://www.journal.viam.ru (accessed: March 06, 2025). DOI: 10.18577/2713-0193-2022-0-4-72-83.