Modern approaches to improving the quality of casting and local repairs of products made of magnesium alloys
Trofimov N.V., Leonov A.A., Duyunova V.A., Tokarev M.S. Modern approaches to improving the quality of casting and local repairs of products made of magnesium alloys // Proceedings of VIAM. 2025. No. 4. DOI: 10.18577/2307-6046-2025-0-4-57-69. URL: https://www.viam-works.ru/en/journal/2025/4/5
Keywords
cold gas dynamic spraying, filtration, magnesium alloys, powders, inductor current
Abstract
The article presents the results of research on the technology of eliminating castingdefects by cold gas-dynamic spraying of serial magnesium alloys ML5hp and ML10 using serial powders. The influence of powder compositions on mechanical properties and adhesion has been studied. The results of studies of samples and castings of magnesium alloy VML26 obtained under various smelting modes are considered. The mode of smelting of magnesium alloy VML26 in the induction melting unit is selected. The microstructure, chemical composition, and mechanical properties of magnesium alloy samples were studied.
Reference list
- Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: August 20, 2024). DOI: 10.18577/2307-6046-2022-0-2-32-51.
- Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, p. 331–334.
- Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
- Kablov E.N., Belov E.V., Trapeznikov A.V., Leonov A.A., Zaitsev D.V. Strengthening features and aging kinetics of high-strength cast aluminum alloy AL4MS based on Al–Si–Cu–Mg system. Aviation materials and technologies, 2021, no. 2 (63), paper no. 03. Available at: http://www.journal.viam.ru (accessed: August 20, 2024). DOI: 10.18577/2713-0193-2021-0-2-24-34.
- Amelin A.S. Criterial assessment of shrinkage porosity in magnesium alloy castings. Reports XLIII Int. Youth Scientific Conf. «Gagarin Readings-2017». Moscow: MAI, 2017, p. 435.
- Trapeznikov A.V., Vlasova K.A., Reshetnikov Yu.V. Tableted modifiers for cast aluminum alloys. Aviation materials and technologies, 2024, no. 1 (74), paper no. 02. Available at: http://www.journal.viam.ru (accessed: August 22, 2024). DOI: 10.18577/2713-0193-2024-0-3-14-24.
- Zhang Y., Rong W., Wu Y. et al. A detailed HAADF-STEM study of precipitate evolution in Mg–Gd alloy. Journal of Alloys and Compounds, 2019, vol. 777, pp. 531–543. DOI: 10.1016/j.jallcom.2018.10.193.
- Fireproof high-strength casting magnesium alloy: pat. 2753660 Rus. Federation; appl. 02.11.20; publ. 20.08.02.
- Yarovaya E.I., Leushin I.O., Spasskaya M.M., Larin M.A. Efficiency of foundry process control. Chernye metally, 2018, no. 3, pp. 29–33.
- Korobkov K.S., Polyansky I.P. Influence of heat treatment modes on the structure and mechanical properties of magnesium alloy ML5pch castings. Sovremennye materialy, tekhnika i tekhnologii, 2022, no. 4 (43), pp. 397–398.
- Trofimov N.V., Leonov A.A. Study of the influence of alloying elements (Nb and Ti) on the impurity content and mechanical properties of high-strength magnesium alloy of the Mg–Zn–Zr system. Metally. 2020, no. 3, pp. 14–18.
- Fomina M.A., Zakharov K.E., Yamshchikov E.I., Trofimov N.V. Selection and research of optimal paste formulation for local removal of corrosion products from magnesium alloys as well as the technology of it’s application. Aviation materials and technologies, 2023, no. 4 (73), paper no. 05. Available at: http://www.journal.viam.ru (accessed: August 20, 2024). DOI: 10.18577/2713-0193-2023-0-4-45-54.
- Du Z., Peng Y., Teng H. et al. Formation and growth of precipitates in a Mg–7Gd–5Y–1Nd–2Zn–0,5Zr alloy aged at 200 °C. Journal of Magnesium and Alloys, 2022, vol. 11, no. 3, pp. 2326–2339. DOI: 10.1016/j.jma.2022.10.012.
- Mukhina I.Yu. Fundamentals of the technology of smelting magnesium alloys in protective environments. Liteynoe proizvodstvo, 2021, no. 1, pp. 2–8.
- Shalomeev V.A. Modification of magnesium alloy Ml-5 during filtration through carbon-containing materials. Konstruktsionnye materialy, 2008, no. 2, pp. 198–201.
- Moiseev K.V., Smykov A.F., Berezhnoy D.V. Automated design of a feed system for large-sized case castings made of light alloys. Tekhnologiya legkikh splavov, 2011, no. 1, pp. 69–72.