Isolation of bacterial strains of polymer materials destructors from samples of recycled cooling water from oil refineries and petrochemical plants

Ermishev V.Yu.
Ermishev V.Yu. Isolation of bacterial strains of polymer materials destructors from samples of recycled cooling water from oil refineries and petrochemical plants // Proceedings of VIAM. 2025. No. 4. DOI: 10.18577/2307-6046-2025-0-4-107-128. URL: https://www.viam-works.ru/en/journal/2025/4/9
Keywords
Pseudomonas, biodegradation, bacterial strains, synthetic polymer and composite materials, fuel, sequencing, 16S rRNA
Abstract

The article presents methods for isolating bacterial strains of potential destructors of polymer materials, using the example of recycled water samples from enterprises producing petroleum products. The cultures were exposed with polymer materials and polymer substrates. Data on the species composition of bacterial cultures were obtained as a result of DNA sequencing of a fragment encoding the V4 site of the 16S rRNA of bacteria. The obtained pure cultures of bacteria of the genus Pseudomonas were used to obtain comparative growth kinetics in a mineral medium with the addition of jet and diesel fuel.

Reference list
  1. Narancic T., Kevin E. Plastic waste as a global challenge: are biodegradable plastics the answer to the plastic waste problem. Microbiology, 2019, vol. 165, pp. 129–137. DOI: 10.1099/mic.0.000749.
  2. Sinha V., Patel M.R., Patel J.V. Pet Waste Management by Chemical Recycling: A Review. Journal of Polymers and the Environment, 2010, no. 18, pp. 8–25. DOI: 10.1007/s10924-008-0106-7.
  3. Kablov E.N., Startsev V.O. Climatic aging of aviation polymer composite materials. II. Development of methods for studying the early stages of aging. Russian metallurgy (Metally), 2020, vol. 2020, no. 10, pp. 1088–1094. DOI: 10.1134/S0036029520100110.
  4. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  5. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 29, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  6. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pр. 331–334.
  7. Startsev O.V., Krotov A., Mashinskaya G. Climatic Ageing of Organic Fiber Reinforced Plastics: Water Effect. Journal Polymeric Material, 1997, vol. 37, pp. 161–171.
  8. Frisch H.L. Diffusion in polymers. Journal of Applied Polymer Science, 1970, no. 14, p. 1657.
  9. Lucas N., Bienaime C., Belloy C. et al. Polymer biodegradation: mechanisms and estimation techniques. Chemosphere, 2008, no. 4, p. 429. DOI: 10.1016/j.chemosphere.2008.06.064.6.
  10. Eskander S., Saleh H. Biodegradation: Process Mechanism. Environmental Science and Engineering, 2017, vol. 8, no. 1, pp. 1–31.
  11. Ermishev V.Yu., Laptev A.B., Startsev V.O. Peculiarities of assessing the resistance of polymeric materials to biodegradation in laboratory conditions. Part 1. Degradation of polymeric materials in natural environments, selection of bacterial strains, nutrient media and cultivation conditions. Trudy VIAM, 2023, no. 7 (125), paper no. 12. Available at: http://www.viam-works.ru (accessed: March 29, 2024). DOI: 10.18577/2307-6046-2023-0-7-138-148.
  12. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), paper no. 12. Available at: http://www.viam-works.ru (accessed: March 29, 2024). DOI: 10.18577/2307-6046-2021-0-1-114-122.
  13. Yoshida S., Hiraga K., Takehana T. et al. A bacterium that degrades and assimilates poly(ethyleneterephthalate). Science, 2016, vol. 353, pp. 759–769.
  14. Ermishev V.Yu. Metabolic possibilities of bacteria with respect to synthetic hydro-carbons used in the production of non-metallic materials (review). Trudy VIAM, 2023, no. 2 (120), paper no. 11. Available at: http://www.viam-works.ru (accessed: March 29, 2024). DOI: 10.18577/2307-6046-2023-0-2-132-146.
  15. Baker G.C., Smith J.J., Cowan D.A. Review and re-analysis of domain-specific 16S primers. Journal of Microbiological Methods, 2003, vol. 55, pp. 541–555. DOI: 10.1016/j.mimet.2003.08.009.
  16. Polz M.F., Cavanaugh C.M. Bias in template-to-product ratios in multitemplate PCR. Applied and Environmental Microbiology, 1998, vol. 11, pp. 3724–3730. DOI: 10.1128/AEM.64.10.3724-3730.1998.
  17. Okonechnikov K., Golosova O., Fursov M. A unified bioinformatics toolkit. Bioinformatics, 2012, vol. 28, pp. 1166–1167. DOI: 10.1093/bioinformatics/bts091.
  18. Vashishtha K., Gaud C., Andrews S., Krueger C. A quality control tool to analyse sequencing library compositions. F1000Research, 2022, vol. 11, pp. 1122. DOI: 10.12688/f1000research.125325.2
  19. Nair A.V., Pradeep M.A., Vijayan K.K. Molecular approach for the rapid detection of Bacillus and Pseudomonas genera dominant antagonistic groups from diverse ecological niches using colony multiplex PCR. Journal of Industrial Microbiology and Biotechnology, 2014, vol. 41, pp. 1367–5435. DOI: 10.1007/s10295-014-1441-4.
  20. Rainey P. A pair of PCR primers for Incp-9 plasmids. Microbiology, 1999, vol. 145, p. 11. DOI: 10.1099/00221287-145-11-3003.
  21. Baldwin B., Nakatsu C., Nies L. Detection and Enumeration of Aromatic Oxygenase Genes by Multiplex and Real-Time PCR. Applied and Environmental Microbiology, 2003, vol. 69, pp. 3350–3358. DOI: 10.1128/AEM.69.6.3350-3358.2003.