Magnesium alloys as the basis of metal matrix composite materials: a study of structure and properties
UDC
669.721.5:621.762.224
DOI
10.18577/2307-6046-2025-0-7-45-60
Article PDF (Russian)
(1.94 MB)
How to cite
Volkova E.F., Akinina M.V., Mostyaev I.V., Alikhanyan A.A., Leonov A.A. Magnesium alloys as the basis of metal matrix composite materials: a study of structure and properties // Proceedings of VIAM. 2025. No. 7. DOI: 10.18577/2307-6046-2025-0-7-45-60. URL: https://www.viam-works.ru/en/journal/2025/7/4
Keywords
metal matrix composite materials, magnesium base of composite materials, reinforcing nanoparticles, mechanical and corrosion properties of composite materials, microstructure of metal matrix composite materials
Abstract
The article presents and describes the results of determining mechanical and corrosion properties, as well as microstructure particularities of metal matrix composite materials (MMC) based on various alloying systems of magnesium alloys: Mg–Al–Zn–Mn, Mg–Zn–Ca, Mg–Zn–Zr–REE (Y, Nd), Mg–Al–Ca. Nanoscale reinforcing particles SiC, Y2O3, Al2O3 were used as a filler. The studies of MMC were carried out in cast and homogenized states. It has been established that Mg–Zn–Ca alloy system/3 wt % SiC should be considered as the optimal composition for the metal matrix composite material.
Reference list
- Kablov E.N. New generation materials – the basis of innovations, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Sazonov M.A., Chernyshova T.A., Rokhlin L.L. Composite materials on a magnesium base reinforced with particles: manufacturing and properties (review). Konstruktsii iz kompozitsionnykh materialov, 2010, no. 2, pp. 3–22.
- Dey A., Pandey K.M. Magnesium metal matrix composites a review. Reviews on Advanced Materials Science, 2015, vol. 42, is. 1, pp. 58–67.
- Annamalai S., Periyakgoundar S., Gunasekaran S. Magnesium alloys: a review of applications. Materials and Technologies, 2019, vol. 53, is. 6, pp. 881–890.
- Ali Y., Qiu D., Jiang B. et al. Current research progress in grain refinement of cast magnesium alloys: a review article. Journal of Alloys and Compounds, 2015, vol. 619, рр. 639–651.
- Song J.F., She J., Chen D.L., Pan F.S. Latest research advances on magnesium and magnesium alloys worldwide. Journal of Magnesium and Alloys, 2020, vol. 8, pp. 1–41.
- Magnesium alloys: a handbook in 2 vols. Eds M.B. Altman, A.F. Belov, V.I. Dobatkin et al. Moscow: Metallurgiya, 1978, vol. 1: Metallurgy of magnesium and its alloys. Application areas, 231 p.
- Volkova E.F., Akinina M.V., Mostyaev I.V., Leonov A.A., Alikhanyan A.A. Characteristic features of heat treatment of composite materials based on magnesium and magnesium alloys. Review. Tekhnologiya legkikh splavov, 2024, no. 3, pp. 15–24.
- Mostyaev I.V., Akinina M.V. Features and development trends in the field of heat treatment of magnesium alloys (review). Trudy VIAM, 2018, no. 7 (67), paper no. 5. Available at: http://www.viam-works.ru (accessed: April 01, 2025). DOI: 10.18577/2307-6046-2018-0-7-41-48.
- Huang S.-J., Ali A.N. Effects of heat treatment on the microstructure and microplastic deformation behavior of SiC particles reinforced AZ61 magnesium metal matrix composite. Materials Science and Engineering: A, 2018, vol. 711, pp. 670–682.
- Leonov A.A., Trofimov N.V., Panaetov V.G., Kudasov S.V., Shirokozhukov А.V. Magnesium alloys in the design of navigation system products. Aviation materials and technologies, 2024, no. 3 (76), paper no. 03. Available at: http://www.journal.viam.ru (accessed: April 01, 2025). DOI: 10.18577/2713-0193-2024-0-3-25-34.
- Volkova E.F., Mostyaev I.V., Akinina M.V., Alikhanyan A.A. Studies of the regularities of the heat treatment influence on the structure, phase composition and mechanical properties of medium-sized forgings made of heat-resistant alloy of the Mg‒Zn‒Zr‒REE system. Trudy VIAM, 2024, no. 1 (131), paper no. 03. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2024-0-1-13-26.
- Rzychoń T., Dybowski B., Gryc A., Dudek M. Mechanical Properties and Microstructure of WE43 Magnesium Matrix Composite Reinforced SiC Particles. Archives of Foundry Engineering, 2015, vol. 15, special issue 1/2015, pp. 99–102.
- Erman A., Groza J., Li X. et al. Nanoparticle effects in cast Mg–1 wt% SiC nano-composites. Material Science and Engineering: A, 2012, vol. 558, pp. 39–43.
- Nie K.B., Wang X.J., Deng K.K. et al. Magnesium matrix composite reinforced by nanoparticles – A review. Journal of Magnesium and Alloys, 2012, vol. 9, is. 1, pp. 57–77.
- Yuan Q.H., Fu D.M., Zeng X.S., Yong L.I. Fabrication of carbon nanotube reinforced AZ91D composite with superior mechanical properties. Transactions of Nonferrous Metals Society of China, 2017, vol. 27, pp. 1716–1724.
- Akinina M.V., Mostyaev I.V., Volkova E.F., Alikhanyan A.A. Investigation of the influence of alloying elements on the temperature threshold of ignition and fire resistance of a VMD16 wrought magnesium alloy. Aviation materials and technologies, 2022, no. 3 (68), paper no. 06. Available at: http://www.journal.viam.ru (accessed: April 05, 2025). DOI: 10.18577/2713-0193-2022-0-3-60-74.
