Strength and moisture resistance of fiberglass plastic VPS-53/T-25 at the initial stage of natural and accelerated aging

Startsev V.O., Startsev O.V., Pavlov M.R., Nechaev A.A.
Startsev V.O., Startsev O.V., Pavlov M.R., Nechaev A.A. Strength and moisture resistance of fiberglass plastic VPS-53/T-25 at the initial stage of natural and accelerated aging // Proceedings of VIAM. 2025. No. 3. DOI: 10.18577/2307-6046-2025-0-3-89-100. URL: https://www.viam-works.ru/en/journal/2025/3/8
Keywords
fiberglass, climatic aging, full-scale exposure, accelerated testing, strength, moisture diffusion coefficient, sorption, desorption
Abstract

Comparative tests of the resistance of fiberglass VPS-53/T-25 to aging were conducted during exposure in natural conditions of moderately warm and moderate climate for 3 and 6 months and to simulating effects in two modes of laboratory accelerated tests. It was found that during 6 months of exposure the strength of fiberglass decreased by 7 %, while the moisture diffusion coefficient increased by 60 and 120 % accordingly. The prospects of using Fick and Langmuir models for comparing the effects of composite materials aging during tests in natural and laboratory conditions were shown.

Reference list
  1. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 15, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  2. Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2020-0-1-68-77.
  3. Gunyaeva A.G., Kurnosov A.O., Gulyaev I.N. High-temperature polymer composite materials developed FSUE «VIAM» for aerospace engineering: past, present and future (review). Trudy VIAM, 2021, no. 1 (95), paper no. 05. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2021-0-1-43-53.
  4. Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  5. Shershak P.V., Yakovlev N.O., Sutubalov A.I. Standards for testing polymer composite materials. Part 1. Tensile properties. Aviation materials and technologies, 2023, no. 3 (72), paper no. 12. Available at: http://www.journal.viam.ru (accessed: August 15, 2024). DOI: 10.18577/2713-0193-2023-0-3-152-166.
  6. Shershak P.V., Sutubalov A.I., Yakovlev N.O., Sherstyuk F.A. Standards test methods for polymer matrix composite materials. Part 2. Compression properties. Aviation materials and technologies, 2024, no. 2 (75), paper no. 12. Available at: http://www.journal.viam.ru (accessed: August 15, 2024). DOI: 10.18577/2713-0193-2024-0-2-149-166.
  7. Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite aviation materials: 3. Significant aging factors. Russian Metallurgy (Metally), 2012, no. 4, pp. 323–329.
  8. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: August 15, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  9. Mishurov K.S., Pavlovskiy K.A., Imametdinov E.Sh. Environmental effects on properties of CFRP (carbon fiber reinforced plastic) VKU-27l. Trudy VIAM, 2018, no. 3 (63), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2018-0-3-60-67.
  10. Startsev V.O., Nechaev A.A. The influence of natural and accelerated weathering on the nanomodified CFRP’S strength. Aviation materials and technologies, 2023, no. 3 (72), paper no. 11. Available at: http://www.journal.viam.ru (accessed: August 15, 2024). DOI: 10.18577/2713-0193-2023-0-3-134-151.
  11. Ivanov М.S., Morozova V.S., Pavlukovich N.G. The influence of operational factors on the properties of carbon fiber based on polyetheretherketone. Aviation materials and technologies, 2024, no. 2 (75), paper no. 08. Available at: http://www.journal.viam.ru (accessed: August 15, 2024). DOI: 10.18577/2713-0193-2024-0-2-99-108.
  12. Heinrick M., Crawford B., Milani A.S. Degradation of Fibreglass Composites under Natural Weathering Conditions. MOJ Polymer Science, 2017, vol. 1, no. 1, pp. 18–24.
  13. Nishizaki I., Kishima T., Sasaki I. Deterioration of mechanical properties of pultruded FRP through exposure tests. Third International Conference on Durability & Field Applications of FRP Composites for Construction. Quebec, 2007, pp. 159–166.
  14. Nishizaki I., Sasaki I., Tomiyama T. Outdoor exposure tests of pultruded CFRP plates. Proceedings of the 6th International Conference on FRP Composites in Civil Engineering (CICE 2012). Rome, 2012, paper 11-096.
  15. Cruz R., Correia L., Dushimimana A. et al. Durability of Epoxy Adhesives and Carbon Fibre Reinforced Polymer Laminates Used in Strengthening Systems: Accelerated Ageing versus Natural Ageing. Materials, 2021, vol. 14, no. 6, p. 1533.
  16. Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 520 p.
  17. Aviation materials: reference book in 13 vols. Ed. E.N. Kablov. Moscow: VIAM, 2015, vol. 13: Climatic and microbiological resistance of non-metallic materials, 270 p.
  18. Startsev O.V., Vapirov Y.M., Lebedev M.P., Kychkin A.K. Comparison of Glass-Transition Temperatures for Epoxy Polymers Obtained by Methods of Thermal Analysis. Mechanics of Composite Materials, 2020, vol. 56, no. 2, pp. 227–240.
  19. Koval’ T.V., Veligodskii I.M., Gromova A.A. Change in the Properties of BSR-3M Binder in VKU-46 Carbon-Fiber-Reinforced Polymer after Prolonged Climatic Aging. Polymer Science. Ser.: D, 2023, vol. 16, no. 3, pp. 687–693.
