The possibilities of using ion-plasma technology in the creation of a wear-resistant coating to protect parts with low tempering temperature

Gorlov D.S., Aleksandrov D.A., Cheredinov P.D.
Gorlov D.S., Aleksandrov D.A., Cheredinov P.D. The possibilities of using ion-plasma technology in the creation of a wear-resistant coating to protect parts with low tempering temperature // Proceedings of VIAM. 2025. No. 7. DOI: 10.18577/2307-6046-2025-0-7-36-44. URL: https://www.viam-works.ru/en/journal/2025/7/3
Keywords
tribological properties, low tempering temperature, wear resistance, assisted vacuum arc deposition
Abstract

The article presents the results of a study of the tribological properties of a wear-resistant ion-plasma coating to increase the service life of parts with a low tempering temperature. It has been found that this wear-resistant coating, with a thickness of 7 to 10 microns, consists of a damping lower and wear-resistant upper layers, has a coefficient of friction of 0.12, the total wear rate of the friction pair is 0,012·10–3mm/m, the average total linear wear of the friction pair is 0,012 mm in an aviation fuel environment paired with antimony lead bronze.

Reference list
  1. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: December 19, 2024). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  3. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovatsii, 2020, no. 6 (260), pp. 3–16.
  4. Evgenov A.G., Shurtakov S.V., Chumanov I.R., Leshchev N.E. New wear-resistant cobalt-based alloy: effect of silicon and carbon on structure and tribotechnical characteristics. Part 1. Aviation materials and technologies, 2021, no. 4 (65), paper no. 07. Available at: http://www.journal.viam.ru (accessed: December 23, 2024). DOI: 10.18577/2713-0193-2021-0-4-59-69.
  5. Batraev I.S., Rybin D.K., Ivanyuk K.V., Ulianitsky V.Yu., Shtertser A.A. Wear resistant detonation coatings based on tungsten carbide for aviation products. Aviation materials and technologies, 2022, no. 1 (66), paper no. 08. Available at: http://www.journal.viam.ru (ассеssed: December 19, 2024). DOI: 10.18577/2713-0193-2022-0-1-92-109.
  6. Khmeleva K.M., Knyazev A.V., Zavarzin S.V. Development of multifunctional lubricant for threaded connections. Aviation materials and technologies, 2024, no. 3 (76), paper no. 10. Available at: http://www.journal.viam.ru (accessed: December 23, 2024). DOI: 10.18577/2713-0193-2024-0-3-119-133.
  7. Artemenko N.I., Muboyadzhyan S.A. Engineering method of estimating the magnitude and nature of the internal stresses in the condensed monolayer reinforcing coatings. Trudy VIAM, 2016, no. 1 (37), paper no. 4. Available at: http://www.viam-works.ru (accessed: December 19, 2024). DOI: 10.18577/2307-6046-2016-0-1-25-35.
  8. Muboyadzhyan S.A. Features of deposition from a two-phase flow of multicomponent vacuum-arc discharge plasma containing microdroplets of evaporated material. Metally, 2008, no. 2, pp. 20–34.
  9. Belous V.Ya., Varlamova V.E., Muboyadzhyan S.A., Aleksandrov D.A. Ion-plasma coatings for corrosion protection of compressor blades and other gas turbine engine parts operated in all-climate conditions. Korroziya: materialy, zashchita, 2012, no. 1, pp. 20–24.
  10. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S. Ion-plasma nanolayer erosion-resistant coatings based on metal carbides and nitrides. Metally, 2010, no. 5, pp. 39–51.
  11. Khrushchov M.M., Marchenko E.A., Dubravina A.A., Semenov A.P. Structural features of diamond-like coatings with different alloying mechanisms and their tribological characteristics. Fizika, khimiya i mekhanika tribosistem, 2011, no. 10, pp. 147–152.
  12. Kononov D.M., Zhdanov A.A., Morozov V.V. Production and study of diamond-like PVD coatings. Nauchno-tekhnicheskiy vestnik Povolzhya, 2012, no. 6, pp. 275‒278.
  13. Muratore C., Jones D.R., Voevodin A.A. Smart tribological coating with wear sensing capability. Wear, 2008, vol. 265, pp. 913–920.
  14. Voevodin A.A., Zabinski J.S. Nanocomposite and nanostructured tribological materials for space applications. MLBT, Air Force Research laboratory (US). Composites Science and Technology, 2005, vol. 55, pp. 741–748.
  15. Mehran Q.M., Fazal M.A., Razak B.A., Rubaiee S. A Critical Review on Physical Vapor Deposition Coatings Applied on Deferent Engine Components. Critical Reviews in Solid State and Material Sciences, 2018, vol. 43, no. 2, pp. 158–175.