- Guo Y.C., Nie K.B., Kang X.K. et al. Achieving high-strength magnesium matrix nanocomposite through synergistical effect of external hybrid (SiC+TiC) nanoparticles and dynamic precipitated phase. Journal of Alloys and Compounds, 2019, vol. 771, pp. 847–856.
- Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metalmatrix composite materials on the basis of Al–SiC. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 373–380.
- You B.-S., Park W.-W., Chung I.-S. Effect of calcium additions on the oxidation behavior in magnesium alloys. Scripta Materialia, 2000, vol. 42, is. 11, pp. 1089–1094.
- Tekumalla S., Seetharaman S., Bau N. et al. Investigation on Microstructural and Mechanical Properties of Mg–0,4Ce/Y2O3 Nanocomposite. Proceedings of the 10th International Conference on Magnesium Alloys and Their Applications, Mg2015. Cheju, 2015, pp. 879–885.
- Volkova E.F., Duyunova V.A., Akinina M.V., Alikhanyan A.A. Characteristic features of heat treatment of composite materials based on magnesium and magnesium alloys. Tekhnologiya legkikh splavov, 2024, no. 3, рр. 15–24.
- Gupta V., Mishra R.K., Singh B. Effect of micro filler reinforcement on mechanical and wear characteristics of metal matrix composites: A review. 1st International Conference on Advances in Mechanical Engineering and Nanotechnology (ICAMEN). New York, Melvill: AIP Publishing, 2019, р. 030011. Available at: http://www.researchgate.net/publication/335591925 (ассеssed: April 05, 2025). DOI: 10/1063/1.5123933.
- Amalan P.A., Sivaram N.M. A state-of-the-art review on magnesium-based composite materials. Advances in Materials and Processing Technologies, 2023, vol. 9, is. 3, pp. 760–778.
- Zhang L., Wang Q., Liao W. et al. Effects of cyclic extrusion and compression on the microstructure and mechanical properties of AZ91D magnesium composites reinforced by SiC nanoparticles. Materials Characterization, 2017, vol. 126, pp. 17–27.
- Wang X.J., Hu X.S., Liu W.Q. et al. Aging behavior of squeeze cast SiCw/AZ91 Mg matrix composites. Materials Science and Engineering: A, 2017, vol. 682, pp. 491–500.
- Sun X.F., Wang C.J., Deng K.K. et al. Aging behavior of AZ91 matrix influenced by 5 μm SiCp: Investigation on the microstructure and mechanical properties. Journal of Alloys and Compounds, 2017, vol. 727, pp. 1263–1272.
- Zheng M.Y., Wu K., Kamado S. et al. Aging behavior of squeeze cast SiCw/AZ91 magnesium matrix composite. Materials Science and Engineering: A, 2003, vol. 348, pp. 67–75.
- Amalan P.A., Sivaram N.M., Subramanya R. Influence of Silicon Carbide and Graphite Reinfocements and T6 Aging Heat Treatment on the Fatigue Characteristics of AZ91D Magnesium Alloy. Journal of Materials Engineering and Performance, 2024, vol. 33 (2), pp. 2751–2764. DOI: 10.1007/s11665-023-08154-3.
- Khandelwal A., Mani K., Srivastava N. et al. Mechanical behavior of AZ31/Al2O3 magnesium alloy nanocomposites prepared using ultrasound assisted stir casting. Composites Part B: Engineering, 2017, vol. 123, pp. 64–73.
- Habibnejad-Korayem M., Mahmudi R., Poole W.J. Enhanced properties of Mg-based nanocomposites reinforced with Al2O3 nanoparticles. Materials Science and Engineering: A, 2009, vol. 519, is. 1-2, pp. 198–203.
- Mallmann C., Hannard F., Ferrié E. et al. Unveling the impact of the effective particles distribution on strengthening mechanisms: A multiscale characterization of Mg+Y2O3 nanocomposites. Materials Science and Engineering: A, 2019, vol. 764, is. 1-2, p. 138170.
- Zhang S., Li M., Wang H. et al. Microstructure and tensile properties of ECAPed Mg–9Al–1Si–1SiC composites: The influence of initial microstructures. Materials, 2018, vol. 11, is. 136. DOI: 10.3390/ma11010136.
- Duyunova V.A., Serebrennikova N.Yu., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Methods of forming metal-polymer composite materials (review). Aviation materials and technologies, 2022, no. 1 (66), paper no. 06. Available at: http://www.journal.viam.ru (ассеssed: April 05, 2025). DOI: 10.18577/2713-0193-2022-0-1-65-77.
- Selvam J.D.-R., Dinaharan I., Rai R.S. Matrix and rainforcement materials for metal matrix and reinforcement material for composites. Encyclopedia of Materials: Composites, 2021, vol. 2, pp. 615–639. DOI: 10/1016/B978-0-12-803581-8.11890-9.
- Kumar M., Gupta R.K. Study and properties of metal matrix composites. Journal of Materials Processing Technology, 1997, vol. 63, is. 1-3, pp. 913–917.
- Timonova M.A. Corrosion and protection of magnesium alloys. Moscow: Mashinostroenie, 1964, 285 p.
- Timonova M.A. Protection from corrosion of magnesium alloys. Moscow: Metallurgiya, 1977, 158 p.
- Emli E.F. Fundamentals of technology of production and processing of magnesium alloys. Ed. M.E. Drits. Moscow: Metallurgiya, 1972, 488 p.