  20. Korkees F. Moisture absorption behavior and diffusion characteristics of continuous carbon fiber reinforced epoxy composites: a review. Polymer-Plastics Technology and Materials, 2023, vol. 62, no. 14, pp. 1789–1822.
  21. Loos A.C., Springer G.S. Moisture Absorption of Graphite-Epoxy Composites Immersed in Liquids and in Humid Air. Journal of Composite Materials, 1979, vol. 13, no. 2, pp. 131–147.
  22. Mei J., Tan P.J., Liu J. et al. Moisture absorption characteristics and mechanical degradation of composite lattice truss core sandwich panel in a hygrothermal environment. Composites Part A: Applied Science and Manufacturing, 2019, vol. 127, art. 105647.
  23. Scott P., Toumpanaki E., Lees J.M. Solution Uptake in Cylindrical Carbon-Fibre-Reinforced Polymer (CFRP) Tendons. Advances in Polymer Technology, 2022, vol. 2022, art. 1981256.
  24. Almudaihesh F., Holford K., Pullin R., Eaton M. A comparison study of water diffusion in unidirectional and 2D woven carbon/epoxy composites. Polymer Composites, 2022, vol. 43, no. 1, pp. 118–129.
  25. Bone J.E., Sims G.D., Maxwell A.S. et al. On the relationship between moisture uptake and mechanical property changes in a carbon fibre/epoxy composite. Journal of Composite Materials, 2022, vol. 56, no. 14, pp. 2189–2199.
  26. Aithal S., Hossagadde P.N., Kini M.V., Pai D. Durability study of quasi-isotropic carbon/epoxy composites under various environmental conditions. Iranian Polymer Journal, 2023, vol. 32, no. 7, pp. 873–885.
  27. Hussnain S.M., Shah S.Z.H., Megat-Yusoff P.S.M., Hussain M.Z. Degradation and mechanical performance of fibre-reinforced polymer composites under marine environments: A review of recent advancements. Polymer Degradation and Stability, 2023, vol. 215, art. 110452.
  28. Mayandi K., Rajini N., Ayrilmis N. et al. An overview of endurance and ageing performance under various environmental conditions of hybrid polymer composites. Journal of Materials Research and Technology, 2020, vol. 9, no. 6, pp. 15962–15988.
  29. Kychkin A.K., Gavrilieva A.A., Vasilieva A.A. et al. Assessment of Extremely Cold Subarctic Climate Environment Destruction of the Basalt Fiber Reinforced Epoxy (BFRE) Rebar Using Its Moisture Uptake Kinetics. Polymers, 2021, vol. 13, no. 24, аrt. 4325.
  30. Kychkin A.K., Gavrilieva A.A., Kychkin A.A. et al. The Initial Stage of Climatic Aging of Basalt-Reinforced and Glass-Reinforced Plastics in Extremely Cold Climates: Regularities. Polymers, 2024, vol. 16, no. 7, art. 866.
  31. Kychkin A.K., Gavrilyeva A.A., Vasilyeva E.D. et al. Study of glass and basalt textolites by the kinetics of moisture sorption and desorption after exposure to cold climate conditions. Vestnik mashinostroyeniya, 2024, vol. 103, no. 4, pp. 336–342.
  32. State Standard R 51369–99. Test methods for resistance to climatic external influencing factors of machines, devices and other technical products. Tests for exposure to humidity. Moscow: Publishing House of Standards, 2000, 15 p.
  33. Koval T.V., Veligodsky I.M., Gromova A.A. Study of the plasticizing effect of moisture on the properties of VSE-34 binder based PCMS after 5 years exposure in the different climate zones. Trudy VIAM, 2021, no. 9 (103), paper no. 11. Available at: http://www.viam-works.ru (accessed: August 15, 2024). DOI: 10.18577/2307-6046-2021-0-9-105-116.
  34. Startsev V.O., Molokov M.V., Postnov V.I., Starostina I.V. Assessment of the influence of climatic impact on the properties of fiberglass VPS-53K. Izvestiya Samarskogo nauchnogo tsentra Rossiyskoy Akademii nauk, 2017, vol. 19, no. 4 (2), pp. 220–228.
  35. State Standard 9.707–81. Unified system of protection against corrosion and aging. Polymer materials. Methods of accelerated tests for climatic aging. Moscow: Publ. house of standards, 1990, 79 p.
  36. State Standard 16350–80. Zoning and statistical parameters of climatic factors for technical purposes. Moscow: Publ. house of standards, 1981, 150 p.
  37. State Standard R 51370–99. Methods of testing resistance to climatic external influencing factors of machines, devices and other technical products. Testing for exposure to solar radiation. Moscow: Publ. House of Standards, 2000, 11 p.
  38. Carslow G., Eger D. Thermal conductivity of solids. Moscow: Nauka, 1964, 488 p.
  39. Lykov A.V. Theory of thermal conductivity. Moscow: Vysshaya shkola, 1967, 600 p.
  40. Crank J. The mathematics of diffusion. 2nd ed. Oxford: Clarendon press, 1975, 414 p.
  41. Bonniau P., Bunsell A.R. A comparative study of water absorption theories applied to glass epoxy composites. Journal of Composite Materials, 1981, vol. 15, no. 5, pp. 272–293.
  42. Carter H.G., Kibler K.G. Langmuir-type model for anomalous moisture diffusion in composite resins. Journal of Composite Materials, 1978, vol. 12, no. 5, pp. 118–131.
  43. Glaskova T.I., Guedes R.M., Morais J.J., Aniskevich A.N. A comparative analysis of moisture transport models as applied to an epoxy binder. Mechanics of Composite Materials, 2007, vol. 43, no. 4, pp. 377–388.