Influence of technological modes of manufacture on properties of consolidated plates of carbon fiber reinforced thermoplastic based on polyetheretherketone

Ivanov M.S., Morozova V.S., Pavlukovich N.G.
Ivanov M.S., Morozova V.S., Pavlukovich N.G. Influence of technological modes of manufacture on properties of consolidated plates of carbon fiber reinforced thermoplastic based on polyetheretherketone // Proceedings of VIAM. 2025. No. 3. DOI: 10.18577/2307-6046-2025-0-3-60-69. URL: https://www.viam-works.ru/en/journal/2025/3/6
Keywords
polyetheretherketone, carbon fiber, pressing temperature, pressing pressure, melt flow rate, strength
Abstract

In the article has been studied dependence of properties of consolidated plates of carbon fiber reinforced thermoplastic based on polyetheretherketone and woven carbon filler on the technological parameters of manufacture: pressure and temperature of pressing, time and cooling rate under pressure, as well as the melt flow rate of polyetheretherketone at a given temperature. The influence of technological molding parameters on the level of consolidation of carbon fiber reinforced thermoplastic plates was assessed using non-destructive testing methods and by determination of their mechanical properties.

Reference list
  1. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), paper no. 08. Available at: http://www.viam-works.ru (accessed: September 13, 2024). DOI: 10.18577/2307-6046-2022-0-11-81-92.
  2. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: September 13, 2024). DOI: 10.18577/2713-0193-2023-0-1-61-81.
  3. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: 13.09.2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  4. Gunyaev G.M., Kablov E.N. Structural carbon fiber reinforced plastics at the turn of the century. Aviation materials. Selected works of «VIAM» 1932–2002. Moscow: VIAM, 2002, pp. 242–247.
  5. Kablov E.N. Trends and guidelines for innovative development of Russia: collection of scientific and information materials. 3rd ed. Moscow: VIAM, 2015, 720 p.
  6. Kablov E.N. What to make the future of? New generation materials, technologies for their creation and processing – the basis of innovations. Krylya Rodiny, 2016, no. 5, pp. 8–18.
  7. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: October 02, 2024). DOI: 10.18577/2713-0193-2022-0-1-41-50.
  8. Ivanov M.S., Sorokin A.E. Sheet thermoplastic carbon fiber based on polyetheretherketone for the manufacture of aircraft engine nacelle parts by thermoforming. Proc. V All-Rus. scientific-technical conf. «Polymer composite materials and production technologies of the new generation». Moscow: NRC «Kurchatov Institute» – VIAM, 2021, art. 03.
  9. Beev A.A., Khashirova S.Yu., Beeva D.A., Shokumova M.U. Powdered aromatic polyetheretherketones and copolyetheretherketones. Plasticheskie massy, 2022, no. 7–8, pp. 6–9. DOI: 10.35164/0554-2901-2022-7-8-6-9.
  10. Mikitaev A.K., Salamov A.Kh., Beev A.A., Beeva D.A. Filling of polyetheretherketones (PEEK) as a method for producing composites with high performance properties. Plasticheskie massy, 2017, no. 5–6, pp. 6–9. DOI: 10.35164/0554-2901-2017-5-6-6-9.
  11. Lyashenko E.Yu., Yakovleva K.A., Andreeva T.I. et al. Composite materials based on polyetheretherketone. Plasticheskie massy, 2023, no. 1–2, pp. 11–13. DOI: 10.35164/0554-2901-2023-1-2-11-13.
  12. Kharaev A.M., Bazheva R.Ch. Polyetheretherketones: synthesis, properties, application (review). Plasticheskie massy, 2018, no. 7–8, pp. 15–23. DOI: 10.35164/0554-2901-2018-7-8-15-23.
  13. May R. Polyetheretherketones. Encyclopedia of Polymer Science and Technology. Wiley, 2008, pp. 1–9. DOI: 10.1002/0471440264.pst266.
  14. Method for producing polyetheretherketone: pat. 2673242 Rus. Federation; appl. 27.06.18; publ. 23.11.18.
  15. Kolpachkov E.D., Petrova A.P., Kurnosov A.O., Sokolov I.I. Methods of molding aviation products from PCM (review). Trudy VIAM, 2019, no. 11 (83), paper no. 03. Available at: http://www.viam-works.ru (accessed: September 13, 2024). DOI: 10.18577/2307-6046-2019-0-11-22-36.
  16. Illig A., Shvatsman P. Thermoforming: A Practical Guide. St. Petersburg: Profession, 2007, 288 p.
  17. Wilkinson S.L. Optimisation of the stamp forming process for thermoplastic composites. University of Bristol, 2021, 167 р.
  18. De Almeida O., Bessard E., Bernhart G. Influence of processing parameters and semi-finished product on consolidation of carbon/PEEK laminates. 15th European Conference on Composite Materials. 2012. URL: https://www.researchgate.net/publication/287042143 (accessed: September 13, 2024).
  19. Pavlukovich N.G., Ivanov М.S., Morozova V.S., Donskih I.N. Investigation of the thermal stability of the melt polyetheretherketone PEEK-50P and carbon fiber based on it. Aviation materials and technologies, 2024, no. 2 (75), paper no. 07. Available at: http://www.journal.viam.ru (accessed: September 13, 2024). DOI: 10.18577/2713-0193-2024-0-2-90-98.
  20. Vasconcelos G.C., Mazur R.L., Ribeiro B., Botehlo E. Evaluation of Decomposition Kinetics of Poly (Ether-Ether-Ketone) by Thermogravimetric Analysis. Materials Research, 2014, vol. 17 (1), pp. 227–235.
  21. Demidov A.A., Krupnina O.A., Mikhaylova N.A., Kosarina E.I. Investigation of polymer composite material samples by x-ray computed tomography and processing of tomograms with the image of the volume fraction of porosity. Trudy VIAM, 2021, no. 5 (99), paper no. 11. Available at: http://www.viam-works.ru (accessed: September 13, 2024). DOI: 10.18577/2307-6046-2021-0-5-105-113.