Production of model compositions for investment casting in the national research center «Kurchatov Institute» – VIAM

Forostovich T.L., Narskiy A.R., Bityutskaya O.N., Mokeev N.A.
Forostovich T.L., Narskiy A.R., Bityutskaya O.N., Mokeev N.A. Production of model compositions for investment casting in the national research center «Kurchatov Institute» – VIAM // Proceedings of VIAM. 2025. No. 4. DOI: 10.18577/2307-6046-2025-0-4-3-13. URL: https://www.viam-works.ru/en/journal/2025/4/1
Keywords
model compositions, wax, paraffin, plasticizer, petroleum polymer resin, aliphatic resin, precision casting, superalloys
Abstract

The article presentsan overview of materials related to the technological process of production of modern model compositions for casting ofcritical parts of gas turbine engines from nickel superalloys made by the National Research Center «Kurchatov Institute» – VIAM. The general characteristics of model compositions are considered, including the composition and basic requirements for them, as well as issues of the activity of the manufacturing area established in the mid-2010s and producing a wide range of high-quality model compositions based on domestic raw materials.

Reference list
  1. Kablov E.N. Aviation Materials Science: Results and Prospects. Vestnik Rossiyskoy Akademii nauk, 2002, vol. 72, no. 1, pp. 3–12.
  2. Demonis I.M. At Full Speed. Nauka i zhizn, 2007, no. 6, pp. 40–44.
  3. Investment Casting. Ed. Ya.I. Shklennik, V.A. Ozerov. 3rd ed. Moscow: Mashinostroyenie, 1984, 408 p.
  4. Gini E.Ch., Zarubin A.M., Rybkin V.A. Special Casting Technologies. Moscow: Publ. House of Bauman Moscow State Tech. Univ., 2010, 368 p.
  5. Ospennikova O.G. Heat-resistant alloys of a new generation and model compositions for investment casting. Liteynoe proizvodstvo, 2016, no. 3, pp. 17–20.
  6. Ospennikova O.G., Aslanyan I.R. Directions for the development of technology for the manufacture of model compositions for blades and other gas turbine engine parts. Liteynoe proizvodstvo, 2018, no. 3, pp. 20–24.
  7. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  8. Kablov E.N. Production of turbine blades for gas turbine engines by directional crystallization. Gazoturbinnye tekhnologii, 2000, no. 3, pp. 10–13.
  9. Kablov E.N. Cast blades for gas turbine engines. Alloys, technologies, coatings. 2nd ed. Moscow: Nauka, 2006, 632 p.
  10. Kolyadov E.V., Visik E.M., Gerasimov V.V., Bityutskaya O.N. Features of the morphology of the structure of nickel superalloy depending on the values of the axial and radial temperature gradients at the crystallization front. Aviation materials and technologies, 2024, no. 2 (75), paper no. 02. Available at: http://www.journal.viam.ru (accessed: November 11, 2024). DOI: 10.18577/2713-0193-2024-0-2-15-24.
  11. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), paper no. 03. Available at: http://www.journal.viam.ru (accessed: November 02, 2024). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  12. Kablov E.N., Toloraia V.N., Demonis I.M., Orekhov N.G. Directional crystallization of heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2007, no. 2, pp. 60–70.
  13. Bratukhin A.G., Shalin R.E., Kablov E.N., Toloraia V.N., Orekhov N.G. Cast single-crystal turbine blades. Liteynoe proizvodstvo, 1993, no. 6, pp. 3–6.
  14. Aslanyan I.R., Ospennikova O.G. Modern trends in the development of technology for the manufacture of model compositions for casting heat-resistant alloys. All-Rus. scientific-technical conf. «Fundamental and applied research in the field of creating heat-resistant nickel and intermetallic casting alloys and highly efficient technologies for manufacturing gas turbine engine parts» (November 9, 2017, Moscow). Moscow: VIAM, 2017, pp. 49–58.
  15. Ospennikova O.G. Thermophysical and rheological characteristics of synthetic resins for model compositions. Liteynoe proizvodstvo, 2016, no. 10, pp. 26–28.
  16. Repyakh S.I. Technological foundations of investment casting. Dnepropetrovsk: Lira, 2006, 1056 p.
  17. Gapankova E.I., Latyshevich I.A. Model compositions for investment casting. Reports Fifth Interdisciplinary Scientific Forum with International Participation «New Materials and Advanced Technologies» (October 30 – November 1, 2019, Moscow): in 2 vols. Moscow: NPP ISIS, 2019, vol. II, pp. 100–102.
  18. Composition for the manufacture of investment models: pat. 2600468 Rus. Federation; appl. 20.03.15; publ. 10.08.16.
  19. Echin A.B., Deynega G.I., Narsky A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys. Trudy VIAM, 2023, no. 8 (126), paper no. 02. Available at: http://www.viam-works.ru (accessed: October 31, 2024). DOI: 10.18577/2307-6046-2023-0-8-13-24.
  20. Forostovich T.L., Narsky A.R., Bityutskaya O.N., Mokeev N.A. Granulation of model compositions produced by National Research Center «Kurchatov Institute» – VIAM for castings on smelted models. Trudy VIAM, 2024, no. 7 (137), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 31, 2024). DOI: 10.18577/2307-6046-2024-0-7-3-11.
  21. Ospennikova O.G. Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  22. Ospennikova O.G. Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
  23. Aslanyan I.R., Guseva M.A., Ospennikova O.G. Comparative study of physical, mechanical and rheological characteristics of model compositions. Vse materialy. Entsiklopedicheskiy spravochnik, 2019, no. 6, pp. 34–39.
  24. Guseva M.A., Aslanyan I.R. The effect of fillers on the rheology of model composition. Trudy VIAM, 2019, no. 5, paper no. 11. Available at: http://www.viam-works.ru (accessed: October 31, 2024). DOI: 10.18577/2307-6046-2019-0-5-94-102.
  25. Aslanyan I.R., Rassokhina L.I., Ospennikova O.G. Definition of quantitative factors, significantly influencing on technological characteristics of model compositions. Trudy VIAM, 2018, no. 12 (72), paper no. 01. Available at: http://www.viam-works.ru (accessed: October 31, 2024). DOI: 10.18577/2307-6046-2018-0-12-3-13.
  26. Aslanyan I.R., Eremkina M.S. Methodology for studying model compositions for casting gas turbine engine blades. Vse materialy. Entsiklopedicheskiy spravochnik, 2022, no. 8, pp. 28–32.
  27. Aslanyan I.R., Rassokhina L.I., Ospennikova O.G. Application of a full factorial experiment in developing model compositions. Vse materialy. Entsiklopedicheskiy spravochnik, 2019, no. 10, pp. 20–26.
  28. Kablov E.N., Demonis I.M., Deev V.V., Bondarenko O.A., Narsky A.R. Technology for removing model masses from ceramic molds for investment casting. Liteynoe proizvodstvo, 2005, no. 3, pp. 12–14.