Pichugin S.S., Yakovleva S.I., Kulakov V.V., Izmailov M.A., Korolev A.P. Selection of eddy current testing parameters during the estimation of defects' depth in carbon-carbon composite materials // Proceedings of VIAM. 2025. No. 6. DOI: 10.18577/2307-6046-2025-0-6-98-109. URL: https://www.viam-works.ru/en/journal/2025/6/8
Keywords
carbon-carbon composite material, eddy current testing, depth estimation, surface eddy current probe, mathematical modeling
Abstract

The article treats the possibility of estimation of specific defects occurring in carbon-carbon composite materials by eddy current method of nondestructive testing. With the help of the developed mathematical model of electromagnetic field distribution, there has been analyzed the influence of the range of parameters on the estimation of the defects’ depth including the diameter of the absolute transformer overhead eddy current converter and the frequency of the excitation current on the estimation of the depth of such defects, as well as the influence of the defect orientation relative to the surface. The article analyzes sensitivity of defect depth estimation for different values of excitation current frequency and transducer diameter. The possibility of large defects estimation is confirmed by means of tests on specimens-simulators with kerfs of different depth made of carbon-carbon material.

Reference list
  1. Kulakov V.V., Golubkov A.K., Kirillova L.N. Identification of factors of increased wear of friction carbon-carbon materials in aircraft taxiing modes. Treniye i iznos, 2024, vol. 45, no. 1, pp. 59–67.
  2. Garshin A.P., Nilov A.S., Galinskaya O.O., Krasnov V.I. Prospects for development and ways to improve aircraft braking systems on the base ceramic matrix composite materials (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 09. Available at: http://www.journal.viam.ru (accessed: October 20, 2024). DOI: 10.18577/2713-0193-2023-0-2-104-121.
  3. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: October 20, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 20, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  6. Chertishchev V.Yu. The estimation of the probability of defects detection by the acoustic methods, depending on their size in constructions from PCM for output control data in the form of binary. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 65–79. DOI: 10.18577/2307-6046-2018-0-3-65-79.
  7. Kenigfest A.M., Kramarenko E.I., Kulakov V.V. et al. Carbon-carbon friction materials for brake systems of automobiles and other modern equipment. Trenie i smazka v mashinakh i mekhanizmakh, 2008, no. 5, pp. 32–34.
  8. Kulakov V.V., Shmelev D.S., Ivanova A.N., Golubkov A.K. Design features of carbon-carbon composites for friction purposes, manufactured by the aerodynamic method, based on discrete fibers. Mekhanika kompozitsionnykh materialov i konstruktsiy, 2021, vol. 27, no. 2, pp. 261–271.
  9. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects for the use of carbon-containing nanoparticles in binders for polymer composite materials. Rossiyskie nanotekhnologii, 2013, vol. 8, no. 3–4, pp. 24–42.
  10. Sidorina A.I. Woven metal-carbon reinforcing fillers for PCM. Aviation materials and technologies, 2023, no. 3 (72), paper no. 08. Available at: http://www.journal.viam.ru (accessed: October 20, 2024). DOI: 10.18577/2713-0193-2023-0-3-101-113.
  11. Agarwal N., Rangamani A., Bhavsar K., Virnedkar S.S. An overview of carbon-carbon composite materials and their applications. Frontiers in Materials, 2024, vol. 11, pp. 1–21.
  12. Scarponi C. Carbon-carbon composites in aerospace engineering. Advanced Composite Materials Aerospace Engineering. Eds. S. Rana, R. Fanguero. Woodhead Publishing, Elsevier, 2016, pp. 385–412. DOI: 10.1016/b978-0-08-100037-3.
  13. Charitidis J.P. Theoretical Review for Non-Destructive Techniques of Composite Materials. International Research Journal of Advanced Engineering and Science, 2024, vol. 9, is. 2, pp. 127–136.
  14. James R., Haider M., Giurgiutio V., Lilienthal D. A simulative and experimental approach toward eddy current nondestructive evaluation of manufacturing flaws and operational damage in CFRP composite. Nondestructive evaluation, diagnostics and prognostics of engineering systems, 2019, vol. 3, pp. 1–14.
  15. Gerasimov V.G., Klyuev V.V., Shaternikov V.E. Methods and devices of electromagnetic control. Ed. V.E. Shaternikov. Moscow: Spectr, 2010, 256 p.
  16. Gerasimov V.G., Pokrovsky A.D., Sukhorukov V.V. Non-destructive testing: a practical guide in 5 books. Ed. V.V. Sukhorukov. Moscow: Vysshaya shkola, 1992, book 3: Electromagnetic testing, 312 p.
  17. Shkatov P.N., Ermolaev A.A., Khvostov A.A. Improving the efficiency of eddy current testing of carbon-fiber objects by increasing sensitivity to the orientation of carbon fibers. Pribory, 2022, no. 4 (262), pp. 10–15.
  18. Bowler J.R., Theodoulidis T.P., Poulakis N. Eddy current probe signals due to a crack at a right-angled corner. IEEE Transactions on magnetics, 2012, vol. 45, pp. 4735–4746.
  19. Shitikov V.S., Kodak N.P., Golovkov A.N., Kudinov I.I. Application of the eddy current testing method in the manufacture of samples with artificial defects. Elektrometallurgiya, 2023, no. 2. pp. 23–31. DOI: 10.31044/1684-5781-2023-0-2-23-31.
  20. Shitikov V.S., Kodak N.P., Golovkov A.N., Kudinov I.I. Analysis of the features of testing parts made of titanium and heat-resistant alloys for cracks by the eddy current method. Elektrometallurgiya, 2020, no. 8, pp. 20–29. DOI: 10.31044/1684-5781-2020-0-8-20-29.